BS 1501 304S31 Steel Plate | BS 1501 Steel - SHH STEEL

BS 1501 304S31 Steel Plate

BS 1501 304S31 is a chromium-nickel corrosion-resisting steel for plates, sheet and strip under BS 1501-3:1990. A public secondary extract of that edition’s cast-analysis table shows carbon 0.07 % maximum, chromium 17.00–19.00 % and nickel 8.00–11.00 %. Solution-annealed material is listed with a 0.2 % proof stress of 195 MPa minimum and tensile strength of 500–700 MPa. SHH STEEL produces and exports 304S31 plate to the ordered edition, delivery condition and dimensions.
Equivalent Grades:
Near names include EN 10028-7 X5CrNi18-10 (1.4301) and AISI 304; not automatic substitutes.
Heat Treatment
Solution annealed at 1000–1100 °C, water or fast-air cooled.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is BS 1501 304S31 plate?

We produce and export BS 1501 304S31 as chromium-nickel corrosion-resisting steel for pressure purposes. Typical service is corrosion- or heat-resisting pressure equipment that specifies this steel number.

BS 1501-3:1990 is the last final edition of the corrosion- and heat-resisting plate, sheet and strip part of BS 1501. It was published on 28 February 1990 and superseded on 15 July 2000. It superseded BS 1501-3:1973. The replacement set includes BS EN 10028-7 for stainless flat products for pressure purposes, together with later dimensional standards such as BS EN 10029, BS EN 10048, BS EN 10051, BS EN 10258 and BS EN 10259. Clause 2 of the 1990 book is titled Designation, but that clause text was not opened. The steel numbers used here (for example 304S11) come from a public materials-database list of 21 BS 1501-3 materials and from the same secondary extract. The letter S is part of those British steel numbers. No extra A or B order suffix was sourced. These numbers are not BS 970 or BS 1502 bar grades and not BS 1449-2 general-purpose stainless grades (those books use some overlapping names, and different numbers such as 309S24).

A public catalogue abstract of BS 1501-3:1990 states that the part covers plates from 3 mm to 100 mm, sheet from 0.30 mm to less than 3 mm, and narrow strip from 0.050 mm to less than 3 mm, for ambient, elevated and low-temperature duty. The same abstract notes that, except for duplex 318S13, the listed steels are considered for ambient temperature and down to −196 °C. That scope note is recorded as an abstract, not as a photographed clause.

Numeric cells below are taken from a public secondary extract headed BS 1501/3-1990, opened on 8 November 2026 (Asia/Shanghai). The extract’s subjects match the official 1990 contents list: Table 1 covers cast analysis, ambient mechanical properties and heat treatment; Tables 13 and 14 cover elevated-temperature Rp0.2 and Rp1.0. Some HTML table tags were broken; manganese and molybdenum bounds were recovered from those broken cells (for example a silicon cell written as 1.00

2.00

for manganese 2.00). The two columns after manganese were headed only as dashes and sit in the conventional phosphorus and sulfur positions; they are labelled that way with this caveat. A photographed BSI PDF of BS 1501-3:1990 was not opened. These figures are a reference basis, not an official-complete 1990 guarantee and not an SHH proprietary guarantee. They are not copied from ASTM A240/ASME SA240 304-family tables or from BS 970 bar grades.

SHH STEEL produces and exports BS 1501 304S31 plate, sheet or strip to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.

Material specification for BS 1501 304S31

The items below follow BS 1501-3:1990 as the historical corrosion- and heat-resisting plate, sheet and strip book. Numeric cells in the chemical and mechanical sections come from the public secondary extract described there, not from a photographed 1990 Table 1. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.

Parameter Detail
Standard BS 1501-3:1990, Steels for pressure purposes — Specification for corrosion- and heat-resisting steels: plates, sheet and strip
Designation used here BS 1501 304S31 (steel number sourced from the opened 21-name list and the secondary extract; Clause 2 text unread)
Steel type Chromium-nickel corrosion-resisting steel
Product form Corrosion- and heat-resisting plate, sheet and strip for pressure purposes (this part does not cover bars, sections, tubes, forgings or carbon/alloy Part 1 and Part 2 plates)
How designations are listed Sourced steel numbers take the form 304S11, 316S13 and similar. The letter S is part of the British steel number. No extra A or B suffix was sourced. These are not BS 970 bar designations
Thickness mentioned in the opened abstract Abstract: plates 3 mm to 100 mm; sheet 0.30 mm to less than 3 mm; narrow strip 0.050 mm to less than 3 mm
Usual heat treatment Solution annealed at 1000–1100 °C, water or fast-air cooled.
Chemical analysis Cast analysis cells from the opened secondary extract of the 1990 composition table, each labelled by source
Tensile properties Ambient Rp0.2, Rp1.0, Rm and elongation from the opened secondary extract
Our supply We produce and export 304S31 plate, sheet or strip to the ordered edition, delivery condition, dimensions and extra tests

Chemical composition of BS 1501 304S31

Numeric cells below are taken from a public secondary extract headed BS 1501/3-1990, opened on 8 November 2026 (Asia/Shanghai). The extract’s subjects match the official 1990 contents list: Table 1 covers cast analysis, ambient mechanical properties and heat treatment; Tables 13 and 14 cover elevated-temperature Rp0.2 and Rp1.0. Some HTML table tags were broken; manganese and molybdenum bounds were recovered from those broken cells (for example a silicon cell written as 1.00

2.00

for manganese 2.00). The two columns after manganese were headed only as dashes and sit in the conventional phosphorus and sulfur positions; they are labelled that way with this caveat. A photographed BSI PDF of BS 1501-3:1990 was not opened. These figures are a reference basis, not an official-complete 1990 guarantee and not an SHH proprietary guarantee. They are not copied from ASTM A240/ASME SA240 304-family tables or from BS 970 bar grades.

Element Value (wt. %) Source opened for this cell
Carbon (C) 0.07 max Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Silicon (Si) 1.00 (single printed figure in the Si column; treated here as a maximum) Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Manganese (Mn) 2.00 max (recovered from a broken HTML cell after silicon) Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Phosphorus (P) 0.045 max (dash-headed column after manganese) Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Sulfur (S) 0.025 max (dash-headed column after phosphorus) Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Chromium (Cr) 17.00–19.00 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Nickel (Ni) 8.00–11.00 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)

Tensile and elevated-temperature properties for BS 1501 304S31

Ambient tensile properties and the listed solution-annealing range below come from the opened secondary extract of the 1990 combined chemistry/mechanical/heat-treatment table.

Item Value Source opened for this cell
0.2 % proof stress Rp0.2, MPa min 195 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
1.0 % proof stress Rp1.0, MPa min 230 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Tensile strength Rm, MPa 500–700 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Elongation A, % min 40 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Solution-annealing temperature, °C 1000–1100 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
Intergranular-corrosion note on the extract Intergranular-corrosion test applicable, but sensitization heat treatment of the test piece is not applicable (extract note 6) Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)

Strength values are in MPa, equivalent to N/mm². On the extract, a disputed elongation test uses a proportional round specimen with gauge length 5.65 √So, or a 12.5 mm wide rectangular specimen with a 50 mm gauge length. Numeric cells below are taken from a public secondary extract headed BS 1501/3-1990, opened on 8 November 2026 (Asia/Shanghai). The extract’s subjects match the official 1990 contents list: Table 1 covers cast analysis, ambient mechanical properties and heat treatment; Tables 13 and 14 cover elevated-temperature Rp0.2 and Rp1.0. Some HTML table tags were broken; manganese and molybdenum bounds were recovered from those broken cells (for example a silicon cell written as 1.00

2.00

for manganese 2.00). The two columns after manganese were headed only as dashes and sit in the conventional phosphorus and sulfur positions; they are labelled that way with this caveat. A photographed BSI PDF of BS 1501-3:1990 was not opened. These figures are a reference basis, not an official-complete 1990 guarantee and not an SHH proprietary guarantee. They are not copied from ASTM A240/ASME SA240 304-family tables or from BS 970 bar grades.

Elevated-temperature minimum proof-stress values below come from the opened secondary extract whose subjects match official 1990 Tables 13 (Rp0.2) and 14 (Rp1.0). They are table values, not allowable design stresses and not a published maximum service temperature.

Temperature Rp0.2, MPa min Rp1.0, MPa min Source
20 °C 195 230 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
100 °C 132 178 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
150 °C 120 160 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
200 °C 109 147 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
250 °C 100 139 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
300 °C 93 132 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
350 °C 87 125 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
400 °C 84 120 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
450 °C 81 117 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
500 °C 79 115 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
550 °C 78 112 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
600 °C 76 109 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
650 °C — 104 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)
700 °C — 99 Public secondary extract headed BS 1501/3-1990, opened 8 November 2026 (Asia/Shanghai)

A dash means no figure was printed at that temperature on the opened extract. In the elevated-temperature tables, some HTML tags were again broken (for example a cell written as 144

132

). Those missing opening tags were recovered in the same way as the manganese and molybdenum cells. The extract listed temperatures through 700 °C; values printed at 650 °C and 700 °C are shown when present. Numeric cells below are taken from a public secondary extract headed BS 1501/3-1990, opened on 8 November 2026 (Asia/Shanghai). The extract’s subjects match the official 1990 contents list: Table 1 covers cast analysis, ambient mechanical properties and heat treatment; Tables 13 and 14 cover elevated-temperature Rp0.2 and Rp1.0. Some HTML table tags were broken; manganese and molybdenum bounds were recovered from those broken cells (for example a silicon cell written as 1.00

2.00

for manganese 2.00). The two columns after manganese were headed only as dashes and sit in the conventional phosphorus and sulfur positions; they are labelled that way with this caveat. A photographed BSI PDF of BS 1501-3:1990 was not opened. These figures are a reference basis, not an official-complete 1990 guarantee and not an SHH proprietary guarantee. They are not copied from ASTM A240/ASME SA240 304-family tables or from BS 970 bar grades.

Delivery conditions for BS 1501 304S31

The opened extract lists solution annealing at 1000–1100 °C. Name the required delivery condition on the purchase order.

On the opened extract, water cooling or rapid cooling in air is stated for the solution treatment, except where a note says that as-rolled supply after a sufficiently hot rolling practice does not apply and the plate is supplied in the final solution-annealed condition. For these steels the extract says annealing, solution treatment and solution annealing have the same meaning.

If the project has moved to EN 10028-7, order the successor designation and edition expressly. A later European name is not by itself a substitute instruction for 304S31.

The purchase order should name the official steel number, the edition required, whether plate, sheet or strip is wanted, thickness, width and length, the delivery condition, any intergranular-corrosion or elevated-temperature tests, and the inspection document required.

This page does not offer heat-treatment or fabrication services.

Welding and thermal cutting

BS 1501-3:1990 does not itself set a welding procedure for 304S31 on the pages opened for this article. Welding and thermal cutting should be qualified for the alloy content, thickness and the specified solution-annealed delivery condition.

304S31 has a higher listed carbon maximum than 304S11. Consumables should match the qualified procedure for this 18/9 chromium-nickel family. Do not assume an EN 10028-7 1.4301 or AISI 304 welding procedure without a project review.

Heat input and any required post-weld treatment belong in the project specification. This page does not publish a pitting-resistance equivalent or a maximum service temperature.

Form, appearance, dimensions and thickness tolerances

Thickness, width, length, flatness and mass tolerances should be stated on the purchase order against the dimensional standard named by the project. The historical replacement set includes BS EN 10029 for plate, and later sheet and strip tolerance standards, when those standards are specified.

Appearance, repair welding and any ultrasonic class are taken from the enquiry. This page does not list stock sizes or mill capacity.

Applications and specification limits

We produce and export 304S31 as corrosion- and heat-resisting steel plate, sheet and strip for pressure purposes. Typical service is corrosion-resisting pressure equipment that specifies 304S31 rather than the low-carbon 304S11 number.

BS 1501-3:1990 is a historical stainless flat-product standard. It is not the current EN 10028-7 order unless that successor standard is written on the enquiry, and it is not a BS 1501-1 carbon, BS 1501-2 alloy, BS 1502 bar or BS 1503 forging order.

Compare BS 1501 304S31 with other steel plates

BS 1501 304S31 is a historical BS 1501-3 corrosion- and heat-resisting flat product. The comparison below is for selection only; these materials are not equivalents.

Material Alloy / type Delivery condition Mechanical requirements Typical service Substitution limit
BS 1501 304S31 (this plate) Cr-Ni steel; C 0.07 % max, Cr 17–19 %, Ni 8–11 % Solution annealed at 1000–1100 °C, water or fast-air cooled. Extract: Rp0.2 195 MPa min; Rm 500–700 MPa; A 40 % min Corrosion- or heat-resisting pressure equipment that specifies this steel number A later EN 10028-7 or ASTM A240 name is not an automatic substitute
EN 10028-7 X5CrNi18-10 (1.4301) Later standard-carbon Cr-Ni pressure-vessel stainless plate Solution annealed (+AT) as specified in EN 10028-7 Live published Rp0.2 at least 210 MPa and Rm 520–720 MPa Modern European 304-family vessel plate Near name only; those EN numbers are not copied onto 304S31
AISI 304 stainless steel plate Standard 18Cr-8Ni stainless plate on the live AISI page Solution annealed Live published yield at least 205 MPa and tensile at least 515 MPa Common mill 304 plate Different book and strength basis; not an automatic substitute
EN 10028-7 X2CrNi18-9 (1.4307) Later low-carbon Cr-Ni pressure-vessel stainless plate Solution annealed (+AT) as specified in EN 10028-7 Live published Rp0.2 at least 200 MPa and Rm 500–700 MPa Modern European low-carbon 304L-family vessel plate Lower listed carbon class than 304S31

Equivalent and related grades by country

The designations below are near names, not automatic substitutes. Confirm chemistry, including residuals such as nitrogen, titanium, niobium or copper where they apply, together with heat treatment, proof stress, tensile properties, intergranular-corrosion testing and product form. EN 10028-7 and ASTM A240/ASME SA240 are later books with their own tables.

Country / region Standard Grade or designation Similarity and key differences Substitution caveat
United Kingdom BS 1501-3:1990 304S31 This plate. Extract Rm 500–700 MPa and Rp0.2 195 MPa minimum, with carbon 0.07 % maximum. This product
Europe EN 10028-7 X5CrNi18-10 (1.4301) Later vessel plate. Live published Rp0.2 210 MPa minimum and Rm 520–720 MPa, against extract 195 MPa and 500–700 MPa for 304S31. Near name only
United States AISI / ASTM A240 family (live AISI 304 page) 304 Live published yield at least 205 MPa and tensile at least 515 MPa, as minima rather than a 500–700 MPa window. Related product form only
China / other — — No separately verified GB plate counterpart was established as an automatic equivalent for 304S31 on this page. Do not assume a local 304 name is a substitute

Why choose SHH STEEL for BS 1501 304S31

  • We produce and export BS 1501 304S31 corrosion- and heat-resisting plate, sheet and strip
  • We review the enquiry for edition, steel number, delivery condition, product form, dimensions and extra tests
  • We keep the historical BS 1501-3 steel number distinct from later EN 10028-7 names, from ASTM A240/ASME SA240 types, and from BS 970 bar grades
  • We match documentation to what the purchase order requires

How to enquire for BS 1501 304S31 plate

Item What to specify
Standard and designation BS 1501 304S31 and the edition required (BS 1501-3:1990)
Or successor standard The EN 10028-7 steel name or number and edition, if that is what the project now requires
Delivery condition Solution annealed at 1000–1100 °C, water or fast-air cooled.
Product form and dimensions Plate, sheet or strip, with required thickness, width and length
Chemistry Cast analysis to the named edition
Mechanical tests Proof stress, tensile strength, elongation and, where specified, intergranular-corrosion or elevated-temperature proof tests to the named edition
Other tests Ultrasonic examination or other extra tests only when written on the order
Documentation State the inspection document type required by the project

Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.

Frequently Asked Questions

Is BS 1501-3 still a current product standard?
No. BS 1501-3:1990 is the last final edition of the corrosion- and heat-resisting plate, sheet and strip part. It was published on 28 February 1990 and superseded on 15 July 2000. EN 10028-7 superseded part of it. Projects still using a historical steel number should name the edition required on the order.
Which numbers on this page are photographed 1990 table values?
None are presented as a photographed BSI PDF. Cast analysis, ambient tensile properties, solution-annealing temperatures and elevated proof-stress figures come from a public secondary extract headed BS 1501/3-1990. Some HTML tags were broken and were recovered as described in the tables. They are a reference basis, not an official-complete guarantee.
Can EN 10028-7 X5CrNi18-10 or AISI 304 replace 304S31?
Only after a project review. Live 1.4301 is published as 210 MPa proof stress and 520–720 MPa tensile. Live AISI 304 is published as 205 MPa yield and 515 MPa tensile minimum. The extract for 304S31 shows 195 MPa and 500–700 MPa. Those later names are not automatic substitutes.
Can EN 10028-7 X2CrNi18-9 or AISI 304L replace 304S11?
Only after a project review. Live 1.4307 is published as 200 MPa proof stress and 500–700 MPa tensile. Live AISI 304L is published as 170 MPa yield and 485 MPa tensile minimum. The extract for 304S11 shows 180 MPa and 480–680 MPa. Those later names are not automatic substitutes.
What should a quotation enquiry include?
BS 1501 304S31, the edition required or the successor designation, whether plate, sheet or strip is wanted, the delivery condition, thickness by width by length, quantity, any intergranular-corrosion or elevated-temperature tests, and the inspection document required.

Request a quotation

Contact SHH STEEL for a quotation for BS 1501 304S31 plate, sheet or strip. Please include your required quantity, thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.

Specify the edition (BS 1501-3:1990, or a named EN 10028-7 successor if that is what the project now requires), the delivery condition and any specimen heat treatment. If your project requires an intergranular-corrosion test, a stated elevated-temperature proof test, ultrasonic examination or another extra test, include the acceptance criteria and the inspection document required.

If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness. A later EN 10028-7 or ASTM A240 name is not by itself a substitute instruction.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X