GB/T 21237 L320M PSL2 Pipeline Steel Plate
What is GB/T 21237 L320M PSL2 steel plate?
GB/T 21237 L320M/X46M is the PSL2 X46 level in TMCP condition. It keeps the Grade B and X42 M chemistry frame (C ≤ 0.22%, V ≤ 0.05%, Nb ≤ 0.05%, Ti ≤ 0.04%) but raises the yield window to 320-525 MPa.
GB/T 21237-2018 covers hot-rolled wide and heavy plates, 6-50 mm thick, for oil and gas line pipe made to ISO 3183, GB/T 9711 and API Spec 5L. At PSL2 the delivery state is part of the grade name: R (hot rolled), N (normalized or normalizing rolled), Q (quenched and tempered) and M (thermomechanically rolled). This page covers the M version; Table 1 also defines the X46 level as L320N, L320Q.
X46M is a project-specific intermediate grade for pipeline extensions, replacement sections and designs optimised between X42 and X52 under PSL2 rules.
Category hubs: Pipeline Steel Plates · API 5L line pipe plates. Pipe-grade reference: API 5L X46 PSL2; PSL1 plate at this level: GB/T 21237 L320 PSL1.
Neighbouring PSL2 TMCP plate grades: GB/T 21237 L290M · GB/T 21237 L360M.
Material Specification for GB/T 21237 L320M
| Parameter | Specification |
|---|---|
| Standard | GB/T 21237-2018 (implemented 2019-02-01). GB/T 21237-2026 was issued 2026-05-25 and takes effect 2026-12-01, replacing the 2018 edition; it widens thickness to 6-90 mm and adds sour, offshore, fittings, high-deformability, bend and station plate annexes. Confirm the edition on the PO and MTC. |
| Grade | L320M/X46M (PSL2) |
| Quality level | PSL2 (product specification level 2) |
| Equivalent pipe grade | X46M / L320M of API 5L, ISO 3183 and GB/T 9711 (GB/T 21237 Annex A) |
| Product form | Hot-rolled wide and heavy plate for line pipe |
| Thickness range (standard) | 6-50 mm |
| Dimensions and tolerances | GB/T 709, or other sizes and tolerances by agreement |
| Delivery condition | Thermomechanically rolled (M, TMCP) |
| Other PSL2 states at this level | L320N, L320Q |
| Steelmaking | BOF or EAF with secondary (ladle) refining |
| Edge condition | Trimmed (EC) or untrimmed (EM) |
| Inspection lot | Same grade, heat, thickness, rolling and heat-treatment schedule; ≤ 60 t |
| Certification | Quality certificate per GB/T 247; EN 10204 3.1 MTC, 3.2 on request |
| Density | 7.85 g/cm³ |
Chemical Composition of L320M/X46M (heat and product analysis, CE)
GB/T 21237-2018 Table 3 limits apply to both heat (ladle) analysis and product analysis, so one table covers both. Values are maximum mass %. The supplier may report heat analysis and the CE calculated from it, but must guarantee product analysis (clause 6.1.4). For plates over 25.0 mm, chemistry may be agreed (clause 6.1.3).
| Grade | C | Si | Mn | P | S | V | Nb | Ti | CEIIW | CEPcm |
|---|---|---|---|---|---|---|---|---|---|---|
| L320M/X46M | 0.22 | 0.45 | 1.30 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | 0.43 | 0.25 |
Notes that apply to this grade:
- (e) Unless otherwise agreed: Cu ≤ 0.50%, Ni ≤ 0.30%, Cr ≤ 0.30%, Mo ≤ 0.15%.
- For each 0.01% below the specified maximum C, Mn may exceed its maximum by 0.05%, up to 1.65% for this grade.
- Boron shall not be intentionally added unless otherwise agreed; residual B ≤ 0.001%.
- Elements other than those listed may be added by agreement (clause 6.1.6).
Carbon equivalent (clause 6.2): when C > 0.12%, CEIIW = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15 applies; when C ≤ 0.12%, CEPcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B applies (B below 0.0005% may be taken as zero). With C allowed up to 0.22%, the formula that applies depends on the actual heat carbon.
Mechanical Properties of L320M/X46M plate
GB/T 21237-2018 Table 5 gives both minimum and maximum strength at PSL2 so that the finished pipe stays inside its own window after forming and expansion. The buyer chooses the test direction and states it in the contract; normally it is transverse to the pipe axis. Buyer and mill may also agree a narrower tensile range and yield ratio to suit the pipe-making route.
| Grade | Rt0.5 (MPa) | Rm (MPa) | Rt0.5/Rm max | A50mm (%) | A (%) | Bend test |
|---|---|---|---|---|---|---|
| L320M/X46M | 320-525 | 435-655 | 0.90 | Per formula (3) | ≥ 20 | 180° transverse, D = 2a |
Rt0.5 is total extension strength at 0.5%. Minimum A50mm is calculated from formula (3) using the specimen area and specified minimum tensile strength, as in ISO 3183 / API 5L. Tensile tests use full-thickness rectangular specimens (clause 6.5.5). The bend specimen must show no cracks.
For comparison, API 5L PSL2 pipe at X46 uses the same Rt0.5 and Rm window with a 0.93 yield ratio cap. The stricter 0.90 cap on the plate leaves room for strain hardening during pipe forming.
Delivery Conditions for L320M/X46M plate
Thermomechanically rolled (M, TMCP). Other PSL2 delivery states at this strength level: L320N (normalized / normalizing rolled (N)), L320Q (quenched and tempered (Q)).
In TMCP the final strength and toughness come from controlled rolling temperatures and reductions, often followed by accelerated cooling, rather than a separate furnace heat treatment. This gives fine grain at a low carbon equivalent, which is why M plate dominates LSAW line-pipe supply. Re-normalizing or hot forming removes the rolled-in properties, so hot bending needs a qualified procedure.
State the grade with its delivery letter, the edge condition and the service (gas, oil or other fluid) on the order. Plate surfaces must not be weld repaired.
Weldability of L320M/X46M line pipe plate
L320M/X46M is designed for longitudinal SAW seam welding in LSAW pipe mills and for field girth welding. The PSL2 CE caps (CEIIW ≤ 0.43, CEPcm ≤ 0.25) and the low P and S limits (≤ 0.025% / ≤ 0.015%) keep HAZ hardness and cold-cracking risk under control. With C up to 0.22% allowed, check the MTC carbon and the applicable CE formula before qualifying the seam-weld procedure.
Welding procedures, preheat and consumables follow the pipe standard and the qualified WPS. The reference maximum hardness for this grade is 240 HV10 (Table 10). High heat input on thick TMCP plate can soften or coarsen the HAZ, so heat input limits belong in the seam-weld procedure.
Dimensional Tolerances for L320M/X46M
Dimensions, shape, weight and tolerances follow GB/T 709 unless other values are agreed in the contract (clause 5.2). State thickness accuracy on the order: plate thickness tolerance feeds directly into the pipe wall tolerance.
Width and camber matter for UOE and JCOE forming, so agree width tolerance, edge condition and flatness with the pipe mill. Surface defects may be removed only within half the thickness tolerance, keeping minimum thickness; weld repair is not allowed.
GB/T 21237-2018 covers 6-50 mm. DWTT on plate thicker than 25.0 mm is by agreement, so heavy-wall orders should define DWTT terms early.
Applications and service limits for L320M/X46M
Typical uses of L320M/X46M plate:
- PSL2 replacement and extension pipe for X46 systems
- Medium-pressure gas lines designed on 320 MPa
- LSAW pipe ordered to L320M / X46M
- Matched fittings for X46 PSL2 lines
Service limits: There is no hot rolled (R) version at this level; the alternatives are L320N and L320Q. The Charpy requirement rises to 90 J at -20 °C from X46.
Sour service: GB/T 21237-2018 contains no HIC or SSC requirements. Sour-service wide plate in China is ordered to GB/T 37599-2019 or to a project sour specification, and the 2026 edition of GB/T 21237 moves sour plate into an annex with an S suffix. Do not treat standard M plate as sour resistant unless HIC/SSC testing is written into the order.
Charpy, DWTT, hardness and cleanliness for L320M/X46M
Clause 6.10 of GB/T 21237-2018 sets toughness and hardness requirements for PSL2 plate that apply when agreed and stated in the contract. Grain size, inclusion and banding limits (clauses 6.6-6.8) are PSL2 requirements; the grain size and banding checks may be waived when the supplier guarantees them and the buyer agrees.
| Requirement | L320M/X46M |
|---|---|
| Charpy V-notch at -20 °C, KV2 (full size) | ≥ 90 J (average of 3; one value may be lower but not below 75% of this) |
| Charpy shear area and DWTT | No values in Table 9 for this grade (DWTT limits start at L360/X52); by agreement |
| Maximum hardness (reference value) | 240 HV10, transverse section at 1/4 width, at least 9 points |
| Grain size, gas lines | No. 8 or finer |
| Grain size, oil and other lines | No. 7 or finer |
| Non-metallic inclusions A, B, C, D (fine and heavy) | Gas ≤ 2.0; oil and other ≤ 2.5 |
| Banded structure, gas lines | ≤ grade 3 (GB/T 13299) |
Sub-size Charpy specimens of 7.5 × 10 × 55 mm or 5 × 10 × 55 mm must reach 75% or 50% of the full-size energy. Other Charpy and DWTT temperatures may be agreed. Sampling per Table 11: tensile at 1/2 width; bend, Charpy (3 per lot), DWTT (2 per lot) and hardness at 1/4 width; inclusions, banding and grain size at 1/2 width.
Equivalent and related grades for L320M/X46M
GB/T 21237 names follow the pipe grades. Annex A maps L320M/X46M to X46M / L320M of GB/T 9711 and ISO 3183, which use the API 5L grade system. These are pipe-grade matches: the plate is ordered so that the finished pipe meets the pipe standard after forming, welding and expansion.
| Standard | Grade | Relation | Product page |
|---|---|---|---|
| GB/T 21237-2018 | L320M/X46M | This page | – |
| API 5L / ISO 3183 / GB/T 9711 | X46M (L320M) PSL2 | Same pipe grade (GB/T 21237 Annex A) | X46 PSL2 |
| GB/T 21237-2018 | L320N | Same level, normalized / normalizing rolled (N) | Covered on this page (Tables 1, 3, 5) |
| GB/T 21237-2018 | L320Q | Same level, quenched and tempered (Q) | Covered on this page (Tables 1, 3, 5) |
| GB/T 21237-2018 | L320/X46 PSL1 | Same strength, PSL1 minimum values only | L320 PSL1 |
| Category | Pipeline plate hubs | Family navigation | Pipeline Steel Plates · API 5L |
L320M/X46M vs other delivery states and neighbouring grades (selection aid)
Same strength level, different PSL2 delivery states (GB/T 21237-2018 Tables 3 and 5). Tensile windows are identical; chemistry and processing route differ.
| Item | L320M | L320N | L320Q |
|---|---|---|---|
| C max (%) | 0.22 | 0.24 | 0.18 |
| Si max (%) | 0.45 | 0.40 | 0.45 |
| Mn max (%) | 1.30 | 1.40 | 1.40 |
| CEIIW / CEPcm max | 0.43 / 0.25 | 0.43 / 0.25 | 0.43 / 0.25 |
| Rt0.5 / Rm (MPa) | 320-525 / 435-655 | 320-525 / 435-655 | 320-525 / 435-655 |
| Route | thermomechanically rolled (M, TMCP) | normalized / normalizing rolled (N) | quenched and tempered (Q) |
Against neighbouring TMCP grades:
| Item | L320M | L290M | L360M |
|---|---|---|---|
| Rt0.5 (MPa) | 320-525 | 290-495 | 360-530 |
| Rm (MPa) | 435-655 | 415-655 | 460-760 |
| Rt0.5/Rm max | 0.90 | 0.90 | 0.90 |
| KV2 at -20 °C | ≥ 90 J | ≥ 80 J | ≥ 90 J |
| C max (%) | 0.22 | 0.22 | 0.22 |
| Page | This page | L290M | L360M |
Why choose SHH STEEL for L320M/X46M plate
- SHH STEEL supplies GB/T 21237 L320M/X46M TMCP plate from Chinese plate mills for LSAW pipe makers and fabricators
- Quality certificate per GB/T 247 with heat analysis, CE, tensile, yield ratio and bend results; EN 10204 3.1 standard, 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Clause 6.10 options written into the contract when required: -20 °C Charpy, DWTT, HV10 hardness, grain size, inclusion and banding checks
- Order data aligned with the pipe mill: service (gas / oil), test-piece direction, thickness accuracy and edge condition
- One supply chain for GB/T 21237 and API 5L referenced plate: Pipeline Steel Plates · API 5L
Supply, testing and inspection for L320M/X46M
| Item | SHH STEEL supply note |
|---|---|
| Thickness | 6-50 mm (GB/T 21237-2018 range) |
| Size | Width and length to suit the pipe size and mill capability, confirmed at quotation |
| Delivery condition | Thermomechanically rolled (M, TMCP); L320N, L320Q on request |
| Edge | Trimmed (EC) or untrimmed (EM) |
| Testing options | Charpy -20 °C, DWTT (by agreement), HV10, grain size, inclusions, banding |
| Certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | GB/T 21237-2018, PSL2, L320M/X46M, thickness × width × length, thickness accuracy, quantity, edge condition, service (gas / oil / other), test-piece direction, clause 6.10 tests, any sour or project requirements |
FAQ
-
What is L320M equal to in API 5L?
- X46M (L320M) PSL2, per Annex A of GB/T 21237-2018, which maps plate grades to GB/T 9711 and ISO 3183 pipe grades in the API 5L grade system.
-
What does the M mean?
- Thermomechanical rolling (TMCP). At this strength level GB/T 21237 also defines L320N, L320Q, with the same tensile window but different chemistry limits.
-
What are the yield, tensile and yield ratio limits?
- Rt0.5 320-525 MPa, Rm 435-655 MPa, Rt0.5/Rm ≤ 0.90, A ≥ 20%.
-
What impact energy applies?
- When agreed in the contract, ≥ 90 J at -20 °C (full size). DWTT limits start at L360/X52.
-
Is L320M suitable for sour (H2S) service?
- Not by itself. The 2018 edition has no HIC/SSC requirements; sour plate must be ordered to a sour specification such as GB/T 37599-2019 or the project specification.
-
Which edition applies?
- This page follows GB/T 21237-2018. GB/T 21237-2026 takes effect on 1 December 2026, so state the edition on the PO and check it on the MTC.
Request a quotation
Send GB/T 21237-2018 L320M/X46M PSL2, plate thickness × width × length, thickness accuracy, quantity, edge condition, service (gas, oil or other), test-piece direction, required clause 6.10 tests (Charpy, DWTT, hardness) and any sour or project requirements. SHH STEEL will confirm mill availability, certification scope and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097