EN 10225-1 S355NLO Offshore Steel Plate

EN 10225-1 S355NLO Offshore Steel Plate

EN 10225-1 S355NLO — EN 10225-1:2019 offshore platform steel plate: yield 355 MPa min., Charpy at −40 °C, normalized / normalized rolled (N); Z-direction, UT and EN 10204 3.2 on request — SHH STEEL.
Keywords
EN 10225-1 S355NLO, S355NLO offshore steel plate, EN 10225-1:2019 plate, offshore platform steel plate, jacket and topside structural plate
Equivalent Grades:
EN 10225 S355G8+N / S355G10+N; API 2H Gr.50; BS 7191 355EMZ
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Through-Thickness Properties
Fracture Toughness and CTOD
Standard Context
Equivalent Grades
Welding Procedure Qualification
Inspection and Certification
Stock and Supply
Specification Mistakes
How to Order
FAQ
Conclusion

EN 10225-1 S355NLO — offshore platform steel plate overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

EN 10225-1 S355NLO is an offshore plate grade of EN 10225-1:2019: yield 355 MPa minimum in thin plate, tensile 470–630 MPa, impact tested at −40 °C (the LO suffix), delivered normalized / normalized rolled (N), with through-thickness and CTOD options for fixed and mobile offshore structures.

Equivalent grades: EN 10225 S355G8+N / S355G10+N · API 2H Gr.50 · BS 7191 355EMZ (nearest designations, plain text — not certificate-equivalent; confirm against the project specification). More grades: Offshore Platform Steel Plates.

EN 10225-1:2019 split the old single-part standard into product parts — Part 1 for plates, Part 2 for sections, Parts 3 and 4 for hollow sections — and renamed the grades: delivery condition letter (N, M or Q) plus the suffix LO for low-temperature offshore. It widened the range to S500, S550, S620 and S690 quenched-and-tempered plate for jack-up legs, cranes and heavy topside nodes, and it tightened the link between steel qualification and welding qualification.

Offshore steel is bought differently from ship plate or building steel. The structure cannot be docked for repair, it is loaded by waves millions of times over a 25–40 year design life, and its joints are thick, highly restrained and inspected by NDT for fatigue cracks. EN 10225-1 S355NLO therefore carries three guarantees beyond strength: toughness at low temperature, weldability with a controlled carbon equivalent, and — where ordered — resistance to lamellar tearing through the thickness.

SHH STEEL supplies EN 10225-1 S355NLO as mill-direct plate with EN 10204 3.1 or 3.2 certification, ultrasonic testing, Z-direction testing and cutting to drawing. The full range is under Offshore Platform Steel Plates.

Where EN 10225-1 S355NLO sits. NLO plate gets its properties from normalizing; it is the conservative choice where hot forming or stress relief must not disturb properties. At S355 it sits at the base of the range of Part 1. Typical members: new-build jackets, wind-turbine jacket and transition structures, topside primary steel and — at the higher strengths — jack-up leg chords, rack plates and spud cans.

EN 10225-1 S355NLO: key data at a glance

Item EN 10225-1 S355NLO
Standard EN 10225-1:2019
Grade S355NLO
Yield strength, min. 355 MPa min. (≤ 16 mm; reduces stepwise with thickness)
Tensile strength 470–630 MPa
Elongation, min. 22 % (indicative)
Charpy V-notch 50 J at −40 °C (indicative; −60 °C option)
Delivery condition normalized / normalized rolled (N)
Through-thickness Z25 / Z35 through-thickness options per order
Thickness range up to about 150 mm (Q grades lower at the highest strengths)
Certification EN 10204 3.1 / 3.2; third-party or operator witness on request

All values are typical of the EN 10225-1:2019 grade table and must be checked against the edition named on the purchase order (no local copy of the standard was available for this page — see the note in the ordering section). Yield decreases in steps as thickness increases; for heavy plate the order must state the design thickness so the correct band applies.

Part 1 options are numbered in the standard and must be selected on the order: impact test temperature, Z-quality, CTOD, simulated PWHT, UT class, surface condition and inspection document.

EN 10225-1 S355NLO chemical composition — every alloy element

Element Heat analysis, % (typical limit) Product (check) analysis, % Note
C 0.14 max. 0.14 max. (same as heat)
Si 0.15–0.55 0.15–0.55 (same as heat)
Mn 1.00–1.65 1.00–1.65 (same as heat)
P 0.015 max. 0.015 max. (same as heat) low P for toughness and HAZ
S 0.007 max. (0.005 option) 0.007 max. (same as heat) low S for Z-direction ductility
Al (total) 0.015–0.055 0.015–0.055 (same as heat) grain refiner
Nb 0.04 max. 0.04 max. (same as heat) microalloy
V 0.06–0.08 max. 0.06–0.08 max. (same as heat) microalloy
Ti 0.025 max. 0.025 max. (same as heat) N-binding
Cu 0.30 max. 0.30 max. (same as heat) residual / alloy
Cr 0.25 max. 0.25 max. (same as heat) residual / alloy
Ni 0.50 max. 0.50 max. (same as heat) toughness
Mo 0.08 max. 0.08 max. (same as heat) hardenability
N 0.010 max. 0.010 max. (same as heat) free N harms CTOD
Nb+V+Ti 0.06–0.12 max. (calculated) not applicable (calculated from heat analysis)
B 0.0005 max. 0.0005 max. (same as heat) residual unless QT
Ca report if Ca-treated same as heat analysis (report if Ca-treated) sulphide shape control
Ceq (IIW) 0.40–0.43 max. (calculated; thickness-dependent) not applicable (calculated from heat analysis)
Pcm 0.20–0.22 max. (calculated) not applicable (calculated from heat analysis) weldability index

Product (check) analysis column: EN 10225-1:2019 clause 7.2.2 requires the product analysis to comply with the same chemical-composition table values as the heat analysis (no extra tolerance).

Offshore chemistries are defined more tightly than general structural steel because every element affects either weldability (C, Mn, Cr, Mo, V, Cu, Ni, B through Ceq and Pcm), heat-affected-zone toughness (N, Ti, Nb, Al) or through-thickness ductility (S, Ca, P). For EN 10225-1 S355NLO the table lists every element the certificate should report; limits shown are indicative values for the EN 10225-1:2019 grade family and must be verified against the governing table.

EN 10225-1 gives the Ceq and Pcm limits by thickness band and delivery condition; QLO grades carry higher Cr, Ni, Mo and permitted B to achieve hardenability, so Pcm becomes the more relevant weldability index.

EN 10225-1 S355NLO tensile properties by thickness

Thickness (mm) Yield ReH min. (MPa) Tensile Rm (MPa) Elongation min.
≤ 16 355 470–630 MPa 22 %
16–25 345 470–630 MPa 22 %
25–40 335 470–630 MPa 22 %
40–63 325 470–630 MPa 22 %
63–100 315 470–630 MPa 22 %

Thickness steps are indicative and must be checked: European offshore standards reduce the minimum yield in steps as thickness grows. Designers working to ISO 19902, API RP 2A or NORSOK N-004 use the yield of the actual thickness band, so the reduction matters for heavy chords and cans.

Many offshore projects add a maximum yield-to-tensile ratio (often 0.85–0.90, grade-dependent) and an upper yield limit to keep weld metal overmatching. For EN 10225-1 S355NLO these are project requirements, not always standard requirements, and must be ordered explicitly.

The 355 MPa level is the backbone of offshore construction. Most jacket legs, braces, deck girders and piles are designed at this level because it balances strength, weldability, fatigue performance and availability; fatigue, not static strength, often governs member size, so going higher in strength does not always save weight.

At the higher strengths of Part 1, the yield-to-tensile ratio, elongation and HAZ softening become design topics. Designers of jack-up legs and heavy nodes use the actual-thickness yield and may limit heat input to keep HAZ strength and toughness within qualification.

EN 10225-1 S355NLO: Charpy at −40 °C and delivery condition

EN 10225-1 S355NLO is delivered normalized / normalized rolled (N). Impact requirement: 50 J at −40 °C (indicative; −60 °C option). Each value is the mean of three full-size specimens; single values must not fall below the minimum fraction stated in the standard (commonly 70 %).

Normalized plate is the safest route when the fabricator will hot-form or stress-relieve; properties are restored by the same heat treatment cycle.

For heavy plate, offshore projects often require Charpy specimens from mid-thickness as well as near the surface, and testing in the transverse direction. These additions change test cost and lead time, so ask for them in the enquiry for EN 10225-1 S355NLO.

A test temperature of −40 °C is chosen to sit well below the lowest anticipated service temperature of the structure, giving margin for the strain-ageing, residual stress and constraint present in welded offshore joints. If the project design temperature is lower than usual — Arctic or sub-Arctic fields — the order should specify a lower test temperature or a higher energy, and the mill must confirm it can certify it for EN 10225-1 S355NLO in the ordered thickness.

EN 10225-1 S355NLO: Z-direction quality and lamellar tearing

Through-thickness status for EN 10225-1 S355NLO: Z25 / Z35 through-thickness options per order. Tubular joints, padeyes, brace-to-chord connections and deck girder flanges carry load perpendicular to the plate surface; plate made from a cast slab has its weakest direction there.

The Z-quality test follows EN 10164 practice (Z15, Z25, Z35 classes by reduction of area) or the equivalent API supplementary requirement; the class must be stated on the order, together with whether testing is per plate or per heat.

For EN 10225-1 S355NLO the mill test is a tensile specimen machined across the plate thickness with friction-welded extensions; the reduction of area is the acceptance value. Low sulphur, calcium treatment and controlled centreline segregation are the levers that make the value reachable in thick plate. At yield level 355 the stiffeners and brace stubs that land on a chord can pull a plate apart through its thickness if inclusions are elongated — lamellar tearing is a fabrication defect that appears during welding, not in service, so it must be prevented by steel choice.

EN 10225-1 S355NLO: CTOD and low-temperature toughness

CTOD testing is part of the expected qualification scope for this grade. In offshore practice CTOD may be required both for steel qualification (per mill and route) and for welding procedure qualification at the node.

Charpy energy at −40 °C is a quality-control test; CTOD is an engineering test. For EN 10225-1 S355NLO, the designer decides whether CTOD testing of parent plate and weld HAZ is required — typically for nodes, thick-walled joint cans and members where fatigue cracks could grow to a critical size. The project specification sets the test temperature (often −10 °C or the lowest design temperature) and the required CTOD value (0.25 mm is frequently quoted — project-specific, UNCERTAIN).

EN 10225-1 S355NLO within EN 10225-1:2019

EN 10225-1:2019 replaces the G-numbers with route letters and the LO suffix. For new projects S355NLO is the designation to quote; old drawings may still cite 2009 G-grades, so cross-reference both on the order when replacing material.

Operators often overlay their own documents: NORSOK M-120 material data sheets (e.g. MDS for structural plate), NORSOK M-101 for fabrication and M-650 for qualification of manufacturers. Where these apply to EN 10225-1 S355NLO, they add test frequency, chemistry limits and documentation beyond the base standard (MDS numbers not quoted here — confirm with the project).

Part 1 also introduced clearer rules for the qualification of the steel itself: the manufacturer demonstrates weldability, HAZ toughness and, where required, CTOD on representative plate for each route and thickness range, and the data are then referenced on production orders. This shifts some testing from every order to a one-off qualification — but only for the qualified route and thickness.

EN 10225-1 S355NLO against other offshore designations

Standard Nearest designation Remark
EN 10225-1:2019 (this page) EN 10225-1 S355NLO ordered grade
EN 10225 EN 10225 S355G8+N / S355G10+N nearest — verify chemistry, impact and Z requirements
API API 2H Gr.50 nearest — verify chemistry, impact and Z requirements
BS 7191 BS 7191 355EMZ nearest — verify chemistry, impact and Z requirements

EN 10225-1:2019 neighbours: S355NLO/MLO … S690QLO. Nearest designations are similar in strength and intent but not interchangeable on paper: impact temperature, Z-quality, CTOD scope and chemistry limits differ. A plate can carry two designations only if one heat meets every requirement of both and the certificate names both.

Ship-plate grades such as EH36 are sometimes offered against offshore orders; they meet a similar strength and −40 °C impact level but lack the offshore chemistry limits, Z-testing and CTOD scope, so they are not substitutes for primary offshore structure.

Welding and fabrication of EN 10225-1 S355NLO

Weld EN 10225-1 S355NLO with low-hydrogen processes (SMAW with basic electrodes, FCAW, SAW) and consumables whose weld-metal Charpy and, where specified, CTOD properties meet the project at −40 °C. Preheat is calculated from Ceq or Pcm, combined thickness and heat input (EN 1011-2 or AWS D1.1 Annex methods) and recorded in the WPS.

EN 10225-1 is designed to be used with ISO 15614-1 qualification and the weldability data the mill provides; high-strength QLO grades need tight heat-input control.

For EN 10225-1 S355NLO the WPS is qualified on plate from the actual supplier and route where possible, covering the heat-input window, preheat, interpass temperature and any PWHT. Offshore projects typically require Charpy tests in weld metal, fusion line and fusion line +2 / +5 mm, plus hardness surveys (often 325 or 350 HV10 max. — project-specific) and, for critical joints, HAZ CTOD.

Normalized plate can be hot formed and normalized again in the yard if the procedure demands it; its properties are restored by the same thermal cycle, which makes it attractive for heavily formed cans and cones.

EN 10225-1 S355NLO: testing, marking and certificates

Part 1 plate is supplied with an EN 10204 3.2 certificate in most offshore contracts; NORSOK M-120 (material data sheets) and M-650 (qualification of manufacturers) are frequently cited alongside it on Norwegian and international projects.

Each plate of EN 10225-1 S355NLO is marked with the manufacturer, standard, grade, heat and plate number and inspector’s stamp. Receiving inspection should match the stencil to the certificate, check thickness at several points, confirm UT class and Z-test results where ordered, and verify Ceq/Pcm against the WPS range.

EN 10225-1 S355NLO sizes, stock and lead time

Thickness (mm) Width (mm) Length (mm) Condition
10 2500 6000–12000 N
12 2500 / 3000 6000–12000 N
16 2500 / 3000 6000–12000 N
20 2500 / 3000 6000–12000 N
25 3000 6000–12000 N
30 3000 8000–12000 N
40 3000 8000–12000 N
50 3000 8000–12000 N
60 2500 / 3000 6000–12000 N
80 2500 6000–10000 N

Offshore plate is mostly rolled to order against a project specification; stock covers common thicknesses only. Mill-campaign lead time for EN 10225-1 S355NLO is typically 6–10 weeks plus testing and freight (commercial estimate).

We cut EN 10225-1 S355NLO to drawing, bevel, shot-blast and prime, transfer heat numbers to every piece and arrange third-party witness on request.

LO plate is newer in stockholder inventories than the 2009 G-grades; S355MLO and S355NLO are increasingly stocked, while S420 and above are almost always rolled to order with qualification data supplied by the mill.

Mistakes we see on EN 10225-1 S355NLO orders

  • Ordering by strength only (“355 MPa offshore”) without the full designation and route
  • Missing Z-quality class for plates loaded through the thickness
  • No CTOD or simulated PWHT requirement stated when the project needs it
  • Hot forming TMCP or QT plate without checking the mill’s limits
  • Accepting ship-plate or general structural grades as substitutes
  • Not stating the UT standard and class

For EN 10225-1 S355NLO the most expensive mistake is late addition of tests — Z, CTOD or simulated PWHT cannot be added once the plates have shipped without re-sampling, and some cannot be done at all.

With EN 10225-1 the recurring error is mixing old and new designations on one drawing set so that the fabricator orders a 2009 G-grade for one member and an LO grade for its neighbour, with different test scopes. A second is forgetting that the steel qualification data supplied by the mill cover a stated thickness and route only; plate outside that window needs additional testing.

Ordering information for EN 10225-1 S355NLO

Sample line: “Plate, EN 10225-1:2019 S355NLO, 40 × 3000 × 12000 mm, 20 pcs, Z35, UT EN 10160 S2E3, EN 10204 3.2” — then send it to SHH STEEL.

  • Standard and edition: EN 10225-1:2019
  • Grade: S355NLO
  • Thickness, width, length, quantity and tolerance class
  • Delivery condition and any limits on fabrication heat treatment
  • Impact: temperature (−40 °C), direction and position; project values if higher
  • Through-thickness class (Z25/Z35) and test frequency
  • CTOD and simulated PWHT if required
  • UT standard and class (EN 10160 / ASTM A578)
  • Inspection document (EN 10204 3.1 / 3.2) and witnessing party; NORSOK M-120 MDS if applicable

Note: no local copy of the standard was checked for this page; clause and table numbers are deliberately not quoted, and indicative values must be confirmed against the edition on the order.

FAQ

What is EN 10225-1 S355NLO?
EN 10225-1 S355NLO is offshore structural plate to EN 10225-1:2019, with minimum yield 355 MPa min. and tensile 470–630 MPa. NLO plate gets its properties from normalizing; it is the conservative choice where hot forming or stress relief must not disturb properties. At S355 it sits at the base of the range of Part 1. In practice EN 10225-1 S355NLO is chosen for new-build jackets, wind-turbine jacket and transition structures, topside primary steel and — at the higher strengths — jack-up leg chords, rack plates and spud cans. The decision usually comes from the design basis: strength level 355, design temperature, joint classification and fatigue category together point to the required grade, and the project material specification then fixes the remaining options. This positioning follows current EN 10225-1 practice; the project material specification can narrow it further. The 355 MPa level is the backbone of offshore construction. Most jacket legs, braces, deck girders and piles are designed at this level because it balances strength, weldability, fatigue performance and availability.
What impact toughness does EN 10225-1 S355NLO guarantee?
50 J at −40 °C (indicative; −60 °C option). Impact testing at −40 °C demonstrates that the plate stays ductile at the lowest service temperatures expected for offshore structures. The Charpy requirement at −40 °C is the quality-control baseline. Projects may tighten it — a higher average, transverse orientation, testing at the plate quarter-thickness and at mid-thickness for heavy plate — and these must be written into the order before rolling. For EN 10225-1 S355NLO, record the test temperature, specimen orientation and position on the certificate so the operator’s inspector can verify compliance without re-testing.
Does EN 10225-1 S355NLO need through-thickness (Z) testing?
Z25 / Z35 through-thickness options per order. Z-testing measures reduction of area across the thickness and is the main protection against lamellar tearing. Lamellar tearing risk rises with plate thickness, joint restraint and weld size. For EN 10225-1 S355NLO in cruciform or T-joints carrying load through the plate, specify Z-quality and ultrasonic testing of the landing zone; buttering and joint redesign are fabrication-side remedies. Plates for nodes, padeyes and brace landings in EN 10225-1 S355NLO benefit most from Z-quality; secondary plating rarely needs it.
How weldable is EN 10225-1 S355NLO?
Weldability is governed by Ceq and Pcm, which for 355 MPa-class offshore steel are capped low; delivered normalized / normalized rolled (N), it is welded with low-hydrogen processes under a qualified procedure. Low carbon equivalent helps, but the qualified procedure decides. For EN 10225-1 S355NLO we provide the actual heat analysis with Ceq and Pcm values so the welding engineer can check the preheat calculation against the WPS range before production starts. Hardness limits in the HAZ, often required for sour or cathodically protected structures, are checked during procedure qualification of EN 10225-1 S355NLO.
What are the nearest equivalents to EN 10225-1 S355NLO?
Nearest designations: EN 10225 S355G8+N / S355G10+N; API 2H Gr.50; BS 7191 355EMZ. These are near matches, not certificate equivalents. Substitution between offshore families is a project decision, not a supplier decision: EN 10225-1 S355NLO can be dual-certified with other offshore grades if one heat meets every requirement of both documents, and the certificate must list both designations. When a project changes standard mid-stream, a written concession listing the replacement grade and any extra tests avoids disputes at final documentation review.
Which certificate comes with EN 10225-1 S355NLO?
EN 10204 3.1 as standard, 3.2 with witness by the purchaser, operator or a classification society on request. The inspector’s stamp and certificate number should be transferred to cut pieces so traceability survives fabrication. Certification is fixed before rolling. Part 1 plate is supplied with an EN 10204 3.2 certificate in most offshore contracts; NORSOK M-120 (material data sheets) and M-650 (qualification of manufacturers) are frequently cited alongside it on Norwegian and international projects. All certificates for EN 10225-1 S355NLO are issued in English with heat analysis, mechanical results and option results on one document.
Is ultrasonic testing included for EN 10225-1 S355NLO?
UT is an order option for EN 10225-1 S355NLO; offshore projects almost always specify it, usually as a full-body scan plus edge-zone scan, with acceptance class agreed with the engineering contractor before rolling. Ultrasonic testing is normally ordered to EN 10160 (class S2/E3 or better) or ASTM A578 for offshore plate; for EN 10225-1 S355NLO in node areas the edge zone and the full body are both scanned (class to be stated on the order). UT results for EN 10225-1 S355NLO are reported plate by plate with the standard and acceptance class named on the certificate.
What are sizes, lead times and payment terms?
Plates 8–150 mm thick, widths to about 3000–4000 mm and lengths to 12–18 m depending on mill. Payment by T/T or L/C at sight; third-party inspection on request. Minimum rolling quantities apply per thickness and grade, and project orders are scheduled into the mill campaign once the specification review is complete. For EN 10225-1 S355NLO we cut to drawing, bevel and shot-blast in our own workshop, keep heat-number traceability on every piece and pack plate flat with timber spacers for sea freight. Quantities, weights and the document list are confirmed in writing before loading, and the operator’s inspector can witness at the mill or at our yard. Mixed-thickness orders of EN 10225-1 S355NLO can be consolidated per mill campaign to reduce minimum-quantity surcharges.

Conclusion

EN 10225-1 S355NLO is a EN 10225-1:2019 offshore structural plate: yield 355 MPa min., impact at −40 °C, delivered normalized / normalized rolled (N). Order it with the full designation, Z-quality, UT and certification stated before rolling.

SHH STEEL supplies EN 10225-1 S355NLO with EN 10204 certificates, third-party witness, cutting and UT. Send grade, sizes, quantities and project specification for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X