JIS G 3106 SM490 Steel Channel
What is JIS G 3106 SM490 Steel Channel?
JIS G 3106 SM490 steel channel is a hot-rolled Japanese channel whose material grade is one of the SM490 qualities under JIS G 3106 — SM490A, SM490B, SM490C, SM490YA or SM490YB — and whose shape, mass and tolerances are ordered to JIS G 3192 Table 12. SM stands for rolled steel for welded structure, and 490 is the tensile-strength class (490–610 N/mm²). There is no suffixless grade in the standard called only “SM490”; the quality letter must be named on the order.
This page covers the SM490 family in channel form. The H-section sister is JIS G 3106 SM490 H-beam. A general-structure comparison on the same channel series is JIS G 3101 SS400 steel channel.
These bars are filed under steel channel profiles in the steel structural profiles category. They are designated H×B×t1×t2, for example 200×90×8×13. They are not GB/T 706 taper-flange channels, and they are not European UPN, UPE or PFC or American C or MC of a similar millimetre depth.
Material, Dimensions and the SM490 Quality Family
The purchase order and the inspection document should name, separately:
- JIS G 3106 and its edition (this page uses the 2020 edition as the numeric basis; the edition named on the order governs), and the full quality symbol SM490A, SM490B, SM490C, SM490YA or SM490YB;
- the JIS G 3192 channel designation (H×B×t1×t2);
- any agreed heat-treatment suffix and any agreed Ceq or PCM limit.
The standard allows thickness to be displayed as t1 only, but several depths share the same H and B with different web and flange thicknesses. The full H×B×t1×t2 string avoids mixing those sections.
SM490 Steel Channel Sizes: JIS G 3192 Table 12
The table is the complete standard channel series in JIS G 3192:2024 Table 12: 16 sizes, from 75×40×5×7 to 380×100×13×20. The tabulated dimensions are representative; other section dimensions may be used by agreement. A Japanese channel is not a GB/T 706 model or a European UPN of similar depth. Not every mill rolls every designation in every SM490 quality.
Swipe horizontally to view all dimensions.
SM490 Chemical Composition (Heat Analysis)
The figures below are heat-analysis maxima from JIS G 3106:2020 Table 2. For these channels the relevant thickness is that at the test-piece location, ordinarily the flange t2, not the overall depth H. In the Table 12 series t2 ranges from 7 mm to 20 mm, so the carbon steps above 50 mm are kept for a thicker special section or a relocated specimen written on the order, not because a tabulated flange already sits in that band.
Clause 7.2 Ceq and PCM tables in JIS G 3106:2020 apply to plates and sheets manufactured by a thermo-mechanical control process. They are not a default as-rolled channel CEV. If a Ceq or PCM limit is required on a section order, it must be agreed and stated on the certificate; no value is invented here.
SM490 Mechanical Properties: Yield, Tensile and 0 °C Impact
Tensile properties follow Table 7 of JIS G 3106:2020. Thickness is that at the location of the test pieces, ordinarily the flange t2. In the tabulated series t2 is 7 mm to 20 mm, so those rows sit in the first or second yield band when the flange is the test location. Later bands remain in the table for a thicker special section. Annex JB (leg length under 40 mm) does not apply: every Table 12 channel has a flange width B of 40 mm or more.
SM490YA and SM490YB use a higher yield table, still in the 490–610 N/mm² tensile class, with a standard section scope of 100 mm or less:
Elongation is as follows:
When impact testing applies (the symbols listed in Table 8, with thickness over 12 mm), the requirements are:
A lower test temperature may be agreed. An A or YA certificate does not demonstrate a 0 °C test, and a 27 J B result is not a 47 J C result. Some of the smaller tabulated flanges are 12 mm or thinner; clause 8.2 is written for thickness over 12 mm.
Delivery Conditions, Inspection and Identification
SM490 channels are commonly supplied as-rolled. Heat treatment, including normalizing or a thermo-mechanical control process, is used when agreed; any agreed suffix is added to the quality symbol. The inspection document should identify JIS G 3106 and its edition, the full quality symbol, the JIS G 3192 designation, heat analysis, and tensile results against the thickness at the test location, plus the Table 8 impact result for B, C or YB when that test applies. A plate or H-beam certificate does not, by itself, identify a channel.
Weldability of SM490 Steel Channels
SM490 is specified as a weldable rolled steel for welded structures. Preheat and consumable choice should use the certified heat analysis, any agreed Ceq or PCM, the actual thickness and the joint design. A CEV figure must not be read off a TMCP plate table as if it automatically applied to an as-rolled channel.
JIS G 3192 Shape Tolerances and Theoretical Mass
Shape, mass and tolerances belong to the ordered edition of JIS G 3192. Mass in the size table is the published theoretical figure. Millimetre tolerance tables are not reproduced here. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
SM490 channels are used in welded frames, bracing and similar work where a Japanese welded-structure grade in the 490 N/mm² tensile class is named. Choose the quality letter for the impact or yield table actually required. They are not a silent substitute for JIS G 3101 SS400 steel channel, for a GB/T 706 channel, or for a European UPN in S355JR.
SM490 Compared with SS400, Q355B and S355JR
The comparisons below are an orientation only; they are not automatic substitutes.
Near-Equivalents: Not Automatic Substitutes
A near-equivalent is a starting point for a discussion, not a licence to swap certificates. If a project names SM490B or SM490C, keep that quality letter and JIS G 3192 on the order. The H-section sister is JIS G 3106 SM490 H-beam.
Sourcing SM490 Steel Channels from SHH STEEL
SHH STEEL supplies JIS G 3106 SM490 steel channels against a named designation list, the quality letter, the material edition and the inspection document type. Enquiries should state the H×B×t1×t2 designations, the quality (A, B, C, YA or YB), cut lengths or mill lengths, any processing, and whether JIS G 3101 SS400 steel channel is acceptable on part of the list.
The size table is the standard series, not a claim that every designation is rolled in every quality. Once the list is clear, a quotation can be prepared against the stated edition and certificate.
SM490 Steel Channel FAQs
-
Is there a single grade called just SM490?
- No. The standard uses SM490A, SM490B, SM490C, SM490YA and SM490YB. A and YA have no standard Table 8 impact test. B and YB require 27 J at 0 °C when testing applies; C requires 47 J at 0 °C. YA and YB use a higher yield table.
-
Which thickness is used for yield and impact on a channel?
- Thickness is that at the location of the test pieces, ordinarily the flange t2, not the depth H. In the Table 12 series t2 ranges from 7 mm to 20 mm. Impact testing, when it applies, is written for thickness over 12 mm.
-
Does a Ceq table apply to every SM490 channel?
- No default as-rolled channel CEV is published in the same way as the TMCP plate tables in clause 7.2. If a Ceq or PCM limit is required on a section order, it should be agreed and written on the certificate.
-
Which edition of JIS G 3106 is used on this page?
- The numeric tables use JIS G 3106:2020. Dimensional sizes use JIS G 3192:2024 Table 12. A later edition of either standard may be named on the order; the ordered edition governs.
Request a Quotation for JIS G 3106 SM490 Steel Channel
JIS G 3106 SM490 steel channel is a welded-structure channel in the 490–610 N/mm² tensile class. Nominate the JIS G 3192 designation (H×B×t1×t2), the quality letter (A, B, C, YA or YB), JIS G 3106:2020 or the edition on the order, and the inspection document type. Send the size list, quality, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.