EN 10208-2

Product Showcase

EN 10208-2 Carbon Steel Plates

SHH STEEL offers EN 10208-2-compliant L245MB/L290NB/L360NB low-alloy steel pipes. EN 10208-2 specifies seamless/welded pipes for sour service pipeline transportation. Corrosion-resistant, certified quality, competitive prices, customizable. Trust SHH STEEL!

EN 10208-2 L290NB Steel Plate | EN 10208-2 Pipeline Steel - SHH STEEL

EN 10208-2 L290NB Steel Plate | Normalized Pipeline Plate

EN 10208-2 L290NB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (normalized or normalizing formed; steel number 1.0484). Pipe-body yield Rt0.5 290-440 MPa with Rm ≥ 415 MPa and yield ratio ≤0.85 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.
View More
EN 10208-2 L290MB Steel Plate | EN 10208-2 Pipeline Steel - SHH STEEL

EN 10208-2 L290MB Steel Plate | TMCP Pipeline Plate

EN 10208-2 L290MB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (thermomechanically rolled; steel number 1.0429). Pipe-body yield Rt0.5 290-440 MPa with Rm ≥ 415 MPa and yield ratio ≤0.85 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.
View More
EN 10208-2 L245NB Steel Plate | EN 10208-2 Pipeline Steel - SHH STEEL

EN 10208-2 L245NB Steel Plate | Normalized Pipeline Plate

EN 10208-2 L245NB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (normalized or normalizing formed; steel number 1.0457). Pipe-body yield Rt0.5 245-440 MPa with Rm ≥ 415 MPa and yield ratio ≤0.80 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.
View More
EN 10208-2 L245MB Steel Plate | EN 10208-2 Pipeline Steel - SHH STEEL

EN 10208-2 L245MB Steel Plate | TMCP Pipeline Plate

EN 10208-2 L245MB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (thermomechanically rolled; steel number 1.0418). Pipe-body yield Rt0.5 245-440 MPa with Rm ≥ 415 MPa and yield ratio ≤0.85 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.
View More

Pipeline Steel Plates

SHH STEEL, a premier Pipeline Steel Plates exporter, produces and exports pipeline steel plates for oil, gas, and water transport systems. Our plates, like API 5L X70, offer high strength and corrosion resistance, meeting API standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Trust SHH STEEL for oil and gas steel plates and custom pipeline infrastructure solutions.