EN 10208-2 L290MB Steel Plate | EN 10208-2 Pipeline Steel - SHH STEEL

EN 10208-2 L290MB Steel Plate | TMCP Pipeline Plate

EN 10208-2 L290MB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (thermomechanically rolled; steel number 1.0429). Pipe-body yield Rt0.5 290-440 MPa with Rm ≥ 415 MPa and yield ratio ≤0.85 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.
Equivalent Grades:
Approximate talk: API 5L X42 / L290 (M); ISO 3183 / API 5L PSL2 related strength and delivery letter. Not automatic substitutes. Confirm against project specs.
Heat Treatment
MB = Thermomechanically rolled. Delivery condition is part of the steel name.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Impact toughness package
Equivalent Material Grade
L290MB vs same-strength family
Why choose Us
Our Service
FAQ
Conclusion

What is EN 10208-2 L290MB steel plate?

EN 10208-2 L290MB (steel number 1.0429) belongs to EN 10208-2 requirement class B with delivery condition MB (Thermomechanically rolled). EN 10208 is a pipe standard for on-land combustible-fluid pipelines, primarily gas supply systems. Part 2 adds Charpy impact (Tables 6 or 7), tighter chemistry, yield-ratio control on the pipe product, and enhanced NDT versus Part 1.

EN 10208-1:2009 and EN 10208-2:2009 specify technical delivery conditions for steel PIPES for pipelines for combustible fluids (primarily on-land gas supply systems). They are not plate product standards. SHH supplies pipeline steel plate as feedstock for forming welded line pipe to the ordered EN 10208 grade chemistry and mechanical package; plate is not automatically certified as finished EN 10208 pipe. Confirm plate-as-feedstock scope, testing and documentation at quotation. Both EN 10208 parts were withdrawn/replaced in CEN catalogs by EN ISO 3183:2012 (later editions of EN ISO 3183 / ISO 3183 and API Spec 5L cover petroleum and natural gas industry line pipe). Historical gas-distribution RFQs may still cite EN 10208; match the project specification.

This page covers pipeline steel plate intended as feedstock for forming line pipe to the L290MB chemistry and mechanical package. Do not treat plate as certified finished EN 10208 pipe unless the order and MTC explicitly cover that scope.

Category hubs: Pipeline Steel Plates · EN 10208-2 · EN 10208-1 · API 5L.

Same delivery family: L245MB · L360MB · L415MB · L450MB · L485MB · L555MB. Other EN 10208-2 grades: L245NB · L290NB · L360NB · L415NB · L360QB · L415QB · L450QB · L485QB · L555QB · L245MB · L360MB · L415MB · L450MB · L485MB · L555MB.

Material Specification for EN 10208-2 L290MB

Parameter Specification
Reference standard EN 10208-2:2009 (withdrawn/replaced by EN ISO 3183 in CEN catalogs; confirm project edition)
Grade / number L290MB / 1.0429
Requirement class B
Delivery condition MB – Thermomechanically rolled
Product form on this page Pipeline steel plate for line-pipe forming (feedstock); confirm at quotation
Underlying EN product Seamless and/or welded steel pipe per grade manufacturing table
Wall basis for tabulated values T ≤ 25 mm in Tables 3 and 5; thicker by agreement up to 40 mm
SHH supply focus About 6-50 mm plate (confirm against mill practice and order)
Width / length About 1500-4000 mm width; length cut-to-size on request
Surface / edge As-rolled or shot blasted; mill edge or cut edge
Certification EN 10204 3.1 / 3.2 as ordered
Density 7.85 g/cm³

Chemical Composition of EN 10208-2 L290MB (heat and product analysis)

Heat (cast) analysis limits for L290MB under EN 10208-2:2009 Table 3 (wall thickness T ≤ 25 mm). Product analysis shall not deviate from cast limits by more than Table 4. CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15 and is specified on the product analysis. Typical residual / deoxidation package (footnote e unless grade footnotes override): 0.015 ≤ Altot < 0.060; N ≤ 0.012; Al/N ≥ 2; Cu ≤ 0.25; Ni ≤ 0.30; Cr ≤ 0.30; Mo ≤ 0.10. For T > 25 mm up to 40 mm, chemistry is by agreement. Always verify the MTC.

Element / index Heat (cast) max / range
C ≤0.16
Si ≤0.45
Mn ≤1.50
P ≤0.025
S ≤0.020
V ≤0.04
Nb ≤0.04
Ti –
CEV max (product analysis) ≤0.40

Product-analysis plus tolerances (Table 4, selected): C +0.02 (≤0.21 cast); Si +0.05 (≤0.45); Mn +0.10 (≤1.80); P +0.005; S +0.005; V +0.01; Nb +0.01; Ti +0.01; Al ±0.005.

Elements not listed shall not be added intentionally without purchaser approval, except for deoxidation and heat finishing.

Mechanical Properties of EN 10208-2 L290MB

Tensile requirements for the pipe body under EN 10208-2:2009 Table 5 (T ≤ 25 mm). Yield is Rt0.5. Yield-to-tensile ratio Rt0.5/Rm applies to the product pipe and cannot be required of the starting plate alone; when ordering plate as feedstock, state whether pipe-body ratio control after forming is required. Elongation A is transverse; longitudinal values are 2 units higher. For T > 25 mm up to 40 mm, mechanics are by agreement.

Grade Rt0.5 (MPa) Rm min (MPa) Rt0.5/Rm max A transverse min (%) Bend mandrel
L290MB 290-440 ≥415 ≤0.85 ≥21 3T

Impact (class B): Charpy V-notch at typically 0 °C; purchaser states Table 6 (safety factor 1.6) or Table 7 (safety factor 1.4). Energies are pipe-diameter and wall-thickness dependent. For D ≤ 510 mm many grades list transverse pipe-body average ≥40 J (individual ≥30 J) as the baseline cell; higher grades and larger diameters require higher values per Tables 6/7. DWT (drop-weight tear) by agreement for D > 500 mm, T > 8 mm and specified yield > 360 MPa. For plate feedstock, state intended pipe OD, wall and Table 6 vs 7 on the enquiry.

Hard spots / flattening: Any hard spot exceeding 50 mm in any direction shall have hardness < 35 HRC (327 HB) per EN 10208-2:2009 8.5.7 (cold-formed pipe surface). Not a sour-service hardness limit. Flattening test applies to HFW pipe production testing (EN ISO 8492), not to plate tensile coupons. Sour-service HIC/SSC or offshore packages are not defined inside EN 10208; specify ISO 3183 / API 5L Annex H/J or NACE/ISO 15156 when needed.

Density approximately 7.85 g/cm³.

Delivery Conditions for EN 10208-2 L290MB

MB means Thermomechanically rolled. The delivery letter is built into the steel name L290MB.

NB: normalizing or normalizing forming. QB: quenching and tempering. MB: thermomechanical rolling (subsequent heating above about 580 °C may lower strength; TMCP properties generally cannot be restored by heat treatment alone).

For plate feedstock, order the plate delivery condition that matches the intended pipe route (Thermomechanically rolled). State intended pipe type (S / HFW / SAW / COW) when it affects starting-material practice.

Weldability of EN 10208-2 L290MB

EN 10208-2 selects chemistry and CEV limits (where tabulated) so class B steels are weldable for pipe and pipeline fabrication. CEV for L290MB: ≤0.40. Welding behaviour still depends on consumables, procedure and joint restraint. Weldability data or weld tests may be agreed (option). Use a qualified WPS.

MB grades typically emphasize lower C / CEV for improved weldability relative to higher-C normalized routes at the same strength class. QB heats need care on heat input and HAZ toughness after Q&T.

Related: API 5L · API 5L X42 / L290 (M) · EN 10208-1 class A.

Dimensional Tolerances for EN 10208-2 L290MB plate

EN 10208-2 dimensional tables cover finished pipe. For plate feedstock, use the agreed plate dimensional standard (for example EN 10029) unless the order cites another agreement. State flatness, edge condition, UT level and cut size when SAW/HFW forming tolerances are tight.

Applications and service limits for EN 10208-2 L290MB

Typical purchasing contexts for L290MB plate feedstock:

  • On-land gas transmission / distribution projects citing EN 10208-2 class B with MB delivery
  • Welded or seamless line-pipe forming requiring Charpy-controlled class B packages
  • RFQs comparing L290MB with API 5L X42 / L290 (M)

Not an automatic substitute for ISO 3183 / API 5L petroleum and natural gas industry line pipe. Not a dedicated sour or offshore annex; add those requirements explicitly when needed.

Related: Pipeline Steel Plates · EN 10208-2 · API 5L X42 / L290 (M) · GB/T 21237 related.

Impact toughness package for EN 10208-2 L290MB

Charpy V-notch at typically 0 °C; purchaser states Table 6 (safety factor 1.6) or Table 7 (safety factor 1.4). Energies are pipe-diameter and wall-thickness dependent. For D ≤ 510 mm many grades list transverse pipe-body average ≥40 J (individual ≥30 J) as the baseline cell; higher grades and larger diameters require higher values per Tables 6/7. DWT (drop-weight tear) by agreement for D > 500 mm, T > 8 mm and specified yield > 360 MPa. For plate feedstock, state intended pipe OD, wall and Table 6 vs 7 on the enquiry.

On the plate enquiry, state: intended pipe outside diameter and wall, Table 6 vs Table 7, test temperature if not 0 °C, and whether DWT is required. Plate CVN orientation and sub-size rules should be agreed when full pipe transverse pieces are not available at plate stage.

Equivalent and related grades for EN 10208-2 L290MB

These grades are commonly compared with L290MB. They are approximate, not automatic substitutes.

Standard / family Grade Relation Product page
EN 10208-2 L290MB This page (MB) –
API 5L / ISO 3183 API 5L X42 / L290 (M) Approximate PSL2 talk API 5L related
GB/T 21237 Related PSL2 grade Planned plate hub GB/T 21237
EN 10208-1 GA class A Lower requirement class; no mandatory Charpy EN 10208-1
Category Pipeline hubs Navigation Pipeline Steel Plates · EN 10208-2 · API 5L

EN 10208-2 L290MB vs related NB/QB/MB grades (selection aid)

Compare delivery routes and ratio/CEV caps at the same or related strength class. Not automatic substitutes.

Grade DC Rt0.5 Rm min Ratio max CEV Page
L290NB NB 290-440 ≥415 ≤0.85 ≤0.42 L290NB
L290MB MB 290-440 ≥415 ≤0.85 ≤0.40 This page

Why choose SHH STEEL for EN 10208-2 L290MB

  • China mill-direct pipeline steel plate aligned to EN 10208-2 L290MB (Thermomechanically rolled) for line-pipe forming
  • EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV) on request
  • Clear feedstock wording: plate for forming to EN 10208 grade requirements, confirm at quotation
  • Full NB / QB / MB coverage under EN 10208-2 · class A under EN 10208-1
  • API 5L / GB/T 21237 talk when the project cites those standards: API 5L related · GB/T 21237

Supply, cutting and inspection for EN 10208-2 L290MB

Item SHH STEEL supply note
Thickness About 6-50 mm focus; T > 25 mm chemistry/mechanics by agreement per standard
Size Width about 1500-4000 mm; cut-to-size length on request
Delivery condition MB – Thermomechanically rolled
Processing Cutting, beveling, shot blasting available
Mill certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV can be arranged
Quotation needs Grade L290MB, thickness × width × length, quantity, CVN table (6 or 7) / OD / wall, UT level, inspection level

FAQ

What does the MB suffix mean on L290MB?
MB means Thermomechanically rolled. It is part of the EN 10208-2 steel name.
Is L415NB a real EN 10208-2 grade?
Yes. L415NB is steel number 1.8972 in EN 10208-2:2009 Table 1 (normalized or normalizing formed).
Is EN 10208-2 a plate standard?
No. It is a pipe standard. This page covers pipeline steel plate for line-pipe forming to L290MB grade requirements; confirm at quotation.
What Charpy values apply?
Diameter- and thickness-dependent per Tables 6 or 7 (typically at 0 °C). State pipe OD, wall and table choice on the enquiry.
Approximate API 5L talk?
API 5L X42 / L290 (M). See API 5L related. Substitution needs project approval.

Request a quotation

Send EN 10208-2 L290MB, thickness × width × length, quantity, Charpy table (6 or 7) with intended pipe OD/wall, any DWT/UT extras and inspection level. SHH STEEL will return mill availability, certification scope and a quotation for pipeline steel plate for line-pipe forming to EN 10208 grade requirements.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: EN 10208-2 · Pipeline Steel Plates · API 5L · EN 10208-1

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X