JIS G3459 SUS310STP Stainless Steel Pipe | JIS G3459 Stainless Steel Pipe - SHH STEEL

JIS G3459 SUS310STP Stainless Steel Pipe

JIS G3459 SUS310STP stainless steel pipe (310S / UNS S31008), austenitic, Table 3 cast analysis, Rm min 520 N/mm² / proof min 205 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS310STP (310S / UNS S31008 — body alias)
Standard
JIS G3459:2021
Product form
Seamless and welded stainless steel pipe, delivery solution annealed
Size
Typically OD 10.5–660.4 mm (6A–650A); schedule or measured wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3459 SUS310STP Stainless Steel Pipe

JIS G3459:2021 is the Japanese Industrial Standard for stainless steel pipes used in corrosion-resistant, low-temperature, high-temperature and fire-protection piping. Grade symbol SUS310STP sits in the austenitic set of Table 1. Most modern JIS G3459 heat-facing RFQs that still say “310” actually want SUS310STP once welding and carbon are discussed honestly. Buyers working Japanese piping packages should treat SUS310STP as a governed product symbol under G3459:2021, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Corrosion framing beside SUS310STP: oxidation performance tracks 310 chemistry; low carbon improves resistance to weld decay in mixed-duty systems.

SHH STEEL can produce and supply JIS G3459 SUS310STP as seamless or welded pipe across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling.

Shop language may still say “310S pipe,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3459 and SUS310STP so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.

Scope discipline: SUS310STP is piping product under JIS G3459, not a boiler tube under JIS G3463 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include SUS310TP, SUS309STP, SUS321HTP, SUS347HTP. Role reminder: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling.

Inside this JIS G3459 series, compare SUS310TP, SUS309STP, SUS321HTP, SUS347HTP. Hub: JIS G3459. ASTM/ASME related product pages (not interchangeable by default): A312 TP310S.

Chemical Composition of JIS G3459 SUS310STP

Cast analysis for JIS G3459 SUS310STP follows Table 3. Key windows on a typical certificate include C ≤0.08, Si ≤1.50, Mn ≤2.00, P ≤0.045, S ≤0.030, Ni 19.00–22.00, Cr 24.00–26.00. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 310S / UNS S31008 is body text only. Corrosion thread: oxidation performance tracks 310 chemistry; low carbon improves resistance to weld decay in mixed-duty systems.

Chemical limits for SUS310STP under JIS G3459:2021 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling.

Grade C Si Mn P S Ni Cr
SUS310STP ≤0.08 ≤1.50 ≤2.00 ≤0.045 ≤0.030 19.00–22.00 24.00–26.00

Mechanical Properties of JIS G3459 SUS310STP

Ambient tensile floors for SUS310STP come from JIS G3459 Table 4: Rm min 520 N/mm², proof stress min 205 N/mm², elongation (No.11/12 longitudinal) min 35%. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A No.11/12 long. min (%) A No.5 trans. min (%) A No.4 long. min (%) A No.4 trans. min (%)
SUS310STP 520 205 35 25 30 22

Ambient values from JIS G3459:2021 Table 4 for SUS310STP. Heat treatment (Table 2): 1030 °C min, rapid cool. Elongation reductions apply for walls under 8 mm; elongation is not mandatory below 40 mm OD (record unless agreed). Note: hot-finished SUS321TP / SUS321HTP may use 460 / 180 N/mm² by agreement.

Manufacture of JIS G3459 SUS310STP Pipe (Seamless and Welded)

For SUS310STP, the mill path is not “seamless only.” Table 1 explicitly pairs austenitic, duplex, and ferritic marks with S/A/L/E process symbols and H/C/B/G finishes. Order the combination that matches hydrostatic or NDT preference, not a habit from ASTM A312 alone. Seamless and welded options remain available for SUS310STP; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Size practice for SUS310STP remains cold-finished seamless for precision OD; hot-finished S or A-welded for larger heat-service diameters.

Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Heat-treatment reference for SUS310STP: 1030 °C min, rapid cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling.

When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS310STP: cold-finished seamless for precision OD; hot-finished S or A-welded for larger heat-service diameters.

Dimensions and Tolerances for JIS G3459 SUS310STP

SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS310STP before the mill slot is locked. Standard Note 1 frames typical OD from 10.5 mm (6A) to 660.4 mm (650A). Size hint: cold-finished seamless for precision OD; hot-finished S or A-welded for larger heat-service diameters. Tolerance class follows the process route ordered for SUS310STP, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside SUS310STP: oxidation performance tracks 310 chemistry; low carbon improves resistance to weld decay in mixed-duty systems.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling. Fixed lengths and multiple cut lengths for SUS310STP are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside SUS310STP: oxidation performance tracks 310 chemistry; low carbon improves resistance to weld decay in mixed-duty systems.

Equivalent Grades for JIS G3459 SUS310STP

Equivalence talk for SUS310STP starts with 310S / UNS S31008: that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3459 SUS310STP. ASTM A312 / A789 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS310TP, SUS309STP, SUS321HTP, SUS347HTP. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.

Heat Treatment and Delivery Condition for JIS G3459 SUS310STP

SUS310STP is delivered solution annealed under JIS G3459. Table 2 reference: 1030 °C min, rapid cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 310L fillers; post-weld solution treatment when the duty and wall thickness demand it. Recorded furnace charts for SUS310STP should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the SUS310STP caution visible here: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.

Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling. Field heat treatment of SUS310STP after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to SUS310STP duty: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling.

Corrosion Resistance of JIS G3459 SUS310STP

Corrosion behaviour of JIS G3459 SUS310STP tracks its austenitic balance: oxidation performance tracks 310 chemistry; low carbon improves resistance to weld decay in mixed-duty systems. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS310STP is filed as austenitic. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS310STP rather than relying on schedule thickness alone. Application context for SUS310STP stays furnace muffles piping, hot-air and flue systems, thermal processing lines, and welded high-temperature interconnects.

Applications of JIS G3459 SUS310STP Pipe

Applications of JIS G3459 SUS310STP pipe centre on furnace muffles piping, hot-air and flue systems, thermal processing lines, and welded high-temperature interconnects. Role summary: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling. When a related chemistry is required under ASTM A312 or A789, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: furnace muffles piping, hot-air and flue systems, thermal processing lines, and welded high-temperature interconnects. Duty thread: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling. Commissioning teams benefit when the as-built dossier repeats SUS310STP beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to SUS310STP: 310L fillers; post-weld solution treatment when the duty and wall thickness demand it.

Weldability of JIS G3459 SUS310STP

SUS310STP is welded both as a mill product (A/L/E routes) and as fabricator joints on spools. Shop guidance: 310L fillers; post-weld solution treatment when the duty and wall thickness demand it. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for SUS310STP should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Weld-shop note tied to SUS310STP: 310L fillers; post-weld solution treatment when the duty and wall thickness demand it.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade. Consumable lot control and shielding-gas notes for SUS310STP stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for SUS310STP remains cold-finished seamless for precision OD; hot-finished S or A-welded for larger heat-service diameters.

Surface Finishes for JIS G3459 SUS310STP

Surface supply for SUS310STP is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling. Roughness or polish callouts for SUS310STP must name OD, ID, or both; ambiguous “bright pipe” language is clarified before finishing slots are booked. Size practice for SUS310STP remains cold-finished seamless for precision OD; hot-finished S or A-welded for larger heat-service diameters.

Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade. Final visual standards for SUS310STP reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Corrosion framing beside SUS310STP: oxidation performance tracks 310 chemistry; low carbon improves resistance to weld decay in mixed-duty systems.

Inspection and Testing for JIS G3459 SUS310STP

Inspection for JIS G3459 SUS310STP covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS310STP keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to SUS310STP: 310L fillers; post-weld solution treatment when the duty and wall thickness demand it.

Marking includes SUS310STP, process/finish symbols, manufacturer, and other mandatory clause-15 data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: furnace muffles piping, hot-air and flue systems, thermal processing lines, and welded high-temperature interconnects. Non-conforming SUS310STP lengths are segregated and retested or rejected under clause 14 rather than reworked into unmarked stock. Size practice for SUS310STP remains cold-finished seamless for precision OD; hot-finished S or A-welded for larger heat-service diameters.

Packaging and Shipping for JIS G3459 SUS310STP

Packaging for SUS310STP uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS310STP repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the SUS310STP caution visible here: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade. Desiccant and wrap choices for SUS310STP follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS310STP stays furnace muffles piping, hot-air and flue systems, thermal processing lines, and welded high-temperature interconnects.

Shipping documents list JIS G3459, SUS310STP, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling. Claims handling for SUS310STP starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to SUS310STP duty: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling.

Why Choose SHH STEEL

SHH STEEL can produce and supply JIS G3459 SUS310STP with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless pipe capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling.

Technical sales can map SUS310STP against sisters SUS310TP, SUS309STP, SUS321HTP, SUS347HTP and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS310STP, the Table 1 process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS310STP to that written scope.

Supply Capability

SHH STEEL can produce and supply JIS G3459 SUS310STP across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS310STP when the mill schedule allows.

Item Capability
Standard JIS G3459:2021 stainless steel pipes
Grade symbol SUS310STP
Product form Seamless (S) and welded (A / L / E) pipe; finishes H / C / B / G
Delivery condition solution annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 10.5–660.4 mm (6A–650A) per standard Note 1; other by agreement
Wall / schedule Schedule 5S–160 class and measured wall within family practice

Stock / Available sizes

SHH STEEL can produce and supply JIS G3459 SUS310STP. Stock / Available sizes: enquiry band typically aligns with 10.5–660.4 mm OD practice under G3459 Note 1, with schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS310STP, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: cold-finished seamless for precision OD; hot-finished S or A-welded for larger heat-service diameters.

Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS310TP, SUS309STP, SUS321HTP, SUS347HTP. Email the size list to start. SHH STEEL can produce trial lengths of SUS310STP for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS310STP for procedure qualification before bulk release when the project calendar needs it. This paragraph is locked to SUS310STP duty: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling.

FAQ

What is JIS G3459 SUS310STP stainless steel pipe used for?
JIS G3459 SUS310STP is stainless pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — furnace muffles piping, hot-air and flue systems, thermal processing lines, and welded high-temperature interconnects. Role summary: lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling. It is a Japanese product standard mark, not an automatic ASTM A312 certificate.
Does JIS G3459 SUS310STP cover seamless and welded pipe?
Yes. Table 1 allows seamless (S) and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish symbols H/C/B/G. SHH STEEL can produce and supply either route for SUS310STP when the mill can meet the ordered size and tests. The title omits Seamless/Welded because the standard itself covers both — the PO must still name the process symbol.
What heat treatment applies to SUS310STP?
SUS310STP is delivered solution annealed under JIS G3459. Table 2 reference: 1030 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS310STP compare with sister grades SUS310TP, SUS309STP, SUS321HTP?
SUS310STP is filed as austenitic. Typical sisters on the same RFQ are SUS310TP, SUS309STP, SUS321HTP. Design caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade Pick the sister when the medium or strength floor outgrows this symbol rather than stretching schedule alone.
What tests appear on the mill certificate for SUS310STP?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 310S / UNS S31008 the same as ordering SUS310STP?
No. 310S / UNS S31008 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3459 and SUS310STP so cast limits, heat treatment, and process symbols are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3459 SUS310STP?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS310STP within the typical 10.5–660.4 mm OD practice, with schedules or measured walls by agreement. Size context: cold-finished seamless for precision OD; hot-finished S or A-welded for larger heat-service diameters. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS310STP be welded?
Shop guidance: 310L fillers; post-weld solution treatment when the duty and wall thickness demand it. Mill heat treatment of seamless or welded pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade
When should I choose a duplex or higher-Mo grade instead of SUS310STP?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade Sister pointers: SUS310TP, SUS309STP, SUS321HTP. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3459 SUS310STP with ASTM A312 or A789?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3459 SUS310STP does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS310STP?
Pickled after heat treatment is the usual piping supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS310STP when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3459 SUS310STP is stainless steel pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — lower-carbon 310S austenitic pipe combining oxidation resistance with a more weld-friendly carbon ceiling. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS310TP, SUS309STP, SUS321HTP. Related ASTM pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process symbol, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X