JIS G3459 SUS444TP Stainless Steel Pipe | JIS G3459 Stainless Steel Pipe - SHH STEEL

JIS G3459 SUS444TP Stainless Steel Pipe

JIS G3459 SUS444TP stainless steel pipe (444 / UNS S44400), ferritic, Table 3 cast analysis, Rm min 410 N/mm² / proof min 245 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS444TP (444 / UNS S44400 — body alias)
Standard
JIS G3459:2021
Product form
Seamless and welded stainless steel pipe, delivery annealed
Size
Typically OD 10.5–660.4 mm (6A–650A); schedule or measured wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3459 SUS444TP Stainless Steel Pipe

When the approved vendor list and isometric notes say JIS G3459, the grade mark has to carry the TP suffix. SUS444TP is the full product symbol for this ferritic pipe. SUS444TP is the ferritic G3459 grade buyers reach for when they want near-316L water performance without austenitic nickel. Buyers working Japanese piping packages should treat SUS444TP as a governed product symbol under G3459:2021, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Size practice for SUS444TP remains welded water-pipe sizes common; seamless for thicker mechanical needs.

SHH STEEL can supply SUS444TP pipe in seamless S or welded A/L/E routes, with plain or bevelled ends, random or cut lengths, and EN 10204 / JIS G 0415 style inspection documents when specified. Role on the line: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS444TP before production starts. Keep the SUS444TP caution visible here: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute.

Equivalence talk to 444 / UNS S44400 belongs in engineering notes, not as a substitute for the JIS symbol. Lock JIS G3459 SUS444TP, OD × wall, process/finish symbols, and any special quality annex items before melt. Watch-out: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute.

Related ASTM pipe pages share chemistry families but not Japanese acceptance text — confirm before dual-cert claims. Sisters on this hub: SUS436LTP, SUS430J1LTP, SUS430LXTP, SUS316LTP. Use thread: hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water. Document the medium, design temperature, and weld map beside the SUS444TP line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for SUS444TP remains welded water-pipe sizes common; seamless for thicker mechanical needs.

Inside this JIS G3459 series, compare SUS436LTP, SUS430J1LTP, SUS430LXTP, SUS316LTP. Hub: JIS G3459.

Chemical Composition of JIS G3459 SUS444TP

Chemistry control on SUS444TP starts at the ladle. Expect C ≤0.025, Si ≤1.00, Mn ≤1.00, P ≤0.040, S ≤0.030, Ni ≤0.60, Cr 17.00–20.00 within Table 3, reported on the inspection document against the heat. Body alias 444 / UNS S44400 does not widen those windows. Every ladle analysis for SUS444TP is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Keep the SUS444TP caution visible here: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute.

Read the table with the family in mind — ferritic — and with caution ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute. Numbers without the matching heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS444TP before the order is acknowledged. Weld-shop note tied to SUS444TP: 444-class fillers; strict heat-input control; anneal when corrosion-critical.

Grade C Si Mn P S Ni Cr Mo N Ti/Nb/Zr
SUS444TP ≤0.025 ≤1.00 ≤1.00 ≤0.040 ≤0.030 ≤0.60 17.00–20.00 1.75–2.50 ≤0.025 8×(C%+N%)–0.80

Mechanical Properties of JIS G3459 SUS444TP

Proof stress and tensile minima for SUS444TP sit at Rm min 410 N/mm², proof stress min 245 N/mm², elongation (No.11/12 longitudinal) min 20%. Flattening or weld-guide-bend testing backs ductility for the ordered process route. Watch-out: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute. Tensile sampling follows clause 13 for the ordered test unit of SUS444TP, and retests follow clause 14 when a result sits under the Table 4 floor. Size practice for SUS444TP remains welded water-pipe sizes common; seamless for thicker mechanical needs.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A No.11/12 long. min (%) A No.5 trans. min (%) A No.4 long. min (%) A No.4 trans. min (%)
SUS444TP 410 245 20 14 16 11

Ambient values from JIS G3459:2021 Table 4 for SUS444TP. Heat treatment (Table 2): Annealing 700 °C min, rapid or slow cool. Elongation reductions apply for walls under 8 mm; elongation is not mandatory below 40 mm OD (record unless agreed). Note: hot-finished SUS321TP / SUS321HTP may use 460 / 180 N/mm² by agreement.

Manufacture of JIS G3459 SUS444TP Pipe (Seamless and Welded)

Both seamless and welded SUS444TP are legitimate under JIS G3459. Pick S when the design pressure, wall, or NDT plan favours a pierced/drawn route; pick A, L, or E when welded economics fit and the weld procedure is qualified. Finish symbols H/C/B/G ride with the process mark on the pipe stencil. Seamless and welded options remain available for SUS444TP; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Application context for SUS444TP stays hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water.

Process control for SUS444TP ends with verified heat treatment (Annealing 700 °C min, rapid or slow cool) and surface conditioning. Ferritic heats are annealed (700 °C min, or 720 °C min for SUS430J1LTP) with rapid or slow cooling as Table 2 allows — not austenitic solution practice. Pickling or bright-anneal decisions for SUS444TP stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. Weld-shop note tied to SUS444TP: 444-class fillers; strict heat-input control; anneal when corrosion-critical.

Bevel geometry for walls ≤22 mm defaults to the standard figure when bevels are ordered without a drawing. Size practice: welded water-pipe sizes common; seamless for thicker mechanical needs. Hydrostatic pressure or NDT class for SUS444TP is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Weld-shop note tied to SUS444TP: 444-class fillers; strict heat-input control; anneal when corrosion-critical.

Dimensions and Tolerances for JIS G3459 SUS444TP

Mass tables in JIS G3459 support schedule-based ordering for common austenitic marks; for SUS444TP, confirm whether your project uses schedule or measured wall. Context: welded water-pipe sizes common; seamless for thicker mechanical needs. Tolerance class follows the process route ordered for SUS444TP, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the SUS444TP caution visible here: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute.

For fire-protection and building services, schedule tables often drive the BOM; for process plants, measured wall and corrosion allowance dominate. SUS444TP supports both conversations when the PO is clear. Fixed lengths and multiple cut lengths for SUS444TP are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to SUS444TP duty: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel.

Equivalent Grades for JIS G3459 SUS444TP

Do not treat 444 / UNS S44400 as interchangeable paperwork. Chemistry kinship is not acceptance kinship. Inside this series see SUS436LTP, SUS430J1LTP, SUS430LXTP, SUS316LTP. Role: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel. When a dual-cert path is required, list both JIS G3459 SUS444TP and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. This paragraph is locked to SUS444TP duty: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel.

Heat Treatment and Delivery Condition for JIS G3459 SUS444TP

Stabilisation or special anneals, where the standard allows purchaser options (notably Ti/Nb grades), must be written on the order — silence means Table 2 defaults only. For SUS444TP: Annealing 700 °C min, rapid or slow cool. Recorded furnace charts for SUS444TP should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Size practice for SUS444TP remains welded water-pipe sizes common; seamless for thicker mechanical needs.

After local hot work in the field, restore annealed practice when the corrosion file demands it. Caution: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute. Field heat treatment of SUS444TP after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to SUS444TP: 444-class fillers; strict heat-input control; anneal when corrosion-critical.

Corrosion Resistance of JIS G3459 SUS444TP

Pick tests that match how SUS444TP is filed — ferritic. Corrosion thread: 1.75–2.50% Mo with Ti/Nb/Zr stabilisation delivers strong ferritic chloride resistance for many water duties. Caution: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute. Coupon orientation, weld condition, and surface finish for SUS444TP belong in the corrosion test order so annex results can be compared to the installed spool honestly. This paragraph is locked to SUS444TP duty: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel.

Fire-protection and potable-adjacent lines still need the right alloy — G3459 scope does not make every mark equal. Use thread: hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS444TP rather than relying on schedule thickness alone. Corrosion framing beside SUS444TP: 1.75–2.50% Mo with Ti/Nb/Zr stabilisation delivers strong ferritic chloride resistance for many water duties.

Applications of JIS G3459 SUS444TP Pipe

Project types that repeatedly call SUS444TP: hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water. Duty: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel. Caution still applies: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute. Spool fabricators should copy SUS444TP onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Application context for SUS444TP stays hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water.

Fire-protection headers, cryogenic-lean transfer and corrosive process lines all appear in G3459’s scope — alloy choice still follows the medium. For this mark: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel. Commissioning teams benefit when the as-built dossier repeats SUS444TP beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS444TP remains welded water-pipe sizes common; seamless for thicker mechanical needs.

Weldability of JIS G3459 SUS444TP

Even seamless S pipe of SUS444TP will see field welds. Use: 444-class fillers; strict heat-input control; anneal when corrosion-critical. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for SUS444TP should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Application context for SUS444TP stays hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water.

Dissimilar welds to carbon steel need buttering and dilution control — especially on heat-facing and Mo grades. Role context: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel. Consumable lot control and shielding-gas notes for SUS444TP stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the SUS444TP caution visible here: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute.

Surface Finishes for JIS G3459 SUS444TP

Iron-free handling after pickle matters — carbon-steel strapping stains show up later as rust blooms on SUS444TP. Finish thread tied to ferritic. Roughness or polish callouts for SUS444TP must name OD, ID, or both; ambiguous “bright pipe” language is clarified before finishing slots are booked. Size practice for SUS444TP remains welded water-pipe sizes common; seamless for thicker mechanical needs.

OD stencil ink and marking paint should be chloride-lean and removable where coating systems follow. Role: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel. Final visual standards for SUS444TP reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Weld-shop note tied to SUS444TP: 444-class fillers; strict heat-input control; anneal when corrosion-critical.

Inspection and Testing for JIS G3459 SUS444TP

Clause 13/14 define sampling and retests. For SUS444TP, keep the heat/lot identity unbroken from melt to bundle tag. Duty: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel. Sampling plans for SUS444TP keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the SUS444TP caution visible here: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute.

Intergranular corrosion testing is annex/special — order it when polythionic or weld-decay risk is written into the duty file for SUS444TP. Non-conforming SUS444TP lengths are segregated and retested or rejected under clause 14 rather than reworked into unmarked stock. Keep the SUS444TP caution visible here: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute.

Packaging and Shipping for JIS G3459 SUS444TP

Small-OD SUS444TP often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water. Bundle tickets for SUS444TP repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside SUS444TP: 1.75–2.50% Mo with Ti/Nb/Zr stabilisation delivers strong ferritic chloride resistance for many water duties.

Bevelled ends get protectors so landing edges survive trucking. Size hint: welded water-pipe sizes common; seamless for thicker mechanical needs. Desiccant and wrap choices for SUS444TP follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS444TP stays hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water.

Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water. Claims handling for SUS444TP starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to SUS444TP duty: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel.

Why Choose SHH STEEL

Project teams working to Japanese piping specs need a supplier that reads TP suffixes correctly. SHH STEEL can make SUS444TP to that discipline. Caution we keep visible: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute. SHH STEEL can produce and supply SUS444TP against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.

Dual-cert discussions (JIS + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: SUS436LTP, SUS430J1LTP, SUS430LXTP, SUS316LTP. Ask for a written acknowledgement that names SUS444TP, the Table 1 process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS444TP to that written scope.

Supply Capability

Whether you need prototype spools or project tonnage of SUS444TP, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS444TP when the mill schedule allows.

Item Capability
Standard JIS G3459:2021 stainless steel pipes
Grade symbol SUS444TP
Product form Seamless (S) and welded (A / L / E) pipe; finishes H / C / B / G
Delivery condition annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 10.5–660.4 mm (6A–650A) per standard Note 1; other by agreement
Wall / schedule Schedule 5S–160 class and measured wall within family practice

Stock / Available sizes

Stock / Available sizes: SHH STEEL quotes rolling/welding slots for SUS444TP rather than promising anonymous warehouse tons. Typical conversation starts around welded water-pipe sizes common; seamless for thicker mechanical needs. SHH STEEL can supply alternate schedules and measured walls for SUS444TP once the design pressure and corrosion allowance are clear. SHH STEEL can supply alternate schedules and measured walls for SUS444TP once design pressure and corrosion allowance are clear. This paragraph is locked to SUS444TP duty: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel.

If the project needs dual JIS G3459 + ASTM documentation, say so before melt. Caution: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute. SHH STEEL can produce trial lengths of SUS444TP for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS444TP for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to SUS444TP: 444-class fillers; strict heat-input control; anneal when corrosion-critical.

FAQ

What is JIS G3459 SUS444TP stainless steel pipe used for?
JIS G3459 SUS444TP is stainless pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — hot water, solar thermal, food equipment, mildly chlorinated water, and nickel-sensitive process water. Role summary: Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel. It is a Japanese product standard mark, not an automatic ASTM A312 certificate.
Does JIS G3459 SUS444TP cover seamless and welded pipe?
Yes. Table 1 allows seamless (S) and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish symbols H/C/B/G. SHH STEEL can produce and supply either route for SUS444TP when the mill can meet the ordered size and tests. The title omits Seamless/Welded because the standard itself covers both — the PO must still name the process symbol.
What heat treatment applies to SUS444TP?
SUS444TP is delivered annealed under JIS G3459. Table 2 reference: Annealing 700 °C min, rapid or slow cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS444TP compare with sister grades SUS436LTP, SUS430J1LTP, SUS430LXTP?
SUS444TP is filed as ferritic. Typical sisters on the same RFQ are SUS436LTP, SUS430J1LTP, SUS430LXTP. Design caution: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute Pick the sister when the medium or strength floor outgrows this symbol rather than stretching schedule alone.
What tests appear on the mill certificate for SUS444TP?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 444 / UNS S44400 the same as ordering SUS444TP?
No. 444 / UNS S44400 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3459 and SUS444TP so cast limits, heat treatment, and process symbols are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3459 SUS444TP?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS444TP within the typical 10.5–660.4 mm OD practice, with schedules or measured walls by agreement. Size context: welded water-pipe sizes common; seamless for thicker mechanical needs. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS444TP be welded?
Shop guidance: 444-class fillers; strict heat-input control; anneal when corrosion-critical. Mill heat treatment of seamless or welded pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute
When should I choose a duplex or higher-Mo grade instead of SUS444TP?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: ferritic welding and toughness limits remain — not a cryogenic or heavily cold-formed austenitic substitute Sister pointers: SUS436LTP, SUS430J1LTP, SUS430LXTP. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3459 SUS444TP with ASTM A312 or A789?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3459 SUS444TP does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS444TP?
Pickled after heat treatment is the usual piping supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS444TP when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3459 SUS444TP is stainless steel pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — Mo-stabilised ferritic pipe that often approaches 316L aqueous performance without nickel. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS436LTP, SUS430J1LTP, SUS430LXTP. Related ASTM pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process symbol, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X