GB/T 11251 15CrMo Alloy Steel Plate | GB/T 11251 Alloy Steel - SHH STEEL

GB/T 11251 15CrMo Alloy Steel Plate

GB/T 11251 15CrMo is chromium-molybdenum alloy structural steel plate under GB/T 11251-2025, Alloy structural steel plate, sheet and strip. It is not one of the fourteen grades listed in Table 1. Clause 6.1.1 requires chemistry to GB/T 3077, and clause 6.2.1.2 leaves mechanical properties of other grades to agreement. It carries more molybdenum than 20CrMo to 42CrMo. It is not vessel-plate 15CrMoR and not Table 1 grade 15Cr. SHH STEEL produces and exports 15CrMo plate to that agreed 11251 order.
Equivalent Grades:
Related only: JIS G 4053 SCM415 (molybdenum window does not match). Not vessel-plate 15CrMoR.
Heat Treatment
Single-rolled: high-temperature tempered, annealed, normalized, normalized and tempered, or quenched and tempered. Continuous-rolled: as-rolled or heat-treated.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is GB/T 11251 Grade 15CrMo plate?

GB/T 11251 15CrMo Alloy Steel Plate is alloy structural steel plate and strip purchased to GB/T 11251-2025. Grade 15CrMo is not one of the fourteen grades listed in Table 1. It may be supplied under that plate specification because clause 6.1.1 requires chemistry to GB/T 3077 and clause 6.2.1.2 sets mechanical properties of other grades by agreement.

15CrMo uses a higher molybdenum window than 20CrMo, 30CrMo, 35CrMo or 42CrMo. That is the main chemistry reason buyers specify it instead of the 0.15-0.25 % Mo series. It is not Table 1 grade 15Cr and it is not GB/T 713 15CrMoR vessel plate.

Single-rolled plate is usually supplied high-temperature tempered unless another condition is agreed. Because Table 1 does not list 15CrMo, any tensile, hardness or toughness acceptance criteria must be written on the contract. Vessel-code allowable stresses from 15CrMoR must not be read across onto this page.

SHH STEEL produces and exports GB/T 11251-2025 Grade 15CrMo plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry. This grade belongs to our Alloy Steel Plates range under GB/T 11251.

Material specification for GB/T 11251 Grade 15CrMo

The items below follow GB/T 11251-2025. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.

Parameter Detail
Standard GB/T 11251-2025, Alloy structural steel plate, sheet and strip. Published 31 October 2025 and implemented 1 May 2026. It replaces GB/T 11251-2020 and GB/T 37601-2019
Grade designation Grade 15CrMo, chromium-molybdenum alloy structural steel, not listed in Table 1
Product forms in the standard Single-rolled hot-rolled plate, nominal thickness 3.0 mm to 250 mm; and continuous-rolled plate and strip, nominal thickness not greater than 25.4 mm (wide strip and cut plate or slit strip 600 mm wide or more, and narrow strip and cut plate under 600 mm)
Chemical composition Shall comply with GB/T 3077 (clause 6.1.1). This grade is not listed in Table 1. Optional phosphorus or sulfur variants may be agreed under clause 6.1.1. Product analysis shall meet GB/T 222
Single-rolled delivery High-temperature tempered as the usual condition; annealed, normalized, normalized and tempered, or quenched and tempered by agreement. Normalizing rolling may replace normalizing if the normalized mechanical requirements can be met
Continuous-rolled delivery As-rolled; heat treatment by agreement. If spheroidize-annealed, surface hardness shall meet GB/T 3077. Tensile tests on continuous-rolled material are by agreement
Annealed single-rolled mechanics Table 1 does not list Grade 15CrMo. Clause 6.2.1.2 says mechanical properties of grades other than those in Table 1 are determined by agreement between the purchaser and the manufacturer. Do not copy a neighbouring Table 1 tensile band onto this grade
Dimensions Single-rolled plate to GB/T 709-2019, thickness tolerance class A. Wide strip and cut plate or slit strip to GB/T 709-2019 Table 4 thickness tolerances; flatness by agreement. Narrow strip and cut plate to Annex A
Ultrasonic testing Single-rolled plate 6 mm thick or thicker shall be tested to GB/T 2970-2016 Class II unless another method and class are agreed
Our supply We produce and export Grade 15CrMo to the GB/T 11251-2025 form, delivery condition, dimensions and extra tests agreed on the order

Chemical composition of GB/T 11251 Grade 15CrMo

GB/T 11251-2025 clause 6.1.1 requires the grade and chemical composition to comply with GB/T 3077. Grade 15CrMo is not listed in Table 1 of the 2025 plate specification. It is supplied as plate or strip when the purchase order names it under GB/T 11251, with chemistry taken from GB/T 3077. The melt-analysis figures below are published GB/T 3077-2015 values for Grade 15CrMo. They are not a separate chemistry table printed inside GB/T 11251-2025 itself, and they must not be read as an older GB/T 11251-2020 or GB/T 37601-2019 reprint labelled as 2025. Product-analysis tolerances shall meet GB/T 222; use the applicable GB/T 222 limits for acceptance.

Element Reference melt analysis (wt. %)
Carbon (C) 0.12-0.18
Silicon (Si) 0.17-0.37
Manganese (Mn) 0.40-0.70
Chromium (Cr) 0.80-1.10
Molybdenum (Mo) 0.40-0.55

Phosphorus and sulfur depend on the GB/T 3077 quality class ordered: ordinary quality steel, high-quality steel designated by adding A, or extra-quality steel designated by adding E. Published secondary tables sometimes round those maxima; confirm the class and the limits on the mill test certificate. GB/T 11251-2025 also allows, by agreement on the contract, sulfur of 0.015% to 0.035% or not greater than 0.005%, or phosphorus not greater than 0.015%. Residual elements that are not specified alloying additions are limited by GB/T 3077.

Mechanical properties and optional tests

Grade 15CrMo is not listed in GB/T 11251-2025 Table 1. Clause 6.2.1.2 states that, for single-rolled plate, the mechanical properties of grades other than those in Table 1 are determined by agreement between the purchaser and the manufacturer. The same clause also sends thickness greater than 100 mm to agreement, even for Table 1 grades. This page therefore does not publish annealed tensile strength or elongation numbers for Grade 15CrMo. Neighbouring Table 1 bands must not be copied onto this grade, and they are not implied guarantees.

When single-rolled plate is delivered high-temperature tempered, clause 6.2.1.1 requires surface hardness in accordance with GB/T 3077. This page does not reprint a numeric hardness table from the bar specification. Normalized, normalized-and-tempered and quenched-and-tempered properties are contractual. The Table 1 normalized rule — elongation not less than Table 1, with the tensile upper limit allowed 50 MPa higher — applies to Table 1 grades; it is not used here as an automatic 15CrMo plate minimum.

Continuous-rolled plate and strip may be tensile-tested only by agreement. Quenched-and-tempered tensile and yield figures published for GB/T 3077 bars are not automatic GB/T 11251 plate minima and are not used on this page.

Delivery conditions for GB/T 11251 Grade 15CrMo

GB/T 11251-2025 distinguishes two product routes:

  • Single-rolled plate is usually delivered high-temperature tempered. Annealed, normalized, normalized and tempered, or quenched and tempered supply may be agreed and written on the contract. Normalizing rolling may replace normalizing if the normalized mechanical requirements can be guaranteed.
  • Continuous-rolled plate and strip are delivered as-rolled unless a heat-treatment condition is agreed. If they are spheroidize-annealed, surface hardness shall meet GB/T 3077.

We produce and export Grade 15CrMo to the agreed route and condition. An enquiry that only says “15CrMo plate” is incomplete, because high-temperature tempered, annealed, normalized and quenched-and-tempered plate are not interchangeable supply states, single-rolled plate is not the same product as continuous-rolled plate or strip, and this grade has no Table 1 default tensile package.

Welding and thermal cutting

15CrMo combines a low carbon window with a higher molybdenum addition than 20CrMo, 30CrMo, 35CrMo or 42CrMo. That chemistry is generally more weldable than the higher-carbon Cr-Mo grades, but chromium-molybdenum joints still need a qualified procedure, including any post-weld heat treatment the project specifies. This plate is not ordered as GB/T 713 15CrMoR vessel plate. Preheat, interpass temperature and any post-weld heat treatment depend on thickness, joint restraint and the qualified procedure. Qualify cutting and welding procedures to the project specification, the ordered delivery condition and the actual thickness.

Thermal cutting can harden the adjacent material. That heat-affected zone should be considered, and removed where later forming or welding requires it.

Form, dimensions and inspection

Single-rolled plate dimensions, shape and mass tolerances follow GB/T 709-2019, with thickness tolerance class A unless another class is agreed. Wide strip and plate or slit strip cut from it follow GB/T 709-2019, using the thickness tolerances in Table 4 of that standard; flatness is agreed on the contract. Narrow strip and plate cut from it follow Annex A of GB/T 11251-2025. Other sizes and tolerances may be agreed.

Single-rolled plate 6 mm thick or thicker shall receive ultrasonic testing to GB/T 2970-2016 Class II unless another standard and class are written on the order. For stamping, single-rolled plate not thicker than 10 mm shall pass a 180° bend test with former diameter D = 2a.

Applications and specification limits

We produce and export this grade when the enquiry asks for chromium-molybdenum engineering plate with the higher molybdenum window of 15CrMo, under GB/T 11251 rather than under a vessel specification. It is commonly considered for elevated-temperature engineering parts, but this page publishes no design temperature, creep strength or allowable-stress table.

Do not confuse this grade with GB/T 713 15CrMoR vessel plate or with Table 1 grade 15Cr. 15CrMoR is a pressure-vessel product with published yield and tensile values. 15Cr is a chromium engineering grade without a specified molybdenum addition.

GB/T 11251 is an alloy structural plate and strip specification. It is not a boiler or pressure-vessel specification, and an order for 15CrMo must not be written as 15CrMoR.

Compare GB/T 11251 15CrMo with other steel plates

GB/T 11251 Grade 15CrMo is alloy structural plate and strip under the 2025 Chinese plate specification. It is not a Table 1 grade. The comparison below uses other plates we already publish. These grades are related by engineering use or chemistry family, not equivalents.

Material Alloy / type Delivery condition Mechanical requirements Typical service Substitution limit
GB/T 11251 Grade 15CrMo (this plate) Chromium-molybdenum alloy structural plate and strip under GB/T 11251-2025, supplied by agreement rather than as a Table 1 grade. Molybdenum window 0.40-0.55 Single-rolled: high-temperature tempered unless annealed, N, NT or QT is agreed. Continuous-rolled: as-rolled unless heat treated by agreement Not listed in Table 1. Mechanical properties are by agreement under clause 6.2.1.2. High-temperature tempered plate is ordered to GB/T 3077 hardness, without a numeric hardness table on this page Chromium-molybdenum engineering plate specified to the 11251 specification rather than to a vessel specification Not GB/T 713 15CrMoR vessel plate and not Table 1 grade 15Cr
ASTM A829 4140 Alloy Steel Plate Chromium-molybdenum alloy structural plate under ASTM A829/A829M-25, usually ordered by heat chemistry. Manufacturer heat-analysis windows on that page: C 0.36–0.44, Mn 0.75–1.00, Si 0.15–0.35, Cr 0.80–1.10 and Mo 0.15–0.25 ASTM A829/A829M-25 permits AR, A, N, NT or QT; specify the required condition. No automatic as-delivered strength package; tensile or hardness only if specified and compatible with analysis, condition and thickness Machinery and general engineering parts, often heat treated after cutting Different purpose and chemistry. 15CrMo carbon is 0.12-0.18 against 4140 at 0.36-0.44, and molybdenum is 0.40-0.55 against 0.15-0.25. Not a 4140-type medium-carbon grade
ASTM A829 4130 Alloy Steel Plate Chromium-molybdenum alloy structural plate under ASTM A829/A829M-25, usually ordered by heat chemistry. Manufacturer heat-analysis windows on that page: C 0.28–0.33, Mn 0.40–0.60, Si 0.15–0.35, Cr 0.80–1.10 and Mo 0.15–0.25 Usually ordered by chemistry; tensile only if specified and compatible No automatic as-delivered strength package Engineering plate with a lower carbon window than Grade 4140 in the same family Lower carbon and higher molybdenum than 4130 (C 0.12-0.18 and Mo 0.40-0.55 against C 0.28-0.33 and Mo 0.15-0.25). Not a 4130 substitute
GB/T 713 15CrMoR Steel Plate 1.25Cr-0.5Mo boiler and pressure-vessel plate under GB/T 713.2-2023, not an engineering-plate GB/T 11251 grade Vessel-plate delivery as specified for 15CrMoR (from our 15CrMoR page) Strength-graded on our 15CrMoR page: yield 295 MPa at 6–60 mm and tensile 450–590 MPa Boilers and pressure vessels This is the comparison that matters most. 15CrMoR is GB/T 713.2-2023 boiler and pressure-vessel plate, strength-graded at yield 295 MPa (6-60 mm) and tensile 450-590 MPa on our vessel page. 15CrMo is 11251 engineering plate with 3077 chemistry and no Table 1 tensile package. Similar family name, different specifications, different guarantees

Related published ranges: Alloy Steel Plates.

Equivalent and related grades by country

The designations below are near equivalents or related chemistry-family grades, not certified or automatic equivalents. Chemistry windows, product form, delivery condition and tests must match the project specification before a substitution is considered. Grades without a live page on this site are shown as plain text unless a live contrast page is named.

Country / region Standard Grade Similarity and key differences Substitution caveat
China GB/T 11251-2025 15CrMo This plate. Chromium-molybdenum alloy structural plate and strip supplied under the 2025 specification by agreement, not listed in Table 1. Molybdenum window 0.40-0.55. This product
China GB/T 3077-2015 15CrMo Chemistry reference (bar specification). Published melt analysis: C 0.12-0.18, Si 0.17-0.37, Mn 0.40-0.70, Cr 0.80-1.10, Mo 0.40-0.55. Do not treat GB/T 3077 bar quenched-and-tempered figures as GB/T 11251 plate minima.
China GB/T 713.2-2023 15CrMoR Boiler and pressure-vessel plate, described on our live 15CrMoR page as 1.25Cr-0.5Mo service plate with yield 295 MPa at 6-60 mm and tensile 450-590 MPa. Different specification and different mechanical model. Not a substitute. Do not write a vessel order as 15CrMo or an engineering-plate order as 15CrMoR.
Japan JIS G 4053 SCM415 Often listed against 15CrMo in comparison tables. Published SCM415 heat analysis: C 0.13-0.18, Si 0.15-0.35, Mn 0.60-0.90, Cr 0.90-1.20, Mo 0.15-0.25. The molybdenum window (0.15-0.25) does not match 15CrMo (0.40-0.55). Not a molybdenum-matched equivalent. Do not substitute on the similar name alone.

No verified official European plate pairing is cited for 15CrMo. Table 1 grade 15Cr is a chromium engineering grade without a specified molybdenum addition and is not a substitute.

Why choose SHH STEEL for GB/T 11251 Grade 15CrMo

  • We produce and export GB/T 11251-2025 Grade 15CrMo alloy structural steel plate
  • We review the enquiry for edition, grade, product route, delivery condition, dimensions and extra tests
  • We keep this by-agreement grade distinct from Table 1 guaranteed mechanics and from GB/T 3077 bar figures
  • We match documentation to what the purchase order requires

How to enquire for GB/T 11251 15CrMo plate

Item What to specify
Standard and grade GB/T 11251-2025 Grade 15CrMo
Product route Single-rolled plate, or continuous-rolled plate or strip
Delivery condition High-temperature tempered, annealed, normalized, normalized and tempered, quenched and tempered, or as-rolled for continuous-rolled material
Dimensions Required thickness, width and length; we confirm production and export feasibility against the enquiry
Chemistry Melt analysis to GB/T 3077, including any A or E quality class; request product analysis to GB/T 222 only if needed; state any agreed phosphorus or sulfur variant
Mechanical tests State the agreed tensile, hardness, toughness or other acceptance criteria. Table 1 annealed values do not apply to this grade
Other tests Ultrasonic class if different from the standard Class II rule, bend testing for stamping, decarburization or inclusion rating only when written on the order
Documentation State the inspection document type required by the project

FAQ

Is GB/T 11251 15CrMo ordered only by chemistry?
Chemistry shall comply with GB/T 3077. Grade 15CrMo is not listed in Table 1, so the specification does not publish annealed tensile and elongation values for it. Write the tensile, hardness or toughness criteria you need on the contract. High-temperature tempered single-rolled plate is ordered to GB/T 3077 hardness rather than to a Table 1 tensile band.
Is GB/T 11251 15CrMo the same as 15CrMoR or 15Cr?
No. 15CrMoR is GB/T 713 chromium-molybdenum boiler and pressure-vessel plate, with published yield and tensile values on our 15CrMoR page. 15Cr is a Table 1 chromium engineering grade without a specified molybdenum addition. 15CrMo is the GB/T 3077 chemistry grade supplied as 11251 plate by agreement. The names are easy to mix up and must not share an order.
Does Table 1 apply to this grade?
No. Table 1 of GB/T 11251-2025 lists fourteen grades; 15CrMo is not among them. Clause 6.2.1.2 sends the mechanical properties of other grades to agreement. Do not copy a neighbouring Table 1 tensile or elongation figure onto 15CrMo. The normalized allowance of a 50 MPa higher tensile upper limit is a Table 1 rule, not an automatic value for this grade.
Did GB/T 11251-2025 replace GB/T 37601?
Yes. The 2025 edition replaces GB/T 11251-2020 and GB/T 37601-2019 and integrates the continuous-rolled content. Do not order this plate to the withdrawn 37601 specification as if it were still current.
What should a quotation enquiry include?
The ordered GB/T 11251 edition, Grade 15CrMo, single-rolled or continuous-rolled route, delivery condition, thickness by width by length, quantity, the agreed mechanical acceptance criteria (because Table 1 does not apply), any extra chemical tests, any NDE, and the inspection document required by the project.

Request a quotation

Contact SHH STEEL for a quotation for GB/T 11251-2025 Grade 15CrMo alloy steel plate. Please include your required quantity, plate thickness, width and length, whether you need single-rolled plate or continuous-rolled plate or strip, delivery destination and preferred delivery schedule so we can review your production and export requirements.

Specify the delivery condition and the mechanical tests you need, because this grade has no Table 1 default tensile package. If your project requires tensile, hardness, toughness or ultrasonic testing beyond the standard rules, include the acceptance criteria and the inspection document required.

If you are comparing 15CrMo with GB/T 713 15CrMoR or with Table 1 grade 15Cr, say so on the enquiry. We will review the differences in product form, chemistry and supply condition rather than assume that related grades are interchangeable.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X