ASTM A829 4140 Alloy Steel Plate | ASTM A829 Alloy Steel - SHH STEEL

ASTM A829 4140 Alloy Steel Plate

ASTM A829 4140 is chromium-molybdenum alloy structural steel plate under ASTM A829/A829M-25, usually ordered to chemical composition. Tensile properties may also be specified when compatible with the composition, delivery condition and thickness. SHH STEEL produces and exports Grade 4140 alloy steel plate to the specified delivery condition and project requirements.
Equivalent Grades:
Near equivalents and related chemistry-family grades, not automatic substitutes: GB/T 11251 42CrMo; EN ISO 683-2 42CrMo4 (1.7225); JIS G 4053 SCM440 (machine-structural steel, not a plate book). AISI/SAE 4140 is the conventional chemistry number, not a separate plate specification.
Heat Treatment
ASTM A829/A829M-25 lists Condition AR (as-rolled), A (annealed), N (normalized), NT (normalized and tempered) and QT (quenched and tempered).
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A829 Grade 4140 plate?

We produce and export ASTM A829 Grade 4140 as structural-quality alloy steel plate to ASTM A829/A829M-25, Standard Specification for Alloy Structural Steel Plates. Grade 4140 is the chromium-molybdenum designation used for this A829 plate grade, and 4140 is the conventional AISI/SAE chemistry-family number. AISI/SAE 4140 is not itself a plate specification.

The plates are usually specified to chemical composition. Tensile properties may also be specified; when they are, the values must be compatible with the chemical composition, the delivery condition and the plate thickness.

This is an engineering alloy structural plate. We supply it as-rolled for later heat treatment or in an agreed heat-treated condition. Typical quenched-and-tempered 4140 bar strengths should not be read as automatic as-delivered plate minima.

SHH STEEL produces and exports ASTM A829/A829M-25 Grade 4140 plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry. This grade belongs to our Alloy Steel Plates range under ASTM A829/A829M.

Material specification for ASTM A829 Grade 4140

The items below follow ASTM A829/A829M-25. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.

Parameter Detail
Standard ASTM A829/A829M-25, Standard Specification for Alloy Structural Steel Plates
Grade designation Grade 4140, chromium-molybdenum alloy plate under ASTM A829/A829M
Product form Alloy structural steel plate
Usual ordering basis Chemical composition; tensile properties may also be specified when compatible with composition, condition and thickness
Delivery conditions Condition AR, as rolled (hot rolled); Condition A, annealed; Condition N, normalized; Condition NT, normalized and tempered; Condition QT, quenched and tempered
Forms Form I rectangular; Form II circular and semi-circular; Form III sketch, including rings
Edge categories Edge 1 mill edge; Edge 2 universal mill edge; Edge 3 sheared edge; Edge 4 gas-cut edge; Edge 5 special cut edge
Finishes Finish 1 as-rolled (hot-rolled); Finish 2 blast cleaned; Finish 3 blast cleaned and oiled; Finish 4 pickled; Finish 5 pickled and oiled; Finish 6 painted, one prime coat; Finish 7 painted, one prime coat and one finish coat. Plates are usually specified to Finish 1
Supplementary requirements Additional requirements may be specified on the order
Heat-analysis elements named by ASTM Carbon, manganese, phosphorus, sulfur, silicon, nickel, chromium, molybdenum, vanadium and copper
Units SI units and inch-pound units are separate; do not combine the two systems
Our supply We produce and export Grade 4140 to the ASTM form, edge, finish and delivery condition agreed on the order

Chemical composition of ASTM A829 Grade 4140

ASTM A829/A829M-25 requires heat analysis to the composition specified for the ordered grade. The figures below are manufacturer heat-analysis values commonly published for ASTM A829 Grade 4140 plate. They are reference data. Contractual chemistry and delivery condition are those of the ordered ASTM A829/A829M edition and the mill test certificate.

Element Reference heat analysis (wt. %)
Carbon (C) 0.36-0.44
Manganese (Mn) 0.75-1.00
Silicon (Si) 0.15-0.35
Chromium (Cr) 0.80-1.10
Molybdenum (Mo) 0.15-0.25

Phosphorus and sulfur shall meet the ordered edition; some manufacturers apply tighter ladle maxima. Confirm both on the mill test certificate. If the project requires product analysis, agree it on the order and check the result on the certificate. Copper is named among the ASTM heat-analysis elements, but a numeric copper limit for Grade 4140 is not listed in the manufacturer tables used here.

Mechanical properties and optional tests

ASTM A829/A829M-25 plates are usually specified to chemical composition. Tensile properties may also be specified when they are compatible with the composition, delivery condition and plate thickness. Mechanical tests are not assumed for every as-rolled order; if you need tensile, hardness or toughness results, state the values, delivery condition and thickness so we can confirm they are compatible.

Typical quenched-and-tempered 4140 bar yield or tensile figures should not be treated as automatic as-delivered plate minima. Those values describe a heat-treated product and cycle that an as-rolled plate order may not include.

Delivery conditions for ASTM A829 Grade 4140

ASTM A829/A829M-25 lists five delivery conditions:

  • Condition AR — as rolled (hot rolled)
  • Condition A — annealed
  • Condition N — normalized
  • Condition NT — normalized and tempered
  • Condition QT — quenched and tempered

We produce and export Grade 4140 to the agreed condition. Not every production route offers every condition on every thickness, so the purchase order should name the required state. An enquiry that only says “4140 plate” is incomplete, because as-rolled, annealed, normalized and quenched-and-tempered plate are not interchangeable supply states.

As-rolled (green) plate is often used for parts that will be heat treated later to obtain high strength and toughness.

Welding and thermal cutting

When the steel is to be welded, ASTM A829/A829M-25 presupposes a welding procedure suitable for the grade and the intended use or service, and refers to Appendix X3 of ASTM A6/A6M for weldability information.

Chromium-molybdenum 4140 plate is commonly welded with low-hydrogen consumables and controlled hydrogen practice. Electrodes and fluxes should be dry and properly stored. Slow cooling after welding and a post-weld heat treatment may be required to limit cold cracking. Preheat and interpass temperature depend on thickness, joint restraint and the qualified procedure.

Thermal cutting can harden the adjacent material. That heat-affected zone should be considered, and removed where later forming or welding requires it. Qualify cutting and welding procedures to the project specification, the ordered delivery condition and the actual plate thickness.

Form, edge, finish and dimensions

ASTM A829/A829M-25 defines form, edge and finish options. Numeric thickness, width, length and flatness tolerances should be stated on the purchase order and confirmed on the mill documents for the ordered edition. If the project requires ASTM A6 or another dimensional standard, write that requirement on the enquiry.

Applications and specification limits

We produce and export this grade for heavy-machinery and general engineering work, including components cut from plate and then heat treated to a stated cycle. Typical uses are machinery parts and fabricated engineering components where a chromium-molybdenum alloy plate is required.

As-rolled, annealed and quenched-and-tempered plate do not machine, form or finish at the same strength. Wear resistance, through-hardness and toughness should be treated as order-specific, not assumed from the grade name alone.

ASTM A829 is an alloy structural plate specification. It is not a tool-steel book such as ASTM A681, and it is not a boiler or pressure-vessel plate specification. Do not use this grade as an automatic substitute for those product standards.

Compare ASTM A829 4140 with other steel plates

ASTM A829 Grade 4140 is chemistry-ordered alloy structural plate. It is not a strength-graded structural plate and not a chromium-molybdenum vessel plate. The comparison below uses other plates we already publish. These grades are related by engineering use, not equivalents.

Material Alloy / type Delivery condition Mechanical requirements Typical service Substitution limit
ASTM A829 Grade 4140 (this plate) Chromium-molybdenum alloy structural plate, usually ordered by heat chemistry AR, annealed, normalized, NT or QT as ordered No automatic as-delivered strength package; tensile or hardness only if specified and compatible with composition, condition and thickness Machinery and general engineering parts, often heat treated after cutting Do not treat it as a 100 ksi QT structural grade or as a 2.25Cr-1Mo vessel grade
ASTM A514 Grade B Quenched-and-tempered alloy structural plate; chemistry includes chromium, molybdenum, vanadium, titanium and boron Quenched and tempered Strength-graded: to 32 mm, yield 100 ksi / 690 MPa min and tensile 110-130 ksi / 760-895 MPa (from our A514 Grade B page). Maximum thickness for Grade B is 1¼ in / 32 mm Welded bridges and other structures that specify A514 QT plate Not a substitute for chemistry-ordered A829 4140, and not interchangeable with A572 Grade 50
ASTM A572 Grade 50 High-strength low-alloy structural plate, microalloyed with niobium and vanadium Hot-rolled or controlled-rolled Strength-graded: minimum yield 345 MPa and tensile 450 MPa minimum (from our A572 Grade 50 page) Bridges, buildings, construction equipment, transmission towers and heavy machinery frames Not a chromium-molybdenum 4140 plate and not a QT 100 ksi grade
ASTM A387 Grade 22 Class 2 Chromium-molybdenum pressure-vessel plate, nominal 2.25Cr-1.00Mo — a different alloy level from 4140 Usually normalized and tempered, or accelerated cooling plus temper Strength-graded Class 2: tensile 75-100 ksi / 515-690 MPa and yield 45 ksi / 310 MPa min (from our A387 Grade 22 Class 2 page) Welded boilers and elevated-temperature vessels Similar only in being a Cr-Mo plate family; not an engineering-plate equivalent to A829 4140

Related published ranges: Structural Steel Plates, ASTM A514/A514M, ASTM A572/A572M and ASTM A387.

Equivalent and related grades by country

The designations below are near equivalents or related chemistry-family grades, not certified or automatic equivalents. Chemistry windows, product form, delivery condition and any mechanical tests must match the project specification before a substitution is considered. Grades without a live page on this site are shown as plain text.

Country / region Standard Grade Similarity and key differences Substitution caveat
United States ASTM A829/A829M-25 Grade 4140 This plate specification. Chromium-molybdenum alloy structural plate, usually ordered by heat chemistry, with optional tensile properties. This product
United States AISI / SAE practice 4140 The conventional chemistry-family number used with this plate grade. AISI/SAE 4140 is not an independent plate specification. Do not treat an AISI/SAE 4140 bar or forging enquiry as an ASTM A829 plate order without restating product form, condition and tests.
China GB/T 11251 42CrMo Chinese alloy structural steel plate and strip standard. Published 42CrMo heat-analysis windows: C 0.38-0.45, Si 0.17-0.37, Mn 0.50-0.80, Cr 0.90-1.20, Mo 0.15-0.25. The chemistry sits in the same Cr-Mo family as 4140, but the manganese and silicon ranges differ from manufacturer-published A829 4140 values (C 0.36-0.44, Mn 0.75-1.00, Si 0.15-0.35, Cr 0.80-1.10, Mo 0.15-0.25). Near equivalent only. Confirm the GB/T 11251 edition, plate or strip form, delivery condition and tests. No dedicated product page is published on this site yet.
Europe EN ISO 683-2 (ISO 683-2) 42CrMo4 (steel number 1.7225) Alloy steels for quenching and tempering. The standard covers finished flat products as well as semi-finished products, bars, wire rod and forgings. Manufacturer heat analysis published to DIN EN ISO 683-2: C 0.38-0.45, Si 0.10-0.40, Mn 0.60-0.90, Cr 0.90-1.20, Mo 0.15-0.30; the standard maxima cited for phosphorus and sulfur are P ≤ 0.025 and S ≤ 0.035. Compared with manufacturer-published A829 4140 values, 42CrMo4 has a higher carbon minimum, a lower manganese range, a higher chromium minimum and a higher molybdenum maximum. When ordered quenched and tempered, EN ISO 683-2 can specify mechanical properties by ruling section. Near equivalent only. Different book and ordering model from ASTM A829 plate. No dedicated product page is published on this site yet.
Japan JIS G 4053 SCM440 Low-alloyed steel for machine structural use, made by hot rolling, hot forging or hot extruding, generally as uniform-section products for later forging, cutting and heat treatment. Published heat analysis for SCM440: C 0.38-0.43, Si 0.15-0.35, Mn 0.60-0.90, P ≤ 0.030, S ≤ 0.030, Cr 0.90-1.20, Mo 0.15-0.30. JIS G 4053 does not itself specify tensile or hardness minima. It is not a plate specification. Not an automatic plate equivalent. Do not order A829 plate as a substitute for G4053 bar or section supply, or the reverse.
Germany / Europe (steel number) Steel number 1.7225 with 42CrMo4 42CrMo4 The European steel number for 42CrMo4 under EN ISO 683-2, not a separate plate book. Order to the current EN ISO 683-2 edition and required condition rather than to a historical national title alone.
United Kingdom and other countries — — No separately verified national plate counterpart was established for this page. Do not assume a local bar designation is an ASTM A829 plate equivalent.

Related A829 plate grades in the same specification family include 4130, 8620 and 4142. They are related grades, not substitutes, and they do not have product pages on this site yet.

Why choose SHH STEEL for ASTM A829 Grade 4140

  • We produce and export ASTM A829/A829M-25 Grade 4140 alloy structural steel plate
  • We review the enquiry for edition, grade, delivery condition, dimensions and any extra mechanical or NDE tests
  • We keep chemistry-ordered plate distinct from optional tensile or hardness testing
  • We match documentation to what the purchase order requires

How to enquire for ASTM A829 4140 plate

Item What to specify
Standard and grade ASTM A829/A829M-25 Grade 4140
Delivery condition AR, annealed (A), normalized (N), normalized and tempered (NT), or quenched and tempered (QT)
Dimensions Required thickness, width and length; we confirm production and export feasibility against the enquiry
Form, edge and finish Use the ASTM options above if needed. Finish 1 is the usual finish
Chemistry Heat analysis to the ordered edition; request product analysis only if the project needs it
Mechanical tests State any tensile, hardness or toughness values and confirm they are compatible with composition, condition and thickness
Other tests Ultrasonic examination or other NDE only when written on the order
Documentation State the inspection document type required by the project
Processing Cutting or other processing only when requested; thermal-cutting practice depends on condition and thickness

FAQ

Is ASTM A829 4140 ordered by chemistry or by mechanical properties?
Usually by chemical composition. Tensile properties may also be specified when they are compatible with the composition, delivery condition and plate thickness. If you need mechanical tests, write them on the enquiry.
Does as-rolled ASTM A829 4140 plate meet typical quenched-and-tempered 4140 bar strengths?
No. Those bar figures describe a heat-treated condition that as-rolled plate does not automatically carry. If a strength or hardness package is needed, state the values and the delivery condition on the purchase order.
Which delivery conditions can we supply?
ASTM A829/A829M-25 lists Condition AR, A, N, NT and QT. We produce and export to the agreed condition. Name the required state on the order, because those conditions are not interchangeable.
Is ASTM A829 4140 a tool steel or the same as 42CrMo / 42CrMo4 / SCM440?
It is an alloy structural steel plate grade under ASTM A829/A829M, not ASTM A681 tool steel. GB/T 11251 42CrMo, EN ISO 683-2 42CrMo4 and JIS G 4053 SCM440 are near equivalents or related chemistry-family grades, not automatic substitutes. JIS G 4053 is not a plate specification.
What should a quotation enquiry include?
The ordered ASTM edition, Grade 4140, delivery condition, thickness by width by length, quantity, any extra chemical or mechanical tests, any NDE, and the inspection document required by the project.

Request a quotation

Contact SHH STEEL for a quotation for ASTM A829/A829M-25 Grade 4140 alloy steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.

Specify the delivery condition: as-rolled, annealed, normalized, normalized and tempered, or quenched and tempered. If your project requires tensile, hardness, toughness or ultrasonic testing, include the acceptance criteria and the inspection document required. Any mechanical requirements must be compatible with the chemistry, delivery condition and plate thickness.

If you are considering 42CrMo, 42CrMo4 or SCM440 as an alternative, send the applicable standard and project specification with your enquiry. We will review the differences in product form, chemistry and supply condition rather than assume that related grades are interchangeable.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X