GB/T 21237 L210 (A) PSL1 Pipeline Steel Plate
What is GB/T 21237 L210/A PSL1 steel plate?
GB/T 21237 L210/A PSL1 is the entry strength level of GB/T 21237. It mirrors Grade A (L210) of API 5L / ISO 3183 / GB/T 9711 and is the only PSL1 grade in the standard that is not listed for thermomechanically rolled delivery.
GB/T 21237-2018 covers hot-rolled wide and heavy plates, 6-50 mm thick, for oil and natural gas line pipe made to ISO 3183, GB/T 9711 and API Spec 5L; plates for other welded fluid pipe may also refer to it. The grade name follows the pipe grade: L for line, then the pipe’s specified minimum yield in MPa, with the API style name (A) as the common alternative. PSL1 grades carry no delivery-state letter.
Buyers use it when the pipe design needs only a 210 MPa minimum yield and the priority is easy forming and welding with a simple C-Mn chemistry: low-pressure water, utility and fluid lines, sleeves and non-critical fabricated pipe.
Category hubs: Pipeline Steel Plates · API 5L line pipe plates. Pipe-grade reference at the same strength: API 5L Grade A PSL1.
Neighbouring PSL1 plate grades: GB/T 21237 L245 PSL1.
Material Specification for GB/T 21237 L210/A PSL1
| Parameter | Specification |
|---|---|
| Standard | GB/T 21237-2018 (implemented 2019-02-01). GB/T 21237-2026 was issued 2026-05-25 and takes effect 2026-12-01, replacing the 2018 edition; it widens thickness to 6-90 mm and adds sour, offshore, fittings, high-deformability, bend and station plate annexes. Confirm the edition on the PO and MTC. |
| Grade | L210/A (PSL1) |
| Quality level | PSL1 (product specification level 1) |
| Equivalent pipe grade | Grade A / L210 of API 5L, ISO 3183 and GB/T 9711 (GB/T 21237 Annex A) |
| Product form | Hot-rolled wide and heavy plate for line pipe |
| Thickness range (standard) | 6-50 mm |
| Dimensions and tolerances | GB/T 709, or other sizes and tolerances by agreement (clause 5) |
| Delivery condition | Hot rolled, normalized or normalizing rolled (thermomechanical rolling is not listed for L210/A) |
| Edge condition | Trimmed (EC) or untrimmed (EM) |
| Steelmaking | Basic oxygen or electric furnace (route chosen by the supplier unless specified) |
| Inspection lot | Same grade, heat, thickness, rolling and heat-treatment schedule; ≤ 60 t per lot |
| Certification | Quality certificate per GB/T 247; EN 10204 3.1 MTC, 3.2 on request |
| Density | 7.85 g/cm³ |
Chemical Composition of L210/A PSL1 (heat and product analysis)
GB/T 21237-2018 Table 2 limits apply to both heat (ladle) analysis and product analysis, so one table covers both. Values are maximum mass %. The supplier may report heat analysis only but must guarantee the product analysis limits (clause 6.1.4). For plates over 25.0 mm, chemistry may be agreed separately (clause 6.1.3).
| Grade (PSL1) | C | Mn | P | S | V | Nb | Ti |
|---|---|---|---|---|---|---|---|
| L210/A | 0.22 | 0.90 | 0.030 | 0.030 | – | – | – |
Table 2 notes that apply:
- Cu ≤ 0.50%, Ni ≤ 0.50%, Cr ≤ 0.50%, Mo ≤ 0.15%.
- Boron shall not be intentionally added unless otherwise specified; residual B ≤ 0.001%.
PSL1 has no Si limit and no carbon-equivalent limit in GB/T 21237-2018. If the pipe mill needs a CE cap for seam welding, write it into the purchase order.
Mechanical Properties of L210/A PSL1 plate
GB/T 21237-2018 Table 4 sets minimum values only for PSL1. Note (a) of the table asks buyer and mill to agree a suitable tensile range so that the finished pipe meets its own standard after forming. The buyer chooses the test direction and states it in the contract; normally it is transverse to the pipe axis.
| Grade | Rt0.5 (MPa) | Rm (MPa) | A50mm (%) | A (%) | Bend test |
|---|---|---|---|---|---|
| L210/A | ≥ 210 | ≥ 335 | Per formula (3), clause 6.5.4 | ≥ 25 | 180°, D = 2a, no cracks |
Rt0.5 is the specified total extension strength at 0.5% extension, the same yield definition used for line pipe. The minimum A50mm elongation is calculated from the specimen cross-section and the specified minimum tensile strength (formula (3), the same approach as ISO 3183 / API 5L). In a dispute, a 50 mm gauge, 38 mm wide specimen is the referee. Tensile tests up to L485/X70 use full-thickness rectangular specimens (clause 6.5.5).
PSL1 has no maximum yield, no yield-to-tensile ratio limit and no Charpy or DWTT requirement. These controls exist only at PSL2.
Delivery Conditions for L210/A PSL1 plate
Hot rolled, normalized or normalizing rolled (thermomechanical rolling is not listed for L210/A).
Table 1 of GB/T 21237-2018 lists the delivery conditions allowed for each PSL1 grade. The mill selects the route that meets Table 4 for the ordered thickness unless the buyer specifies one. For L210/A the standard lists hot rolled, normalized and normalizing rolled only.
State the delivery condition and edge condition (EC trimmed or EM untrimmed) on the order. Weld repair of the plate surface is not permitted (clause 6.9.5); surface defects may be ground out only within half the thickness tolerance while keeping the minimum thickness.
Weldability of L210/A PSL1 line pipe plate
L210/A PSL1 is a C-Mn line-pipe plate intended for longitudinal seam welding, most often SAW for LSAW pipe, followed by girth welding in the field. With C up to 0.22% allowed, weldability depends on the actual heat chemistry, so check the MTC carbon and manganese before qualifying the seam-weld procedure.
Because PSL1 has no CE limit, many pipe mills add a CEIIW or CEPcm cap to the plate order. Preheat, heat input and consumables follow the qualified WPS for the pipe standard (for example ISO 3183 / API 5L / GB/T 9711 welding requirements).
Dimensional Tolerances for L210/A PSL1
Dimensions, shape, weight and tolerances follow GB/T 709 (hot-rolled steel plates and strips) unless other sizes, shapes and tolerances are agreed and written into the contract (clause 5.2). The order must state the size and the required thickness accuracy (clause 4).
For pipe making, plate width sets the pipe circumference, so state the width tolerance and edge condition that suit the forming route (UOE, JCOE or roll bending). Untrimmed edges must not have cracks or defects deeper than half the width tolerance (clause 6.9.3).
GB/T 21237-2018 plates are 6-50 mm. Thicker line-pipe plate falls under the 2026 edition (6-90 mm) or a project specification.
Applications and service limits for L210/A PSL1
Typical uses of L210/A PSL1 plate:
- Low-pressure water and utility pipe made from plate
- Non-critical fluid lines and casing sleeves where Grade A pipe is specified
- Fabricated bends, reducers and spools made to an A / L210 pipe order
- Projects that still cite Grade A in older line-pipe drawings
Service limits: L210/A has no PSL2 version in GB/T 21237-2018, so it carries no carbon-equivalent cap and no Charpy, DWTT or hardness requirement. It is not an option where the pipe order requires PSL2, toughness testing or sour service. In that case move up to GB/T 21237 L245M.
Testing and inspection for L210/A PSL1 plate
GB/T 21237-2018 Table 11 sets the tests and sampling. For PSL1 the mandatory items are:
| Test | Quantity and location | Method |
|---|---|---|
| Chemical composition | 1 per heat | GB/T 20066 |
| Tensile test | 1 per lot, at 1/2 plate width | GB/T 228.1 |
| Bend test (180°, D = 2a) | 1 per lot, at 1/4 plate width | GB/T 232 |
| Dimensions and shape | Every plate | Suitable gauges |
| Surface quality | Every plate | Visual |
Charpy, DWTT, hardness, grain size, non-metallic inclusion and banding requirements (clauses 6.6-6.8 and 6.10) apply to PSL2 plates only. A PSL1 order can still ask for selected tests, but they then become contract terms rather than standard PSL1 requirements. Retests follow GB/T 17505 and results are rounded per GB/T 8170.
Order checklist from clause 4: standard number, PSL, grade (L210/A), size and thickness accuracy, delivery condition, weight, edge condition, test-piece direction, service (gas, oil or other fluid) and any special requirement.
Equivalent and related grades for L210/A PSL1
GB/T 21237 grade names match the pipe grades they feed. Annex A of the standard maps L210/A to Grade A / L210 in GB/T 9711 and ISO 3183, which share the API 5L grade system. The match is at pipe-grade level: the plate must still be ordered so that the finished pipe, after forming and expansion, meets the pipe standard.
| Standard | Grade | Relation | Product page |
|---|---|---|---|
| GB/T 21237-2018 | L210/A PSL1 | This page | – |
| API 5L / ISO 3183 / GB/T 9711 | Grade A (L210) PSL1 | Same pipe grade (GB/T 21237 Annex A) | Grade A PSL1 |
| EN 10208-1 (superseded by EN ISO 3183) | L210GA | Approximate legacy class A pipe grade | EN 10208-1 hub |
| Category | Pipeline plate hubs | Family navigation | Pipeline Steel Plates · API 5L |
L210/A PSL1 vs neighbouring grades and PSL2 (selection aid)
L210/A PSL1 against its neighbouring PSL1 grades (GB/T 21237-2018 Tables 1, 2 and 4):
| Item | L210/A | L245/B |
|---|---|---|
| Rt0.5 min (MPa) | ≥ 210 | ≥ 245 |
| Rm min (MPa) | ≥ 335 | ≥ 415 |
| A min (%) | 25 | 21 |
| C / Mn max (%) | 0.22 / 0.90 | 0.26 / 1.20 |
| TMCP listed | No | Yes |
| Page | This page | L245 PSL1 |
Why choose SHH STEEL for L210/A PSL1 plate
- SHH STEEL supplies GB/T 21237 L210/A PSL1 plate from Chinese plate mills for line-pipe makers and fabricators
- Quality certificate per GB/T 247 with heat analysis, tensile and bend results; EN 10204 3.1 standard, 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Plate ordered to the pipe maker’s needs: thickness accuracy, width tolerance, edge condition and delivery state written into the contract
- Optional extras on request, such as a CE cap, ultrasonic testing or impact tests, agreed as contract terms
- One supply chain for PSL1, PSL2 and API 5L referenced plate: Pipeline Steel Plates · API 5L
Supply, cutting and inspection for L210/A PSL1
| Item | SHH STEEL supply note |
|---|---|
| Thickness | 6-50 mm (GB/T 21237-2018 range) |
| Size | Width and length to suit the pipe size and mill capability, confirmed at quotation |
| Delivery condition | Hot rolled, normalized or normalizing rolled (thermomechanical rolling is not listed for L210/A) |
| Edge | Trimmed (EC) or untrimmed (EM) |
| Processing | Cutting to size and edge preparation on request |
| Certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | GB/T 21237-2018, PSL1, L210/A, thickness × width × length, thickness accuracy, quantity, delivery condition, edge condition, pipe standard and service (gas / oil / other) |
FAQ
-
What API 5L grade is GB/T 21237 L210/A PSL1 equal to?
- Pipe grade Grade A (L210) of API 5L, ISO 3183 and GB/T 9711, as listed in Annex A of GB/T 21237-2018. Table 2 chemistry and Table 4 minimum strengths follow the PSL1 pipe values.
-
What thickness range does GB/T 21237-2018 cover?
- 6-50 mm. Plates above 25.0 mm may have chemistry agreed between buyer and mill.
-
Does L210/A PSL1 require Charpy or DWTT testing?
- No. Toughness, hardness, grain size and cleanliness requirements apply only to PSL2 plates. Any test added to a PSL1 order is a contract term.
-
Can L210/A be supplied TMCP?
- Table 1 lists hot rolled, normalized or normalizing rolled delivery for L210/A. TMCP is listed from L245/B upward.
-
Is there a PSL2 version?
- No. GB/T 21237-2018 has no PSL2 L210 grade. The lowest PSL2 level is Grade B (L245R, L245N, L245Q, L245M).
-
Which edition should the order quote?
- This page follows GB/T 21237-2018. GB/T 21237-2026 takes effect on 1 December 2026, so state the edition on the PO and check it on the MTC.
Request a quotation
Send GB/T 21237-2018 L210/A PSL1, plate thickness × width × length, thickness accuracy, quantity, delivery condition, edge condition (EC / EM), the pipe standard and service (gas, oil or other fluid), and any extra tests or inspection. SHH STEEL will confirm mill availability, certification scope and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: Pipeline Steel Plates · API 5L · Grade A PSL1