EN 10225 S355G9+N Offshore Steel Plate

EN 10225 S355G9+N Offshore Steel Plate

EN 10225 S355G9+N — EN 10225:2009 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, normalized / normalized rolled (+N); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.
Keywords
EN 10225 S355G9+N, S355G9+N offshore steel plate, EN 10225:2009 plate, offshore platform steel plate, jacket and topside structural plate
Equivalent Grades:
EN 10225-1 S355NLO; API 2H Gr.50; BS 7191 355EMZ
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Through-Thickness Properties
Fracture Toughness and CTOD
Standard Context
Equivalent Grades
Welding Procedure Qualification
Inspection and Certification
Stock and Supply
Specification Mistakes
How to Order
FAQ
Conclusion

EN 10225 S355G9+N — offshore platform steel plate overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

EN 10225 S355G9+N is a weldable structural steel for fixed offshore structures to EN 10225:2009: yield 355 MPa minimum in thin plate, tensile 470–630 MPa, impact tested at −40 °C, delivered normalized / normalized rolled (+N). G9 is a special-structure S355 grade with very low P and S and an expectation of CTOD testing for critical nodes.

Equivalent grades: EN 10225-1 S355NLO · API 2H Gr.50 · BS 7191 355EMZ (nearest designations, plain text — not certificate-equivalent; confirm against the project specification). More grades: Offshore Platform Steel Plates.

EN 10225:2009 is the European standard for weldable structural steels for fixed offshore structures. It replaced the national offshore specifications (BS 7191 in the UK, NORSOK-based practice in Norway) with a single grade matrix: strength level (S355, S420, S460), a G-number that encodes the chemistry and testing regime, and a delivery condition (+N, +M or +Q). It is the grade list most jacket, topside and pile fabricators in the North Sea still quote from.

Offshore steel is bought differently from ship plate or building steel. The structure cannot be docked for repair, it is loaded by waves millions of times over a 25–40 year design life, and its joints are thick, highly restrained and inspected by NDT for fatigue cracks. EN 10225 S355G9+N therefore carries three guarantees beyond strength: toughness at low temperature, weldability with a controlled carbon equivalent, and — where ordered — resistance to lamellar tearing through the thickness.

SHH STEEL supplies EN 10225 S355G9+N as mill-direct plate with EN 10204 3.1 or 3.2 certification, ultrasonic testing, Z-direction testing and cutting to drawing. The full range is under Offshore Platform Steel Plates.

Where EN 10225 S355G9+N sits. G9 is a special-structure S355 grade with very low P and S and an expectation of CTOD testing for critical nodes; the “+N” suffix tells the mill it must be delivered normalized / normalized rolled (+N). Typical members: jacket nodes, legs and braces, topside deck girders, module support frames, piles and conductor guides for North Sea and other harsh-environment fixed platforms.

EN 10225 S355G9+N: key data at a glance

Item EN 10225 S355G9+N
Standard EN 10225:2009
Grade S355G9+N
Yield strength, min. 355 MPa min. (≤ 16 mm; reduces stepwise with thickness)
Tensile strength 470–630 MPa
Elongation, min. 22 % (indicative)
Charpy V-notch 50 J longitudinal at −40 °C (transverse on option; values to verify)
Delivery condition normalized / normalized rolled (+N)
Through-thickness Z35 through-thickness option
Thickness range up to about 150 mm (thickness limits by grade)
Certification EN 10204 3.1 / 3.2; third-party or operator witness on request

All values are typical of the EN 10225:2009 grade table and must be checked against the edition named on the purchase order (no local copy of the standard was available for this page — see the note in the ordering section). Yield decreases in steps as thickness increases; for heavy plate the order must state the design thickness so the correct band applies.

In EN 10225:2009 the grade name already fixes the chemistry family and testing scope, so the order mainly adds options: Z-quality, CTOD, UT class, test direction and test location for heavy plate.

EN 10225 S355G9+N chemical composition — every alloy element

Element Heat analysis, % (typical limit) Product (check) analysis, % Note
C 0.14 max. 0.14 max. (same as heat)
Si 0.15–0.55 0.15–0.55 (same as heat)
Mn 1.00–1.65 1.00–1.65 (same as heat)
P 0.015 max. 0.015 max. (same as heat) low P for toughness and HAZ
S 0.007 max. 0.007 max. (same as heat) low S for Z-direction ductility
Al (total) 0.015–0.055 0.015–0.055 (same as heat) grain refiner
Nb 0.04 max. 0.04 max. (same as heat) microalloy
V 0.06–0.08 max. 0.06–0.08 max. (same as heat) microalloy
Ti 0.025 max. 0.025 max. (same as heat) N-binding
Cu 0.30 max. 0.30 max. (same as heat) residual / alloy
Cr 0.25 max. 0.25 max. (same as heat) residual / alloy
Ni 0.50 max. 0.50 max. (same as heat) toughness
Mo 0.08 max. 0.08 max. (same as heat) hardenability
N 0.010 max. 0.010 max. (same as heat) free N harms CTOD
Nb+V+Ti 0.06–0.12 max. (calculated) not applicable (calculated from heat analysis)
B 0.0005 max. 0.0005 max. (same as heat) residual unless QT
Ca report if Ca-treated same as heat analysis (report if Ca-treated) sulphide shape control
Ceq (IIW) 0.40–0.43 max. (calculated; thickness-dependent) not applicable (calculated from heat analysis)
Pcm 0.20–0.22 max. (calculated) not applicable (calculated from heat analysis) weldability index

Product (check) analysis column: EN 10225:2009 Table 3 heads the limits for this grade “Ladle and product analysis”, so the product analysis must meet the same values as the heat analysis (no extra tolerance).

Offshore chemistries are defined more tightly than general structural steel because every element affects either weldability (C, Mn, Cr, Mo, V, Cu, Ni, B through Ceq and Pcm), heat-affected-zone toughness (N, Ti, Nb, Al) or through-thickness ductility (S, Ca, P). For EN 10225 S355G9+N the table lists every element the certificate should report; limits shown are indicative values for the EN 10225:2009 grade family and must be verified against the governing table.

EN 10225:2009 tightens residuals as the G-number rises: G7 to G10 carry lower P, S and N, a capped Nb+V+Ti and stricter Ceq/Pcm than the basic G2/G3 grades.

EN 10225 S355G9+N tensile properties by thickness

Thickness (mm) Yield ReH min. (MPa) Tensile Rm (MPa) Elongation min.
≤ 16 355 470–630 MPa 22 %
16–25 345 470–630 MPa 22 %
25–40 335 470–630 MPa 22 %
40–63 325 470–630 MPa 22 %
63–100 315 470–630 MPa 22 %

Thickness steps are indicative and must be checked: European offshore standards reduce the minimum yield in steps as thickness grows. Designers working to ISO 19902, API RP 2A or NORSOK N-004 use the yield of the actual thickness band, so the reduction matters for heavy chords and cans.

Many offshore projects add a maximum yield-to-tensile ratio (often 0.85–0.90, grade-dependent) and an upper yield limit to keep weld metal overmatching. For EN 10225 S355G9+N these are project requirements, not always standard requirements, and must be ordered explicitly.

The 355 MPa level is the backbone of offshore construction. Most jacket legs, braces, deck girders and piles are designed at this level because it balances strength, weldability, fatigue performance and availability; fatigue, not static strength, often governs member size, so going higher in strength does not always save weight.

EN 10225 grades are tested on specimens taken transverse to the main rolling direction for plate, with location defined relative to the plate surface; for heavy plate an additional mid-thickness test may apply. The certificate should state orientation and location so values can be compared with design data.

EN 10225 S355G9+N: Charpy at −40 °C and delivery condition

EN 10225 S355G9+N is delivered normalized / normalized rolled (+N). Impact requirement: 50 J longitudinal at −40 °C (transverse on option; values to verify). Each value is the mean of three full-size specimens; single values must not fall below the minimum fraction stated in the standard (commonly 70 %).

Normalized plate is the safest route when the fabricator will hot-form or stress-relieve; properties are restored by the same heat treatment cycle.

For heavy plate, offshore projects often require Charpy specimens from mid-thickness as well as near the surface, and testing in the transverse direction. These additions change test cost and lead time, so ask for them in the enquiry for EN 10225 S355G9+N.

A test temperature of −40 °C is chosen to sit well below the lowest anticipated service temperature of the structure, giving margin for the strain-ageing, residual stress and constraint present in welded offshore joints. If the project design temperature is lower than usual — Arctic or sub-Arctic fields — the order should specify a lower test temperature or a higher energy, and the mill must confirm it can certify it for EN 10225 S355G9+N in the ordered thickness.

EN 10225 S355G9+N: Z-direction quality and lamellar tearing

Through-thickness status for EN 10225 S355G9+N: Z35 through-thickness option. Tubular joints, padeyes, brace-to-chord connections and deck girder flanges carry load perpendicular to the plate surface; plate made from a cast slab has its weakest direction there.

The Z-quality test follows EN 10164 practice (Z15, Z25, Z35 classes by reduction of area) or the equivalent API supplementary requirement; the class must be stated on the order, together with whether testing is per plate or per heat.

For EN 10225 S355G9+N the mill test is a tensile specimen machined across the plate thickness with friction-welded extensions; the reduction of area is the acceptance value. Low sulphur, calcium treatment and controlled centreline segregation are the levers that make the value reachable in thick plate. At yield level 355 the stiffeners and brace stubs that land on a chord can pull a plate apart through its thickness if inclusions are elongated — lamellar tearing is a fabrication defect that appears during welding, not in service, so it must be prevented by steel choice.

EN 10225 S355G9+N: CTOD and low-temperature toughness

CTOD testing is part of the expected qualification scope for this grade. In offshore practice CTOD may be required both for steel qualification (per mill and route) and for welding procedure qualification at the node.

Charpy energy at −40 °C is a quality-control test; CTOD is an engineering test. For EN 10225 S355G9+N, the designer decides whether CTOD testing of parent plate and weld HAZ is required — typically for nodes, thick-walled joint cans and members where fatigue cracks could grow to a critical size. The project specification sets the test temperature (often −10 °C or the lowest design temperature) and the required CTOD value (0.25 mm is frequently quoted — project-specific, UNCERTAIN).

EN 10225 S355G9+N within EN 10225:2009

In EN 10225:2009, S355G9+N belongs to the S355 family. The G-numbers are not a toughness ladder like ship-steel letters; they are chemistry and testing packages. Lower numbers suit secondary steel, higher numbers primary and special structure. The suffix (+N, +M, +Q) fixes the route.

Operators often overlay their own documents: NORSOK M-120 material data sheets (e.g. MDS for structural plate), NORSOK M-101 for fabrication and M-650 for qualification of manufacturers. Where these apply to EN 10225 S355G9+N, they add test frequency, chemistry limits and documentation beyond the base standard (MDS numbers not quoted here — confirm with the project).

The 2009 edition remains the reference cited in a large share of North Sea and Middle East contracts placed before the 2019 revision, and many stockists still certify to it. Replacing a 2009 G-grade with a 2019 LO grade during a project needs a concession from the engineering contractor, even if strength and toughness match, because test scope and chemistry limits are not identical.

EN 10225 S355G9+N against other offshore designations

Standard Nearest designation Remark
EN 10225:2009 (this page) EN 10225 S355G9+N ordered grade
EN 10225-1 EN 10225-1 S355NLO nearest — verify chemistry, impact and Z requirements
API API 2H Gr.50 nearest — verify chemistry, impact and Z requirements
BS 7191 BS 7191 355EMZ nearest — verify chemistry, impact and Z requirements

EN 10225:2009 neighbours: S355G2…G10 in +N and +M. Nearest designations are similar in strength and intent but not interchangeable on paper: impact temperature, Z-quality, CTOD scope and chemistry limits differ. A plate can carry two designations only if one heat meets every requirement of both and the certificate names both.

Ship-plate grades such as EH36 are sometimes offered against offshore orders; they meet a similar strength and −40 °C impact level but lack the offshore chemistry limits, Z-testing and CTOD scope, so they are not substitutes for primary offshore structure.

Welding and fabrication of EN 10225 S355G9+N

Weld EN 10225 S355G9+N with low-hydrogen processes (SMAW with basic electrodes, FCAW, SAW) and consumables whose weld-metal Charpy and, where specified, CTOD properties meet the project at −40 °C. Preheat is calculated from Ceq or Pcm, combined thickness and heat input (EN 1011-2 or AWS D1.1 Annex methods) and recorded in the WPS.

EN ISO 15614-1 qualification with offshore supplements — HAZ Charpy at several locations, hardness and CTOD — is the norm in North Sea projects.

For EN 10225 S355G9+N the WPS is qualified on plate from the actual supplier and route where possible, covering the heat-input window, preheat, interpass temperature and any PWHT. Offshore projects typically require Charpy tests in weld metal, fusion line and fusion line +2 / +5 mm, plus hardness surveys (often 325 or 350 HV10 max. — project-specific) and, for critical joints, HAZ CTOD.

Normalized plate can be hot formed and normalized again in the yard if the procedure demands it; its properties are restored by the same thermal cycle, which makes it attractive for heavily formed cans and cones.

EN 10225 S355G9+N: testing, marking and certificates

EN 10225 plate is normally supplied with an EN 10204 3.2 certificate countersigned by the purchaser’s inspector or a classification society; many projects also impose NORSOK M-120 material data sheets and M-650 manufacturer qualification.

Each plate of EN 10225 S355G9+N is marked with the manufacturer, standard, grade, heat and plate number and inspector’s stamp. Receiving inspection should match the stencil to the certificate, check thickness at several points, confirm UT class and Z-test results where ordered, and verify Ceq/Pcm against the WPS range.

EN 10225 S355G9+N sizes, stock and lead time

Thickness (mm) Width (mm) Length (mm) Condition
10 2500 6000–12000 N
12 2500 / 3000 6000–12000 N
16 2500 / 3000 6000–12000 N
20 2500 / 3000 6000–12000 N
25 3000 6000–12000 N
30 3000 8000–12000 N
40 3000 8000–12000 N
50 3000 8000–12000 N
60 2500 / 3000 6000–12000 N
80 2500 6000–10000 N

Offshore plate is mostly rolled to order against a project specification; stock covers common thicknesses only. Mill-campaign lead time for EN 10225 S355G9+N is typically 6–10 weeks plus testing and freight (commercial estimate).

We cut EN 10225 S355G9+N to drawing, bevel, shot-blast and prime, transfer heat numbers to every piece and arrange third-party witness on request.

Because the G-number fixes chemistry and testing scope, a mill can often satisfy several G-grades from one heat. Buyers can use this to consolidate small quantities across a project, provided the certificate states every designation actually met.

Mistakes we see on EN 10225 S355G9+N orders

  • Ordering by strength only (“355 MPa offshore”) without the full designation and route
  • Missing Z-quality class for plates loaded through the thickness
  • No CTOD or simulated PWHT requirement stated when the project needs it
  • Hot forming TMCP or QT plate without checking the mill’s limits
  • Accepting ship-plate or general structural grades as substitutes
  • Not stating the UT standard and class

For EN 10225 S355G9+N the most expensive mistake is late addition of tests — Z, CTOD or simulated PWHT cannot be added once the plates have shipped without re-sampling, and some cannot be done at all.

With EN 10225:2009 the recurring error is quoting the strength and delivery condition but not the G-number — “S355+N offshore” leaves the chemistry package undefined. Another is accepting a G2 or G3 certificate for a member the design classifies as primary or special, where G7 to G10 is expected; the strength is the same, the testing scope is not.

Ordering information for EN 10225 S355G9+N

Sample line: “Plate, EN 10225:2009 S355G9+N, 40 × 3000 × 12000 mm, 20 pcs, Z35, UT EN 10160 S2E3, EN 10204 3.2” — then send it to SHH STEEL.

  • Standard and edition: EN 10225:2009
  • Grade: S355G9+N
  • Thickness, width, length, quantity and tolerance class
  • Delivery condition and any limits on fabrication heat treatment
  • Impact: temperature (−40 °C), direction and position; project values if higher
  • Through-thickness class (Z25/Z35) and test frequency
  • CTOD and simulated PWHT if required
  • UT standard and class (EN 10160 / ASTM A578)
  • Inspection document (EN 10204 3.1 / 3.2) and witnessing party; NORSOK M-120 MDS if applicable

Note: no local copy of the standard was checked for this page; clause and table numbers are deliberately not quoted, and indicative values must be confirmed against the edition on the order.

FAQ

What is EN 10225 S355G9+N?
EN 10225 S355G9+N is offshore structural plate to EN 10225:2009, with minimum yield 355 MPa min. and tensile 470–630 MPa. G9 is a special-structure S355 grade with very low P and S and an expectation of CTOD testing for critical nodes; the “+N” suffix tells the mill it must be delivered normalized / normalized rolled (+N). In practice EN 10225 S355G9+N is chosen for jacket nodes, legs and braces, topside deck girders, module support frames, piles and conductor guides for North Sea and other harsh-environment fixed platforms. The decision usually comes from the design basis: strength level 355, design temperature, joint classification and fatigue category together point to the required grade, and the project material specification then fixes the remaining options. This positioning follows North Sea fixed-platform practice under EN 10225:2009; the project material specification can narrow it further. The 355 MPa level is the backbone of offshore construction. Most jacket legs, braces, deck girders and piles are designed at this level because it balances strength, weldability, fatigue performance and availability.
What impact toughness does EN 10225 S355G9+N guarantee?
50 J longitudinal at −40 °C (transverse on option; values to verify). Impact testing at −40 °C demonstrates that the plate stays ductile at the lowest service temperatures expected for offshore structures. The Charpy requirement at −40 °C is the quality-control baseline. Projects may tighten it — a higher average, transverse orientation, testing at the plate quarter-thickness and at mid-thickness for heavy plate — and these must be written into the order before rolling. For EN 10225 S355G9+N, record the test temperature, specimen orientation and position on the certificate so the operator’s inspector can verify compliance without re-testing.
Does EN 10225 S355G9+N need through-thickness (Z) testing?
Z35 through-thickness option. Z-testing measures reduction of area across the thickness and is the main protection against lamellar tearing. Lamellar tearing risk rises with plate thickness, joint restraint and weld size. For EN 10225 S355G9+N in cruciform or T-joints carrying load through the plate, specify Z-quality and ultrasonic testing of the landing zone; buttering and joint redesign are fabrication-side remedies. Plates for nodes, padeyes and brace landings in EN 10225 S355G9+N benefit most from Z-quality; secondary plating rarely needs it.
How weldable is EN 10225 S355G9+N?
Weldability is governed by Ceq and Pcm, which for 355 MPa-class offshore steel are capped low; delivered normalized / normalized rolled (+N), it is welded with low-hydrogen processes under a qualified procedure. Low carbon equivalent helps, but the qualified procedure decides. For EN 10225 S355G9+N we provide the actual heat analysis with Ceq and Pcm values so the welding engineer can check the preheat calculation against the WPS range before production starts. Hardness limits in the HAZ, often required for sour or cathodically protected structures, are checked during procedure qualification of EN 10225 S355G9+N.
What are the nearest equivalents to EN 10225 S355G9+N?
Nearest designations: EN 10225-1 S355NLO; API 2H Gr.50; BS 7191 355EMZ. These are near matches, not certificate equivalents. Substitution between offshore families is a project decision, not a supplier decision: EN 10225 S355G9+N can be dual-certified with other offshore grades if one heat meets every requirement of both documents, and the certificate must list both designations. When a project changes standard mid-stream, a written concession listing the replacement grade and any extra tests avoids disputes at final documentation review.
Which certificate comes with EN 10225 S355G9+N?
EN 10204 3.1 as standard, 3.2 with witness by the purchaser, operator or a classification society on request. The inspector’s stamp and certificate number should be transferred to cut pieces so traceability survives fabrication. Certification is fixed before rolling. EN 10225 plate is normally supplied with an EN 10204 3.2 certificate countersigned by the purchaser’s inspector or a classification society; many projects also impose NORSOK M-120 material data sheets and M-650 manufacturer qualification. All certificates for EN 10225 S355G9+N are issued in English with heat analysis, mechanical results and option results on one document.
Is ultrasonic testing included for EN 10225 S355G9+N?
UT is an order option for EN 10225 S355G9+N; offshore projects almost always specify it, usually as a full-body scan plus edge-zone scan, with acceptance class agreed with the engineering contractor before rolling. Ultrasonic testing is normally ordered to EN 10160 (class S2/E3 or better) or ASTM A578 for offshore plate; for EN 10225 S355G9+N in node areas the edge zone and the full body are both scanned (class to be stated on the order). UT results for EN 10225 S355G9+N are reported plate by plate with the standard and acceptance class named on the certificate.
What are sizes, lead times and payment terms?
Plates 8–150 mm thick, widths to about 3000–4000 mm and lengths to 12–18 m depending on mill. Payment by T/T or L/C at sight; third-party inspection on request. Minimum rolling quantities apply per thickness and grade, and project orders are scheduled into the mill campaign once the specification review is complete. For EN 10225 S355G9+N we cut to drawing, bevel and shot-blast in our own workshop, keep heat-number traceability on every piece and pack plate flat with timber spacers for sea freight. Quantities, weights and the document list are confirmed in writing before loading, and the operator’s inspector can witness at the mill or at our yard. Mixed-thickness orders of EN 10225 S355G9+N can be consolidated per mill campaign to reduce minimum-quantity surcharges.

Conclusion

EN 10225 S355G9+N is a EN 10225:2009 offshore structural plate: yield 355 MPa min., impact at −40 °C, delivered normalized / normalized rolled (+N). Order it with the full designation, Z-quality, UT and certification stated before rolling.

SHH STEEL supplies EN 10225 S355G9+N with EN 10204 certificates, third-party witness, cutting and UT. Send grade, sizes, quantities and project specification for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X