Product Showcase
Offshore Platform Steel Plates Carbon Steel Plates
SHH STEEL offers Offshore Platform Steel Plates and offshore-compliant S355G7/EH36 steel plates for platforms. Standards like DNV/API specify high-strength, corrosion-resistant steels for marine structures, ensuring durability in harsh environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
EN 10225 S420G2+M Offshore Steel Plate
EN 10225 S420G2+M — EN 10225:2009 offshore platform steel plate: yield 420 MPa min., Charpy at −20 °C, thermomechanical rolled (+M, TMCP); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S420G2+Q Offshore Steel Plate
EN 10225 S420G2+Q — EN 10225:2009 offshore platform steel plate: yield 420 MPa min., Charpy at −20 °C, quenched and tempered (+Q / +QT); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S420G1+M Offshore Steel Plate
EN 10225 S420G1+M — EN 10225:2009 offshore platform steel plate: yield 420 MPa min., Charpy at −40 °C, thermomechanical rolled (+M, TMCP); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S420G1+Q Offshore Steel Plate
EN 10225 S420G1+Q — EN 10225:2009 offshore platform steel plate: yield 420 MPa min., Charpy at −40 °C, quenched and tempered (+Q / +QT); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S355G10+M Offshore Steel Plate
EN 10225 S355G10+M — EN 10225:2009 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, thermomechanical rolled (+M, TMCP); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S355G10+N Offshore Steel Plate
EN 10225 S355G10+N — EN 10225:2009 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, normalized / normalized rolled (+N); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S355G9+M Offshore Steel Plate
EN 10225 S355G9+M — EN 10225:2009 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, thermomechanical rolled (+M, TMCP); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S355G9+N Offshore Steel Plate
EN 10225 S355G9+N — EN 10225:2009 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, normalized / normalized rolled (+N); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S355G8+M Offshore Steel Plate
EN 10225 S355G8+M — EN 10225:2009 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, thermomechanical rolled (+M, TMCP); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S355G8+N Offshore Steel Plate
EN 10225 S355G8+N — EN 10225:2009 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, normalized / normalized rolled (+N); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S355G7+M Offshore Steel Plate
EN 10225 S355G7+M — EN 10225:2009 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, thermomechanical rolled (+M, TMCP); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More -
EN 10225 S355G7+N Offshore Steel Plate
EN 10225 S355G7+N — EN 10225:2009 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, normalized / normalized rolled (+N); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.View More
Offshore Platform Steel Plates Carbon Steel Plates
Shipbuilding Steel Plates
SHH STEEL, a premier Shipbuilding Steel Plates exporter, produces and exports shipbuilding steel plates for marine vessels and offshore structures. Our plates, such as AH36 and DH36, provide high strength, toughness, and corrosion resistance, meeting ABS and BV standards. With a 5,000-ton inventory, we guarantee 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for reliable marine-grade steel plates and custom maritime solutions.
Shipbuilding Steel Plates