BS 1501 141 Grade 360A Steel Plate | BS 1501 Steel - SHH STEEL

BS 1501 141 Grade 360A Steel Plate

BS 1501-141 Grade 360A is a rimmed carbon steel plate intended only for hard glass enamelled pressure vessels. Heat-analysis carbon is 0.16 % maximum and manganese is 0.50 % maximum. Yield strength is 205 N/mm² minimum up to 16 mm, and tensile strength is 360–480 N/mm². Only suffix A applies; elevated-temperature B properties are not specified. Plates are supplied hot finished, up to 19 mm thick. SHH STEEL produces and exports 141 Grade 360A plate to the ordered edition, condition and dimensions.
Equivalent Grades:
EN 10028-2 P265GH is a later carbon vessel name (near name only).
Heat Treatment
Hot finished.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is BS 1501-141 Grade 360A plate?

We produce and export BS 1501-141 Grade 360A as rimmed carbon steel plate for hard glass enamelled pressure vessels. Typical service is limited to that enamelled duty when the enquiry specifies type 141 grade 360A.

BS 1501-1:1980 lists eight steel types, each with one or more tensile grades and, where Table 1 allows, suffix A or B and optional impact suffixes. This page specifies only 141 Grade 360A. It is not type 151, 154, 161 or 164, and it is not a BS 1501-2 alloy or BS 1501-3 stainless plate. Only suffix A applies; suffix B is not specified for type 141.

Composition and room-temperature tensile properties on this page follow BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates, the last final edition of Part 1. BS 1501-1:1980 was published on 28 November 1980 and withdrawn on 15 February 1993. It replaced BS 1501: Part 1: 1964 and that edition’s addenda. It was replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Those successor designations are not automatic aliases for the 1980 type-and-grade names. Name the edition or successor standard required on the purchase order.

The chemical and tensile figures below follow BS 1501-1:1980 as tabulated for this designation, including a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 values. BS 1501-2 (alloy plates) and BS 1501-3 (corrosion- and heat-resisting plates, sheet and strip) are different parts of the same historical series.

SHH STEEL produces and exports BS 1501-141 Grade 360A plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.

Material specification for BS 1501-141 Grade 360A

The items below follow BS 1501-1:1980. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.

Parameter Detail
Standard BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates
Official designation BS 1501-141 Grade 360A
Steel type Rimmed carbon steel (for hard glass enamelled vessels)
Product form Hot-rolled steel plate (this part does not cover bars, sections, forgings, tubes or stainless sheet)
How designations are listed Type number, tensile grade and suffix A or B; optional LT or RT impact suffixes where Table 1 allows; optional L after types 223, 224 and 225 when nickel is limited to 0.30 %
Applicable thickness Up to and including 19 mm
Usual heat treatment Hot finished.
Chemical analysis Ladle analysis as tabulated for this type and grade in BS 1501-1:1980
Tensile properties Yield strength, tensile strength and elongation, by thickness, from that edition
Our supply We produce and export 141 Grade 360A plate to the ordered edition, delivery condition, dimensions and extra tests

Chemical composition of BS 1501-141 Grade 360A

The figures below are ladle analysis for BS 1501-141 Grade 360A from BS 1501-1:1980. Values are in weight percent and follow BS 1501-1:1980, including a reprint incorporating Amendments No. 1 to No. 3. They are not current EN 10028 values.

Element 141 Grade 360A ladle analysis, BS 1501-1:1980 (wt. %)
Carbon (C) 0.16 max
Manganese (Mn) 0.50 max
Phosphorus (P) 0.050 max
Sulfur (S) 0.050 max
Chromium (Cr) 0.25 max
Copper (Cu) 0.30 max
Molybdenum (Mo) 0.10 max
Nickel (Ni) 0.30 max

Figures are ladle analysis as tabulated for type 141 in BS 1501-1:1980. Silicon is not specified for this rimmed steel. The combined total of residual chromium, copper, molybdenum and nickel is 0.70 % maximum. Nitrogen shall not exceed 0.009 %. Product analysis is not applicable to type 141. To reduce the risk of hot shortness, copper (%) plus ten times tin (%) shall not exceed 0.4 %, and the tin content shall be reported. Project acceptance of the chemical analysis should be agreed against the named edition.

Tensile and related properties for BS 1501-141 Grade 360A

141 Grade 360A has thickness-dependent yield strength, tensile strength and elongation. Values below are from BS 1501-1:1980, including a reprint incorporating Amendments No. 1 to No. 3, and are not current EN 10028 values. Strength values are in N/mm², equivalent to MPa.

Thickness Tensile strength Rm, N/mm² Yield strength Re, N/mm² min Elongation A, % min
Over 3 mm up to and including 16 mm 360–480 205 25
Over 16 mm up to and including 19 mm 360–480 195 25

The tensile window is that stated for type 141 grade 360 in BS 1501-1:1980 (360–480 N/mm²). Type 141 covers plates up to and including 19 mm. Impact properties and suffix B elevated-temperature values are not specified for type 141. Project acceptance of the tensile figures should be agreed against the named edition.

Delivery conditions for BS 1501-141 Grade 360A

Type 141 is supplied as rimmed carbon steel plate for hard glass enamelled pressure vessels. The 1980 text specifies supply in the hot finished condition. Name the required delivery condition on the purchase order.

If the project has moved to EN 10028-2 or EN 10028-3, order the successor designation and edition expressly. A later name is not by itself a substitute instruction.

The purchase order should name the official designation including the A or B suffix, any required impact suffix, thickness, width and length, the delivery condition, any extra tests, and the inspection document required.

This page does not offer heat-treatment or fabrication services.

Welding and thermal cutting

BS 1501-1:1980 does not set a welding procedure. Type 141 is a rimmed carbon plate for enamelled pressure equipment. Welding and thermal cutting should be qualified for the carbon content, thickness and delivery condition.

Heat input and any required post-weld heat treatment belong in the project specification.

Form, appearance, dimensions and thickness tolerances

Thickness, width, length, flatness and mass tolerances should be stated on the purchase order against the dimensional standard named by the project. The historical replacement set includes BS EN 10029 for plate tolerances when that standard is specified.

Appearance, repair welding and any ultrasonic class are taken from the enquiry. This page does not list stock sizes or mill capacity.

Applications and specification limits

We produce and export 141 Grade 360A plate as rimmed carbon steel plate for hard glass enamelled pressure vessels. Typical service is limited to that enamelled duty when the enquiry specifies type 141 grade 360A. The 1980 type 141 clauses cover plates up to and including 19 mm thick in grade 360 only, and only for hard glass enamelled pressure vessels.

BS 1501-1:1980 is a historical carbon and carbon-manganese plate standard for pressure purposes. It is not the current EN 10028-2 or EN 10028-3 order unless that successor standard is written on the enquiry, and it is not a BS 1501-2 alloy, BS 1501-3 stainless, BS 1502 bar or BS 1503 forging order.

Compare BS 1501-141 Grade 360A with other steel plates

141 Grade 360A is a BS 1501-1:1980 pressure-vessel plate. The comparison below is for selection only; these materials are not equivalents.

Material Alloy / type Delivery condition Mechanical requirements Typical service Substitution limit
BS 1501-141 Grade 360A (this plate) BS 1501-1:1980 official designation Hot finished. Yield 205 N/mm² minimum up to 16 mm; tensile 360–480 N/mm² Typical service is hard glass enamelled pressure vessels that specify type 141 grade 360A A different standard, later EN name, or 1980 type is not an automatic substitute
EN 10028-2 P265GH Non-alloy elevated-temperature vessel plate, steel number 1.0425 As specified in EN 10028-2 Published yield 265 MPa and tensile 410–530 MPa Modern European carbon boiler and vessel plate Related carbon class only; a later EN name is not an automatic substitute
ASTM A516 Grade 60 ASTM carbon vessel plate As specified in ASTM A516/A516M Published yield 220 MPa and tensile 415–550 MPa Carbon pressure-vessel plate to the ASTM book Related product form only
GB/T 713 Q245R Later Chinese carbon vessel plate As specified in GB/T 713 Published yield 245 MPa and tensile 400–520 MPa Modern Chinese carbon boiler and vessel plate Related carbon class only

Equivalent and related grades by country

The designations below are near names, not automatic substitutes. A later EN 10028 designation does not by itself authorize substitution. Confirm chemistry, heat treatment, tensile properties, impact temperature and product form.

Country / region Standard Grade or designation Similarity and key differences Substitution caveat
Europe EN 10028-2 P265GH (1.0425) Later non-alloy elevated-temperature vessel plate. Live published yield 265 MPa and tensile 410–530 MPa, against 205 N/mm² and 360–480 N/mm² for 141 Grade 360. Near name only; type 141 is rimmed steel for enamelled vessels and is not an automatic substitute
United States ASTM A516/A516M Grade 60 Carbon vessel plate. Live published yield 220 MPa and tensile 415–550 MPa. Related product form only
China GB/T 713 Q245R Later Chinese carbon vessel plate. Live published yield 245 MPa and tensile 400–520 MPa. Related carbon class only

Why choose SHH STEEL for BS 1501-141 Grade 360A

  • We produce and export BS 1501-141 Grade 360A pressure-vessel steel plate
  • We review the enquiry for edition, designation, delivery condition, dimensions and extra tests
  • We keep the 1980 type, tensile grade and A/B suffix distinct from later EN 10028 names and from BS 1501-2 / BS 1501-3
  • We match documentation to what the purchase order requires

How to enquire for BS 1501-141 Grade 360A plate

Item What to specify
Standard and designation BS 1501-141 Grade 360A and the edition required
Or successor standard EN 10028-2 or EN 10028-3 designation and edition, if that is what the project now requires
Delivery condition Hot finished.
Dimensions Required thickness, width and length
Chemistry Ladle analysis to BS 1501-1:1980, or to another named edition
Mechanical tests Yield strength, tensile strength, elongation and, where specified, elevated-temperature or impact tests to the named edition
Other tests Ultrasonic examination or other extra tests only when written on the order
Documentation State the inspection document type required by the project

Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.

FAQ

Is BS 1501 still a current product standard?
No. BS 1501-1:1980 is the last final edition of Part 1. It was withdrawn on 15 February 1993 and replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Projects still using the 1980 designation should name that edition on the order.
Which edition do the tables on this page follow?
They follow BS 1501-1:1980, including tabulated values from a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 tables. Specify the edition or successor standard required on the purchase order.
Does BS 1501-1 cover alloy or stainless pressure-vessel plates?
No. Part 1 covers carbon and carbon-manganese plates. Alloy plates belong to BS 1501-2:1988. Corrosion- and heat-resisting plates, sheet and strip belong to BS 1501-3:1990. Bars and sections belong to BS 1502, and forgings to BS 1503. This page is 141 Grade 360A only.
Can P265GH be used instead of 141 Grade 360A?
Only after a project review. Type 141 is a rimmed steel intended only for hard glass enamelled vessels, limited to 19 mm, and supplied hot finished. Live P265GH is a later killed elevated-temperature vessel plate stated as 265 MPa yield and 410–530 MPa tensile, against 205 N/mm² and 360–480 N/mm² for 141 Grade 360. It is not an automatic substitute.
What should a quotation enquiry include?
BS 1501-141 Grade 360A, the edition required or the successor designation, the delivery condition, plate thickness by width by length, quantity, any extra tests, and the inspection document required.

Request a quotation

Contact SHH STEEL for a quotation for BS 1501-141 Grade 360A steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.

Specify the edition (BS 1501-1:1980 or a named successor such as EN 10028-2 or EN 10028-3), the A or B suffix, any required impact suffix, the delivery condition and any specimen heat treatment. If your project requires ultrasonic examination, a stated impact temperature or another extra test, include the acceptance criteria and the inspection document required.

If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X