GB/T 11251 50B Alloy Steel Plate
What is GB/T 11251 Grade 50B plate?
GB/T 11251 50B Alloy Steel Plate is alloy structural steel plate and strip purchased to GB/T 11251-2025. Grade 50B is one of the fourteen grades for which the 2025 edition publishes annealed single-rolled tensile and elongation values in Table 1. It has a higher carbon window than Grades 40B and 45B and a specified boron addition.
The 2025 edition is a plate and strip specification. Chemical composition shall comply with GB/T 3077, used here as the chemistry reference, not as the delivery specification.
Single-rolled plate is usually supplied high-temperature tempered unless another condition is agreed. Table 1 tensile values apply only to annealed single-rolled plate not thicker than 100 mm. Grade 50B is not an automatic substitute for Grade 40B, 45B or 40Cr.
SHH STEEL produces and exports GB/T 11251-2025 Grade 50B plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry. This grade belongs to our Alloy Steel Plates range under GB/T 11251.
Material specification for GB/T 11251 Grade 50B
The items below follow GB/T 11251-2025. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | GB/T 11251-2025, Alloy structural steel plate, sheet and strip. Published 31 October 2025 and implemented 1 May 2026. It replaces GB/T 11251-2020 and GB/T 37601-2019 |
| Grade designation | Grade 50B, boron alloy structural steel plate listed in GB/T 11251-2025 Table 1 |
| Product forms in the standard | Single-rolled hot-rolled plate, nominal thickness 3.0 mm to 250 mm; and continuous-rolled plate and strip, nominal thickness not greater than 25.4 mm (wide strip and cut plate or slit strip 600 mm wide or more, and narrow strip and cut plate under 600 mm) |
| Chemical composition | Shall comply with GB/T 3077. Optional phosphorus or sulfur variants may be agreed under clause 6.1.1. Product analysis shall meet GB/T 222 |
| Single-rolled delivery | High-temperature tempered as the usual condition; annealed, normalized, normalized and tempered, or quenched and tempered by agreement. Normalizing rolling may replace normalizing if the normalized mechanical requirements can be met |
| Continuous-rolled delivery | As-rolled; heat treatment by agreement. If spheroidize-annealed, surface hardness shall meet GB/T 3077. Tensile tests on continuous-rolled material are by agreement |
| Annealed single-rolled mechanics | Table 1 applies to Grade 50B at nominal thickness not greater than 100 mm. Thickness over 100 mm, and grades other than Table 1, are by agreement |
| Dimensions | Single-rolled plate to GB/T 709-2019, thickness tolerance class A. Wide strip and cut plate or slit strip to GB/T 709-2019 Table 4 thickness tolerances; flatness by agreement. Narrow strip and cut plate to Annex A |
| Ultrasonic testing | Single-rolled plate 6 mm thick or thicker shall be tested to GB/T 2970-2016 Class II unless another method and class are agreed |
| Our supply | We produce and export Grade 50B to the GB/T 11251-2025 form, delivery condition, dimensions and extra tests agreed on the order |
Chemical composition of GB/T 11251 Grade 50B
GB/T 11251-2025 requires the grade and chemical composition to comply with GB/T 3077. The melt-analysis figures below are published GB/T 3077-2015 values for Grade 50B. They are not a separate chemistry table printed inside GB/T 11251-2025 itself, and they must not be read as an older GB/T 11251-2020 or GB/T 37601-2019 reprint labelled as 2025. Product-analysis tolerances shall meet GB/T 222; use the applicable GB/T 222 limits for acceptance.
| Element | Reference melt analysis (wt. %) |
|---|---|
| Carbon (C) | 0.47-0.55 |
| Silicon (Si) | 0.17-0.37 |
| Manganese (Mn) | 0.60-0.90 |
| Boron (B) | 0.0008-0.0035 |
Phosphorus and sulfur depend on the GB/T 3077 quality class ordered: ordinary quality steel, high-quality steel designated by adding A, or extra-quality steel designated by adding E. Published secondary tables sometimes round those maxima; confirm the class and the limits on the mill test certificate. GB/T 11251-2025 also allows, by agreement on the contract, sulfur of 0.015% to 0.035% or not greater than 0.005%, or phosphorus not greater than 0.015%. Residual elements that are not specified alloying additions are limited by GB/T 3077.
Mechanical properties and optional tests
For annealed single-rolled plate of Grade 50B with nominal thickness not greater than 100 mm, GB/T 11251-2025 Table 1 specifies tensile strength Rm of 550-750 MPa and elongation A of not less than 16 %. For nominal thickness greater than 20 mm and not greater than 100 mm, elongation may be reduced by 0.25 % (absolute) for each 1 mm increase in thickness, but by not more than 5 % (absolute).
When single-rolled plate is delivered normalized, elongation shall still meet the Table 1 value and the upper limit of tensile strength may be 50 MPa higher than Table 1. High-temperature tempered single-rolled plate is ordered to surface hardness in accordance with GB/T 3077, not to the annealed Table 1 tensile band. Normalized-and-tempered and quenched-and-tempered single-rolled plate have mechanical properties agreed on the contract. Thickness greater than 100 mm is also by agreement.
Continuous-rolled plate and strip may be tensile-tested only by agreement; those results are not Table 1 values. Quenched-and-tempered GB/T 3077 bar figures must not be read as automatic GB/T 11251 plate minima.
Delivery conditions for GB/T 11251 Grade 50B
GB/T 11251-2025 distinguishes two product routes:
- Single-rolled plate is usually delivered high-temperature tempered. Annealed, normalized, normalized and tempered, or quenched and tempered supply may be agreed and written on the contract. Normalizing rolling may replace normalizing if the normalized mechanical requirements can be guaranteed.
- Continuous-rolled plate and strip are delivered as-rolled unless a heat-treatment condition is agreed. If they are spheroidize-annealed, surface hardness shall meet GB/T 3077.
We produce and export Grade 50B to the agreed route and condition. An enquiry that only says “50B plate” is incomplete, because high-temperature tempered, annealed, normalized and quenched-and-tempered plate are not interchangeable supply states, and single-rolled plate is not the same product as continuous-rolled plate or strip.
Welding and thermal cutting
Boron-treated 50B plate should be welded to a procedure suited to the carbon level, thickness and delivery condition. Preheat, interpass temperature and any post-weld heat treatment depend on thickness, joint restraint and the qualified procedure. Qualify cutting and welding procedures to the project specification, the ordered delivery condition and the actual thickness.
Thermal cutting can harden the adjacent material. That heat-affected zone should be considered, and removed where later forming or welding requires it.
Form, dimensions and inspection
Single-rolled plate dimensions, shape and mass tolerances follow GB/T 709-2019, with thickness tolerance class A unless another class is agreed. Wide strip and plate or slit strip cut from it follow GB/T 709-2019, using the thickness tolerances in Table 4 of that standard; flatness is agreed on the contract. Narrow strip and plate cut from it follow Annex A of GB/T 11251-2025. Other sizes and tolerances may be agreed.
Single-rolled plate 6 mm thick or thicker shall receive ultrasonic testing to GB/T 2970-2016 Class II unless another standard and class are written on the order. For stamping, single-rolled plate not thicker than 10 mm shall pass a 180° bend test with former diameter D = 2a.
Applications and specification limits
We produce and export this grade for general engineering and machinery parts cut from plate and later heat treated to a stated cycle. Buyers specify 50B when they want the higher-carbon boron-treated chemistry listed in Table 1, not when they need Grade 40B, 45B or chromium Grade 40Cr.
As-rolled, high-temperature tempered, annealed and quenched-and-tempered plate do not machine or form at the same strength.
GB/T 11251 is an alloy structural plate and strip specification. It is not a boiler or pressure-vessel specification such as GB/T 713.
Compare GB/T 11251 50B with other steel plates
GB/T 11251 Grade 50B is alloy structural plate and strip under the 2025 Chinese plate specification. The comparison below uses other plates we already publish. These grades are related by engineering use, not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| GB/T 11251 Grade 50B (this plate) | Boron-treated medium-carbon alloy structural plate and strip under GB/T 11251-2025, with a higher carbon window than Grades 40B and 45B | Single-rolled: high-temperature tempered unless annealed, N, NT or QT is agreed. Continuous-rolled: as-rolled unless heat treated by agreement | Annealed single-rolled plate ≤ 100 mm: Rm 550-750 MPa and A ≥ 16 % (Table 1). Other conditions by the rules of the 2025 edition or by agreement | Engineering and machinery parts, often heat treated after cutting | Not Grade 40B, 45B or 40Cr, not a 100 ksi QT structural grade, and not a vessel plate |
| ASTM A829 4140 Alloy Steel Plate | Chromium-molybdenum alloy structural plate under ASTM A829/A829M, usually ordered by heat chemistry | ASTM A829/A829M-25 permits AR, A, N, NT or QT; specify the required condition. | No automatic as-delivered strength package; tensile or hardness only if specified and compatible | Machinery and general engineering parts, often heat treated after cutting | Related alloy structural plate, not a GB/T 11251 equivalent and not a chromium-only or manganese grade substitute |
| ASTM A514 Grade B | Quenched-and-tempered alloy structural plate; chemistry includes chromium, molybdenum, vanadium, titanium and boron | Quenched and tempered | Strength-graded: to 32 mm, yield 100 ksi / 690 MPa min and tensile 110-130 ksi / 760-895 MPa (from our A514 Grade B page). Maximum thickness for Grade B is 1¼ in / 32 mm | Welded bridges and other structures that specify A514 QT plate | Not a substitute for chemistry-referenced GB/T 11251 engineering plate |
| ASTM A572 Grade 50 | High-strength low-alloy structural plate, microalloyed with niobium and vanadium | Hot-rolled or controlled-rolled | Strength-graded: minimum yield 345 MPa and tensile 450 MPa minimum (from our A572 Grade 50 page) | Bridges, buildings, construction equipment, transmission towers and heavy machinery frames | Not an alloy engineering plate of the GB/T 11251 type |
Related published ranges: Structural Steel Plates, ASTM A514/A514M and ASTM A572/A572M.
Equivalent and related grades by country
The designations below are near equivalents or related chemistry-family grades, not certified or automatic equivalents. Chemistry windows, product form, delivery condition and tests must match the project specification before a substitution is considered. Grades without a live page on this site are shown as plain text unless a live contrast page is named.
| Country / region | Standard | Grade | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| China | GB/T 11251-2025 | 50B | This plate and strip specification. Table 1 lists annealed single-rolled tensile and elongation values for this grade at thickness not greater than 100 mm. Carbon is higher than Grades 40B and 45B. | This product |
| China | GB/T 3077-2015 | 50B | The chemistry source cited by GB/T 11251-2025, including the specified boron range. GB/T 3077 is not a plate specification. | Do not treat a 3077 bar enquiry as a 11251 plate order without restating product form, condition and tests. |
| China | GB/T 11251-2025 Table 1 | 40B and 45B | Related boron grades in the same specification, with lower published carbon windows. They do not all have product pages on this site yet. | Related grades, not automatic substitutes. |
| United States, Europe and Japan | — | — | No dedicated foreign plate equivalent is established here; GB/T 3077-2015 Annex A similarity does not establish plate interchangeability. | Do not assume a local boron-bar designation, or Grade 40Cr, is a 11251 50B plate equivalent. |
Table 1 also lists 40B and 45B as related boron grades in the same specification. They are not automatic substitutes and do not all have product pages on this site yet.
Why choose SHH STEEL for GB/T 11251 Grade 50B
- We produce and export GB/T 11251-2025 Grade 50B alloy structural steel plate
- We review the enquiry for edition, grade, product route, delivery condition, dimensions and extra tests
- We keep Table 1 annealed plate values distinct from high-temperature tempered hardness and from GB/T 3077 bar figures
- We match documentation to what the purchase order requires
How to enquire for GB/T 11251 50B plate
| Item | What to specify |
|---|---|
| Standard and grade | GB/T 11251-2025 Grade 50B |
| Product route | Single-rolled plate, or continuous-rolled plate or strip |
| Delivery condition | High-temperature tempered, annealed, normalized, normalized and tempered, quenched and tempered, or as-rolled for continuous-rolled material |
| Dimensions | Required thickness, width and length; we confirm production and export feasibility against the enquiry |
| Chemistry | Melt analysis to GB/T 3077, including any A or E quality class; request product analysis to GB/T 222 only if needed; state any agreed phosphorus or sulfur variant |
| Mechanical tests | State whether Table 1 annealed values, hardness, normalized values or an agreed quenched-and-tempered package applies |
| Other tests | Ultrasonic class if different from the standard Class II rule, bend testing for stamping, decarburization or inclusion rating only when written on the order |
| Documentation | State the inspection document type required by the project |
FAQ
-
Is GB/T 11251 50B ordered only by chemistry?
- Chemistry shall comply with GB/T 3077. For annealed single-rolled plate not thicker than 100 mm, Table 1 of GB/T 11251-2025 also sets tensile strength and elongation. High-temperature tempered plate is ordered to GB/T 3077 hardness. Other conditions are agreed on the contract.
-
How does Grade 50B differ from Grades 40B and 45B?
- Published 3077 melt analysis uses a higher carbon window for 50B (0.47-0.55) than for 45B (0.42-0.49) or 40B (0.37-0.44). Table 1 annealed elongation is also lower for 50B (not less than 16 %) than for 45B (18 %) or 40B (20 %). They are related boron grades, not automatic substitutes.
-
Does Table 1 apply to every delivery condition and thickness?
- No. Table 1 applies to annealed single-rolled plate not thicker than 100 mm. Normalized plate keeps the Table 1 elongation and may use a tensile upper limit 50 MPa higher. Thickness over 100 mm, continuous-rolled tensile tests, and NT or QT supply are by agreement.
-
Did GB/T 11251-2025 replace GB/T 37601?
- Yes. The 2025 edition replaces GB/T 11251-2020 and GB/T 37601-2019 and integrates the continuous-rolled content. Do not order this plate to the withdrawn 37601 specification as if it were still current.
-
What should a quotation enquiry include?
- The ordered GB/T 11251 edition, Grade 50B, single-rolled or continuous-rolled route, delivery condition, thickness by width by length, quantity, any extra chemical or mechanical tests, any NDE, and the inspection document required by the project.
Request a quotation
Contact SHH STEEL for a quotation for GB/T 11251-2025 Grade 50B alloy steel plate. Please include your required quantity, plate thickness, width and length, whether you need single-rolled plate or continuous-rolled plate or strip, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the delivery condition. If your project requires tensile, hardness, toughness or ultrasonic testing beyond the standard rules, include the acceptance criteria and the inspection document required.
If you are considering Grade 40B, 45B or 40Cr as an alternative, send the applicable standard and project specification with your enquiry. We will review the differences in product form, chemistry and supply condition rather than assume that related grades are interchangeable.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com