JIS G 3101 SS490 H Beam | JIS G 3101 H Beams - SHH STEEL

JIS G 3101 SS490 H Beam

JIS G 3101 SS490 H beam is named for a 490–610 N/mm² tensile range, not a 490 N/mm² yield. Yield is 285 N/mm² to 16 mm and 275 N/mm² from 16 to 40 mm, by flange. Sizes follow JIS G 3192 Table 15. This page is SS490 only, not SS400 or SM490. SHH STEEL reviews grade and certificate before quoting.
Keywords
JIS G 3101 SS490 H Beam, SS490 H-beam, SS490 JIS G 3192 H-section, SS490 285 N/mm² yield, Japanese SS490 H beam
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of JIS G 3101 SS490 H Beam
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source JIS G 3101 SS490 H Beams from SHH STEEL
FAQ
Conclusion

What is a JIS G 3101 SS490 H Beam?

A JIS G 3101 SS490 H beam is a general-structure rolled H-section whose material conforms to JIS G 3101 and whose standard sizes follow JIS G 3192 Table 15. The grade is named for a 490–610 N/mm² tensile range, not for a 490 N/mm² yield. Minimum yield is 285 N/mm² up to 16 mm and 275 N/mm² between 16 mm and 40 mm, based on flange thickness. This page is SS490 only, not SS400, SS540 or SM490.

This page covers the rolled H-section, not plate, not a channel, and not a JIS I-beam. I-beam dimensions from JIS G 3192 Table 11 are not tabulated here. The lower-tensile sister in the same standard, on the same Table 15 series, is JIS G 3101 SS400 H-Beam. JIS G 3106 SM490 H-Beam is a JIS G 3106 welded-structure grade, not a G 3101 general-structure grade.

These beams are filed under JIS G 3101 in H Beams and Wide Flange Beams, in the steel structural profiles category. Chinese HW/HM/HN and European HEA/HEB names are different series. A similar depth or mass is not a substitute designation.

SS490 H-sections are used in general building and fabrication where this tensile class is specified. JIS G 3101 does not specify a Charpy test for SS490; a toughness value must not be inferred from the grade name. They are not a weathering grade and not a pressure-vessel material.

Material, Dimensions and Tolerances for JIS G 3101 SS490 H-Sections

Two documents should appear, separately, on the purchase order and on the inspection certificate:

  • JIS G 3101 is the material standard for rolled steels for general structure. This article uses Table 2 chemistry and Table 3 mechanical values for SS490, with the issued 2015 figures recovered for chemistry and with JIS G 3101:2024 as the current listed edition. The edition named on the order governs acceptance. The SS490 row is the same chemistry row as SS330 and SS400: only phosphorus and sulfur have maxima.
  • JIS G 3192 is the dimensional standard. The size table below is the Table 15 standard H-section series, used as reference dimensions and theoretical masses, not a rolling list. Shape tolerances follow JIS G 3192, not G 3101.

Do not treat “SS490 H-beam” as if it automatically meant a square 300×300 section, and do not substitute a Chinese HW or a European HEB by matching a nominal 300 mm depth. JIS G 3101 SS400 H-Beam and JIS G 3101 SS540 H Beam share the Table 15 series but are different grades.

JIS G 3101 SS490 H-Beam Sizes: JIS G 3192 Table 15

The table lists the 53 standard H-sections of JIS G 3192 Table 15, from H 100×50×5×7 to H 918×303×19×37. The designation is written H × flange width × web thickness × flange thickness, in millimetres. Actual depth is not always the series name: H 148×100×6×9 belongs to the 150×100 series, and H 194×150×6×9 belongs to the 200×150 series. Within one series the inner depth is constant.

Thickness at the test-piece location, usually the flange, is what sets the SS490 yield. H 200×200×8×12 and H 300×300×10×15 have 12 mm and 15 mm flanges, so both remain in the 285 N/mm² band. H 350×350×12×19 has a 19 mm flange, so the minimum yield is 275 N/mm².

These figures are for identification and estimating, not a claim that every row is produced in SS490. Mid-range square and narrow H-sections are the usual enquiry core; rows marked * are identified in Table 15 as other than general-purpose and should be confirmed size by size. The tabulated dimensions are representative; other section sizes may be used by agreement.

Swipe horizontally to view all dimensions.

Designation (H×B×t1×t2) h (mm) b (mm) t1 (mm) t2 (mm) r (mm) A (cm²) Mass (kg/m)
H 100×50×5×7 100 50 5 7 8 11.85 9.30
H 100×100×6×8 100 100 6 8 8 21.59 16.9
H 125×60×6×8 125 60 6 8 8 16.69 13.1
H 125×125×6.5×9 125 125 6.5 9 8 30.00 23.6
H 150×75×5×7 150 75 5 7 8 17.85 14.0
H 148×100×6×9 148 100 6 9 8 26.35 20.7
H 150×150×7×10 150 150 7 10 8 39.65 31.1
H 175×90×5×8 175 90 5 8 8 22.90 18.0
H 175×175×7.5×11 175 175 7.5 11 13 51.43 40.4
* H 198×99×4.5×7 198 99 4.5 7 8 22.69 17.8
H 200×100×5.5×8 200 100 5.5 8 8 26.67 20.9
H 194×150×6×9 194 150 6 9 8 38.11 29.9
H 200×200×8×12 200 200 8 12 13 63.53 49.9
* H 248×124×5×8 248 124 5 8 8 31.99 25.1
H 250×125×6×9 250 125 6 9 8 36.97 29.0
H 244×175×7×11 244 175 7 11 13 55.49 43.6
H 250×250×9×14 250 250 9 14 13 91.43 71.8
* H 298×149×5.5×8 298 149 5.5 8 13 40.80 32.0
H 300×150×6.5×9 300 150 6.5 9 13 46.78 36.7
H 294×200×8×12 294 200 8 12 13 71.05 55.8
H 300×300×10×15 300 300 10 15 13 118.5 93.0
* H 346×174×6×9 346 174 6 9 13 52.45 41.2
H 350×175×7×11 350 175 7 11 13 62.91 49.4
H 340×250×9×14 340 250 9 14 13 99.53 78.1
H 350×350×12×19 350 350 12 19 13 171.9 135
* H 396×199×7×11 396 199 7 11 13 71.41 56.1
H 400×200×8×13 400 200 8 13 13 83.37 65.4
H 390×300×10×16 390 300 10 16 13 133.3 105
H 400×400×13×21 400 400 13 21 22 218.7 172
* H 414×405×18×28 414 405 18 28 22 295.4 232
* H 428×407×20×35 428 407 20 35 22 360.7 283
* H 458×417×30×50 458 417 30 50 22 528.6 415
* H 498×432×45×70 498 432 45 70 22 770.1 605
* H 446×199×8×12 446 199 8 12 13 82.97 65.1
H 450×200×9×14 450 200 9 14 13 95.43 74.9
H 440×300×11×18 440 300 11 18 13 153.9 121
* H 496×199×9×14 496 199 9 14 13 99.29 77.9
H 500×200×10×16 500 200 10 16 13 112.3 88.2
* H 482×300×11×15 482 300 11 15 13 141.2 111
H 488×300×11×18 488 300 11 18 13 159.2 125
* H 596×199×10×15 596 199 10 15 13 117.8 92.5
H 600×200×11×17 600 200 11 17 13 131.7 103
* H 582×300×12×17 582 300 12 17 13 169.2 133
H 588×300×12×20 588 300 12 20 13 187.2 147
* H 594×302×14×23 594 302 14 23 13 217.1 170
* H 692×300×13×20 692 300 13 20 18 207.5 163
H 700×300×13×24 700 300 13 24 18 231.5 182
* H 792×300×14×22 792 300 14 22 18 239.5 188
H 800×300×14×26 800 300 14 26 18 263.5 207
* H 890×299×15×23 890 299 15 23 18 266.9 210
H 900×300×16×28 900 300 16 28 18 305.8 240
* H 912×302×18×34 912 302 18 34 18 360.1 283
* H 918×303×19×37 918 303 19 37 18 387.4 304

Rows marked * are the 20 sizes that Table 15 identifies as other than general-purpose. Constant outside-dimension H-sections (JIS G 3192 Table 16) and I-beams can be reviewed when they are named on the enquiry; I-beam dimensions are not tabulated here. Chinese HW, HM and HN names belong to GB/T 11263; European HEA, HEB and IPE names belong to EN 10025-2 practice, not to this table. The live JIS G 3101 SS400 H-Beam page uses the same Table 15 series for a different grade.

JIS G 3101 SS490 Chemical Composition (Heat Analysis)

The ladle analysis shall comply with Table 2 of JIS G 3101, using the issued 2015 figures given below. JIS G 3101:2024 is the current listed edition; the edition named on the order governs. The SS490 row is the same row as SS330 and SS400: only phosphorus and sulfur have maxima. Carbon and manganese are shown as having no tabulated requirement. Silicon is not a tabulated column on that row. This page does not invent carbon or manganese windows from mill catalogues or from the SS540 row.

Element SS490 ladle analysis, Table 2 (mass %)
C No specified requirement
Mn No specified requirement
P, max 0.050
S, max 0.050

Elements shown as having no tabulated requirement, and alloying elements not listed in Table 2, may be added as necessary. Table 2 is a ladle-analysis table. The issued 2015 text recovered for this page specifies ladle analysis only and does not give a separate numeric product-analysis table. This page does not invent one.

JIS G 3101 SS490 Mechanical Properties: Yield, Tensile, Elongation and Bend

Mechanical properties of SS490 plates, strip, flats and sections follow Table 3 of the issued JIS G 3101:2015 text, which is a single mechanical table that includes plate, strip, flat, section and bar rows. These H-sections use the plate, strip, flat and section rows, not the bar rows. The recovered 2015 Table 3 notes do not add an upper-yield or 0.2% proof-stress instruction, and this page does not add one. Thickness for a section is the thickness at the test-piece location; on this page the usual basis for selecting a yield band is the flange thickness t2.

Property Table 3 requirement for SS490 sections
Minimum yield, t ≤ 16 mm 285 N/mm²
Minimum yield, 16 mm < t ≤ 40 mm 275 N/mm²
Minimum yield, 40 mm < t ≤ 100 mm 255 N/mm²
Minimum yield, t > 100 mm 245 N/mm²
Tensile strength, all those bands 490–610 N/mm²
Elongation, t ≤ 5 mm 19% min, test piece No. 5
Elongation, 5 mm < t ≤ 16 mm 15% min, test piece No. 1A
Elongation, 16 mm < t ≤ 50 mm 19% min, test piece No. 1A
Bend 180°, inner radius 2.0 × thickness, test piece No. 1 (No. 3 may be used at 5 mm and under)

A 2015 Table 3 note reduces the No. 4 elongation on plates thicker than 90 mm; that is a plate rule and is not extended here to invent a section value. This page does not reprint a No. 4 elongation percentage, because that figure was not recovered from the issued 2015 table image. The 255 N/mm² and 245 N/mm² yield bands do not appear among the tabulated G 3192 sizes on this page, all of which have a flange thickness of 20 mm or less. JIS G 3101 does not specify Charpy absorbed-energy values. The bend test may be omitted unless the purchaser specifies it; the steel still has to satisfy the bendability requirement, and the outside of the bend piece must be free of cracks.

Annex JA, which applies to sections with a leg length under 40 mm, is not used for the standard H-sections in the size table above, whose flange widths are 50 mm or more.

Delivery, Inspection and Identification of JIS G 3101 SS490 H Beams

SS490 H-sections are commonly delivered in the as-rolled condition unless the order names a different condition. The inspection document should identify JIS G 3101 SS490, the edition, and the H×B×t1×t2 designation. Marking should follow the ordered product standards so the piece can be matched to the certificate.

An SS400 certificate on the same Table 15 size is not a SS490 certificate. If a Charpy test or a G 3106 welded-structure grade is required, name that standard; it is not implied by SS490.

Weldability and Surface Condition of JIS G 3101 SS490 H Beams

JIS G 3101 does not, by itself, provide a carbon-equivalent table or a welding procedure for SS490. Procedure qualification, consumables and preheat remain the fabricator’s responsibility for the thickness and joint actually used. The SS490 row is the same chemistry row as SS330 and SS400: only phosphorus and sulfur have maxima.

Surface condition and any special finish should be named when they matter. Do not assume that a narrow H and a square H of similar depth will present the same flange for detailing or for painting.

JIS G 3192 Shape Tolerances and Theoretical Mass for JIS G 3101 SS490 H Beams

Dimensional and mass tolerances for these H-sections are those of JIS G 3192, not of JIS G 3101. This article does not reproduce the tolerance tables; acceptance is against the edition named on the order.

The size table above gives representative reference dimensions. A delivered H 300×300×10×15 will measure close to the tabulated values within those tolerances, not as a set of exact advertised millimetres. The kg/m column is a theoretical catalogue mass. Settlement should follow the contract.

Applications and Service Limits for JIS G 3101 SS490 H Beams

SS490 H-sections are used in general-structure frames and fabrication where this tensile class is specified. This page is SS490 only, not SS400, SS540 or SM490. JIS G 3101 does not specify a Charpy test for this grade.

This page is not a design guide and does not give span tables. If the project needs a welded-structure grade, a lower-temperature quality, or a European or American shape system, nominate that product instead of stretching this certificate.

JIS G 3101 SS490 Compared with SS400, SS540 and SM490

JIS G 3101 SS400 H-Beam uses the same JIS G 3192 Table 15 series but a lower tensile and yield band. JIS G 3101 SS540 H Beam is the other G 3101 grade in this pack and is not interchangeable with SS490. An SS400 certificate is not a SS490 certificate.

JIS G 3106 SM490 H-Beam is a JIS G 3106 welded-structure grade; the shared “490” tensile class does not make the certificates interchangeable. Q355B and S355JR H-beams use different shape systems as well as different material standards. Dual certification is possible only when the delivered piece meets every requirement of each named standard.

Near-Equivalents for JIS G 3101 SS490 H Beams: Not Automatic Substitutes

The comparisons above are for orientation. They are not a licence to substitute one grade, one certificate or one shape system for another. SS490 chemistry is only P and S have maxima. Use the sister pages for their own standards.

Near-equivalents only, not automatic substitutes: SS400 is a lower-tensile grade in the same standard; SS540 is a higher-tensile grade with a 40 mm cap; SM490 is a different JIS standard (G 3106); A572 Grade 50; Q355B; S355JR. The same grade as a channel is a different product form. Use the sister pages for their own standards: JIS G 3101 SS400 H-Beam, JIS G 3106 SM490 H-Beam, and the matching SS490 or SS540 page in this pair.

Sourcing JIS G 3101 SS490 H Beams from SHH STEEL

SHH STEEL reviews enquiries for JIS G 3101 SS490 H-sections against a named Table 15 size list and a named edition. We distinguish SS490 from SS400, from SS540, and from SM490, and we do not treat a Chinese HW or a European HEB of similar depth as the same item. JIS I-beam sizes are reviewed only when they are named; they are not tabulated on this page.

Send the H×B×t1×t2 list, the G 3101 edition, the certificate type and delivery notes. Images on this page stay empty; photographs can be provided with a quotation when they are available.

SS490 H Beam FAQs

Is SS490 a 490 N/mm² yield grade?
No. The 490 in the grade name is the lower end of the specified tensile range, 490–610 N/mm². Minimum yield is 285 N/mm² for flange thickness up to 16 mm, and 275 N/mm² between 16 mm and 40 mm. Do not read the grade number as a yield class.
Is an SS400 H-beam automatically acceptable as SS490?
No. SS400 and SS490 share the same G 3192 Table 15 series, but they are different grades with different tensile and yield bands. An SS400 certificate is not a SS490 certificate.
Is SS490 the same as SM490?
No. SM490 is a JIS G 3106 welded-structure grade, not a JIS G 3101 general-structure grade. The shared “490” tensile class does not make the certificates interchangeable.
Which thickness is used to pick the yield band?
Thickness for a section is the thickness at the test-piece location. On this page the usual basis is the flange thickness t2, not the H-section depth. H 350×350×12×19 has a 19 mm flange, so it uses the lower of the two common bands described above, not the ≤16 mm band.
Does JIS G 3101 require a Charpy test for SS490?
No. JIS G 3101 does not specify Charpy absorbed-energy values for SS490. If an impact test is required, it has to be named on the order; it is not implied by the grade name.

Request a Quotation for JIS G 3101 SS490 H Beams

JIS G 3101 SS490 H beam is a general-structure section with a 490–610 N/mm² tensile range and 285 N/mm² minimum yield up to 16 mm (275 N/mm² between 16 mm and 40 mm, based on flange thickness). Nominate the JIS G 3192 H-section size (H×B×t1×t2) and the material to JIS G 3101:2024 (or the edition on the order). The table is the standard Table 15 series, used as reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review them before quoting.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response