ASTM A529 Grade 50 Equal and Unequal Steel Angles
What is ASTM A529 Grade 50 Steel Angle?
ASTM A529 Grade 50 steel angle is a hot-rolled equal-leg or unequal-leg L-shape in high-strength carbon-manganese structural steel Grade 50 [345]. The material standard is ASTM A529/A529M. Dimensions, mass and general requirements for the rolled section are those of ASTM A6/A6M. SHH STEEL supplies these angles to the grade, L designation, edition and certificate named on the order.
This page is written for Grade 50 angles. It is not a Grade 55 data sheet, not a plate page, and not a substitute for ASTM A36 steel angle or for ASTM A572 Grade 50 steel angle. Equal angles have both legs the same length, for example L 4×4×1/2. Unequal angles have a longer and a shorter leg, for example L 8×6×1. The designation is the A6/A6M L-shape, not a bar cut from plate and not a metric angle that merely looks similar.
The specification covers carbon-manganese steel shapes, plates and bars of structural quality for riveted, bolted or welded construction of buildings and for general structural purposes. For Grade 50, shapes are limited to a flange or leg thickness of 1-1/2 in [40 mm] inclusive. These angles are filed under ASTM A529 in the steel angle profiles category of steel structural profiles.
This page covers Equal and Unequal Steel Angles in ASTM A529 Grade 50. The Equal Leg Steel Angles and Unequal Leg Steel Angles follow the ASTM A6/A6M L series; the material standard does not by itself define the dimensions.
Material, Dimensions and Tolerances for A529 Grade 50 Angles
Keep the material specification and the dimensional standard distinct:
ASTM A529/A529M is the material standard. This article uses the Grade 50 shapes chemistry and tensile figures consistent with the A529/A529M-19 tables and with the publicly posted scope of the current ASTM listing, A529/A529M-26 (shapes with flange or leg thickness to 1-1/2 in inclusive). The edition named on the order governs acceptance.
ASTM A6/A6M is the general-requirements and dimensional standard for these rolled L-shapes. The size tables below are the standard equal-leg and unequal-leg L series used as a reference, not a mill rolling list. The edition of A6/A6M named on the order governs dimensional acceptance.
A documented special combination is valid only if every requirement of each named standard is met. Matching a nominal 4 in or 100 mm leg is not a substitution method, and an A36 or A572 Grade 50 certificate is not an A529 Grade 50 certificate.
ASTM A529 Grade 50 Equal Leg Steel Angles
The tables below are the standard ASTM A6/A6M equal-leg L series: designation, both leg lengths, thickness and theoretical mass, in inch-pound and SI units. ASTM A529/A529M does not publish a size list of its own. Grade 50 covers shapes whose flange or leg thickness is 1-1/2 in [40 mm] or less. Every tabulated standard L thickness on this page is at or below 1.38 in, so the listed equal-leg rows sit inside that Grade 50 shape limit. A special bar thicker than 1-1/2 in is outside the scope of this grade.
Use the figures to identify a designation and to estimate mass, not as a rolling programme and not as a warehouse list. Mid-range L 3 to L 8 sizes are the usual enquiry core; 12 in legs and the heaviest tabulated thicknesses should be confirmed line by line.
Equal-leg angles (61 sizes, L 2×2×1/8 to L 12×12×1-3/8)
L 2 to L 4 equal (28 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 equal (16 sizes)
Swipe horizontally to view all dimensions.
L 8 to L 12 equal (17 sizes)
Swipe horizontally to view all dimensions.
ASTM A529 Grade 50 Unequal Leg Steel Angles
The tables below are the standard ASTM A6/A6M unequal-leg L series, under the same Grade 50 shape thickness limit of 1-1/2 in [40 mm]. L 8×6×1 is an 8 in by 6 in angle, 1 in thick; it is not L 8×8×1, and it is not a metric unequal angle of a similar millimetre size.
These rows are reference dimensions and theoretical masses, not a list of certified lengths on the floor. The third number is the thickness of both legs and is the thickness that must be checked against the 1-1/2 in Grade 50 cap.
Unequal-leg angles (76 sizes, L 2-1/2×1-1/2×3/16 to L 8×6×1)
L 2½ to L 4 unequal (35 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 unequal (22 sizes)
Swipe horizontally to view all dimensions.
L 7 to L 8 unequal (19 sizes)
Swipe horizontally to view all dimensions.
The 137 rows above are the standard equal and unequal L series used for this page. Other special-bar-size or non-standard angles can be reviewed when they are named on the enquiry; they are not invented here. European, Chinese or Japanese angle designations belong to their own dimensional standards, not to these L rows.
A529 Grade 50 Chemical Composition for Angles
The figures below are heat-analysis limits for Grades 50 and 55 from Table 1 of ASTM A529/A529M, as commonly tabulated. They are limits, not typical heat results. Product analysis, when required, shall conform to those same heat-analysis limits, subject to the numeric permitted variations below, taken from Table A of ASTM A6/A6M-19. Where Table A shows no under-minimum or over-maximum figure, none is applied on this page.
The following product-analysis variations apply to those heat-analysis limits.
Table A footnote A gives a different manganese variation for bars and bar-size shapes: ±0.03% up to 0.90% inclusive, and ±0.06% over 0.90% to 2.20% inclusive. Where a heat-analysis limit is a maximum only, the over-maximum variation is the figure that raises the product-analysis ceiling. The A6/A6M edition named on the order governs.
In addition to the Table 1 elements, the test report is required to include, for information, the chemical analysis for copper, columbium (niobium), chromium, nickel, molybdenum and vanadium. Those entries are reporting requirements, not invented composition maxima on this page. When the amount of copper, chromium, nickel, molybdenum or silicon is less than 0.02%, the analysis may be reported as “<0.02%.” When the amount of columbium or vanadium is less than 0.008%, the analysis may be reported as “<0.008%.”
A529 Grade 50 Angle Mechanical Properties: Yield, Tensile and Elongation
Tensile properties of these Grade 50 angles follow Table 2 of ASTM A529/A529M, including the shapes footnote. For Grade 50 shapes with flange or leg thickness to 1-1/2 in [40 mm] inclusive, the minimum tensile strength is 65 ksi [450 MPa], not the 70 ksi [485 MPa] minimum that applies to other Grade 50 product forms. All of the standard L rows tabulated here are inside that 1-1/2 in limit, so 65–100 ksi is the tensile band that belongs on this page.
Grade 55 has a 55 ksi [380 MPa] minimum yield and different elongation minima. It is not this page. Charpy testing is not a default A529 requirement; supplementary requirements such as S5 apply only when they are named on the order. Tension-test orientation follows A6/A6M.
Delivery, Inspection and Identification of A529 Grade 50 Angles
The steel shall be killed. That has to be confirmed by a statement of killed steel on the test report, or by a report of a sufficient quantity of a strong deoxidizing element, such as silicon at 0.10% or higher, or aluminum at 0.015% or higher.
A529 Grade 50 angles are commonly supplied as-rolled. The inspection document should identify ASTM A529/A529M and its edition, Grade 50, the A6/A6M L designation, the heat number, the heat analysis (including the information elements required to be reported), the killed-steel confirmation, and the tensile results. If copper steel, a Charpy supplementary, or single-heat bundling is required, that must appear on the order and on the certificate. An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request. Length is a matter for the rolling programme and the order, often in the region of 20–40 ft or 6–12 m; those lengths are enquiry ranges, not a stock list.
Weldability and Surface Condition of A529 Grade 50 Angles
A529 Grade 50 is a weldable carbon-manganese structural steel when thickness, joint design and hydrogen control are taken into account. The specification presupposes a welding procedure suitable for the grade and the intended use or service, and points to Appendix X3 of A6/A6M for weldability information. This page does not table a carbon-equivalent limit as a default requirement and does not prescribe a preheat chart. Procedure should be set from the certificate analysis and the applicable welding specification.
The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry.
A6/A6M Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these L-shapes are those of ASTM A6/A6M, not of A529/A529M itself. This article does not reproduce the inch or millimetre tolerance tables; acceptance is against the edition of A6/A6M named on the order. Out-of-square at the heel and variation of the two legs matter for connections. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
A529 Grade 50 steel angles are used where a 50 ksi carbon-manganese L-shape is specified for buildings and general structural work: bracing, frames, clips, trusses and fabrications that name this grade rather than A36 or a weathering grade. The 50 ksi yield is the same figure used for A572 Grade 50 steel angle, but the chemistry tables are not the same, and the two certificates are not interchangeable.
The grade is not specified here as a pressure-vessel or nuclear-safety material, and it is not a substitute for A588 when atmospheric corrosion resistance is what the order requires. Durability comes from the coating or fire-protection system named on the order, not from the A529 designation itself.
A529 Grade 50 Angle Compared with A36 and A572 Grade 50
ASTM A36 steel angle is a lower-strength carbon grade with a 36 ksi yield and a different chemistry column. An A36 certificate is not an A529 Grade 50 certificate.
ASTM A572 Grade 50 steel angle also has a 50 ksi minimum yield and can use the same L series, but it is a high-strength low-alloy grade with its own chemistry and no 100 ksi tensile cap of this kind. Do not treat the two Grade 50 names as one specification.
A529 Grade 55 is a higher-yield grade in the same standard, with its own tensile and elongation rows and the same 1-1/2 in shape-thickness cap. It is not covered on this page.
Near-Equivalents: Not Automatic Substitutes
Published sister pages in other systems include GB/T 706 Q355B, EN 10025-2 S355JR and JIS G 3101 SS400 (a lower-tensile JIS grade). Use those pages for their own standards.
Stock and Supply of A529 Grade 50 Steel Angles from SHH STEEL
SHH STEEL supplies ASTM A529 Grade 50 equal-leg and unequal-leg steel angles as an export trading house, coordinating mill production and project procurement. The useful work on this product is to keep Grade 50 distinct from A36 and from A572 Grade 50, to apply the 65 ksi tensile minimum that belongs to these shapes rather than the 70 ksi figure used for other Grade 50 forms, and to keep the 1-1/2 in leg-thickness cap in view before a rolling programme is committed.
Sizes, lengths and certificates are confirmed per enquiry. The tables are the standard L series, not a list of pieces on the floor. Mid-range L 3 to L 8 sizes are the usual core; 12 in equal legs and the heaviest thicknesses are confirmed per line.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every equal or unequal L size in A529 Grade 50. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
A529 Grade 50 Steel Angle FAQs
-
Do these Grade 50 angles use a 70 ksi minimum tensile strength?
- Not on this page. Table 2 of ASTM A529/A529M gives 70 ksi as the ordinary Grade 50 minimum, but a footnote lowers that minimum to 65 ksi [450 MPa] for Grade 50 shapes with flange or leg thickness to 1-1/2 in inclusive. The standard L series tabulated here is inside that limit, so the tensile band is 65–100 ksi. The 70 ksi figure should not be copied onto these angles from a plate or bar row.
-
Is A529 Grade 50 the same as A572 Grade 50?
- No. Both have a 50 ksi minimum yield and both can be furnished as A6/A6M L-shapes, but they are different specifications with different chemistry tables. An A572 Grade 50 certificate is not an A529 Grade 50 certificate.
-
Can I order a 2 in thick A529 Grade 50 angle?
- Not under Grade 50 as written. The specification limits Grade 50 shapes to a flange or leg thickness of 1-1/2 in [40 mm] inclusive. None of the standard L rows on this page exceed 1.38 in. A thicker special would be outside this grade’s scope.
-
Is an equal angle interchangeable with an unequal angle of the same long-leg length?
- No. L 8×8 and L 8×6 are different sections. The short-leg length, the mass and the connection details are those of the designation that the specification actually names.
-
How is killed steel shown on the certificate?
- The steel shall be killed, confirmed by a statement of killed steel on the test report, or by a report of silicon at 0.10% or higher, or aluminum at 0.015% or higher. That confirmation should appear with the heat analysis and the Grade 50 tensile results.
Request a Quotation for ASTM A529 Grade 50 Steel Angle
ASTM A529 Grade 50 steel angle is a carbon-manganese L-shape with 50 ksi [345 MPa] minimum yield. For the standard A6/A6M L series the tensile band is 65–100 ksi [450–690 MPa], because these shapes fall under the 1-1/2 in leg-thickness footnote. Nominate the equal or unequal L size to ASTM A6/A6M and the material to ASTM A529/A529M Grade 50 (or the edition on the order). The tables are reference dimensions, not a rolling list. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.