ASTM A131 Grade B shipbuilding steel plate to ASTM A131/A131M, stacked hull plates

ASTM A131 Grade B Shipbuilding Steel Plate

ASTM A131 Grade B ordinary-strength hull plate to ASTM A131/A131M (A6/A6M general requirements): yield 235 MPa [34 ksi], impact 0 °C [32 °F]. Mill test report, ABS or other class certificate on request — SHH STEEL.
Keywords
ASTM A131 Grade B steel plate, A131 B shipbuilding steel, A131/A131M B hull plate, ASTM A131 B ship plate, ordinary-strength marine steel plate
Equivalent Grades:
ABS Grade B; DNV VL B; LR Grade B; BV Grade B; CCS Grade B; KR Grade B (RB); NK Grade B (KB); RINA Grade B; GB 712 Grade B; IACS UR W11 B
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
A6/A6M General Requirements
Relation to ABS Rules
Equivalent Grades
Grade Selection
Welding and Fabrication
Mill Test Report and Marking
Stock and Supply
Specification Mistakes
How to Order
FAQ
Conclusion

ASTM A131 Grade B shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

ASTM A131 Grade B keeps the Grade A strength — 235 MPa [34 ksi] yield, 400–520 MPa [58–75 ksi] tensile — and adds what A lacks: a tighter manganese/silicon balance and a Charpy V-notch requirement at 0 °C [32 °F] in the thicknesses where the specification calls for it.

Equivalent grades: ABS B · DNV NV B · LR Grade B · BV Grade B · CCS Grade B · NK KB · KR RB · RINA Grade B · GB 712 Grade B.

Grade B fills the gap between plain A and fine-grain D — slightly more steelmaking discipline and a toughness number for a small price step.

ASTM A131/A131M is a product specification: it tells a mill what to make and test, while the general rules for plate — dimensions, tolerances, test methods, retests, marking and test reports — come from ASTM A6/A6M, which A131 references. Read the two together; neither is complete alone.

A131 was developed to mirror the American Bureau of Shipping material rules, which is why its grade letters match the IACS system. The important difference is legal, not metallurgical: an A131 plate is certified by the mill; a classed plate is additionally certified by a surveyor. US Coast Guard plan reviewers and many US owners accept A131 for non-classed or domestic work, while classed hulls normally require the society certificate (confirm with the approving authority).

SHH STEEL supplies ASTM A131 Grade B with the mill test report, ABS or other class certification on the same heat when ordered, and cutting to drawing. The full range is under ASTM A131 Grade B.

Where Grade B sits. In A131 terms Grade B is the first A131 letter with a defined impact temperature, and the cheapest way to put a toughness number on a mild-steel plate. Grade B is a thin market in North America: service centres stock A and the AH36 family deeply but B in fewer sizes, so mills frequently ship dual-certified material.

ASTM A131 Grade B: key data at a glance

ItemASTM A131 Grade B
SpecificationASTM A131/A131M (structural steel for ships), ordinary-strength Grade B — edition to be stated on the order
General requirementsASTM A6/A6M (dimensions, tolerances, testing, marking, test reports)
Yield strength, min.235 MPa [34 ksi]
Tensile strength400–520 MPa [58–75 ksi]
Elongation, min.21 % in 200 mm [8 in.] / 24 % in 50 mm [2 in.] (UNCERTAIN — verify edition)
Charpy V-notch0 °C [32 °F]
Deoxidationkilled or semi-killed up to 50 mm; killed above
Condition of supplyas-rolled, controlled-rolled, normalized or TMCP as the thickness and grade permit
Usual plate rangeabout 5–100 mm [3/16–4 in.] thick; shapes and bars are also within A131 scope
Certificationmill test report per A6/A6M; class certificate or third-party witness on request

Dual units are deliberate: A131 is written in inch-pound units and A131M in SI. The two are not exact conversions of each other, so the order must name one system as governing — mixing them on a mill order is the classic source of a borderline rejection.

For Grade B check the manganese minimum and whether your thickness triggers the 0 °C test.

ASTM A131 Grade B chemical composition — every element on the report

ElementHeat analysis, %Product (check) analysis, %Note
C0.21 max.0.25 max. (0.21 + 0.04)
Si0.35 max.0.40 max. (0.35 + 0.05)
Mn0.80 min. (0.60 min. when fully killed / cold-flanging quality)0.80 min. (ASTM A6/A6M Table A has no minimum-only row for Mn – heat limit applies)
P0.035 max.0.045 max. (0.035 + 0.010)
S0.035 max.0.045 max. (0.035 + 0.010)
Al (acid-soluble)not specified (report if added)no heat limit specified – report actual value
Nbreport if intentionally addedno numeric heat limit – report actual value
Vreport if intentionally addedno numeric heat limit – report actual value
Tireport if intentionally addedno numeric heat limit – report actual value
Cu0.35 max. (residual)0.38 max. (0.35 + 0.03)residual
Cr0.20 max. (residual)0.24 max. (0.20 + 0.04)residual
Ni0.40 max. (residual)0.43 max. (0.40 + 0.03)residual
Mo0.08 max. (residual)0.09 max. (0.08 + 0.01)residual
Nnot specifiedno heat limit specified – report actual valuereport on request
Nb+V+Tinot specified for mild grades (calculated if added)not applicable (calculated from heat analysis)
C + Mn/6 (Ceq)0.40 max. (calculated)not applicable (calculated from heat analysis)carbon-equivalent cap

Product (check) analysis column = heat (ladle) limit adjusted by ASTM A6/A6M-19 Table A “Permitted Variations in Product Analysis”, which ASTM A131/A131M invokes through A6/A6M (maximum + “over”, minimum − “under”; row chosen by the specified upper limit); arithmetic shown in brackets.

Values follow the IACS UR W11 / ABS basis that A131 tracks; the A131 table in the edition named on your order governs (no local copy checked — UNCERTAIN). Grade B needs 0.80 % Mn (0.60 % if fully killed) and caps Si at 0.35 % — the two lines that separate B from A on a report.

US mill test reports print a fixed analysis list — commonly C, Mn, P, S, Si, Cu, Ni, Cr, Mo, V, Nb, Al and sometimes Ti, N, B and Ca — regardless of grade. That makes residual-element screening easy: compare every line, not only the ones A131 limits.

A131 requires the heat analysis to be reported for every element with a limit in its table; where a grade allows grain-refining elements, the one actually used must be shown so the inspector can confirm fine-grain practice. Residuals that A6/A6M asks to be reported (Cu, Ni, Cr, Mo, V, Nb) normally appear even when A131 itself sets no limit (confirm A6/A6M reporting rule for the cited edition).

ASTM A131 Grade B tensile requirements

PropertySI (A131M)Inch-pound (A131)
Yield strength, min.235 MPa34 ksi
Tensile strength400–520 MPa58–75 ksi
Elongation in 200 mm [8 in.], min.21 %same
Elongation in 50 mm [2 in.], min.24 %same

A131 follows A6/A6M practice for specimens: rectangular 200 mm [8 in.] or 50 mm [2 in.] gauge specimens, or round specimens in heavy plate, with elongation minimums tied to the gauge length — not the proportional 5.65√S₀ gauge used in European and class certificates. That is why the elongation figure on an A131 report can look lower than on a class certificate for the same steel (gauge-length adjustments for thin/thick plate per A6/A6M — UNCERTAIN).

All four mild letters share these values; A, B, D and E differ only in chemistry, deoxidation and impact testing.

A131 reports tensile results in both unit systems when the order is written to A131M or to the dual standard; the order must say which system governs, because rounding is not identical. For mild grades a missing distinct yield point is handled by the A6/A6M yield method (0.2 % offset or 0.5 % extension-under-load) — the report should name the method.

ASTM A131 Grade B: Charpy V-notch at 0 °C [32 °F] and condition of supply

Grade B is tested at 0 °C where thickness and condition of supply require it; thin as-rolled B is often exempt — buyers expecting a result on every report should order it.

ThicknessAvg. longitudinal (J)Avg. transverse (J)
≤ 50 mm [2 in.]2720
50–70 mm3424
70–100 mm4127

Each value is the average of three full-size specimens; one may fall below the average but not below 70 % of it. Longitudinal specimens apply unless transverse are ordered. Impact testing itself is done to ASTM A370 / E23 practice referenced through A6/A6M (clause numbers not quoted — UNCERTAIN).

The test lot rule is where A131 and the society rules are most often confused on the shop floor: the report should state the condition of supply, because it decides whether one set of three covers a batch, a plate-as-rolled or each heat-treated plate.

How ASTM A6/A6M governs ASTM A131 Grade B

Almost everything a receiving inspector checks on ASTM A131 Grade B apart from chemistry and mechanical values comes from A6/A6M: thickness, width, length and flatness tolerances; camber; permissible variations in weight; surface-imperfection removal by grinding; weld repair limits; retest rules; and the content of the test report.

Thickness tolerance is the point to watch. Class rules apply a small fixed minus tolerance to hull plate (IACS UR W13, commonly −0.3 mm), while A6/A6M expresses plate tolerances as variations over ordered thickness and weight (table numbers not quoted — UNCERTAIN). For classed hulls state on the order that the class minus tolerance applies; for domestic A131 work, A6/A6M governs.

Supplementary requirements in A6/A6M — for example ultrasonic examination (to A435 or A578), product analysis, through-thickness testing or additional tension tests — apply only when ordered by number. If it is not on the purchase order, the mill is not obliged to do it.

Heat vs. plate-as-rolled. A6/A6M distinguishes the heat (the melt) from the plate-as-rolled (the product of one slab or ingot). Test frequencies in A131 are expressed against those units, so a report listing one heat but several plates-as-rolled should show results for each unit the standard requires.

ASTM A131 Grade B and the ABS Rules for Materials and Welding

A131 and the ABS Rules (Part 2) share grade letters, chemistry columns and test values because A131 was written to align with them. A plate certified only to A131 is, however, not an ABS plate: ABS certification requires an ABS-approved mill, survey of testing and the ABS stamp on the plate.

In practice US and Gulf Coast yards order “ASTM A131 B / ABS B” dual-certified material. The mill makes one heat, the surveyor witnesses or audits the tests, and the plate is stencilled with both. Where a vessel is not classed — many inland barges and domestic workboats — A131 alone is often what the owner and the approving authority require.

Edition mismatches happen: the ABS Rules are revised yearly, while the A131 year is fixed on the order. If the contract cites both, state which governs in case of difference.

ASTM A131 Grade B against classification-society grades

Standard / societyDesignationRemark
ASTM A131/A131M (this page)ASTM A131 Grade BUS product specification; general requirements in A6/A6M
ABSABS Grade BRules Part 2 — the reference A131 was written to mirror
DNVDNV VL BVL prefix
LRLR Grade B
BVBV Grade B
CCSCCS Grade B
KRKR Grade B (RB)R-prefix
NKNK Grade B (KB)K-prefix
RINARINA Grade B
GB 712GB 712 Grade BChinese national standard

The table maps designations, not certificates. Every grade in it is built on the same IACS unified requirement, so chemistry, tensile and impact values line up closely; what differs is who tests, who stamps and which rule book the yard’s approved plan cites.

A plate can carry ASTM A131 Grade B plus one or more society marks when the mill holds the approvals and each surveyor witnesses the tests before shipment. Ordering the extra marks after rolling is not possible.

Choosing ASTM A131 Grade B within the A131 grade matrix

B is the cheapest A131 letter carrying an impact test. D or E may replace B if they meet B limits; A may not.

The letter is set by the structural category and thickness on the approved plan; the specification supplies the steel, it does not choose it.

Typical uses: shell and deck strakes of moderate thickness on coastal tugs, fishing vessels and Gulf Coast workboats, and repair inserts where the plan specifies 0 °C mild steel.

A131 also lists the cold-flanging and special-quality mild grades (designated CS and DS in the standard — confirm current status in the edition you cite). They are not part of this page set; if your plan calls for them, quote that designation on the order rather than substituting one of A, B, D or E.

Cutting, forming and welding ASTM A131 Grade B

ASTM A131 Grade B cuts by oxy-fuel, plasma or laser without preheat and forms readily, including cold flanging. Weld with AWS A5.1 / A5.20 / A5.17 consumables of matching strength and suitable toughness (e.g. E7018, E71T-1 or F7A2 classes as chosen in the WPS) or class-approved consumables for classed hulls.

With C + Mn/6 capped at 0.40, preheat is normally unnecessary, but thick restrained joints and cold, damp yards still call for the minimum preheat in the qualified procedure (AWS D1.1 or the class rule, as the contract states).

ASTM A131 Grade B mill test report, marking and receiving checks

A6/A6M requires a test report showing the specification and year, grade, heat number, heat analysis, tensile results, impact results, condition of supply and any supplementary requirements. Ask for the report before shipment and check it against the purchase order line by line.

Plates are marked with the manufacturer’s name or brand, heat number, specification and grade — for example “A131 B” — and, where class certified, the society stamp. On receipt check the stencil, match heat and plate numbers, confirm 0 °C [32 °F] and measure thickness at several points.

Electronic MTRs. A6/A6M allows the test report to be transmitted electronically provided it carries the same content and is traceable to the mill’s quality system. Keep the PDF with the heat number in the file name — classification surveyors and US Coast Guard plan reviewers ask for it years later.

ASTM A131 Grade B stock, sizes and lead time

Thickness (mm)Width (mm)Length (mm)ConditionApprox. qty
61829 / 24386096–12192AR / N100+ t
824386096–12192AR / N120+ t
1024386096–12192AR / N150+ t
122438 / 30486096–12192AR / N200+ t
162438 / 30486096–12192AR / N150+ t
2024386096–12192AR / N120+ t
2524386096–12192AR / N100+ t
3224386096–12192AR / N60+ t
4024386096–12192AR / N40+ t
5024386096–12192AR / N30+ t

Widths of 1829, 2438 and 3048 mm [72, 96, 120 in.] follow North American plate practice; metric widths are also available. Quantities change weekly — confirm before booking.

Non-stock sizes go into the next mill campaign: about 3–5 weeks plus freight (commercial estimate).

Processing. We cut Grade B to drawing by plasma or oxy-fuel, bevel, shot-blast and prime, and transfer the heat number, grade and specification to every cut piece so the mill test report stays valid for each part.

Mistakes we see on ASTM A131 Grade B purchase orders

  • Accepting a Grade A report against a B order
  • Missing the Mn minimum
  • Expecting impact results on every thickness without ordering them
  • No condition of supply on the report
  • Assuming B is fine-grain

A36 and A572 are building and bridge steels; they share yield levels with some A131 grades but not the hull-steel deoxidation, letter-graded toughness or marking. They are not substitutes on a ship plan.

The one we see most. The usual non-conformance is a Grade A test report re-labelled against a B purchase order, with no 0 °C result and manganese below the B minimum.

Ordering information for ASTM A131 Grade B

A6/A6M lists the information the purchaser must supply; A131 adds grade-specific items. Missing ordering information is the most common reason a mill delivers something technically compliant but commercially wrong.

Sample line: “Plate, ASTM A131/A131M-xx Grade B, 12.7 × 2438 × 12192 mm [1/2 × 96 × 480 in.], 40 pcs, SI governs, mill test report per A6/A6M, ABS certificate, UT per A578 Level B” — then send it to SHH STEEL.

Purchase-order checklist (A131/A6 ordering information):

  • Specification and year: ASTM A131/A131M-xx (state A131 or A131M units)
  • Grade: Grade B
  • Quantity (weight or pieces), dimensions and thickness tolerance basis per A6/A6M
  • Condition of supply / heat treatment (as-rolled, CR, N or TMCP as permitted)
  • Impact test frequency and orientation where the order requires more than the basic rule
  • Supplementary requirements (e.g. UT, through-thickness, product analysis) by number from A6/A6M
  • Certification: mill test report, ABS (or other society) witness if required, EN 10204 3.1/3.2 if requested
  • Marking, packing and destination

FAQ

What is ASTM A131 Grade B?
It is the ordinary-strength Grade B of ASTM A131/A131M, the US purchase specification for structural steel for ships, with general requirements from A6/A6M. Its letter matches the ABS and IACS mild-steel grade. Grade B gives a documented 0 °C toughness level where a plan or flag requirement asks for one but D would be over-specification. Within A131, Grade B is the first impact-graded mild letter. In steel terms it is semi-killed or killed C–Mn plate with a raised manganese minimum, which is what you should see reflected in the deoxidation statement and analysis on the mill test report. The specification year matters too: quote it on the purchase order so both sides read the same table, and keep a copy of that edition with the job file.
What impact toughness does Grade B need?
0 °C [32 °F]. Average energies are 27/20 J up to 50 mm, 34/24 J at 50–70 mm and 41/27 J at 70–100 mm (longitudinal/transverse), with one value allowed down to 70 % of the average. Check the report states orientation and test temperature. For Grade B the practical point is the thickness at which testing starts and how often it is repeated. A6/A6M and A131 tie test lots to the heat, the plate-as-rolled or the heat-treated plate depending on condition, so a report with one result for a mixed delivery should be queried before the plate is cut. If your yard specification wants more frequent tests, order them as a supplementary requirement.
Is A131 Grade B the same as ASTM A36?
No. A36 is a structural steel for buildings and bridges. The yield level is close, but A36 has no hull-steel deoxidation rules, no letter-graded toughness and no ship-plate marking. Approved ship plans and surveyors do not accept A36 in place of an A131 grade. Mixing A36 into a hull because the yield matches is the most common shortcut we are asked about. For Grade B, the answer stays no: a surveyor or plan reviewer will reject it, and the cost of removing fitted plate is far higher than the price difference. If A36 is already in stock, keep it for foundations, brackets on shore structures or tooling.
Is an A131 Grade B plate also an ABS Grade B plate?
Metallurgically it can be, but not on paper. ABS certification needs an ABS-approved mill and an ABS-witnessed or audited test; only then is the plate stamped “ABS B”. Order dual certification before rolling. If you receive dual-certified plate, the B line must be on the mill test report and on the plate stencil. For Grade B, dual certification is common and cheap when it is planned: the mill tests once, the surveyor witnesses, and both stencils go on the plate. It becomes expensive when it is forgotten — retesting cut plate may not be accepted at all, and re-ordering costs a rolling cycle. Put the class line on the first enquiry, not the final order.
Can Grade B be swapped with another letter?
D or E may replace B if they also meet B limits; A cannot. Any substitution should be recorded on the purchase order or agreed in writing with the yard and, for classed hulls, the surveyor. Substitution upward is a commercial decision as much as a technical one: mills sometimes ship a higher letter because it is what they have on the floor. Make sure the mill test report and stencil show Grade B (or both letters) so the receiving inspector can sign it off against the purchase order without a concession request.
Does Grade B need preheat?
Normally not in usual thicknesses, because C + Mn/6 is capped at 0.40. The qualified welding procedure still governs thick, restrained joints and cold, damp conditions; AWS D1.1 or the class rule sets the minimum where the contract cites it. For moderate-thickness shell and deck strakes, welding is rarely the limiting factor with Grade B; fit-up, distortion control and consumable toughness are. Choose consumables whose impact rating covers the letter of the plate, and record the plate heat number on the weld map so any later question about base-metal properties can be traced to the report.
What must the mill test report show?
Specification and year, Grade B, heat and plate numbers, heat analysis, tensile results, impact results, condition of supply and any supplementary requirements, as A6/A6M requires. Reports may be electronic if traceable. Match the heat number to the plate stencil on receipt. If the report lacks any of those items, ask the mill for a corrected report before shipment rather than after arrival. For Grade B the items most often missing are the specification year, the condition of supply and, for thick plate, the impact orientation. A6/A6M allows corrections, but they must come from the mill’s quality system, not from a reseller.
What are sizes, lead times and payment terms?
Stock covers about 6–50 mm in 1829–3048 mm widths and 6–12 m lengths; other sizes roll in about 3–5 weeks plus freight (estimate). Payment by T/T with balance after inspection, or L/C at sight; third-party inspection on request. For Grade B we also cut, bevel, shot-blast and prime in our own workshop and transfer heat numbers to every piece. Mixed-size orders can share a container; break bulk is used for long or heavy plate. We confirm quantities, weights and the final document list in writing before loading.

Conclusion

ASTM A131 Grade B is the ordinary-strength grade of ASTM A131/A131M, the US purchase specification for ship structural steel aligned with the ABS Rules: yield 235 MPa [34 ksi], tensile 400–520 MPa, impact 0 °C [32 °F]. Order it by specification, year and grade, with A6/A6M ordering information complete.

SHH STEEL supplies ASTM A131 Grade B with mill test reports, dual ABS/class certification on request, cutting and UT. Send grade, sizes, quantities and port for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X