EN 10028-7 Stainless Steel Products
SHH STEEL offers EN 10028-7-compliant 304/316 stainless steel plates. EN 10028-7 specifies technical delivery conditions for flat stainless steel products, including creep-resistant austenitic steels, for pressure purposes. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
EN 10028-7 X2CrNiN23-4 1.4362 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiN23-4 (1.4362) is an austenitic-ferritic (duplex) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 400 MPa and Rm 600 – 800 MPa (Table 10). SHH STEEL supplies it up to 50 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1NiCrMoCu31-27-4 1.4563 Pressure Vessel Stainless Plate
EN 10028-7 X1NiCrMoCu31-27-4 (1.4563) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 500 – 700 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1CrNiMoCuN20-18-7 1.4547 Pressure Vessel Stainless Plate
EN 10028-7 X1CrNiMoCuN20-18-7 (1.4547) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 300 MPa and Rm 650 – 850 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1NiCrMoCuN25-20-7 1.4529 Pressure Vessel Stainless Plate
EN 10028-7 X1NiCrMoCuN25-20-7 (1.4529) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 300 MPa and Rm 650 – 850 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1CrNiMoCuN25-25-5 1.4537 Pressure Vessel Stainless Plate
EN 10028-7 X1CrNiMoCuN25-25-5 (1.4537) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 290 MPa and Rm 600 – 800 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1NiCrMoCu25-20-5 1.4539 Pressure Vessel Stainless Plate
EN 10028-7 X1NiCrMoCu25-20-5 (1.4539) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 520 – 720 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X6CrNiMoNb17-12-2 1.4580 Pressure Vessel Stainless Plate
EN 10028-7 X6CrNiMoNb17-12-2 (1.4580) is a stabilized austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 520 – 720 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X6CrNiMoTi17-12-2 1.4571 Pressure Vessel Stainless Plate
EN 10028-7 X6CrNiMoTi17-12-2 (1.4571) is a stabilized austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 520 – 670 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1CrNiMoN25-22-2 1.4466 Pressure Vessel Stainless Plate
EN 10028-7 X1CrNiMoN25-22-2 (1.4466) is a high-chromium, high-nickel austenitic stainless steel for special corrosive duties for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 250 MPa and Rm 540 – 740 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X2CrNiMoN17-13-5 1.4439 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiMoN17-13-5 (1.4439) is a molybdenum-alloyed austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 270 MPa and Rm 580 – 780 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X2CrNiMo18-15-4 1.4438 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiMo18-15-4 (1.4438) is a molybdenum-alloyed austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 520 – 720 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X3CrNiMo17-13-3 1.4436 Pressure Vessel Stainless Plate
EN 10028-7 X3CrNiMo17-13-3 (1.4436) is a molybdenum-alloyed austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 530 – 730 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More
EN 10028-7 Stainless Steel Products
Stainless Steel Sheets and Plates
SHH STEEL, a leading Stainless Steel Sheets and Plates exporter, produces and exports stainless steel sheets (0.3–6 mm) and plates (>6 mm) for marine, chemical, and structural applications. Our products, like 304 and 316L (ASTM A240), offer corrosion resistance and durability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for 316L stainless steel plates and custom solutions for your projects.