BS 1501 223 Grade 460A Steel Plate
What is BS 1501-223 Grade 460A plate?
We produce and export BS 1501-223 Grade 460A as fully killed niobium-treated carbon-manganese steel plate for fired and unfired pressure equipment. Typical service includes welded boilers, vessels and similar parts that specify type 223 grade 460A.
BS 1501-1:1980 lists eight steel types, each with one or more tensile grades and, where Table 1 allows, suffix A or B and optional impact suffixes. This page specifies only 223 Grade 460A. It is not type 161 or 224, grade 490 of the same type, or a BS 1501-2 alloy or BS 1501-3 stainless plate. Suffix A specifies room-temperature tensile properties only.
Composition and room-temperature tensile properties on this page follow BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates, the last final edition of Part 1. BS 1501-1:1980 was published on 28 November 1980 and withdrawn on 15 February 1993. It replaced BS 1501: Part 1: 1964 and that edition’s addenda. It was replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Those successor designations are not automatic aliases for the 1980 type-and-grade names. Name the edition or successor standard required on the purchase order.
The chemical and tensile figures below follow BS 1501-1:1980 as tabulated for this designation, including a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 values. BS 1501-2 (alloy plates) and BS 1501-3 (corrosion- and heat-resisting plates, sheet and strip) are different parts of the same historical series.
SHH STEEL produces and exports BS 1501-223 Grade 460A plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.
Material specification for BS 1501-223 Grade 460A
The items below follow BS 1501-1:1980. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates |
| Official designation | BS 1501-223 Grade 460A |
| Steel type | Fully killed niobium-treated carbon-manganese steel |
| Product form | Hot-rolled steel plate (this part does not cover bars, sections, forgings, tubes or stainless sheet) |
| How designations are listed | Type number, tensile grade and suffix A or B; optional LT or RT impact suffixes where Table 1 allows; optional L after types 223, 224 and 225 when nickel is limited to 0.30 % |
| Applicable thickness | Up to and including 150 mm in the 1980 tensile table |
| Usual heat treatment | Normalized, unless an alternative condition is agreed. |
| Chemical analysis | Ladle analysis as tabulated for this type and grade in BS 1501-1:1980 |
| Tensile properties | Yield strength, tensile strength and elongation, by thickness, from that edition |
| Our supply | We produce and export 223 Grade 460A plate to the ordered edition, delivery condition, dimensions and extra tests |
Chemical composition of BS 1501-223 Grade 460A
The figures below are ladle analysis for BS 1501-223 Grade 460A from BS 1501-1:1980. Values are in weight percent.
| Element | 223 Grade 460A ladle analysis, BS 1501-1:1980 (wt. %) |
|---|---|
| Carbon (C) | 0.20 max (0.22 max when samples are given a simulated post-weld heat treatment, as noted in the 1980 table) |
| Silicon (Si) | 0.10–0.40 |
| Manganese (Mn) | 0.80–1.60 |
| Phosphorus (P) | 0.030 max |
| Sulfur (S) | 0.030 max |
| Niobium (Nb) | 0.010–0.060 |
| Chromium (Cr) | 0.25 max |
| Copper (Cu) | 0.30 max |
| Molybdenum (Mo) | 0.10 max |
| Nickel (Ni) | 0.75 max |
Figures are ladle analysis as tabulated for this designation in BS 1501-1:1980. The combined total of chromium, copper and molybdenum is 0.50 % maximum. A suffix L may be added after the type number when a maximum nickel content of 0.30 % is specified; in that case the combined total of chromium, copper, molybdenum and nickel is 0.70 % maximum. Nitrogen shall not exceed 0.012 %. The 1980 edition allows the purchaser to specify tighter phosphorus and sulfur limits.
Tensile and related properties for BS 1501-223 Grade 460A
223 Grade 460A has thickness-dependent yield strength, tensile strength and elongation. Values below are from BS 1501-1:1980. Strength values are in N/mm², equivalent to MPa.
| Thickness | Tensile strength Rm, N/mm² | Yield strength Re, N/mm² min | Elongation A, % min |
|---|---|---|---|
| Over 3 mm up to and including 16 mm | 460–580 | 340 | 22 |
| Over 16 mm up to and including 40 mm | 460–580 | 330 | 22 |
| Over 40 mm up to and including 63 mm | 460–580 | 320 | 21 |
| Over 63 mm up to and including 100 mm | 460–580 | See note | 20 |
| Over 100 mm up to and including 150 mm | 460–580 | See note | 20 |
For thickness greater than 63 mm, the 1980 tensile table states that the minimum yield strength is the 40 mm to 63 mm value reduced by 1 % for each 5 mm increase over 63 mm. Those thicker yields are not recalculated here. Impact options listed for type 223 are RT, LT0, LT15 and LT30; energies should be taken from the edition named on the order. These tensile figures are the grade 460 row, not the grade 490 row of the same type.
Delivery conditions for BS 1501-223 Grade 460A
Type 223 is supplied as fully killed niobium-treated carbon-manganese steel plate. The 1980 text specifies normalized supply unless an alternative condition is agreed. Clause 8 allows controlled rolling in place of normalizing when the purchaser and manufacturer agree. Name the required delivery condition on the purchase order.
If the project has moved to EN 10028-2 or EN 10028-3, order the successor designation and edition expressly. A later name is not by itself a substitute instruction.
The purchase order should name the official designation including the A or B suffix, any required impact suffix, thickness, width and length, the delivery condition, any extra tests, and the inspection document required.
This page does not offer heat-treatment or fabrication services.
Welding and thermal cutting
BS 1501-1:1980 does not set a welding procedure. Type 223 is a niobium-treated carbon-manganese vessel plate intended for welded pressure equipment. Welding and thermal cutting should be qualified for the carbon content, thickness and delivery condition.
Heat input and any required post-weld heat treatment belong in the project specification.
Form, appearance, dimensions and thickness tolerances
Thickness, width, length, flatness and mass tolerances should be stated on the purchase order against the dimensional standard named by the project. The historical replacement set includes BS EN 10029 for plate tolerances when that standard is specified.
Appearance, repair welding and any ultrasonic class are taken from the enquiry. This page does not list stock sizes or mill capacity.
Applications and specification limits
We produce and export 223 Grade 460A plate as fully killed niobium-treated carbon-manganese steel plate for fired and unfired pressure equipment. Typical service includes welded boilers, vessels and similar parts that specify type 223 grade 460A. The 1980 clauses cover type 223 plates up to 150 mm in grades 460 and 490. This page specifies grade 460 only.
BS 1501-1:1980 is a historical carbon and carbon-manganese plate standard for pressure purposes. It is not the current EN 10028-2 or EN 10028-3 order unless that successor standard is written on the enquiry, and it is not a BS 1501-2 alloy, BS 1501-3 stainless, BS 1502 bar or BS 1503 forging order.
Compare BS 1501-223 Grade 460A with other steel plates
223 Grade 460A is a BS 1501-1:1980 pressure-vessel plate. The comparison below is for selection only; these materials are not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| BS 1501-223 Grade 460A (this plate) | BS 1501-1:1980 official designation | Normalized, unless an alternative condition is agreed. | Yield 340 N/mm² minimum up to 16 mm; tensile 460–580 N/mm² | Typical service includes welded boilers and vessels that specify type 223 grade 460A | A different standard, later EN name, or 1980 type is not an automatic substitute |
| BS 1501 224 Grade 460B steel plate | BS 1501-1:1980 official designation | Normalized, unless an alternative condition is agreed. | Yield 325 N/mm² minimum up to 16 mm; tensile 460–580 N/mm², with suffix B elevated-temperature properties | An aluminium-treated type 224 plate from the same 1980 part | A different 1980 type, not an automatic substitute |
| EN 10028-2 P295GH | Non-alloy elevated-temperature vessel plate, steel number 1.0481 | As specified in EN 10028-2 | Published yield 295 MPa and tensile 460–580 MPa | Modern European carbon boiler and vessel plate | Related tensile window only; yield is lower and the steel is not niobium treated |
| EN 10028-3 P355NH | Weldable fine-grain elevated-temperature vessel plate, steel number 1.0565 | As specified in EN 10028-3 | Published yield 355 MPa and tensile 490–630 MPa | Modern European fine-grain boiler and vessel plate | Related strength class only; chemistry and impact rules follow EN 10028-3 |
| ASTM A516 Grade 70 | Carbon steel pressure-vessel plate, offered here as a normalized-product comparison. | Normalized plate is described on the linked product page; specify the actual ordered condition. | Use its own ordered specification, thickness and delivery condition; no strength or toughness value is transferred to this grade. | Welded pressure vessels and storage equipment in moderate- and lower-temperature service. | Different standard and acceptance rules; BS type, deoxidation practice and A/B elevated-temperature suffix are not carried into the ASTM name. Strength, impact testing and design approval must be checked under the actual order. |
Equivalent and related grades by country
The designations below are near names, not automatic substitutes. A later EN 10028 designation does not by itself authorize substitution. Confirm chemistry, heat treatment, tensile properties, impact temperature and product form.
| Country / region | Standard | Grade or designation | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| United Kingdom (this plate) | BS 1501-1:1980 | 223 Grade 460A | Fully killed niobium-treated C-Mn plate. Niobium 0.010–0.060 %. Silicon 0.10–0.40 % and manganese 0.80–1.60 %. Yield 340 N/mm² minimum up to 16 mm; tensile 460–580 N/mm². Suffix A is room-temperature tensile only. Product form is plate up to 150 mm. Delivery is normalized unless an alternative is agreed. | This product |
| Europe | EN 10028-2 | P295GH (1.0481) | Related carbon vessel plate. Live product states yield 295 MPa and tensile 460–580 MPa, matching the 223 Grade 460 tensile window but not the yield or niobium treatment. | Near name only. |
| Europe | EN 10028-3 | P355NH (1.0565) | Related fine-grain vessel plate. Live product states yield 355 MPa and tensile 490–630 MPa. | Related strength class only. |
| United States | ASTM A516/A516M | Grade 65 | Related carbon vessel plate. Live product states yield 240 MPa and tensile 450–585 MPa. | Related product form only. |
Why choose SHH STEEL for BS 1501-223 Grade 460A
- We produce and export BS 1501-223 Grade 460A pressure-vessel steel plate
- We review the enquiry for edition, designation, delivery condition, dimensions and extra tests
- We keep the 1980 type, tensile grade and A/B suffix distinct from later EN 10028 names and from BS 1501-2 / BS 1501-3
- We match documentation to what the purchase order requires
How to enquire for BS 1501-223 Grade 460A plate
| Item | What to specify |
|---|---|
| Standard and designation | BS 1501-223 Grade 460A and the edition required |
| Or successor standard | EN 10028-2 or EN 10028-3 designation and edition, if that is what the project now requires |
| Delivery condition | Normalized, unless an alternative condition is agreed. |
| Dimensions | Required thickness, width and length |
| Chemistry | Ladle analysis to BS 1501-1:1980, or to another named edition |
| Mechanical tests | Yield strength, tensile strength, elongation and, where specified, elevated-temperature or impact tests to the named edition |
| Other tests | Ultrasonic examination or other extra tests only when written on the order |
| Documentation | State the inspection document type required by the project |
Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.
FAQ
-
Is BS 1501 still a current product standard?
- No. BS 1501-1:1980 is the last final edition of Part 1. It was withdrawn on 15 February 1993 and replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Projects still using the 1980 designation should name that edition on the order.
-
Which edition do the tables on this page follow?
- They follow BS 1501-1:1980, including tabulated values from a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 tables. Specify the edition or successor standard required on the purchase order.
-
Does BS 1501-1 cover alloy or stainless pressure-vessel plates?
- No. Part 1 covers carbon and carbon-manganese plates. Alloy plates belong to BS 1501-2:1988. Corrosion- and heat-resisting plates, sheet and strip belong to BS 1501-3:1990. Bars and sections belong to BS 1502, and forgings to BS 1503. This page is 223 Grade 460A only.
-
Can P295GH be used instead of 223 Grade 460A?
- Only after a project review. Live P295GH is stated as 295 MPa yield and 460–580 MPa tensile. 223 Grade 460 shares that 460–580 N/mm² tensile window but has a higher yield of 340 N/mm² minimum up to 16 mm and is niobium treated. A later EN name is not an automatic substitute.
-
What should a quotation enquiry include?
- BS 1501-223 Grade 460A, the edition required or the successor designation, the delivery condition, plate thickness by width by length, quantity, any extra tests, and the inspection document required.
Request a quotation
Contact SHH STEEL for a quotation for BS 1501-223 Grade 460A steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the edition (BS 1501-1:1980 or a named successor such as EN 10028-2 or EN 10028-3), the A or B suffix, any required impact suffix, the delivery condition and any specimen heat treatment. If your project requires ultrasonic examination, a stated impact temperature or another extra test, include the acceptance criteria and the inspection document required.
If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com