JIS G3459 SUS347HTP stainless steel pipe (347H / UNS S34709), austenitic, Table 3 cast analysis, Rm min 520 N/mm² / proof min 205 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS347HTP (347H / UNS S34709 — body alias)
Standard
JIS G3459:2021
Product form
Seamless and welded stainless steel pipe, delivery solution annealed
Size
Typically OD 10.5–660.4 mm (6A–650A); schedule or measured wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3459 SUS347HTP Stainless Steel Pipe

JIS G3459 covers both seamless and welded stainless pipe for process, utility, cryogenic-lean and fire-protection duties. Inside that standard, SUS347HTP is filed as austenitic. SUS347HTP is the JIS mark that keeps niobium and a high-temperature carbon window on the same pipe certificate. Buyers working Japanese piping packages should treat SUS347HTP as a governed product symbol under G3459:2021, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Application context for SUS347HTP stays high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems.

From pierce/draw or weld-and-anneal through marking and bundle protection, SHH STEEL can produce JIS G3459 SUS347HTP for the sizes and tests on your RFQ. Application sketch: high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS347HTP before production starts. This paragraph is locked to SUS347HTP duty: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping.

On the floor people shorten marks; in QA they must not. SUS347HTP under JIS G3459 carries specific Table 3 windows and Table 4 floors that a loose “347H” note will not enforce. Caution: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply.

Fire-protection, cryogenic-lean and corrosive piping all sit in G3459’s scope statement; still match the alloy to the medium. For SUS347HTP, that means: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping. Nearby marks: SUS347TP, SUS321HTP, SUS304HTP, SUS316HTP. Document the medium, design temperature, and weld map beside the SUS347HTP line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the SUS347HTP caution visible here: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply.

Inside this JIS G3459 series, compare SUS347TP, SUS321HTP, SUS304HTP, SUS316HTP. Hub: JIS G3459. ASTM/ASME related product pages (not interchangeable by default): A312 TP347H.

Chemical Composition of JIS G3459 SUS347HTP

For SUS347HTP, the melt ticket has to show Table 3 compliance — C 0.04–0.10, Si ≤1.00, Mn ≤2.00, P ≤0.030, S ≤0.030, Ni 9.00–13.00, Cr 17.00–20.00. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: Nb stabilisation plus carbon floor for hot service; aqueous chlorides still want Mo or duplex.

Where Mo, Cu, Ti, Nb or N appear, they are intentional levers for SUS347HTP, not optional marketing. Confirm them on the MTC line-by-line. Role: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS347HTP before the order is acknowledged. This paragraph is locked to SUS347HTP duty: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping.

Grade C Si Mn P S Ni Cr Nb
SUS347HTP 0.04–0.10 ≤1.00 ≤2.00 ≤0.030 ≤0.030 9.00–13.00 17.00–20.00 8×C%–1.00

Mechanical Properties of JIS G3459 SUS347HTP

Do not confuse Table 4 pipe tensile floors with plate or tube standards that share the 347H / UNS S34709 alias. For SUS347HTP under G3459 expect Rm min 520 N/mm², proof stress min 205 N/mm², elongation (No.11/12 longitudinal) min 35%, verified per heat/lot rules in clause 13. Tensile sampling follows clause 13 for the ordered test unit of SUS347HTP, and retests follow clause 14 when a result sits under the Table 4 floor. Weld-shop note tied to SUS347HTP: 347H fillers; confirm any austenite grain-size requirement on the order.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A No.11/12 long. min (%) A No.5 trans. min (%) A No.4 long. min (%) A No.4 trans. min (%)
SUS347HTP 520 205 35 25 30 22

Ambient values from JIS G3459:2021 Table 4 for SUS347HTP. Heat treatment (Table 2): Cold finish 1095 °C min / hot finish 1050 °C min, rapid cool. Elongation reductions apply for walls under 8 mm; elongation is not mandatory below 40 mm OD (record unless agreed). Note: hot-finished SUS321TP / SUS321HTP may use 460 / 180 N/mm² by agreement.

Manufacture of JIS G3459 SUS347HTP Pipe (Seamless and Welded)

JIS G3459 manufactures SUS347HTP by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, weld-bead worked B, or ERW-as-welded G. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.

Welded SUS347HTP needs weld-bead work or as-welded finish called out (B vs G) so NDT and corrosion expectations match. Heat treatment: Cold finish 1095 °C min / hot finish 1050 °C min, rapid cool. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it.

Hydrostatic testing or NDT (eddy current / ultrasonic per JIS G 0582/0583) replaces or accompanies pressure proof as the order states. Manufacture stays honest to the S/A/L/E choice. Size: seamless elevated-temperature sizes; heavy walls usually hot finished. Hydrostatic pressure or NDT class for SUS347HTP is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Application context for SUS347HTP stays high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems.

Dimensions and Tolerances for JIS G3459 SUS347HTP

Out-of-table OD×wall combinations are by agreement — still under the same grade symbol SUS347HTP. Duty: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping. Tolerance class follows the process route ordered for SUS347HTP, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside SUS347HTP: Nb stabilisation plus carbon floor for hot service; aqueous chlorides still want Mo or duplex.

Ovality, wall eccentricity (where applicable), and weld bead height limits are part of clause 10 — not optional cosmetics. Size reminder: seamless elevated-temperature sizes; heavy walls usually hot finished. Fixed lengths and multiple cut lengths for SUS347HTP are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS347HTP caution visible here: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply.

Equivalent Grades for JIS G3459 SUS347HTP

European EN pipe/tube numbers and ASTM marks may sit near 347H / UNS S34709, yet hydrostatic, NDT and heat-treatment text diverge. Keep SUS347HTP as the governing symbol unless a written dual-cert plan exists. Caution: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply.

Heat Treatment and Delivery Condition for JIS G3459 SUS347HTP

Hot-finished seamless austenitics may use in-line rapid cool in lieu of a separate solution treatment under Table 2 note (a) unless the purchaser forbids it. Confirm for SUS347HTP. Band: Cold finish 1095 °C min / hot finish 1050 °C min, rapid cool. Recorded furnace charts for SUS347HTP should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the SUS347HTP caution visible here: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply.

Grain-size testing applies where the standard requires it for specific H grades — state any extra metallographic demand on the PO for SUS347HTP. Field heat treatment of SUS347HTP after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside SUS347HTP: Nb stabilisation plus carbon floor for hot service; aqueous chlorides still want Mo or duplex.

Corrosion Resistance of JIS G3459 SUS347HTP

Medium, temperature, crevice geometry and weld condition decide whether SUS347HTP is enough. Summary: Nb stabilisation plus carbon floor for hot service; aqueous chlorides still want Mo or duplex. Escalate via sisters SUS347TP, SUS321HTP, SUS304HTP, SUS316HTP when coupons fail. Coupon orientation, weld condition, and surface finish for SUS347HTP belong in the corrosion test order so annex results can be compared to the installed spool honestly. Application context for SUS347HTP stays high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems.

Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for SUS347HTP. Corrosion framing: Nb stabilisation plus carbon floor for hot service; aqueous chlorides still want Mo or duplex. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS347HTP rather than relying on schedule thickness alone. Corrosion framing beside SUS347HTP: Nb stabilisation plus carbon floor for hot service; aqueous chlorides still want Mo or duplex.

Applications of JIS G3459 SUS347HTP Pipe

From utility rooms to process racks, SUS347HTP shows up wherever Japanese piping specs want austenitic behaviour. Use list: high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems. Spool fabricators should copy SUS347HTP onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Weld-shop note tied to SUS347HTP: 347H fillers; confirm any austenite grain-size requirement on the order.

If the only reason for SUS347HTP is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply. Commissioning teams benefit when the as-built dossier repeats SUS347HTP beside heat numbers, linking isometric revisions to the same mill certificates. Application context for SUS347HTP stays high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems.

Weldability of JIS G3459 SUS347HTP

Automatic mill welds and manual field welds need different procedure packs, but both must respect SUS347HTP chemistry. Guidance: 347H fillers; confirm any austenite grain-size requirement on the order. Procedure qualification for SUS347HTP should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. This paragraph is locked to SUS347HTP duty: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping.

Ferrite control on duplex SUS347HTP and hot-crack control on high-Ni austenitics are procedure items, not afterthoughts. Guidance: 347H fillers; confirm any austenite grain-size requirement on the order. Consumable lot control and shielding-gas notes for SUS347HTP stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Application context for SUS347HTP stays high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems.

Surface Finishes for JIS G3459 SUS347HTP

Welded pipe may need bead dressing for flow or inspection; call that out rather than assuming mill habit. Size/finish context: seamless elevated-temperature sizes; heavy walls usually hot finished. Roughness or polish callouts for SUS347HTP must name OD, ID, or both; ambiguous “bright pipe” language is clarified before finishing slots are booked. Application context for SUS347HTP stays high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems.

Do not polish over unresolved weld defects — inspection comes before cosmetics on SUS347HTP. Final visual standards for SUS347HTP reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Keep the SUS347HTP caution visible here: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply.

Inspection and Testing for JIS G3459 SUS347HTP

Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks G3459 for SUS347HTP. Sampling plans for SUS347HTP keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the SUS347HTP caution visible here: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply.

Dimensional inspection against clause 10 tolerances closes the lot. Failures retest per clause 14 — they are not silently shipped. Role: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping. Non-conforming SUS347HTP lengths are segregated and retested or rejected under clause 14 rather than reworked into unmarked stock. Size practice for SUS347HTP remains seamless elevated-temperature sizes; heavy walls usually hot finished.

Packaging and Shipping for JIS G3459 SUS347HTP

Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark SUS347HTP stays visible on outer tags. Bundle tickets for SUS347HTP repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to SUS347HTP duty: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping.

Container loading plans should keep heavy schedules from crushing thin-wall SUS347HTP layers. Desiccant and wrap choices for SUS347HTP follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS347HTP stays high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems Desiccant and wrap choices for SUS347HTP follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Order-line discipline for SUS347HTP still points at role: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping.

Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read SUS347HTP. Claims handling for SUS347HTP starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside SUS347HTP: Nb stabilisation plus carbon floor for hot service; aqueous chlorides still want Mo or duplex.

Why Choose SHH STEEL

From RFQ clarification through MTC release, SHH STEEL treats SUS347HTP as a governed product symbol, not a marketing synonym for 347H / UNS S34709. Role: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping. SHH STEEL can produce and supply SUS347HTP against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.

Response time stays short because common SUS347HTP enquiry sizes and document packs are already exercised on prior Japanese-spec orders. Use: high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems. Ask for a written acknowledgement that names SUS347HTP, the Table 1 process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS347HTP to that written scope.

Supply Capability

Capability framing for SUS347HTP: Japanese-spec piping product, dual-route manufacture, documented heats. Caution remains: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS347HTP when the mill schedule allows.

Item Capability
Standard JIS G3459:2021 stainless steel pipes
Grade symbol SUS347HTP
Product form Seamless (S) and welded (A / L / E) pipe; finishes H / C / B / G
Delivery condition solution annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 10.5–660.4 mm (6A–650A) per standard Note 1; other by agreement
Wall / schedule Schedule 5S–160 class and measured wall within family practice

Stock / Available sizes

Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of SUS347HTP change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping. SHH STEEL can supply alternate schedules and measured walls for SUS347HTP once the design pressure and corrosion allowance are clear.

Repeat orders for SUS347HTP go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping. SHH STEEL can produce trial lengths of SUS347HTP for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS347HTP for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to SUS347HTP: 347H fillers; confirm any austenite grain-size requirement on the order.

FAQ

What is JIS G3459 SUS347HTP stainless steel pipe used for?
JIS G3459 SUS347HTP is stainless pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — high-temperature refinery headers, hot chemical transfer, and heat-facing Nb-stabilised systems. Role summary: controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping. It is a Japanese product standard mark, not an automatic ASTM A312 certificate.
Does JIS G3459 SUS347HTP cover seamless and welded pipe?
Yes. Table 1 allows seamless (S) and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish symbols H/C/B/G. SHH STEEL can produce and supply either route for SUS347HTP when the mill can meet the ordered size and tests. The title omits Seamless/Welded because the standard itself covers both — the PO must still name the process symbol.
What heat treatment applies to SUS347HTP?
SUS347HTP is delivered solution annealed under JIS G3459. Table 2 reference: Cold finish 1095 °C min / hot finish 1050 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS347HTP compare with sister grades SUS347TP, SUS321HTP, SUS304HTP?
SUS347HTP is filed as austenitic. Typical sisters on the same RFQ are SUS347TP, SUS321HTP, SUS304HTP. Design caution: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply Pick the sister when the medium or strength floor outgrows this symbol rather than stretching schedule alone.
What tests appear on the mill certificate for SUS347HTP?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 347H / UNS S34709 the same as ordering SUS347HTP?
No. 347H / UNS S34709 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3459 and SUS347HTP so cast limits, heat treatment, and process symbols are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3459 SUS347HTP?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS347HTP within the typical 10.5–660.4 mm OD practice, with schedules or measured walls by agreement. Size context: seamless elevated-temperature sizes; heavy walls usually hot finished. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS347HTP be welded?
Shop guidance: 347H fillers; confirm any austenite grain-size requirement on the order. Mill heat treatment of seamless or welded pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply
When should I choose a duplex or higher-Mo grade instead of SUS347HTP?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Table 2 cold-finish 1095 °C vs hot-finish 1050 °C solution bands — name the finish; grain-size testing may apply Sister pointers: SUS347TP, SUS321HTP, SUS304HTP. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3459 SUS347HTP with ASTM A312 or A789?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3459 SUS347HTP does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS347HTP?
Pickled after heat treatment is the usual piping supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS347HTP when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3459 SUS347HTP is stainless steel pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — controlled-carbon Nb-stabilised pipe for elevated-temperature stabilised austenitic piping. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS347TP, SUS321HTP, SUS304HTP. Related ASTM pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process symbol, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X