GB/T 21237 L290M PSL2 Pipeline Steel Plate | GB/T 21237 Pipeline Steel - SHH STEEL

GB/T 21237 L290M PSL2 Pipeline Steel Plate

GB/T 21237 L290M/X42M is a PSL2 thermomechanically rolled wide and heavy plate, 6-50 mm thick, for welded oil and gas line pipe at the X42M level of API 5L, ISO 3183 and GB/T 9711. It is specified by Rt0.5 290-495 MPa, Rm 415-655 MPa, Rt0.5/Rm ≤ 0.90, C ≤ 0.22% and CEIIW ≤ 0.43% or CEPcm ≤ 0.25% (by carbon level), with optional -20 °C Charpy and hardness limits. SHH STEEL supplies it with a GB/T 247 quality certificate (EN 10204 3.1, or 3.2 on request).
Equivalent Grades:
API 5L / ISO 3183 / GB/T 9711 X42M (L290M) PSL2 per GB/T 21237 Annex A; legacy EN 10208-2 L290MB (approximate); same level in GB/T 21237: L290R, L290N, L290Q. Confirm against the pipe specification.
Heat Treatment
Thermomechanically rolled (TMCP, M). No separate furnace heat treatment; do not normalize or hot form without a qualified procedure.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Toughness, DWTT and hardness
Equivalent Material Grade
L290M vs related grades
Why choose Us
Our Service
FAQ
Conclusion

What is GB/T 21237 L290M PSL2 steel plate?

GB/T 21237 L290M/X42M is the PSL2 X42 level in TMCP condition. Compared with the PSL1 grade it adds an upper yield limit of 495 MPa, a 0.90 yield ratio cap and optional -20 °C Charpy testing.

GB/T 21237-2018 covers hot-rolled wide and heavy plates, 6-50 mm thick, for oil and gas line pipe made to ISO 3183, GB/T 9711 and API Spec 5L. At PSL2 the delivery state is part of the grade name: R (hot rolled), N (normalized or normalizing rolled), Q (quenched and tempered) and M (thermomechanically rolled). This page covers the M version; Table 1 also defines the X42 level as L290R, L290N, L290Q.

X42M plate is used for city gas, gathering and lateral lines where PSL2 is mandatory but pressure is moderate. TMCP gives fine-grained plate at low carbon equivalent for good field weldability.

Category hubs: Pipeline Steel Plates · API 5L line pipe plates. Pipe-grade reference: API 5L X42 PSL2; PSL1 plate at this level: GB/T 21237 L290 PSL1.

Neighbouring PSL2 TMCP plate grades: GB/T 21237 L245M · GB/T 21237 L320M.

Material Specification for GB/T 21237 L290M

Parameter Specification
Standard GB/T 21237-2018 (implemented 2019-02-01). GB/T 21237-2026 was issued 2026-05-25 and takes effect 2026-12-01, replacing the 2018 edition; it widens thickness to 6-90 mm and adds sour, offshore, fittings, high-deformability, bend and station plate annexes. Confirm the edition on the PO and MTC.
Grade L290M/X42M (PSL2)
Quality level PSL2 (product specification level 2)
Equivalent pipe grade X42M / L290M of API 5L, ISO 3183 and GB/T 9711 (GB/T 21237 Annex A)
Product form Hot-rolled wide and heavy plate for line pipe
Thickness range (standard) 6-50 mm
Dimensions and tolerances GB/T 709, or other sizes and tolerances by agreement
Delivery condition Thermomechanically rolled (M, TMCP)
Other PSL2 states at this level L290R, L290N, L290Q
Steelmaking BOF or EAF with secondary (ladle) refining
Edge condition Trimmed (EC) or untrimmed (EM)
Inspection lot Same grade, heat, thickness, rolling and heat-treatment schedule; ≤ 60 t
Certification Quality certificate per GB/T 247; EN 10204 3.1 MTC, 3.2 on request
Density 7.85 g/cm³

Chemical Composition of L290M/X42M (heat and product analysis, CE)

GB/T 21237-2018 Table 3 limits apply to both heat (ladle) analysis and product analysis, so one table covers both. Values are maximum mass %. The supplier may report heat analysis and the CE calculated from it, but must guarantee product analysis (clause 6.1.4). For plates over 25.0 mm, chemistry may be agreed (clause 6.1.3).

Grade C Si Mn P S V Nb Ti CEIIW CEPcm
L290M/X42M 0.22 0.45 1.30 0.025 0.015 0.05 0.05 0.04 0.43 0.25

Notes that apply to this grade:

  • (e) Unless otherwise agreed: Cu ≤ 0.50%, Ni ≤ 0.30%, Cr ≤ 0.30%, Mo ≤ 0.15%.
  • For each 0.01% below the specified maximum C, Mn may exceed its maximum by 0.05%, up to 1.65% for this grade.
  • Boron shall not be intentionally added unless otherwise agreed; residual B ≤ 0.001%.
  • Elements other than those listed may be added by agreement (clause 6.1.6).

Carbon equivalent (clause 6.2): when C > 0.12%, CEIIW = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15 applies; when C ≤ 0.12%, CEPcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B applies (B below 0.0005% may be taken as zero). With C allowed up to 0.22%, the formula that applies depends on the actual heat carbon.

Mechanical Properties of L290M/X42M plate

GB/T 21237-2018 Table 5 gives both minimum and maximum strength at PSL2 so that the finished pipe stays inside its own window after forming and expansion. The buyer chooses the test direction and states it in the contract; normally it is transverse to the pipe axis. Buyer and mill may also agree a narrower tensile range and yield ratio to suit the pipe-making route.

Grade Rt0.5 (MPa) Rm (MPa) Rt0.5/Rm max A50mm (%) A (%) Bend test
L290M/X42M 290-495 415-655 0.90 Per formula (3) ≥ 21 180° transverse, D = 2a

Rt0.5 is total extension strength at 0.5%. Minimum A50mm is calculated from formula (3) using the specimen area and specified minimum tensile strength, as in ISO 3183 / API 5L. Tensile tests use full-thickness rectangular specimens (clause 6.5.5). The bend specimen must show no cracks.

For comparison, API 5L PSL2 pipe at X42 uses the same Rt0.5 and Rm window with a 0.93 yield ratio cap. The stricter 0.90 cap on the plate leaves room for strain hardening during pipe forming.

Delivery Conditions for L290M/X42M plate

Thermomechanically rolled (M, TMCP). Other PSL2 delivery states at this strength level: L290R (hot rolled (R)), L290N (normalized / normalizing rolled (N)), L290Q (quenched and tempered (Q)).

In TMCP the final strength and toughness come from controlled rolling temperatures and reductions, often followed by accelerated cooling, rather than a separate furnace heat treatment. This gives fine grain at a low carbon equivalent, which is why M plate dominates LSAW line-pipe supply. Re-normalizing or hot forming removes the rolled-in properties, so hot bending needs a qualified procedure.

State the grade with its delivery letter, the edge condition and the service (gas, oil or other fluid) on the order. Plate surfaces must not be weld repaired.

Weldability of L290M/X42M line pipe plate

L290M/X42M is designed for longitudinal SAW seam welding in LSAW pipe mills and for field girth welding. The PSL2 CE caps (CEIIW ≤ 0.43, CEPcm ≤ 0.25) and the low P and S limits (≤ 0.025% / ≤ 0.015%) keep HAZ hardness and cold-cracking risk under control. With C up to 0.22% allowed, check the MTC carbon and the applicable CE formula before qualifying the seam-weld procedure.

Welding procedures, preheat and consumables follow the pipe standard and the qualified WPS. The reference maximum hardness for this grade is 240 HV10 (Table 10). High heat input on thick TMCP plate can soften or coarsen the HAZ, so heat input limits belong in the seam-weld procedure.

Dimensional Tolerances for L290M/X42M

Dimensions, shape, weight and tolerances follow GB/T 709 unless other values are agreed in the contract (clause 5.2). State thickness accuracy on the order: plate thickness tolerance feeds directly into the pipe wall tolerance.

Width and camber matter for UOE and JCOE forming, so agree width tolerance, edge condition and flatness with the pipe mill. Surface defects may be removed only within half the thickness tolerance, keeping minimum thickness; weld repair is not allowed.

GB/T 21237-2018 covers 6-50 mm. DWTT on plate thicker than 25.0 mm is by agreement, so heavy-wall orders should define DWTT terms early.

Applications and service limits for L290M/X42M

Typical uses of L290M/X42M plate:

  • PSL2 city gas mains and laterals
  • Gathering and injection lines needing toughness certification
  • LSAW pipe for X42M / L290M pipe orders
  • Fittings and bends from PSL2 plate

Service limits: The X42 level is also defined as L290R, L290N and L290Q. All share the 290-495 MPa yield window, while chemistry and delivery route differ.

Sour service: GB/T 21237-2018 contains no HIC or SSC requirements. Sour-service wide plate in China is ordered to GB/T 37599-2019 or to a project sour specification, and the 2026 edition of GB/T 21237 moves sour plate into an annex with an S suffix. Do not treat standard M plate as sour resistant unless HIC/SSC testing is written into the order.

Charpy, DWTT, hardness and cleanliness for L290M/X42M

Clause 6.10 of GB/T 21237-2018 sets toughness and hardness requirements for PSL2 plate that apply when agreed and stated in the contract. Grain size, inclusion and banding limits (clauses 6.6-6.8) are PSL2 requirements; the grain size and banding checks may be waived when the supplier guarantees them and the buyer agrees.

Requirement L290M/X42M
Charpy V-notch at -20 °C, KV2 (full size) ≥ 80 J (average of 3; one value may be lower but not below 75% of this)
Charpy shear area and DWTT No values in Table 9 for this grade (DWTT limits start at L360/X52); by agreement
Maximum hardness (reference value) 240 HV10, transverse section at 1/4 width, at least 9 points
Grain size, gas lines No. 8 or finer
Grain size, oil and other lines No. 7 or finer
Non-metallic inclusions A, B, C, D (fine and heavy) Gas ≤ 2.0; oil and other ≤ 2.5
Banded structure, gas lines ≤ grade 3 (GB/T 13299)

Sub-size Charpy specimens of 7.5 × 10 × 55 mm or 5 × 10 × 55 mm must reach 75% or 50% of the full-size energy. Other Charpy and DWTT temperatures may be agreed. Sampling per Table 11: tensile at 1/2 width; bend, Charpy (3 per lot), DWTT (2 per lot) and hardness at 1/4 width; inclusions, banding and grain size at 1/2 width.

Equivalent and related grades for L290M/X42M

GB/T 21237 names follow the pipe grades. Annex A maps L290M/X42M to X42M / L290M of GB/T 9711 and ISO 3183, which use the API 5L grade system. These are pipe-grade matches: the plate is ordered so that the finished pipe meets the pipe standard after forming, welding and expansion.

Standard Grade Relation Product page
GB/T 21237-2018 L290M/X42M This page –
API 5L / ISO 3183 / GB/T 9711 X42M (L290M) PSL2 Same pipe grade (GB/T 21237 Annex A) X42 PSL2
GB/T 21237-2018 L290R Same level, hot rolled (R) Covered on this page (Tables 1, 3, 5)
GB/T 21237-2018 L290N Same level, normalized / normalizing rolled (N) Covered on this page (Tables 1, 3, 5)
GB/T 21237-2018 L290Q Same level, quenched and tempered (Q) Covered on this page (Tables 1, 3, 5)
GB/T 21237-2018 L290/X42 PSL1 Same strength, PSL1 minimum values only L290 PSL1
EN 10208-2 (superseded by EN ISO 3183) L290MB Approximate legacy TMCP pipe grade EN 10208-2 hub
Category Pipeline plate hubs Family navigation Pipeline Steel Plates · API 5L

L290M/X42M vs other delivery states and neighbouring grades (selection aid)

Same strength level, different PSL2 delivery states (GB/T 21237-2018 Tables 3 and 5). Tensile windows are identical; chemistry and processing route differ.

Item L290M L290R L290N L290Q
C max (%) 0.22 0.24 0.24 0.18
Si max (%) 0.45 0.40 0.40 0.45
Mn max (%) 1.30 1.20 1.20 1.40
CEIIW / CEPcm max 0.43 / 0.25 0.43 / 0.25 0.43 / 0.25 0.43 / 0.25
Rt0.5 / Rm (MPa) 290-495 / 415-655 290-495 / 415-655 290-495 / 415-655 290-495 / 415-655
Route thermomechanically rolled (M, TMCP) hot rolled (R) normalized / normalizing rolled (N) quenched and tempered (Q)

Against neighbouring TMCP grades:

Item L290M L245M L320M
Rt0.5 (MPa) 290-495 245-450 320-525
Rm (MPa) 415-655 415-655 435-655
Rt0.5/Rm max 0.90 0.90 0.90
KV2 at -20 °C ≥ 80 J ≥ 80 J ≥ 90 J
C max (%) 0.22 0.22 0.22
Page This page L245M L320M

Why choose SHH STEEL for L290M/X42M plate

  • SHH STEEL supplies GB/T 21237 L290M/X42M TMCP plate from Chinese plate mills for LSAW pipe makers and fabricators
  • Quality certificate per GB/T 247 with heat analysis, CE, tensile, yield ratio and bend results; EN 10204 3.1 standard, 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
  • Clause 6.10 options written into the contract when required: -20 °C Charpy, DWTT, HV10 hardness, grain size, inclusion and banding checks
  • Order data aligned with the pipe mill: service (gas / oil), test-piece direction, thickness accuracy and edge condition
  • One supply chain for GB/T 21237 and API 5L referenced plate: Pipeline Steel Plates · API 5L

Supply, testing and inspection for L290M/X42M

Item SHH STEEL supply note
Thickness 6-50 mm (GB/T 21237-2018 range)
Size Width and length to suit the pipe size and mill capability, confirmed at quotation
Delivery condition Thermomechanically rolled (M, TMCP); L290R, L290N, L290Q on request
Edge Trimmed (EC) or untrimmed (EM)
Testing options Charpy -20 °C, DWTT (by agreement), HV10, grain size, inclusions, banding
Certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV or ABS can be arranged
Quotation needs GB/T 21237-2018, PSL2, L290M/X42M, thickness × width × length, thickness accuracy, quantity, edge condition, service (gas / oil / other), test-piece direction, clause 6.10 tests, any sour or project requirements

FAQ

What is L290M equal to in API 5L?
X42M (L290M) PSL2, per Annex A of GB/T 21237-2018, which maps plate grades to GB/T 9711 and ISO 3183 pipe grades in the API 5L grade system.
What does the M mean?
Thermomechanical rolling (TMCP). At this strength level GB/T 21237 also defines L290R, L290N, L290Q, with the same tensile window but different chemistry limits.
What are the yield, tensile and yield ratio limits?
Rt0.5 290-495 MPa, Rm 415-655 MPa, Rt0.5/Rm ≤ 0.90, A ≥ 21%.
What impact energy applies?
When agreed in the contract, ≥ 80 J at -20 °C (full size). DWTT limits start at L360/X52.
Is L290M suitable for sour (H2S) service?
Not by itself. The 2018 edition has no HIC/SSC requirements; sour plate must be ordered to a sour specification such as GB/T 37599-2019 or the project specification.
Which edition applies?
This page follows GB/T 21237-2018. GB/T 21237-2026 takes effect on 1 December 2026, so state the edition on the PO and check it on the MTC.

Request a quotation

Send GB/T 21237-2018 L290M/X42M PSL2, plate thickness × width × length, thickness accuracy, quantity, edge condition, service (gas, oil or other), test-piece direction, required clause 6.10 tests (Charpy, DWTT, hardness) and any sour or project requirements. SHH STEEL will confirm mill availability, certification scope and a quotation.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: Pipeline Steel Plates · API 5L · X42 PSL2 · L290 PSL1

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X