GB/T 21237 L320 (X46) PSL1 Pipeline Steel Plate
What is GB/T 21237 L320/X46 PSL1 steel plate?
GB/T 21237 L320/X46 PSL1 is the X46 (L320) level of the standard at PSL1. It sits between X42 and X52 and is seldom stocked, so it is usually rolled to order for a specific pipe project.
GB/T 21237-2018 covers hot-rolled wide and heavy plates, 6-50 mm thick, for oil and natural gas line pipe made to ISO 3183, GB/T 9711 and API Spec 5L; plates for other welded fluid pipe may also refer to it. The grade name follows the pipe grade: L for line, then the pipe’s specified minimum yield in MPa, with the API style name (X46) as the common alternative. PSL1 grades carry no delivery-state letter.
Designers choose X46 when wall-thickness optimisation between X42 and X52 matters, or when an existing pipeline is extended or repaired with matching X46 pipe.
Category hubs: Pipeline Steel Plates · API 5L line pipe plates. Pipe-grade reference at the same strength: API 5L X46 PSL1; PSL2 plate at this level: GB/T 21237 L320M.
Neighbouring PSL1 plate grades: GB/T 21237 L290 PSL1 · GB/T 21237 L360 PSL1.
Material Specification for GB/T 21237 L320/X46 PSL1
| Parameter | Specification |
|---|---|
| Standard | GB/T 21237-2018 (implemented 2019-02-01). GB/T 21237-2026 was issued 2026-05-25 and takes effect 2026-12-01, replacing the 2018 edition; it widens thickness to 6-90 mm and adds sour, offshore, fittings, high-deformability, bend and station plate annexes. Confirm the edition on the PO and MTC. |
| Grade | L320/X46 (PSL1) |
| Quality level | PSL1 (product specification level 1) |
| Equivalent pipe grade | X46 / L320 of API 5L, ISO 3183 and GB/T 9711 (GB/T 21237 Annex A) |
| Product form | Hot-rolled wide and heavy plate for line pipe |
| Thickness range (standard) | 6-50 mm |
| Dimensions and tolerances | GB/T 709, or other sizes and tolerances by agreement (clause 5) |
| Delivery condition | Hot rolled, normalized, normalizing rolled or thermomechanically rolled (TMCP) |
| Edge condition | Trimmed (EC) or untrimmed (EM) |
| Steelmaking | Basic oxygen or electric furnace (route chosen by the supplier unless specified) |
| Inspection lot | Same grade, heat, thickness, rolling and heat-treatment schedule; ≤ 60 t per lot |
| Certification | Quality certificate per GB/T 247; EN 10204 3.1 MTC, 3.2 on request |
| Density | 7.85 g/cm³ |
Chemical Composition of L320/X46 PSL1 (heat and product analysis)
GB/T 21237-2018 Table 2 limits apply to both heat (ladle) analysis and product analysis, so one table covers both. Values are maximum mass %. The supplier may report heat analysis only but must guarantee the product analysis limits (clause 6.1.4). For plates over 25.0 mm, chemistry may be agreed separately (clause 6.1.3).
| Grade (PSL1) | C | Mn | P | S | V | Nb | Ti |
|---|---|---|---|---|---|---|---|
| L320/X46 | 0.26 | 1.40 | 0.030 | 0.030 | see (d) | see (d) | see (d) |
Table 2 notes that apply:
- Cu ≤ 0.50%, Ni ≤ 0.50%, Cr ≤ 0.50%, Mo ≤ 0.15%.
- Boron shall not be intentionally added unless otherwise specified; residual B ≤ 0.001%.
- For each 0.01% below the specified maximum C, Mn may exceed its maximum by 0.05%, up to 1.65% for this grade.
- (d) Nb + V + Ti ≤ 0.15%.
- For L290/X42 and higher, elements other than those listed (including Nb, V, Ti) may be added by agreement (clause 6.1.6).
PSL1 has no Si limit and no carbon-equivalent limit in GB/T 21237-2018. If the pipe mill needs a CE cap for seam welding, write it into the purchase order.
Mechanical Properties of L320/X46 PSL1 plate
GB/T 21237-2018 Table 4 sets minimum values only for PSL1. Note (a) of the table asks buyer and mill to agree a suitable tensile range so that the finished pipe meets its own standard after forming. The buyer chooses the test direction and states it in the contract; normally it is transverse to the pipe axis.
| Grade | Rt0.5 (MPa) | Rm (MPa) | A50mm (%) | A (%) | Bend test |
|---|---|---|---|---|---|
| L320/X46 | ≥ 320 | ≥ 435 | Per formula (3), clause 6.5.4 | ≥ 20 | 180°, D = 2a, no cracks |
Rt0.5 is the specified total extension strength at 0.5% extension, the same yield definition used for line pipe. The minimum A50mm elongation is calculated from the specimen cross-section and the specified minimum tensile strength (formula (3), the same approach as ISO 3183 / API 5L). In a dispute, a 50 mm gauge, 38 mm wide specimen is the referee. Tensile tests up to L485/X70 use full-thickness rectangular specimens (clause 6.5.5).
PSL1 has no maximum yield, no yield-to-tensile ratio limit and no Charpy or DWTT requirement. These controls exist only at PSL2: L320M is held to Rt0.5 320-525 MPa, Rm 435-655 MPa and Rt0.5/Rm ≤ 0.90.
Delivery Conditions for L320/X46 PSL1 plate
Hot rolled, normalized, normalizing rolled or thermomechanically rolled (TMCP).
Table 1 of GB/T 21237-2018 lists the delivery conditions allowed for each PSL1 grade. The mill selects the route that meets Table 4 for the ordered thickness unless the buyer specifies one. For X46 plate at heavier thickness, TMCP is the usual route because it reaches the strength at a lower carbon equivalent; hot rolled or normalized plate is used where the pipe maker prefers it.
State the delivery condition and edge condition (EC trimmed or EM untrimmed) on the order. Weld repair of the plate surface is not permitted (clause 6.9.5); surface defects may be ground out only within half the thickness tolerance while keeping the minimum thickness.
Weldability of L320/X46 PSL1 line pipe plate
L320/X46 PSL1 is a C-Mn, optionally micro-alloyed, line-pipe plate intended for longitudinal seam welding, most often SAW for LSAW pipe, followed by girth welding in the field. With C up to 0.26% allowed, weldability depends on the actual heat chemistry, so check the MTC carbon and manganese before qualifying the seam-weld procedure.
Because PSL1 has no CE limit, many pipe mills add a CEIIW or CEPcm cap to the plate order. Preheat, heat input and consumables follow the qualified WPS for the pipe standard (for example ISO 3183 / API 5L / GB/T 9711 welding requirements).
Dimensional Tolerances for L320/X46 PSL1
Dimensions, shape, weight and tolerances follow GB/T 709 (hot-rolled steel plates and strips) unless other sizes, shapes and tolerances are agreed and written into the contract (clause 5.2). The order must state the size and the required thickness accuracy (clause 4).
For pipe making, plate width sets the pipe circumference, so state the width tolerance and edge condition that suit the forming route (UOE, JCOE or roll bending). Untrimmed edges must not have cracks or defects deeper than half the width tolerance (clause 6.9.3).
GB/T 21237-2018 plates are 6-50 mm. Thicker line-pipe plate falls under the 2026 edition (6-90 mm) or a project specification.
Applications and service limits for L320/X46 PSL1
Typical uses of L320/X46 PSL1 plate:
- Extensions and repairs of existing X46 lines
- Medium-pressure oil, gas and water lines where X46 pipe is specified
- Fabricated fittings matched to X46 line pipe
- Water and slurry pipe designed on a 320 MPa yield
Service limits: Because X46 is an intermediate level, confirm early whether the pipe order really needs X46 or accepts X52. PSL1 has no toughness or CE requirements; use L320M when the pipe standard calls for PSL2.
Testing and inspection for L320/X46 PSL1 plate
GB/T 21237-2018 Table 11 sets the tests and sampling. For PSL1 the mandatory items are:
| Test | Quantity and location | Method |
|---|---|---|
| Chemical composition | 1 per heat | GB/T 20066 |
| Tensile test | 1 per lot, at 1/2 plate width | GB/T 228.1 |
| Bend test (180°, D = 2a) | 1 per lot, at 1/4 plate width | GB/T 232 |
| Dimensions and shape | Every plate | Suitable gauges |
| Surface quality | Every plate | Visual |
Charpy, DWTT, hardness, grain size, non-metallic inclusion and banding requirements (clauses 6.6-6.8 and 6.10) apply to PSL2 plates only. A PSL1 order can still ask for selected tests, but they then become contract terms rather than standard PSL1 requirements. Retests follow GB/T 17505 and results are rounded per GB/T 8170.
Order checklist from clause 4: standard number, PSL, grade (L320/X46), size and thickness accuracy, delivery condition, weight, edge condition, test-piece direction, service (gas, oil or other fluid) and any special requirement.
Equivalent and related grades for L320/X46 PSL1
GB/T 21237 grade names match the pipe grades they feed. Annex A of the standard maps L320/X46 to X46 / L320 in GB/T 9711 and ISO 3183, which share the API 5L grade system. The match is at pipe-grade level: the plate must still be ordered so that the finished pipe, after forming and expansion, meets the pipe standard.
| Standard | Grade | Relation | Product page |
|---|---|---|---|
| GB/T 21237-2018 | L320/X46 PSL1 | This page | – |
| API 5L / ISO 3183 / GB/T 9711 | X46 (L320) PSL1 | Same pipe grade (GB/T 21237 Annex A) | X46 PSL1 |
| GB/T 21237-2018 | L320M/X46M PSL2 | Same strength level, PSL2 TMCP plate | L320M |
| API 5L | X46 PSL2 | Pipe grade at PSL2 | API 5L X46 PSL2 |
| Category | Pipeline plate hubs | Family navigation | Pipeline Steel Plates · API 5L |
L320/X46 PSL1 vs neighbouring grades and PSL2 (selection aid)
L320/X46 PSL1 against its neighbouring PSL1 grades (GB/T 21237-2018 Tables 1, 2 and 4):
| Item | L320/X46 | L290/X42 | L360/X52 |
|---|---|---|---|
| Rt0.5 min (MPa) | ≥ 320 | ≥ 290 | ≥ 360 |
| Rm min (MPa) | ≥ 435 | ≥ 415 | ≥ 460 |
| A min (%) | 20 | 21 | 19 |
| C / Mn max (%) | 0.26 / 1.40 | 0.26 / 1.30 | 0.26 / 1.40 |
| TMCP listed | Yes | Yes | Yes |
| Page | This page | L290 PSL1 | L360 PSL1 |
Same strength, PSL1 vs PSL2:
| Item | L320/X46 PSL1 | L320M/X46M PSL2 |
|---|---|---|
| Rt0.5 (MPa) | ≥ 320 | 320-525 |
| Rm (MPa) | ≥ 435 | 435-655 |
| Rt0.5/Rm max | Not specified | 0.90 |
| C max (%) | 0.26 | 0.22 |
| P / S max (%) | 0.030 / 0.030 | 0.025 / 0.015 |
| CE limit | None | CEIIW 0.43 / CEPcm 0.25 |
| Charpy at -20 °C (when contracted) | Not specified | ≥ 90 J |
| Page | This page | L320M |
Why choose SHH STEEL for L320/X46 PSL1 plate
- SHH STEEL supplies GB/T 21237 L320/X46 PSL1 plate from Chinese plate mills for line-pipe makers and fabricators
- Quality certificate per GB/T 247 with heat analysis, tensile and bend results; EN 10204 3.1 standard, 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Plate ordered to the pipe maker’s needs: thickness accuracy, width tolerance, edge condition and delivery state written into the contract
- Optional extras on request, such as a CE cap, ultrasonic testing or impact tests, agreed as contract terms
- One supply chain for PSL1, PSL2 and API 5L referenced plate: Pipeline Steel Plates · API 5L
Supply, cutting and inspection for L320/X46 PSL1
| Item | SHH STEEL supply note |
|---|---|
| Thickness | 6-50 mm (GB/T 21237-2018 range) |
| Size | Width and length to suit the pipe size and mill capability, confirmed at quotation |
| Delivery condition | Hot rolled, normalized, normalizing rolled or thermomechanically rolled (TMCP) |
| Edge | Trimmed (EC) or untrimmed (EM) |
| Processing | Cutting to size and edge preparation on request |
| Certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | GB/T 21237-2018, PSL1, L320/X46, thickness × width × length, thickness accuracy, quantity, delivery condition, edge condition, pipe standard and service (gas / oil / other) |
FAQ
-
What API 5L grade is GB/T 21237 L320/X46 PSL1 equal to?
- Pipe grade X46 (L320) of API 5L, ISO 3183 and GB/T 9711, as listed in Annex A of GB/T 21237-2018. Table 2 chemistry and Table 4 minimum strengths follow the PSL1 pipe values.
-
What thickness range does GB/T 21237-2018 cover?
- 6-50 mm. Plates above 25.0 mm may have chemistry agreed between buyer and mill.
-
Does L320/X46 PSL1 require Charpy or DWTT testing?
- No. Toughness, hardness, grain size and cleanliness requirements apply only to PSL2 plates. Any test added to a PSL1 order is a contract term.
-
What delivery conditions are allowed?
- Hot rolled, normalized, normalizing rolled or thermomechanically rolled, per Table 1 of GB/T 21237-2018.
-
Is there a PSL2 version?
- Yes: L320M (TMCP), plus the same strength level in the other PSL2 delivery states listed in Table 1.
-
Which edition should the order quote?
- This page follows GB/T 21237-2018. GB/T 21237-2026 takes effect on 1 December 2026, so state the edition on the PO and check it on the MTC.
Request a quotation
Send GB/T 21237-2018 L320/X46 PSL1, plate thickness × width × length, thickness accuracy, quantity, delivery condition, edge condition (EC / EM), the pipe standard and service (gas, oil or other fluid), and any extra tests or inspection. SHH STEEL will confirm mill availability, certification scope and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097