ASME SA202 Grade B Steel Plate | SA202 Gr.B Cr-Mn-Si Vessel Plate supplier
What is ASME SA202 Grade B Steel?
ASME SA202 Grade B, also searched as SA202 Gr.B, SA202GR B, SA202GR.B, SA202GRB, SA-202 Grade B and A202 Grade B, is the higher-strength grade in ASME SA-202 / SA-202M. The book is chromium-manganese-silicon alloy plate for welded boilers and pressure vessels. This page is not SA202 Grade A. Grade A is 515–655 MPa. This page is not ASME SA204 Grade B. SA-204 is molybdenum plate. This page is not ASME SA203 Grade B. SA-203 is nickel plate. This page is not ASME SA515 Grade 70. SA-515 is carbon high-temp plate.
Tensile is 85–110 ksi / 585–760 MPa. Yield is 47 ksi / 325 MPa min. Usual practice limits thickness to about 50 mm / 2 in. Delivery is normally as-rolled. Normalized or stress-relieved plate is supplied when ordered. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against ASME SA-202 / SA-20, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.
If a drawing says SA202 Grade A, we will not ship Grade B and call stronger automatically acceptable. If a drawing says ASTM A202 Grade B, we can discuss dual marking only when the heat meets both books. For ASME Code work the name on the certificate should be SA-202 Grade B.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | ASME SA-202 / SA-202M Grade B | Confirmed |
| Other search names | SA202 Gr.B, SA202GR B, SA202GR.B, SA202GRB, A202 Grade B | Covered |
| Steel type | Killed Cr-Mn-Si alloy vessel plate | Confirmed |
| Usual delivery | As-rolled; N or SR when ordered | Confirmed |
| Tensile | 585–760 MPa (85–110 ksi) | Confirmed |
| Yield | 325 MPa (47 ksi) min | Confirmed |
| Usual thickness | About 6–50 mm | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates. Mo sisters belong on ASME SA204. Nickel sisters belong on ASME SA203. Carbon high-temp sisters belong on ASME SA515.
Chemical Composition
Heat analysis and product analysis follow ASME SA-202 Table 1.
Heat Analysis and Product Analysis — ASME SA202 Grade B
| Element | Heat Analysis (%) | Product Analysis (%) |
|---|---|---|
| Carbon (C), max | 0.25 | 0.25 |
| Manganese (Mn) | 1.05 – 1.40 | 0.97 – 1.52 |
| Phosphorus (P), max | 0.035 | 0.035 |
| Sulfur (S), max | 0.035 | 0.035 |
| Silicon (Si) | 0.60 – 0.90 | 0.54 – 0.96 |
| Chromium (Cr) | 0.35 – 0.60 | 0.31 – 0.64 |
Grade A and Grade B share the same Mn, Si and Cr windows. The difference on chemistry is carbon: Grade A is 0.17% max, Grade B is 0.25% max. This is not a 0.5Mo heat. If the file wants molybdenum, the book is ASME SA204 Grade B. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.
Mechanical Properties
Buyers search SA202 Gr.B mechanical properties, SA202GRB yield and SA202 Grade B tensile.
Tensile and Yield — ASME SA202 Grade B
| Item | Requirement |
|---|---|
| Tensile strength | 85–110 ksi / 585–760 MPa |
| Yield strength, min | 47 ksi / 325 MPa |
| Elongation in 8 in. [200 mm], min | 15% |
| Elongation in 2 in. [50 mm], min | 18% |
| Density | 7.85 g/cm³ |
Do not quote 310 MPa yield on Grade B. That number belongs to Grade A. Do not treat 585–760 MPa as permission to stamp ASME SA515 Grade 70 or EN 10028-2 P355GH without checking both books.
Material Comparison
| Grade | Book | What buyers search | Swap? |
|---|---|---|---|
| ASME SA202 Grade A | SA-202 | SA202 Gr.A | No |
| ASME SA202 Grade B | SA-202 | SA202 Gr.B / SA202GRB | This page |
| ASME SA204 Grade B | SA-204 | SA204 Gr.B | No |
| ASME SA204 Grade C | SA-204 | SA204 Gr.C | No |
| ASME SA203 Grade B | SA-203 | SA203 Gr.B | No |
| ASME SA515 Grade 70 | SA-515 | SA515 Gr.70 | No |
| EN 10028-2 16Mo3 | EN 10028-2 | 16Mo3 | No |
| EN 10028-2 P295GH | EN 10028-2 | P295GH | No |
Equivalent Material Grades
| Designation | Standard / region | Notes |
|---|---|---|
| ASME SA-202 Grade B / SA202 Gr.B / SA202GRB | SA-202 | Name on this page |
| ASTM A202 Grade B | A202 | Same chemistry family; ASTM book later withdrawn |
| ASME SA202 Grade A | SA-202 | Lower tensile sister |
| ASME SA204 Grade B | SA-204 | Mo vessel, not Cr-Mn-Si |
| ASME SA204 Grade C | SA-204 | Higher tensile Mo |
| ASME SA515 Grade 70 | SA-515 | Carbon high-temp |
| EN 10028-2 P295GH | EN 10028-2 | Carbon comparison only |
| JIS G3103 SB480 | JIS G3103 | Japanese carbon boiler comparison |
Cr-Mn-Si Pressure-Vessel Service
Buyers pick SA202 Gr.B when an ASME file wants Cr-Mn-Si plate at 585–760 MPa. Search phrases such as SA202 Grade B, SA202GRB, SA202GR.B and SA-202 Grade B all point here.
It is not a substitute for ASME SA204 Grade B. That grade is molybdenum. It is not a substitute for ASME SA203 Grade B. That grade is nickel. It is not a substitute for EN 10028-2 16Mo3. Dual marking is possible only when both books are met.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.
Weldability
SA202 Grade B is killed Cr-Mn-Si alloy vessel plate at 585–760 MPa. Treat welding as production welding, and as ASME Section VIII / PED welding when the equipment is a vessel.
Qualify to the applicable code. Consumables must match the 585–760 MPa band and the Cr-Mn-Si chemistry. A carbon procedure written for ASME SA516 Grade 70 is a comparison only. A Mo procedure written for ASME SA204 Grade C is the wrong family. Preheat and interpass must stay inside the qualified WPS. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is as-rolled ASME SA202 Grade B. The specification allows the plate to be ordered normalized, stress-relieved, or both.
This is not QT from EN 10028-6 P355Q. This is not the 50 mm normalizing rule from JIS G3103 carbon grades.
If the vessel will see PWHT, say so. Simulated PWHT on test coupons is worth naming. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists ASME SA-202 Grade B; heat number; heat analysis; product analysis when ordered; tensile to Table 2; delivery condition. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for SA202 Gr.B Cr-Mn-Si vessel plate:
- Thickness: commonly 6 mm – 50 mm, thicker only by mill agreement
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
Current practice in the specification normally limits thickness to about 2 in. [50 mm]. Mo plate belongs on ASME SA204 Grade B. Nickel plate belongs on ASME SA203 Grade B.
Tolerances
Dimensional limits for ASME SA202 Grade B follow ASME SA-20 unless the purchase order names another table. Do not apply ASTM A36 structural tolerances to a Cr-Mn-Si vessel plate without writing them.
Typical thickness tolerance idea for SA202 Gr.B (SA-20 reference)
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 6 – 16 | −0.3 | +0.8 |
| 16 – 25 | −0.4 | +0.9 |
| 25 – 40 | −0.5 | +1.0 |
| 40 – 50 | −0.8 | +1.2 |
Width on 1500–4000 mm plate is commonly held to about ±20–25 mm unless the mill quote names a tighter extra. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness follows SA-20 unless a tighter class is written. Edge condition is mill edge or cut edge as ordered. If the vessel calculation used minimum thickness after corrosion, write the allowed minus on the RFQ. SHH STEEL will not assume a zero-minus extra on SA202 Gr.B unless the order says so.
Supplementary Requirements
ASME SA-202 Grade B already defines chemistry and tensile. Extra items still have to be written on the purchase order. SHH STEEL will not assume them from the grade name alone.
Heat treatment extras. Write normalized, stress-relieved, or both when as-rolled is not enough.
Charpy details. SA202 Grade B does not assume a default impact temperature. Write temperature, joules, location and orientation if impact is required.
Simulated PWHT. When the vessel will be stress-relieved, name hold temperature, hold time and cooling rate on the coupon.
Product analysis. Especially C, Mn, Si and Cr. Grade B carbon must stay at 0.25% max.
Through-thickness / Z-test. Name Z15, Z25 or Z35 when the plate will be welded in the thickness direction.
NDE. SA-20 ultrasonic extras, ASTM A435 or ASTM A578 as named. Write scanning extent and acceptance class.
Hardness. If the destination file caps hardness after rolling or after simulated PWHT, write the max HB and the test location.
HIC / SSC / NACE. Only when the equipment is sour service. SA202 Grade B is not automatically NACE MR0175 / ISO 15156.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS, CCS, DNV or the inspector named. Hold points for chemistry, tensile and UT should be listed on the ITP.
Identification and stamping. Heat number, grade SA-202 Grade B / SA202 Gr.B / SA202GRB, thickness and mill logo on each plate. Transfer marks after cutting if the plate will be cut before shipment.
Applications
| Industry | Typical components |
|---|---|
| ASME Cr-Mn-Si boilers | SA202 Gr.B / SA202GRB shells and drums |
| Welded pressure vessels | SA202 Grade B courses from SHH STEEL |
| Dual-name export | SA202 Gr.B / A202 Grade B when both books fit |
| Comparison vs Mo plate | SA202GRB next to ASME SA204 Grade B |
SA202 Grade B is the plate for an ASME file that wants Cr-Mn-Si alloy at 585–760 MPa. It is the wrong plate for 0.5Mo service. That work is ASME SA204 Grade B. It is the wrong plate for nickel low-temp service. That work is ASME SA203 Grade B.
Supply Capability
SHH STEEL sources ASME SA202 Grade B from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or heat-treatment route requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, thicker by mill agreement.
Processing: CNC or flame cutting, bevel, flattening, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days; standard rolling about 45–60 days; normalizing / simulated PWHT / 3.2 about 2 months.
Why Choose SHH STEEL
Experience on this grade is simple: keep Grade A and Grade B apart, and keep SA-202 away from SA-203 and SA-204. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices SA202 Gr.B from first-line mills, reports Cr-Mn-Si chemistry, records as-rolled or ordered heat treatment, and issues 3.1 as standard or 3.2 when specified.
We keep the grade on the order. SA202 Grade B is not SA202 Grade A. SA202GRB is not ASME SA204 Grade B. SA202GR.B is not ASME SA515 Grade 70. If the drawing says Grade A, we will not ship Grade B and call stronger automatically acceptable.
FAQ
-
What is SA202 Grade B steel plate?
- ASME SA202 Grade B, also searched as SA202 Gr.B, SA202GR B, SA202GR.B, SA202GRB, SA-202 Grade B and A202 Grade B, is an ASME Cr-Mn-Si alloy pressure-vessel plate. Tensile is 585–760 MPa and yield is 325 MPa min. Usual supply is as-rolled, commonly up to about 50 mm. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
What is the equivalent of SA202 Gr.B?
- Related comparisons are ASTM A202 Grade B, SA202 Grade A, SA-515 Grade 70 and P295GH. Dual marking is possible only when both books are fully met. ASTM A202 was later withdrawn; Code work should name SA-202.
-
How is SA202 Grade B different from Grade A?
- Grade A is 515–655 MPa with 0.17% C max. Grade B is 585–760 MPa with 0.25% C max. Same Mn, Si and Cr windows.
-
How is SA202GRB different from SA204 Grade B?
- SA-204 is molybdenum vessel plate. SA-202 is Cr-Mn-Si vessel plate. Do not ship one against the other.
-
How is SA-202 Grade B different from SA203 Grade B?
- SA-203 is nickel steel for low-temperature vessels. SA-202 is Cr-Mn-Si alloy plate.
Conclusion
ASME SA202 Grade B Steel Plate is Cr-Mn-Si alloy pressure-vessel plate at 585–760 MPa tensile and 325 MPa yield. Whether the inquiry says ASME SA202 Grade B, SA202 Gr.B, SA202GR B, SA202GR.B, SA202GRB, SA-202 Grade B or A202 Grade B, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with SA202 Grade B chemistry, recorded delivery condition, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies ASME SA202 Grade B / SA202 Gr.B Cr-Mn-Si Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.
Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.
ASME SA202 Grade B Steel Plate, SA202 Gr.B, SA202GRB, SA202GR.B, Cr-Mn-Si vessel plate, SA202 Gr.B supplier, SHH STEEL