GB/T 3280 10Cr17 S11710 Cold Rolled Stainless Steel Plate
What is GB/T 3280 10Cr17 S11710 Cold Rolled Stainless Steel Plate?
Equivalent grades: 10Cr17 (S11710) ≈ UNS S43000 ≈ EN 1.4016 X6Cr17 ≈ JIS SUS430.
10Cr17 (S11710) is a ferritic grade. 10Cr17 is the Chinese 430: a nickel-free 17Cr ferritic grade with moderate corrosion resistance, magnetic and cheaper than 304.
GB/T 3280-2015 is the Chinese national standard for cold-rolled stainless steel plate, sheet and strip. It is the cold-rolled counterpart of GB/T 4237 (hot rolled) and uses the same grade names and unified numeric codes (ISC) from GB/T 20878. Cold-rolled sheet is the normal product for thin gauges with 2B, BA or polished finishes.
This page sets out the GB/T 3280-2015 requirements for 10Cr17 (S11710) sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.
10Cr17 (S11710) sheet: specification summary
| Item | 10Cr17 (S11710) data |
|---|---|
| Standard | GB/T 3280-2015, cold-rolled stainless steel plate, sheet and strip |
| Product form | cold-rolled plate, sheet and strip |
| Typical thickness | 0.3–6.0 mm |
| Widths | 1000, 1219, 1250, 1500 mm; slit coil to order |
| Lengths | 2000, 2438, 2500, 3000 mm or cut to size |
| Finishes | 2D, 2B, BA, No.3, No.4, HL |
| Heat treatment | solution treated (austenitic, duplex) or annealed (ferritic) |
| Tests | chemical analysis, tensile, hardness; bend and intergranular corrosion (GB/T 4334) where specified |
| Certificates | mill certificate to GB/T 18253 (EN 10204 3.1 type); 3.2 on request |
| Grade family | ferritic |
Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. 10Cr17 (S11710) is one of the high-volume grades produced by most Chinese stainless mills, so common sizes are held in stock and non-stock sizes are usually rolled within a normal mill cycle.
Chemical composition of 10Cr17 (S11710) (GB/T 3280-2015)
| Element | wt % |
|---|---|
| C | 0.12 max |
| Si | 1 max |
| Mn | 1 max |
| P | 0.04 max |
| S | 0.03 max |
| Cr | 16–18 |
| Ni | 0.75 max |
Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.
Low carbon and nitrogen, together with titanium and/or niobium where specified, are what make modern ferritic grades weldable. Check that the stabiliser content on the certificate meets the formula in the standard for the actual C and N.
Mechanical properties of 10Cr17 (S11710) sheet
| Rp0.2 min, MPa | Rm min, MPa | A min, % | HBW max | HRB max | HV max |
|---|---|---|---|---|---|
| 205 | 420 | 22 | 183 | 89 | 200 |
The minimum proof strength is 205 MPa. Ferritic grades have lower elongation than austenitic grades and work-harden less, which helps in stretch forming but limits deep drawing. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.
Corrosion resistance of 10Cr17 (S11710): PREN and limits
Ferritic stainless steels contain chromium but little or no nickel, so they are magnetic, cheaper and less sensitive to nickel price swings. They have good resistance to chloride stress-corrosion cracking, lower thermal expansion and higher thermal conductivity than austenitic grades, which helps in thermal cycling. Stabilisation with titanium and/or niobium ties up carbon and nitrogen and protects welds against intergranular corrosion.
The limits are toughness and formability in heavy sections: ferritic grades have a ductile-to-brittle transition, grain growth in the weld zone, and 475 °C embrittlement in the higher-chromium grades. They are therefore supplied mainly as sheet and light plate, and they are welded with low heat input.
How 10Cr17 (S11710) compares with related grades
| Grade | Cr | Ni | Mo | N | PREN (min) | YS / Rp0.2 min, MPa |
|---|---|---|---|---|---|---|
| 10Cr17 (S11710) | 16–18 | 0.75 max | — | — | 16.0 | 205 |
| UNS S44100 | 17.5–19.5 | 1.00 max | — | 0.030 max | 17.5 | 241 |
| UNS S43940 | 17.5–18.5 | — | — | — | 17.5 | 250 |
| UNS S44600 | 23.0–27.0 | 0.75 max | — | 0.25 max | 23.0 | 275 |
| UNS S44100 | 17.5–19.5 | 1.00 max | — | 0.030 max | 17.5 | 241 |
Choose 10Cr17 (S11710) when nickel-free cost, thermal-cycling behaviour or resistance to chloride stress-corrosion cracking matters more than toughness in heavy sections. It is not a good choice for heavy welded plate or for cryogenic service.
The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.
Heat treatment and delivery condition of 10Cr17 (S11710)
Heat treatment: 780 – 800 °C, air cooling.
Ferritic grades are annealed and cooled rapidly or in air; they are not hardenable by quenching. Avoid long holding in the 400–550 °C range, which causes 475 °C embrittlement in higher-chromium grades.
Surface finishes for 10Cr17 (S11710) sheet
GB/T 3280 sheet is supplied in cold-rolled finishes: 2D (dull, for deep drawing), 2B (skin passed, the general-purpose finish), BA (bright annealed), and polished No.3, No.4 or HL (hairline). Decorative finishes and PVC or laser film are available. State the finish and film side on the order.
Dimensions, tolerances and flatness
Thickness, width, length and flatness tolerances are tabulated in GB/T 3280, with normal and higher precision classes. For laser-cut blanks, specify flatness and, if needed, tension-levelled sheet. Coil slit to width keeps edge camber low.
Chinese grade names and codes. GB/T 3280 uses the GB/T 20878 grade names, which spell out the composition (carbon in hundredths of a percent followed by alloying elements), and the unified numeric code (ISC) such as S11710. GB/T 20878-2024 renamed a few grades, so a certificate may show either the 2007 or the 2024 form; the ISC code is the safest identifier. Order with both the grade name and the code, the finish, the thickness tolerance class and the certificate type. Export orders often also ask for the ASTM or JIS designation on the certificate as a reference only.
10Cr17 (S11710) sheet stock in China
| Thickness (mm) | Width (mm) | Length (mm) | Finish | Approx. quantity | Location |
|---|---|---|---|---|---|
| 0.5 | 1000 / 1219 | 2000 / 2438 | 2B | 300+ t | China |
| 0.8 | 1219 | 2438 | 2B | 300+ t | China |
| 1.0 | 1219 / 1250 | 2438 / 2500 | 2B | 300+ t | China |
| 1.5 | 1219 / 1500 | 2438 / 3000 | 2B | 200+ t | China |
| 2.0 | 1219 / 1500 | 2438 / 3000 | 2B | 200+ t | China |
| 3.0 | 1500 | 3000 | 2B / No.1 | 100+ t | China |
| 4.0 | 1500 | 3000 / 6000 | No.1 | 100+ t | China |
Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.
Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.
10Cr17 (S11710) equivalents in other standards
| Standard | Designation | Comment |
|---|---|---|
| ASTM / UNS | UNS S43000 | same alloy family and limits closely matched; compare each limit on the certificate |
| EN | 1.4016 X6Cr17 | same alloy family and limits closely matched; compare each limit on the certificate |
| JIS | SUS430 | same alloy family and limits closely matched; compare each limit on the certificate |
Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.
Related grades by alloy family
Ferritic
Nickel-free, magnetic grades for heat and mild corrosion: A240 S43932, A240 S44400, A240 S40920, A240 S40910, A240 S40930, 1.4509 plate, 1.4512 plate, 1.4510 plate.
Same standard
Other grades in this standard: GB/T 3280 S35350, GB/T 3280 S35450, GB/T 3280 S30408.
Same grade, other specification
Applications, forming and welding of 10Cr17 (S11710)
Typical uses: appliance panels, kitchenware, indoor decoration, washing-machine drums, and automotive trim.
Ferritic sheet is formed cold; heavy gauges should be warmed to 100–200 °C before bending in cold weather. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a stabilised ferritic filler such as ER409Nb or ER430LNb, or an austenitic ER309L where weld ductility matters more than matching expansion. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.
Welding practice. Use low heat input and avoid preheat above about 200 °C to limit grain growth in the HAZ. Stabilised grades do not need post-weld heat treatment for corrosion resistance. Thin sheet is commonly joined by GTAW, plasma, laser or resistance welding. Cold forming should be done above room temperature for thicker gauges to avoid brittle fracture.
Certificates, testing and receiving inspection
Every delivery carries a mill certificate to GB/T 3280-2015 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: intergranular corrosion testing (ASTM A763 or equivalent), bend test, hardness, and PMI. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.
On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.
Common mistakes when specifying 10Cr17 (S11710)
- Ordering heavy plate for welded pressure parts, where toughness is limited.
- Assuming all ferritic grades are stabilised; check Ti and Nb on the certificate.
- Using a ferritic grade in hot chloride solutions without checking pitting resistance.
Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.
Sourcing 10Cr17 (S11710): buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Toughness of heavy gauges | thickness range agreed; bend tests on the heat |
| Weld-zone grain growth | low-heat-input welding advice and stabilised filler |
| Small quantities across many sizes | mixed thicknesses and grades combined in one shipment |
| Cutting and edge preparation | in-house shearing, plasma, laser and waterjet cutting, bevelling |
| Delivery delays | weekly production and shipping updates with photos |
How to order 10Cr17 (S11710) sheet
State the standard and edition (GB/T 3280-2015), the grade (10Cr17 (S11710)), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.
FAQ
-
What is the difference between GB/T 3280 and GB/T 4237 10Cr17?
- GB/T 3280 covers cold-rolled plate, sheet and strip; GB/T 4237 covers hot-rolled material. The grade names and chemistry are the same, but thickness ranges, finishes and tolerances differ.
-
Is 10Cr17 (S11710) equivalent to UNS S43000?
- They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
-
Is 10Cr17 (S11710) magnetic?
- Yes. Ferritic grades are magnetic in all conditions.
-
Can I order small quantities or cut sizes?
- Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
-
Which certificates and tests can you provide?
- Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.
Conclusion
10Cr17 (S11710) sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.