ABS EQ70 shipbuilding steel plate at SHH STEEL

ABS EQ70 Shipbuilding Steel Plate Supplier

ABS EH70 Extra High Strength hull plate (ABS rule grade EQ70), yield 690 N/mm², Charpy at −40 °C, stamped AB/EQ70. SHH STEEL supplies mill-approved plate in China with UT, multi-class and 3.2 inspection.
Keywords
ABS EH70 steel plate, ABS EQ70, Extra High Strength hull steel, AB/EQ70, 690 MPa ship plate
Equivalent Grades:
ABS EQ70; society extra-high ~690 MPa class; GB 712 / A131 — verify listing
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is ABS EH70 (ABS EQ70) shipbuilding steel plate?

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

Equivalent grades: ABS EH70 / EQ70 ≈ ASTM A131 (no direct grade at this strength) ≈ DNV NV E690 ≈ LR EH69 ≈ BV E690 ≈ CCS EH690 ≈ NK KE690 ≈ KR RE70 ≈ RINA E690 ≈ GB 712 Grade EH690 (all class-approved, stamped by the issuing society).

Naming note: commercial and many yard enquiries use ABS EH70 for the ~690 N/mm² yield band. In ABS Rules Part 2, Section 2-1-8 Extra High Strength Steel, the official designation is EQ70 (category 70 = 690 N/mm² yield; letter EQ sets Charpy temperature). This page uses the title grade EH70 and states the ABS rule grade EQ70 wherever requirements are cited.

EQ70 provides minimum yield 690 N/mm², tensile 770–940 N/mm², elongation 14 % min., and Charpy at −40 °C with average energy 69 J longitudinal or 46 J transverse (2-1-8/5.11 Table 5A). It sits above the AH–FH 40 higher-strength family (2-1-3, max yield 390 N/mm²).

SHH STEEL sources Extra High Strength plate from mills with ABS approval for the grade, under Surveyor attendance. Related: ABS AH40 / ABS FH40 (higher-strength 40 band); live ABS Grade A; BV FH36 / BV FH40.

Category 70 (690 N/mm²) requires vacuum degassing for all thicknesses, not only t > 50 mm. FQ70 remains available; 91/98 FQ grades are specially considered.

ABS EH70 / EQ70: specification summary

ItemData
RuleABS Rules Part 2, 2-1-8 Extra High Strength Steel (2018/2022 updates in 2023 edition); plus applicable 2-1-1/2/3
ABS official gradeEQ70
Commercial / title gradeEH70
Yield / tensile / elongation690 / 770–940 N/mm² / 14 % min.
Impact−40 °C; 69 J L or 46 J T average
Deoxidationfully killed, fine grain (≥6 capability); N-binding elements per manufacturing specification
Delivery conditionN, NR/CR, TM (+AcC/+DQ), or QT — within Table 3 thickness limits and mill approval
Vacuum degassingmandatory for category 70 (and 91/98) and for all EHS grades t > 50 mm
MarkingAB/EQ70 (plus delivery-condition marking; “R” suffix for MOU leg/rack/chord)
UT≥15 mm: EN10160 or ASTM A578 or agreed standard (2-1-8/11.1)
Thickness tolerance2-1-1/15 (0.3 mm minus for hull plates unless otherwise agreed)
CertificateABS Surveyor-endorsed; includes Ceq/CET/Pcm as applicable

Maximum plate thickness depends on delivery condition (Table 3): e.g. N/QT up to 250 mm, TM/NR/CR up to 150 mm — actual approval limit is as per standard and mill certificate.

ABS EQ70 chemical composition (heat analysis envelope)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C (depends on route)0.14–0.20 max. by grade/condition (Table 4A)0.17–0.24 max. (each heat max.: 0.14 + 0.03; 0.20 + 0.04)EQ/FQ and TM routes tighter than N/NR/CR AQ/DQ
Mn1.0–1.70 (QT: 1.70 max.)0.89–1.84 (1.0 − 0.11; 1.70 + 0.14)
Si0.60 max. (QT 0.80 max.)0.66 max. (0.60 + 0.06)
P / S0.010–0.030 max. by route0.020–0.040 max. (each heat max. + 0.010, same row for P and S)EQ/FQ and QT tighter; sections may be +0.005
Al total min.0.02 (N/TM) / 0.018 (QT)0.02 (N/TM) / 0.018 (QT) (Al not listed in ASTM A6/A6M Table A – heat limit applies)Al/N ≥ 2:1 unless other N-binders used
Nb / V / Tilimits per Table 4ATable 4A heat max. + 0.01 for each of Nb, V, Ti (ASTM A6/A6M Table A: Nb to 0.10, V to 0.10, Ti to 0.15 incl.)Nb+V+Ti < 0.26 % for N/TM (not QT)
Ni / Cu / Cr / Moper Table 4ATable 4A heat max. + Ni 0.03 (to 1.00), Cu 0.03 (to 1.00), Cr 0.04 (to 0.90), Mo 0.01 (to 0.20) / 0.03 (0.20–0.40) / 0.04 (0.40–1.15) per ASTM A6/A6M Table ANi agreement at qualification for some routes
Ceq / CET / Pcmmaxima in Table 4B by category and conditionnot applicable (calculated from heat analysis)report on certificate; choice agreed mill/purchaser

Product (check) analysis column = heat (ladle) limit adjusted by ASTM A6/A6M-19 Table A “Permitted Variations in Product Analysis”, as required by ABS Rules Part 2, 2-1-2/5.3 (maximum + “over”, minimum − “under”; row chosen by the specified upper limit); arithmetic shown in brackets.

Source: ABS 2-1-8/4 Tables 4A and 4B. Exact ladle limits depend on delivery condition (N/NR/CR vs TM vs QT) and on AQ/DQ vs EQ/FQ. Values above are the rule envelope — the purchase order and mill approval sheet govern. Product analysis tolerances: as per standard and mill certificate (ABS references general sampling; numeric product limits are not tabulated like ASTM A6 offsets in 2-1-2). All intentionally added elements and Ceq (or CET/Pcm) are to be reported.

ABS EQ70 tensile and impact properties

PropertyRequirement (Table 5A)
Yield strength ReH (or Rp0.2)690 N/mm² min.
Tensile strength Rm770–940 N/mm²
Elongation (transverse, 5.65√A)14 % min.
Impact test temperature−40 °C
Impact energy69 J L or 46 J T average

Alternative B specimen elongations: 2-1-8 Table 5B (thickness-dependent). For t > 100 mm, tensile reductions may be considered except MOU leg/rack/chord “R” material (Note 3). Test frequency: each heat-treatment batch of same cast/condition/thickness for plates (2-1-8/5.7).

Delivery condition and toughness for EQ70

Charpy temperature is fixed by the grade letter: EQ → −40 °C. Energy does not increase with thickness in Table 5A the way 2-1-3 Table 4 does — the listed 69 / 46 J applies, with mid-thickness rules for t > 100 mm (at least 2/3 energy or +10 °C test option).

Allowed delivery conditions and max thicknesses are in Table 3 (N, NR/CR, TM, QT). Vacuum degassing is mandatory when t > 50 mm and for category 70. State N / TM / QT on the PO; do not assume AR for Extra High Strength.

Thickness tolerance, UT and surface

Tolerances per 2-1-1/15 unless agreed otherwise (hull plates: 0.3 mm minus). Internal soundness: ultrasonic examination required for thickness ≥ 15 mm (EN10160 / ASTM A578 or agreed). Surface per EN 10163 or equivalent agreed with ABS. Edge discontinuities > 25 mm need investigation (2-1-8/9.1).

ABS EH70 / EQ70 plate availability in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
61800 / 20006000 / 8000N / TM / QT100+ tChina
81800 / 20008000 / 12000N / TM / QT200+ tChina
102000 / 22008000 / 12000N / TM / QT200+ tChina
122000 / 2200 / 250012000N / TM / QT200+ tChina
142000 / 220012000N / TM / QT100+ tChina
162000 / 250012000N / TM / QT200+ tChina
202000 / 250012000N / TM / QT100+ tChina
252200 / 250012000N / TM / QT100+ tChina
30220010000 / 12000N / TM / QT100+ tChina
40220010000N / TM / QT50+ tChina
5022008000 / 10000N / TM / QT50+ tChina

Quantities are approximate and change daily; all stock plates carry AB/EQ70 marking and ABS-endorsed mill certificates. Sizes outside the table are produced in the next mill rolling cycle, typically 3–6 weeks including ABS survey (as per standard and mill certificate for exact lead time). Send your size list and we will reply with stock vs roll.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and ABS stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

Extra High Strength EQ70 is less commonly stocked than AH36; many sizes are mill-roll only. Confirm available approved thicknesses with us before fixing the cutting plan.

ABS EH70 / EQ70 equivalents

Standard / societyDesignationComment
ABS Rules 2-1-8EQ70official ABS Extra High Strength grade for this page’s EH70 title
ASTM A131/A131MASTM A131/A131Mno direct EH70/EQ70 listing; A131 stops at FH40 for higher-strength hull grades
IACS / other societiesextra-high / 690 MPa class (society designation as per their rules)confirm exact society grade mark at enquiry
GB 712GB 712verify whether the specific extra-high grade is listed; otherwise as per standard and mill certificate
ABS higher-strength 40ABS AH40 / ABS EH40 / ABS FH40390 N/mm² band below EHS
Same letter other EHSABS EH42 / ABS EH46 / ABS EH50 / ABS EH55 / ABS EH62EH commercial family

Comparisons, not substitutions. Dual classification for Extra High Strength needs mills approved by each society for that strength level.

When to order EH70 / EQ70

Use Extra High Strength when design yield exceeds the 390 N/mm² of AH–FH 40. Category steps: 43→420, 47→460, 51→500, 56→550, 63→620, 70→690 N/mm². Letter AQ/DQ/EQ/FQ (commercial AH/DH/EH/FH) sets 0/−20/−40/−60 °C.

Do not substitute ABS FH40 for EH70 without design approval — yield and rule section differ (2-1-3 vs 2-1-8).

When ABS EH70 is the right choice: typical uses are special and primary category members, crack-arrest strakes, and hull structure for cold-route or ice-strengthened vessels needing −40 °C toughness. The Charpy temperature (−40 °C) is fixed by the letter, and the strength by the number (ReH 690 N/mm²). Pick the strength from the scantling calculation and the letter from the material class and design temperature on the approved drawing. Swapping to a different letter or strength needs class approval of the drawing change, not just a new purchase order.

Applications and fabrication notes for EQ70

Typical uses: weight-critical hull and offshore members, MOU legs/racks/chords (order “R” designation when required), high-stress deck and bulkhead plating specified at 690 N/mm². See offshore platform steel plates.

Fabrication: welding and PWHT windows are narrower than for AH36; use WPS qualified for the strength level and follow mill Ceq/CET/Pcm and hydrogen-control guidance. Incorrect post-weld or flame-straightening heat can damage toughness (2-1-8/13). Parameters from weldability tests may be requested from the mill (2-1-8/15).

Project pattern for category 70: Typical projects: ultra-high-strength inserts and offshore components where 690 MPa is specified and welding/PWHT plans are already qualified. Compared with ABS AH36 / ABS FH40, this grade changes both rule section (2-1-8 vs 2-1-3) and yield.

Order checklist unique to EH70: write ABS EQ70 on the PO; Charpy −40 °C; yield 690 N/mm²; UT level for t≥15 mm; vacuum degassing (mandatory for cat 70); delivery condition N/TM/QT; optional R suffix for MOU leg/rack/chord.

Processing notes for ABS EH70: EQ70 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and ABS. Cold forming and bending radii should follow the mill’s data sheet.

Survey, UT and documentation

Surveyor witnesses mechanical tests and verifies process/NDE. Certificates include cast/batch/plate ID, grade, chemistry + Ceq/CET/Pcm, delivery condition with heat-treatment temperatures, mechanical results, surface and UT reports (2-1-8/23). Optional EN 10204 3.2 and multi-class.

Charpy acceptance for ABS EH70 by thickness (from 2-1-8; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
as per 2-1-8 Table 5A−40 °C6946

On receipt, check that the test temperature on the certificate is −40 °C and that the energy matches the band for the delivered thickness, not the thinnest band. Also check that the plate number on the stamp matches the certificate line, and that the ABS Surveyor endorsement is present. For thickness ≥ 15 mm, 2-1-8 requires ultrasonic examination; check the UT report and the agreed acceptance level. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.

Common mistakes ordering ABS EH70

  • Using title EH70 on the PO without ABS grade EQ70 / 2-1-8 reference — mill may mis-route to 2-1-3
  • Assuming A131 / GB 712 automatically cover Extra High Strength
  • Omitting delivery condition (N/TM/QT) and UT class
  • Skipping vacuum-degassing / t>50 mm requirements
  • No “R” suffix when ordering MOU leg/rack/chord plate
  • Substituting FH40 for EHS without design change
  • How does ABS EH70 differ from ABS FH40?: FH40 is higher-strength 2-1-3 steel at 390 N/mm² yield and −60 °C. EH70 is Extra High Strength 2-1-8 (official EQ70) at 690 N/mm² and −40 °C. Chemistry, UT rules and vacuum-degassing requirements differ — do not substitute without design approval.

Sourcing ABS EH70: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Mill not approved for EHS gradewe only quote mills with ABS approval for the specific EQ70 / condition
Payment / quality riskT/T or L/C; inspection before balance; 3.2 witness available
Long lead timephoto updates; combine with AH36/FH40 tonnage when possible
Fabrication damage riskmill WPS data forwarded on request; cutting plan reviewed before ship
Prepcutting, bevelling, drilling, machining in-house

How to order ABS EH70 / EQ70

State both ABS EQ70 (rule) and commercial EH70 if used in the yard BOM; delivery condition; thickness × width × length × qty; UT level; Z/R if needed; multi-class; certificate type; port. Email SHH STEEL.

Sample PO line: “Steel plate to ABS Rules Part 2 2-1-8, Grade EQ70 (commercial EH70), delivery condition [AR/CR/N/TM/QT], 20 × 2500 × 12000 mm, 30 pcs, marked AB/EQ70, certificate endorsed by ABS Surveyor, EN 10204 3.2 [if required], UT [if required], CIF [port].” Each bracketed item changes price, lead time and which mills can supply, so fix them at enquiry stage.

FAQ

What sizes and minimum order quantity can you supply for ABS EH70 plate?
ABS EH70 is ordered as ABS Extra High Strength grade EQ70 under 2-1-8. The plate is fully killed, and the maximum thickness depends on the delivery condition (TM or QT) under 2-1-8/3.3 Table 3. In practice EQ70 is nearly always produced by an approved mill to order rather than taken from stock, so a mill minimum per heat or rolling usually applies. Send thickness × width × length × quantity per size and we will say whether the order fits a scheduled rolling or needs its own heat. Small balance quantities can sometimes ride on another EQ70 order.
How is ABS EH70 certified, and can you arrange EN 10204 3.2 witness inspection?
Every plate is made by an ABS-approved mill under ABS survey. It is die-stamped or stencilled AB/EQ70 with the heat or plate number, and the mill test certificate is endorsed by the ABS Surveyor. The certificate gives the ladle chemistry, the tensile results (ReH ≥ 690 N/mm², Rm 770–940 N/mm², A ≥ 14 %), the Charpy results at −40 °C, the delivery condition and the plate identity. If your contract asks for EN 10204 3.2, we arrange it before rolling. The witness can be the ABS Surveyor, a second class society (dual or multi-class stamping, e.g. ABS + DNV or LR), or a third-party inspector such as SGS or BV who witnesses the tests and checks the markings. 3.2 cannot be added after the plates have been tested, so please state it on the enquiry.
What is the impact test temperature and energy for ABS EH70 (EQ70), and do thickness limits apply?
EQ70 is tested at −40 °C with an average of at least 69 J longitudinal or 46 J transverse (2-1-8 Table 5A). Impact specimens come from the quarter-thickness position (t/4). For plates thicker than 100 mm, ABS requires additional positions. Rule maximum thickness depends on whether the plate is TM or QT (2-1-8/3.3 Table 3), so give the delivery condition as well as the thickness, and we will check the approved mill’s range before quoting. Final values are as per standard and mill certificate.
What welding and preheat guidance applies to ABS EH70?
EQ70 is an extra high strength steel (yield ≥ 690 N/mm²) supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by ABS. Under 2-1-8/4, Ceq is calculated from the ladle analysis and limited by Table 4B. For grades 47 and above, the mill may report CET, and for low-carbon TM/QT steel (C ≤ 0.12 %) it may report Pcm. Hydrogen control, preheat, interpass temperature and heat-input windows come from the approved WPS and the mill’s recommendations. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits.
What is the delivery time for ABS EH70 plate?
EQ70 is normally rolled to order. Typical commercial lead time is about 6–10 weeks from confirmed PO and deposit, depending on the mill rolling schedule, QT capacity, UT and any 3.2 witness. Ocean transit comes on top of that. This is a commercial estimate, not a rule value, and we confirm it with each quotation. Every week, your coordinator sends the rolling, heat-treatment, testing and stamping status with photos. Delays are reported as soon as the mill tells us, not at the shipping date.
Which payment terms do you accept for ABS EH70, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the AB/EQ70 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance, so the plate is verified before most of the money moves. With L/C, payment is tied to the presented documents (commercial invoice, packing list, B/L, mill certificate, and the 3.2 or class certificate if you require one). For first orders we can start with a smaller trial lot. The proforma invoice shows the grade, sizes and certificate type, so the contract and the delivered plate match.
What are the equivalent grades of ABS EH70 among class societies and GB 712?
ABS lists ABS EH70 as EQ70 in 2-1-8; "EH70" is the commercial name. ASTM A131/A131M stops at FH40, so it has no direct equivalent. Other societies (DNV / LR / BV / CCS / NK / KR / RINA) have their own extra-high-strength grades at 690 N/mm² and −40 °C, and their marks must be confirmed against each society’s rules. Whether GB 712 lists this exact grade has to be checked per edition; otherwise the requirements are as per standard and mill certificate. Always write EQ70 on the PO, plus any additional society stamps you need.
Can you cut, bevel or machine ABS EH70 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut EH70 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the AB/EQ70 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For QT extra high strength plate, thermal cutting parameters follow the mill’s recommendations so the cut edge is not damaged. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. Shot blasting and shop primer are available on request. Loading photos and a packing list come with each shipment. See SHH STEEL for our processing capabilities.

Conclusion

ABS EH70 maps to rule grade EQ70: yield 690 N/mm², tensile 770–940 N/mm², Charpy −40 °C (69 J L / 46 J T). Fix on the order: official grade, delivery condition, UT, vacuum-degassing/t>50 needs, R-suffix if MOU, multi-class and 3.2.

SHH STEEL quotes only ABS-approved EHS mills, arranges Surveyor attendance, and can add third-party 3.2 and multi-class stamps.

T/T or L/C with inspection before balance; dedicated photo follow-up; workshop cutting/bevelling/drilling/machining.

Request a quotation: send SHH STEEL ABS EQ70 (title EH70), sizes, qty, delivery condition, port and inspection needs.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X