BS 1501 154 Grade 360A Steel Plate

BS 1501-154 Grade 360A is an aluminium semi-killed carbon steel plate for vessels designed on room-temperature tensile or yield strength. Heat-analysis carbon is 0.20 % maximum and manganese is 0.30–1.20 %. Yield strength is 205 N/mm² minimum, and tensile strength is 360–480 N/mm², for plates up to 9.5 mm. Only suffix A applies; elevated-temperature B properties are not specified. The plate is supplied hot finished. SHH STEEL produces and exports 154 Grade 360A plate to the ordered edition, condition and dimensions.
Equivalent Grades:
EN 10028-2 P265GH is a later carbon vessel name (near name only).
Heat Treatment
Hot finished.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is BS 1501-154 Grade 360A plate?

We produce and export BS 1501-154 Grade 360A as aluminium semi-killed carbon steel plate for fired and unfired pressure equipment. Typical service includes thinner vessels designed on room-temperature tensile or yield strength that specify type 154 grade 360A.

BS 1501-1:1980 lists eight steel types, each with one or more tensile grades and, where Table 1 allows, suffix A or B and optional impact suffixes. This page specifies only 154 Grade 360A. It is not type 141, 151 or 161, grade 400 or 430 of type 154, or a BS 1501-2 alloy plate. Only suffix A applies; suffix B is not specified for type 154.

Composition and room-temperature tensile properties on this page follow BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates, the last final edition of Part 1. BS 1501-1:1980 was published on 28 November 1980 and withdrawn on 15 February 1993. It replaced BS 1501: Part 1: 1964 and that edition’s addenda. It was replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Those successor designations are not automatic aliases for the 1980 type-and-grade names. Name the edition or successor standard required on the purchase order.

The chemical and tensile figures below follow BS 1501-1:1980 as tabulated for this designation, including a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 values. BS 1501-2 (alloy plates) and BS 1501-3 (corrosion- and heat-resisting plates, sheet and strip) are different parts of the same historical series.

SHH STEEL produces and exports BS 1501-154 Grade 360A plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.

Material specification for BS 1501-154 Grade 360A

The items below follow BS 1501-1:1980. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.

Parameter Detail
Standard BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates
Official designation BS 1501-154 Grade 360A
Steel type Aluminium semi-killed carbon steel
Product form Hot-rolled steel plate (this part does not cover bars, sections, forgings, tubes or stainless sheet)
How designations are listed Type number, tensile grade and suffix A or B; optional LT or RT impact suffixes where Table 1 allows; optional L after types 223, 224 and 225 when nickel is limited to 0.30 %
Applicable thickness Up to and including 9.5 mm
Usual heat treatment Hot finished.
Chemical analysis Ladle analysis as tabulated for this type and grade in BS 1501-1:1980
Tensile properties Yield strength, tensile strength and elongation, by thickness, from that edition
Our supply We produce and export 154 Grade 360A plate to the ordered edition, delivery condition, dimensions and extra tests

Chemical composition of BS 1501-154 Grade 360A

The figures below are ladle analysis for BS 1501-154 Grade 360A from BS 1501-1:1980. Values are in weight percent and follow BS 1501-1:1980, including a reprint incorporating Amendments No. 1 to No. 3. They are not current EN 10028 values.

Element 154 Grade 360A ladle analysis, BS 1501-1:1980 (wt. %)
Carbon (C) 0.20 max
Manganese (Mn) 0.30–1.20
Phosphorus (P) 0.050 max
Sulfur (S) 0.050 max
Chromium (Cr) 0.25 max
Copper (Cu) 0.30 max
Molybdenum (Mo) 0.10 max
Nickel (Ni) 0.30 max

Figures are ladle analysis as tabulated for this type 154 grade in BS 1501-1:1980. Type 154 is semi-killed with aluminium only; silicon is not specified as a ladle limit in the opened table for this type. The combined total of residual chromium, copper, molybdenum and nickel is 0.70 % maximum. The 1980 edition allows the purchaser to specify tighter phosphorus and sulfur limits. Project acceptance of the chemical analysis should be agreed against the named edition.

Tensile and related properties for BS 1501-154 Grade 360A

154 Grade 360A has thickness-dependent yield strength, tensile strength and elongation. Values below are from BS 1501-1:1980, including a reprint incorporating Amendments No. 1 to No. 3, and are not current EN 10028 values. Strength values are in N/mm², equivalent to MPa.

Thickness Tensile strength Rm, N/mm² Yield strength Re, N/mm² min Elongation A, % min
Up to and including 9.5 mm 360–480 205 23

The tensile window is that stated for this type 154 grade in BS 1501-1:1980. Type 154 covers plates up to and including 9.5 mm and is intended primarily for ambient-temperature service and for vessels designed on minimum tensile or room-temperature yield strength only. Impact properties and suffix B elevated-temperature values are not specified for type 154. Project acceptance of the tensile figures should be agreed against the named edition.

Delivery conditions for BS 1501-154 Grade 360A

Type 154 is supplied as aluminium semi-killed carbon steel plate. The 1980 text specifies supply in the hot finished condition. The type is intended primarily for ambient-temperature service. Name the required delivery condition on the purchase order.

If the project has moved to EN 10028-2 or EN 10028-3, order the successor designation and edition expressly. A later name is not by itself a substitute instruction.

The purchase order should name the official designation including the A or B suffix, any required impact suffix, thickness, width and length, the delivery condition, any extra tests, and the inspection document required.

This page does not offer heat-treatment or fabrication services.

Welding and thermal cutting

BS 1501-1:1980 does not set a welding procedure. Type 154 is an aluminium semi-killed carbon vessel plate intended for welded pressure equipment of limited thickness. Welding and thermal cutting should be qualified for the carbon content, thickness and delivery condition.

Heat input and any required post-weld heat treatment belong in the project specification.

Form, appearance, dimensions and thickness tolerances

Thickness, width, length, flatness and mass tolerances should be stated on the purchase order against the dimensional standard named by the project. The historical replacement set includes BS EN 10029 for plate tolerances when that standard is specified.

Appearance, repair welding and any ultrasonic class are taken from the enquiry. This page does not list stock sizes or mill capacity.

Applications and specification limits

We produce and export 154 Grade 360A plate as aluminium semi-killed carbon steel plate for fired and unfired pressure equipment. Typical service includes thinner vessels designed on room-temperature tensile or yield strength that specify type 154 grade 360A. The 1980 type 154 clauses cover plates up to and including 9.5 mm thick in grades 360, 400 and 430. This page specifies grade 360 only.

BS 1501-1:1980 is a historical carbon and carbon-manganese plate standard for pressure purposes. It is not the current EN 10028-2 or EN 10028-3 order unless that successor standard is written on the enquiry, and it is not a BS 1501-2 alloy, BS 1501-3 stainless, BS 1502 bar or BS 1503 forging order.

Compare BS 1501-154 Grade 360A with other steel plates

154 Grade 360A is a BS 1501-1:1980 pressure-vessel plate. The comparison below is for selection only; these materials are not equivalents.

Material Alloy / type Delivery condition Mechanical requirements Typical service Substitution limit
BS 1501-154 Grade 360A (this plate) BS 1501-1:1980 official designation Hot finished. Yield 205 N/mm² minimum; tensile 360–480 N/mm² Typical service includes welded boilers and vessels that specify type 154 grade 360A A different standard, later EN name, or 1980 type is not an automatic substitute
EN 10028-2 P265GH Non-alloy elevated-temperature vessel plate, steel number 1.0425 As specified in EN 10028-2 Published yield 265 MPa and tensile 410–530 MPa Modern European carbon boiler and vessel plate Related carbon class only; a later EN name is not an automatic substitute
ASTM A516 Grade 60 ASTM carbon vessel plate As specified in ASTM A516/A516M Published yield 220 MPa and tensile 415–550 MPa Carbon pressure-vessel plate to the ASTM book Related product form only
GB/T 713 Q245R Later Chinese carbon vessel plate As specified in GB/T 713 Published yield 245 MPa and tensile 400–520 MPa Modern Chinese carbon boiler and vessel plate Related carbon class only

Equivalent and related grades by country

The designations below are near names, not automatic substitutes. A later EN 10028 designation does not by itself authorize substitution. Confirm chemistry, heat treatment, tensile properties, impact temperature and product form.

Country / region Standard Grade or designation Similarity and key differences Substitution caveat
Europe EN 10028-2 P265GH (1.0425) Later non-alloy elevated-temperature vessel plate. Live published yield 265 MPa and tensile 410–530 MPa, against 205 N/mm² and 360–480 N/mm² for 154 Grade 360. Near name only
United States ASTM A516/A516M Grade 60 Carbon vessel plate. Live published yield 220 MPa and tensile 415–550 MPa. Related product form only
China GB/T 713 Q245R Later Chinese carbon vessel plate. Live published yield 245 MPa and tensile 400–520 MPa. Related carbon class only

Why choose SHH STEEL for BS 1501-154 Grade 360A

  • We produce and export BS 1501-154 Grade 360A pressure-vessel steel plate
  • We review the enquiry for edition, designation, delivery condition, dimensions and extra tests
  • We keep the 1980 type, tensile grade and A/B suffix distinct from later EN 10028 names and from BS 1501-2 / BS 1501-3
  • We match documentation to what the purchase order requires

How to enquire for BS 1501-154 Grade 360A plate

Item What to specify
Standard and designation BS 1501-154 Grade 360A and the edition required
Or successor standard EN 10028-2 or EN 10028-3 designation and edition, if that is what the project now requires
Delivery condition Hot finished.
Dimensions Required thickness, width and length
Chemistry Ladle analysis to BS 1501-1:1980, or to another named edition
Mechanical tests Yield strength, tensile strength, elongation and, where specified, elevated-temperature or impact tests to the named edition
Other tests Ultrasonic examination or other extra tests only when written on the order
Documentation State the inspection document type required by the project

Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.

FAQ

Is BS 1501 still a current product standard?
No. BS 1501-1:1980 is the last final edition of Part 1. It was withdrawn on 15 February 1993 and replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Projects still using the 1980 designation should name that edition on the order.
Which edition do the tables on this page follow?
They follow BS 1501-1:1980, including tabulated values from a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 tables. Specify the edition or successor standard required on the purchase order.
Does BS 1501-1 cover alloy or stainless pressure-vessel plates?
No. Part 1 covers carbon and carbon-manganese plates. Alloy plates belong to BS 1501-2:1988. Corrosion- and heat-resisting plates, sheet and strip belong to BS 1501-3:1990. Bars and sections belong to BS 1502, and forgings to BS 1503. This page is 154 Grade 360A only.
Can P265GH be used instead of 154 Grade 360A?
Only after a project review. Type 154 is aluminium semi-killed, limited to 9.5 mm and supplied hot finished, with yield 205 N/mm² minimum and tensile 360–480 N/mm². Live P265GH is stated as 265 MPa yield and 410–530 MPa tensile. A later EN name is not an automatic substitute.
What should a quotation enquiry include?
BS 1501-154 Grade 360A, the edition required or the successor designation, the delivery condition, plate thickness by width by length, quantity, any extra tests, and the inspection document required.

Request a quotation

Contact SHH STEEL for a quotation for BS 1501-154 Grade 360A steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.

Specify the edition (BS 1501-1:1980 or a named successor such as EN 10028-2 or EN 10028-3), the A or B suffix, any required impact suffix, the delivery condition and any specimen heat treatment. If your project requires ultrasonic examination, a stated impact temperature or another extra test, include the acceptance criteria and the inspection document required.

If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X