GB/T 21237 L390 (X56) PSL1 Pipeline Steel Plate | GB/T 21237 Pipeline Steel - SHH STEEL

GB/T 21237 L390 (X56) PSL1 Pipeline Steel Plate

GB/T 21237 L390/X56 PSL1 is a hot-rolled wide and heavy plate, 6-50 mm thick, for welded oil and gas line pipe at the X56 (L390) level of API 5L, ISO 3183 and GB/T 9711. It is specified by Rt0.5 ≥ 390 MPa, Rm ≥ 490 MPa and elongation A ≥ 18%, with C ≤ 0.26% and Mn ≤ 1.40%. SHH STEEL supplies it with a GB/T 247 quality certificate (EN 10204 3.1, or 3.2 on request).
Equivalent Grades:
API 5L / ISO 3183 / GB/T 9711 X56 (L390) PSL1 per GB/T 21237 Annex A; PSL2 counterpart GB/T 21237 L390M/X56M. Confirm against the pipe specification.
Heat Treatment
Hot rolled, normalized, normalizing rolled or thermomechanically rolled (TMCP). Per GB/T 21237-2018 Table 1.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Testing and inspection
Equivalent Material Grade
L390/X56 PSL1 vs related grades
Why choose Us
Our Service
FAQ
Conclusion

What is GB/T 21237 L390/X56 PSL1 steel plate?

GB/T 21237 L390/X56 PSL1 is the X56 (L390) level of the standard at PSL1. Table 2 keeps the X52 limits for carbon and manganese (C ≤ 0.26%, Mn ≤ 1.40%), while the C/Mn trade-off cap rises to 1.75% Mn.

GB/T 21237-2018 covers hot-rolled wide and heavy plates, 6-50 mm thick, for oil and natural gas line pipe made to ISO 3183, GB/T 9711 and API Spec 5L; plates for other welded fluid pipe may also refer to it. The grade name follows the pipe grade: L for line, then the pipe’s specified minimum yield in MPa, with the API style name (X56) as the common alternative. PSL1 grades carry no delivery-state letter.

X56 is used where a moderate strength increase over X52 reduces wall thickness for medium-pressure oil and gas lines, without going to the X60-plus class.

Category hubs: Pipeline Steel Plates · API 5L line pipe plates. Pipe-grade reference at the same strength: API 5L X56 PSL1; PSL2 plate at this level: GB/T 21237 L390M.

Neighbouring PSL1 plate grades: GB/T 21237 L360 PSL1 · GB/T 21237 L415 PSL1.

Material Specification for GB/T 21237 L390/X56 PSL1

Parameter Specification
Standard GB/T 21237-2018 (implemented 2019-02-01). GB/T 21237-2026 was issued 2026-05-25 and takes effect 2026-12-01, replacing the 2018 edition; it widens thickness to 6-90 mm and adds sour, offshore, fittings, high-deformability, bend and station plate annexes. Confirm the edition on the PO and MTC.
Grade L390/X56 (PSL1)
Quality level PSL1 (product specification level 1)
Equivalent pipe grade X56 / L390 of API 5L, ISO 3183 and GB/T 9711 (GB/T 21237 Annex A)
Product form Hot-rolled wide and heavy plate for line pipe
Thickness range (standard) 6-50 mm
Dimensions and tolerances GB/T 709, or other sizes and tolerances by agreement (clause 5)
Delivery condition Hot rolled, normalized, normalizing rolled or thermomechanically rolled (TMCP)
Edge condition Trimmed (EC) or untrimmed (EM)
Steelmaking Basic oxygen or electric furnace (route chosen by the supplier unless specified)
Inspection lot Same grade, heat, thickness, rolling and heat-treatment schedule; ≤ 60 t per lot
Certification Quality certificate per GB/T 247; EN 10204 3.1 MTC, 3.2 on request
Density 7.85 g/cm³

Chemical Composition of L390/X56 PSL1 (heat and product analysis)

GB/T 21237-2018 Table 2 limits apply to both heat (ladle) analysis and product analysis, so one table covers both. Values are maximum mass %. The supplier may report heat analysis only but must guarantee the product analysis limits (clause 6.1.4). For plates over 25.0 mm, chemistry may be agreed separately (clause 6.1.3).

Grade (PSL1) C Mn P S V Nb Ti
L390/X56 0.26 1.40 0.030 0.030 see (d) see (d) see (d)

Table 2 notes that apply:

  • Cu ≤ 0.50%, Ni ≤ 0.50%, Cr ≤ 0.50%, Mo ≤ 0.15%.
  • Boron shall not be intentionally added unless otherwise specified; residual B ≤ 0.001%.
  • For each 0.01% below the specified maximum C, Mn may exceed its maximum by 0.05%, up to 1.75% for this grade.
  • (d) Nb + V + Ti ≤ 0.15%.
  • For L290/X42 and higher, elements other than those listed (including Nb, V, Ti) may be added by agreement (clause 6.1.6).

PSL1 has no Si limit and no carbon-equivalent limit in GB/T 21237-2018. If the pipe mill needs a CE cap for seam welding, write it into the purchase order.

Mechanical Properties of L390/X56 PSL1 plate

GB/T 21237-2018 Table 4 sets minimum values only for PSL1. Note (a) of the table asks buyer and mill to agree a suitable tensile range so that the finished pipe meets its own standard after forming. The buyer chooses the test direction and states it in the contract; normally it is transverse to the pipe axis.

Grade Rt0.5 (MPa) Rm (MPa) A50mm (%) A (%) Bend test
L390/X56 ≥ 390 ≥ 490 Per formula (3), clause 6.5.4 ≥ 18 180°, D = 2a, no cracks

Rt0.5 is the specified total extension strength at 0.5% extension, the same yield definition used for line pipe. The minimum A50mm elongation is calculated from the specimen cross-section and the specified minimum tensile strength (formula (3), the same approach as ISO 3183 / API 5L). In a dispute, a 50 mm gauge, 38 mm wide specimen is the referee. Tensile tests up to L485/X70 use full-thickness rectangular specimens (clause 6.5.5).

PSL1 has no maximum yield, no yield-to-tensile ratio limit and no Charpy or DWTT requirement. These controls exist only at PSL2: L390M is held to Rt0.5 390-545 MPa, Rm 490-760 MPa and Rt0.5/Rm ≤ 0.90.

Delivery Conditions for L390/X56 PSL1 plate

Hot rolled, normalized, normalizing rolled or thermomechanically rolled (TMCP).

Table 1 of GB/T 21237-2018 lists the delivery conditions allowed for each PSL1 grade. The mill selects the route that meets Table 4 for the ordered thickness unless the buyer specifies one. For X56 plate at heavier thickness, TMCP is the usual route because it reaches the strength at a lower carbon equivalent; hot rolled or normalized plate is used where the pipe maker prefers it.

State the delivery condition and edge condition (EC trimmed or EM untrimmed) on the order. Weld repair of the plate surface is not permitted (clause 6.9.5); surface defects may be ground out only within half the thickness tolerance while keeping the minimum thickness.

Weldability of L390/X56 PSL1 line pipe plate

L390/X56 PSL1 is a C-Mn, optionally micro-alloyed, line-pipe plate intended for longitudinal seam welding, most often SAW for LSAW pipe, followed by girth welding in the field. With C up to 0.26% allowed, weldability depends on the actual heat chemistry, so check the MTC carbon and manganese before qualifying the seam-weld procedure.

Because PSL1 has no CE limit, many pipe mills add a CEIIW or CEPcm cap to the plate order. Preheat, heat input and consumables follow the qualified WPS for the pipe standard (for example ISO 3183 / API 5L / GB/T 9711 welding requirements).

Dimensional Tolerances for L390/X56 PSL1

Dimensions, shape, weight and tolerances follow GB/T 709 (hot-rolled steel plates and strips) unless other sizes, shapes and tolerances are agreed and written into the contract (clause 5.2). The order must state the size and the required thickness accuracy (clause 4).

For pipe making, plate width sets the pipe circumference, so state the width tolerance and edge condition that suit the forming route (UOE, JCOE or roll bending). Untrimmed edges must not have cracks or defects deeper than half the width tolerance (clause 6.9.3).

GB/T 21237-2018 plates are 6-50 mm. Thicker line-pipe plate falls under the 2026 edition (6-90 mm) or a project specification.

Applications and service limits for L390/X56 PSL1

Typical uses of L390/X56 PSL1 plate:

  • Medium-pressure oil and gas transmission lines
  • Regional gas pipelines where X56 pipe is specified
  • Water and product lines designed on a 390 MPa yield
  • Fittings and bends matched to X56 pipe

Service limits: Like other PSL1 grades, L390/X56 plate carries no impact, DWTT, CE or hardness requirement. For PSL2 pipe use L390M.

Testing and inspection for L390/X56 PSL1 plate

GB/T 21237-2018 Table 11 sets the tests and sampling. For PSL1 the mandatory items are:

Test Quantity and location Method
Chemical composition 1 per heat GB/T 20066
Tensile test 1 per lot, at 1/2 plate width GB/T 228.1
Bend test (180°, D = 2a) 1 per lot, at 1/4 plate width GB/T 232
Dimensions and shape Every plate Suitable gauges
Surface quality Every plate Visual

Charpy, DWTT, hardness, grain size, non-metallic inclusion and banding requirements (clauses 6.6-6.8 and 6.10) apply to PSL2 plates only. A PSL1 order can still ask for selected tests, but they then become contract terms rather than standard PSL1 requirements. Retests follow GB/T 17505 and results are rounded per GB/T 8170.

Order checklist from clause 4: standard number, PSL, grade (L390/X56), size and thickness accuracy, delivery condition, weight, edge condition, test-piece direction, service (gas, oil or other fluid) and any special requirement.

Equivalent and related grades for L390/X56 PSL1

GB/T 21237 grade names match the pipe grades they feed. Annex A of the standard maps L390/X56 to X56 / L390 in GB/T 9711 and ISO 3183, which share the API 5L grade system. The match is at pipe-grade level: the plate must still be ordered so that the finished pipe, after forming and expansion, meets the pipe standard.

Standard Grade Relation Product page
GB/T 21237-2018 L390/X56 PSL1 This page –
API 5L / ISO 3183 / GB/T 9711 X56 (L390) PSL1 Same pipe grade (GB/T 21237 Annex A) X56 PSL1
GB/T 21237-2018 L390M/X56M PSL2 Same strength level, PSL2 TMCP plate L390M
API 5L X56 PSL2 Pipe grade at PSL2 API 5L X56 PSL2
Category Pipeline plate hubs Family navigation Pipeline Steel Plates · API 5L

L390/X56 PSL1 vs neighbouring grades and PSL2 (selection aid)

L390/X56 PSL1 against its neighbouring PSL1 grades (GB/T 21237-2018 Tables 1, 2 and 4):

Item L390/X56 L360/X52 L415/X60
Rt0.5 min (MPa) ≥ 390 ≥ 360 ≥ 415
Rm min (MPa) ≥ 490 ≥ 460 ≥ 520
A min (%) 18 19 17
C / Mn max (%) 0.26 / 1.40 0.26 / 1.40 0.26 / 1.40
TMCP listed Yes Yes Yes
Page This page L360 PSL1 L415 PSL1

Same strength, PSL1 vs PSL2:

Item L390/X56 PSL1 L390M/X56M PSL2
Rt0.5 (MPa) ≥ 390 390-545
Rm (MPa) ≥ 490 490-760
Rt0.5/Rm max Not specified 0.90
C max (%) 0.26 0.22
P / S max (%) 0.030 / 0.030 0.025 / 0.015
CE limit None CEIIW 0.43 / CEPcm 0.25
Charpy at -20 °C (when contracted) Not specified ≥ 120 J
Page This page L390M

Why choose SHH STEEL for L390/X56 PSL1 plate

  • SHH STEEL supplies GB/T 21237 L390/X56 PSL1 plate from Chinese plate mills for line-pipe makers and fabricators
  • Quality certificate per GB/T 247 with heat analysis, tensile and bend results; EN 10204 3.1 standard, 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
  • Plate ordered to the pipe maker’s needs: thickness accuracy, width tolerance, edge condition and delivery state written into the contract
  • Optional extras on request, such as a CE cap, ultrasonic testing or impact tests, agreed as contract terms
  • One supply chain for PSL1, PSL2 and API 5L referenced plate: Pipeline Steel Plates · API 5L

Supply, cutting and inspection for L390/X56 PSL1

Item SHH STEEL supply note
Thickness 6-50 mm (GB/T 21237-2018 range)
Size Width and length to suit the pipe size and mill capability, confirmed at quotation
Delivery condition Hot rolled, normalized, normalizing rolled or thermomechanically rolled (TMCP)
Edge Trimmed (EC) or untrimmed (EM)
Processing Cutting to size and edge preparation on request
Certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV or ABS can be arranged
Quotation needs GB/T 21237-2018, PSL1, L390/X56, thickness × width × length, thickness accuracy, quantity, delivery condition, edge condition, pipe standard and service (gas / oil / other)

FAQ

What API 5L grade is GB/T 21237 L390/X56 PSL1 equal to?
Pipe grade X56 (L390) of API 5L, ISO 3183 and GB/T 9711, as listed in Annex A of GB/T 21237-2018. Table 2 chemistry and Table 4 minimum strengths follow the PSL1 pipe values.
What thickness range does GB/T 21237-2018 cover?
6-50 mm. Plates above 25.0 mm may have chemistry agreed between buyer and mill.
Does L390/X56 PSL1 require Charpy or DWTT testing?
No. Toughness, hardness, grain size and cleanliness requirements apply only to PSL2 plates. Any test added to a PSL1 order is a contract term.
What delivery conditions are allowed?
Hot rolled, normalized, normalizing rolled or thermomechanically rolled, per Table 1 of GB/T 21237-2018.
Is there a PSL2 version?
Yes: L390M (TMCP), plus the same strength level in the other PSL2 delivery states listed in Table 1.
Which edition should the order quote?
This page follows GB/T 21237-2018. GB/T 21237-2026 takes effect on 1 December 2026, so state the edition on the PO and check it on the MTC.

Request a quotation

Send GB/T 21237-2018 L390/X56 PSL1, plate thickness × width × length, thickness accuracy, quantity, delivery condition, edge condition (EC / EM), the pipe standard and service (gas, oil or other fluid), and any extra tests or inspection. SHH STEEL will confirm mill availability, certification scope and a quotation.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: Pipeline Steel Plates · API 5L · X56 PSL1 · L390M

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X