ASTM A131/A131M Carbon Steel Plates
SHH STEEL offers ASTM A131/A131M-compliant AH32/DH32/EH36 shipbuilding steel plates. ASTM A131/A131M specifies structural steel plates for ship hulls, with high-strength low-alloy grades for weldability and toughness in marine environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASTM A131 Grade E Shipbuilding Steel Plate
ASTM A131 Grade E ordinary-strength hull plate to ASTM A131/A131M (A6/A6M general requirements): yield 235 MPa [34 ksi], impact −40 °C [−40 °F]. Mill test report, ABS or other class certificate on request — SHH STEEL.View More -
ASTM A131 Grade D Shipbuilding Steel Plate
ASTM A131 Grade D ordinary-strength hull plate to ASTM A131/A131M (A6/A6M general requirements): yield 235 MPa [34 ksi], impact −20 °C [−4 °F]. Mill test report, ABS or other class certificate on request — SHH STEEL.View More -
ASTM A131 Grade B Shipbuilding Steel Plate
ASTM A131 Grade B ordinary-strength hull plate to ASTM A131/A131M (A6/A6M general requirements): yield 235 MPa [34 ksi], impact 0 °C [32 °F]. Mill test report, ABS or other class certificate on request — SHH STEEL.View More -
ASTM A131 Grade A Shipbuilding Steel Plate
ASTM A131 Grade A ordinary-strength hull plate to ASTM A131/A131M (A6/A6M general requirements): yield 235 MPa [34 ksi], impact none ≤ 50 mm. Mill test report, ABS or other class certificate on request — SHH STEEL.View More
ASTM A131/A131M Carbon Steel Plates
Shipbuilding Steel Plates
SHH STEEL, a premier Shipbuilding Steel Plates exporter, produces and exports shipbuilding steel plates for marine vessels and offshore structures. Our plates, such as AH36 and DH36, provide high strength, toughness, and corrosion resistance, meeting ABS and BV standards. With a 5,000-ton inventory, we guarantee 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for reliable marine-grade steel plates and custom maritime solutions.
Shipbuilding Steel Plates