JIS G3459 SUS310TP Stainless Steel Pipe | JIS G3459 Stainless Steel Pipe - SHH STEEL

JIS G3459 SUS310TP Stainless Steel Pipe

JIS G3459 SUS310TP stainless steel pipe (310 / high-Cr-Ni), austenitic, Table 3 cast analysis, Rm min 520 N/mm² / proof min 205 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS310TP (310 / high-Cr-Ni — body alias)
Standard
JIS G3459:2021
Product form
Seamless and welded stainless steel pipe, delivery solution annealed
Size
Typically OD 10.5–660.4 mm (6A–650A); schedule or measured wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3459 SUS310TP Stainless Steel Pipe

When the approved vendor list and isometric notes say JIS G3459, the grade mark has to carry the TP suffix. SUS310TP is the full product symbol for this austenitic pipe. JIS G3459 SUS310TP is what Japanese heat-equipment specs reach for when 309 still looks thin on chromium and nickel. Buyers working Japanese piping packages should treat SUS310TP as a governed product symbol under G3459:2021, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Application context for SUS310TP stays radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters.

SHH STEEL can supply SUS310TP pipe in seamless S or welded A/L/E routes, with plain or bevelled ends, random or cut lengths, and EN 10204 / JIS G 0415 style inspection documents when specified. Role on the line: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS310TP before production starts. Application context for SUS310TP stays radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters.

Equivalence talk to 310 / high-Cr-Ni belongs in engineering notes, not as a substitute for the JIS symbol. Lock JIS G3459 SUS310TP, OD × wall, process/finish symbols, and any special quality annex items before melt. Watch-out: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters.

Related ASTM pipe pages share chemistry families but not Japanese acceptance text — confirm before dual-cert claims. Sisters on this hub: SUS310STP, SUS309TP, SUS309STP, SUS321HTP. Use thread: radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters. Document the medium, design temperature, and weld map beside the SUS310TP line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. This paragraph is locked to SUS310TP duty: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service.

Inside this JIS G3459 series, compare SUS310STP, SUS309TP, SUS309STP, SUS321HTP. Hub: JIS G3459.

Chemical Composition of JIS G3459 SUS310TP

Chemistry control on SUS310TP starts at the ladle. Expect C ≤0.15, Si ≤1.50, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 19.00–22.00, Cr 24.00–26.00 within Table 3, reported on the inspection document against the heat. Body alias 310 / high-Cr-Ni does not widen those windows. Every ladle analysis for SUS310TP is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Keep the SUS310TP caution visible here: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters.

Read the table with the family in mind — austenitic — and with caution carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters. Numbers without the matching heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS310TP before the order is acknowledged. This paragraph is locked to SUS310TP duty: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service.

Grade C Si Mn P S Ni Cr
SUS310TP ≤0.15 ≤1.50 ≤2.00 ≤0.040 ≤0.030 19.00–22.00 24.00–26.00

Mechanical Properties of JIS G3459 SUS310TP

Proof stress and tensile minima for SUS310TP sit at Rm min 520 N/mm², proof stress min 205 N/mm², elongation (No.11/12 longitudinal) min 35%. Flattening or weld-guide-bend testing backs ductility for the ordered process route. Watch-out: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A No.11/12 long. min (%) A No.5 trans. min (%) A No.4 long. min (%) A No.4 trans. min (%)
SUS310TP 520 205 35 25 30 22

Ambient values from JIS G3459:2021 Table 4 for SUS310TP. Heat treatment (Table 2): 1030 °C min, rapid cool. Elongation reductions apply for walls under 8 mm; elongation is not mandatory below 40 mm OD (record unless agreed). Note: hot-finished SUS321TP / SUS321HTP may use 460 / 180 N/mm² by agreement.

Manufacture of JIS G3459 SUS310TP Pipe (Seamless and Welded)

Both seamless and welded SUS310TP are legitimate under JIS G3459. Pick S when the design pressure, wall, or NDT plan favours a pierced/drawn route; pick A, L, or E when welded economics fit and the weld procedure is qualified. Finish symbols H/C/B/G ride with the process mark on the pipe stencil. Seamless and welded options remain available for SUS310TP; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Keep the SUS310TP caution visible here: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters.

Process control for SUS310TP ends with verified heat treatment (1030 °C min, rapid cool) and surface conditioning. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Pickling or bright-anneal decisions for SUS310TP stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. Application context for SUS310TP stays radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters.

Bevel geometry for walls ≤22 mm defaults to the standard figure when bevels are ordered without a drawing. Size practice: heavy-wall seamless dominates furnace RFQs; large-OD welded pipe for ducting by agreement. Hydrostatic pressure or NDT class for SUS310TP is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Size practice for SUS310TP remains heavy-wall seamless dominates furnace RFQs; large-OD welded pipe for ducting by agreement.

Dimensions and Tolerances for JIS G3459 SUS310TP

Mass tables in JIS G3459 support schedule-based ordering for common austenitic marks; for SUS310TP, confirm whether your project uses schedule or measured wall. Context: heavy-wall seamless dominates furnace RFQs; large-OD welded pipe for ducting by agreement. Tolerance class follows the process route ordered for SUS310TP, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to SUS310TP: 310/310L fillers; control heat input on thick walls to limit hot cracking risk.

For fire-protection and building services, schedule tables often drive the BOM; for process plants, measured wall and corrosion allowance dominate. SUS310TP supports both conversations when the PO is clear. Fixed lengths and multiple cut lengths for SUS310TP are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to SUS310TP duty: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service.

Equivalent Grades for JIS G3459 SUS310TP

Do not treat 310 / high-Cr-Ni as interchangeable paperwork. Chemistry kinship is not acceptance kinship. Inside this series see SUS310STP, SUS309TP, SUS309STP, SUS321HTP. Role: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service. When a dual-cert path is required, list both JIS G3459 SUS310TP and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. This paragraph is locked to SUS310TP duty: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service.

Heat Treatment and Delivery Condition for JIS G3459 SUS310TP

Stabilisation or special anneals, where the standard allows purchaser options (notably Ti/Nb grades), must be written on the order — silence means Table 2 defaults only. For SUS310TP: 1030 °C min, rapid cool. Recorded furnace charts for SUS310TP should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside SUS310TP: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is a secondary concern.

After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters. Field heat treatment of SUS310TP after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for SUS310TP stays radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters.

Corrosion Resistance of JIS G3459 SUS310TP

Pick tests that match how SUS310TP is filed — austenitic. Corrosion thread: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is a secondary concern. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters. Coupon orientation, weld condition, and surface finish for SUS310TP belong in the corrosion test order so annex results can be compared to the installed spool honestly. Weld-shop note tied to SUS310TP: 310/310L fillers; control heat input on thick walls to limit hot cracking risk.

Fire-protection and potable-adjacent lines still need the right alloy — G3459 scope does not make every mark equal. Use thread: radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS310TP rather than relying on schedule thickness alone. Corrosion framing beside SUS310TP: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is a secondary concern.

Applications of JIS G3459 SUS310TP Pipe

Project types that repeatedly call SUS310TP: radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters. Duty: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service. Caution still applies: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters.

Fire-protection headers, cryogenic-lean transfer and corrosive process lines all appear in G3459’s scope — alloy choice still follows the medium. For this mark: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service. Commissioning teams benefit when the as-built dossier repeats SUS310TP beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS310TP remains heavy-wall seamless dominates furnace RFQs; large-OD welded pipe for ducting by agreement.

Weldability of JIS G3459 SUS310TP

Even seamless S pipe of SUS310TP will see field welds. Use: 310/310L fillers; control heat input on thick walls to limit hot cracking risk. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for SUS310TP should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. This paragraph is locked to SUS310TP duty: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service.

Dissimilar welds to carbon steel need buttering and dilution control — especially on heat-facing and Mo grades. Role context: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service. Consumable lot control and shielding-gas notes for SUS310TP stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the SUS310TP caution visible here: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters.

Surface Finishes for JIS G3459 SUS310TP

Iron-free handling after pickle matters — carbon-steel strapping stains show up later as rust blooms on SUS310TP. Finish thread tied to austenitic. Roughness or polish callouts for SUS310TP must name OD, ID, or both; ambiguous “bright pipe” language is clarified before finishing slots are booked. Weld-shop note tied to SUS310TP: 310/310L fillers; control heat input on thick walls to limit hot cracking risk.

OD stencil ink and marking paint should be chloride-lean and removable where coating systems follow. Role: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service. Final visual standards for SUS310TP reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Corrosion framing beside SUS310TP: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is a secondary concern.

Inspection and Testing for JIS G3459 SUS310TP

Clause 13/14 define sampling and retests. For SUS310TP, keep the heat/lot identity unbroken from melt to bundle tag. Duty: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service. Sampling plans for SUS310TP keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to SUS310TP duty: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service.

Intergranular corrosion testing is annex/special — order it when polythionic or weld-decay risk is written into the duty file for SUS310TP. Non-conforming SUS310TP lengths are segregated and retested or rejected under clause 14 rather than reworked into unmarked stock. Keep the SUS310TP caution visible here: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters.

Packaging and Shipping for JIS G3459 SUS310TP

Small-OD SUS310TP often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters. Bundle tickets for SUS310TP repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside SUS310TP: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is a secondary concern.

Bevelled ends get protectors so landing edges survive trucking. Size hint: heavy-wall seamless dominates furnace RFQs; large-OD welded pipe for ducting by agreement. Desiccant and wrap choices for SUS310TP follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside SUS310TP: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is a secondary concern.

Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters. Claims handling for SUS310TP starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to SUS310TP: 310/310L fillers; control heat input on thick walls to limit hot cracking risk.

Why Choose SHH STEEL

Project teams working to Japanese piping specs need a supplier that reads TP suffixes correctly. SHH STEEL can make SUS310TP to that discipline. Caution we keep visible: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters. SHH STEEL can produce and supply SUS310TP against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.

Dual-cert discussions (JIS + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: SUS310STP, SUS309TP, SUS309STP, SUS321HTP. Ask for a written acknowledgement that names SUS310TP, the Table 1 process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS310TP to that written scope.

Supply Capability

Whether you need prototype spools or project tonnage of SUS310TP, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS310TP when the mill schedule allows.

Item Capability
Standard JIS G3459:2021 stainless steel pipes
Grade symbol SUS310TP
Product form Seamless (S) and welded (A / L / E) pipe; finishes H / C / B / G
Delivery condition solution annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 10.5–660.4 mm (6A–650A) per standard Note 1; other by agreement
Wall / schedule Schedule 5S–160 class and measured wall within family practice

Stock / Available sizes

Stock / Available sizes: SHH STEEL quotes rolling/welding slots for SUS310TP rather than promising anonymous warehouse tons. Typical conversation starts around heavy-wall seamless dominates furnace RFQs; large-OD welded pipe for ducting by agreement. SHH STEEL can supply alternate schedules and measured walls for SUS310TP once the design pressure and corrosion allowance are clear.

If the project needs dual JIS G3459 + ASTM documentation, say so before melt. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters. SHH STEEL can produce trial lengths of SUS310TP for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is JIS G3459 SUS310TP stainless steel pipe used for?
JIS G3459 SUS310TP is stainless pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — radiant-tube adjacent piping, sulphur-bearing hot gas lines, cement kiln ducts, and high-temperature process heaters. Role summary: 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service. It is a Japanese product standard mark, not an automatic ASTM A312 certificate.
Does JIS G3459 SUS310TP cover seamless and welded pipe?
Yes. Table 1 allows seamless (S) and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish symbols H/C/B/G. SHH STEEL can produce and supply either route for SUS310TP when the mill can meet the ordered size and tests. The title omits Seamless/Welded because the standard itself covers both — the PO must still name the process symbol.
What heat treatment applies to SUS310TP?
SUS310TP is delivered solution annealed under JIS G3459. Table 2 reference: 1030 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS310TP compare with sister grades SUS310STP, SUS309TP, SUS309STP?
SUS310TP is filed as austenitic. Typical sisters on the same RFQ are SUS310STP, SUS309TP, SUS309STP. Design caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters Pick the sister when the medium or strength floor outgrows this symbol rather than stretching schedule alone.
What tests appear on the mill certificate for SUS310TP?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 310 / high-Cr-Ni the same as ordering SUS310TP?
No. 310 / high-Cr-Ni is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3459 and SUS310TP so cast limits, heat treatment, and process symbols are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3459 SUS310TP?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS310TP within the typical 10.5–660.4 mm OD practice, with schedules or measured walls by agreement. Size context: heavy-wall seamless dominates furnace RFQs; large-OD welded pipe for ducting by agreement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS310TP be welded?
Shop guidance: 310/310L fillers; control heat input on thick walls to limit hot cracking risk. Mill heat treatment of seamless or welded pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters
When should I choose a duplex or higher-Mo grade instead of SUS310TP?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STP when weld IGC matters Sister pointers: SUS310STP, SUS309TP, SUS309STP. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3459 SUS310TP with ASTM A312 or A789?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3459 SUS310TP does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS310TP?
Pickled after heat treatment is the usual piping supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS310TP when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3459 SUS310TP is stainless steel pipe for corrosion-resistant, low-temperature, high-temperature and fire-protection piping — 25Cr-20Ni austenitic pipe for severe oxidation and carburising-lean hot-gas service. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS310STP, SUS309TP, SUS309STP. Related ASTM pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process symbol, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X