EN 10248-1 S355GP U-Type and Z-Type Steel Sheet Pile
What is EN 10248-1 S355GP U-Type and Z-Type Steel Sheet Pile?
EN 10248-1 S355GP U-type and Z-type steel sheet pile is a hot-rolled interlocking section whose material grade is S355GP under EN 10248-1. In EN 10248-1:2023, S355GP has a minimum yield strength ReH of 355 MPa, a minimum tensile strength Rm of 480 MPa, and a minimum elongation of 22% on L0 = 5.65 √S0. The same edition specifies a minimum KV2 impact energy of 27 J at 0 °C and a product-analysis CEV of 0.50% maximum.
This page covers the EN 10248-1 GP family — S240GP, S270GP, S320GP, S355GP, S390GP, S430GP, S460GP and S500GP — in both U-type and Z-type form. S355GP is the usual enquiry grade. Dimensions and shape tolerances are ordered to EN 10248-2:2024 and are not a separate filing term. These piles are filed under the steel sheet piles category in the steel structural profiles catalog. They are not H-beams, channels, or bearing piles, and they are not JIS or Chinese U-type piles of similar width.
Material, Dimensions and the EN 10248-1 GP Family
The purchase order and the inspection document should name, separately:
- EN 10248-1 and its edition (this page uses the 2023 edition as reprinted for these grades; the edition named on the order governs), and the grade (for example S355GP);
- EN 10248-2:2024, or the agreed options in that standard, for shape and dimension tolerances;
- the U-type or Z-type geometry (effective width, height and thickness) and the required length;
- any agreed coating, galvanizing chemistry, copper addition, interlock check or additional impact test.
EN 10248-1 is not EN 10249 (cold-formed) and is not JIS A 5528, CNS 7851, GB/T 20933 or an ASTM sheet-piling specification.
EN 10248-1 S355GP Sizes: Typical Hot-Rolled U-Type and Z-Type Series
The tables below are typical hot-rolled Z-type and U-type mill series, described by geometry only (type, effective width, height and thickness). They are published mill-series dimensions, not an EN 10248-2 size table. Trade names are not used. Not every section is rolled in every GP grade. A European U-type or Z-type of a given width is not a JIS Type IV or a Chinese U-type of similar width.
Effective width is the interlocking-wall pitch used for the series. Wall mass and wall section properties are published per metre of wall, not as a claim that every wall is built from one section alone. Where the same geometry appears in more than one mill series, the U-type table lists it once.
Typical hot-rolled Z-type mill series
Typical hot-rolled Z-type series, 800 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.
Swipe horizontally to view all dimensions.
Typical hot-rolled Z-type series, 770 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.
Swipe horizontally to view all dimensions.
Typical hot-rolled Z-type series, 750 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.
Swipe horizontally to view all dimensions.
Typical hot-rolled Z-type series, 700 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.
Swipe horizontally to view all dimensions.
Typical hot-rolled Z-type series, 630 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.
Swipe horizontally to view all dimensions.
Typical hot-rolled U-type mill series
Typical hot-rolled U-type series, 750 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. Duplicate geometries that appear in more than one mill series are listed once. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.
Swipe horizontally to view all dimensions.
Typical hot-rolled U-type series, 600 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. Duplicate geometries that appear in more than one mill series are listed once. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.
Swipe horizontally to view all dimensions.
Typical hot-rolled U-type series, 400 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. Duplicate geometries that appear in more than one mill series are listed once. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.
Swipe horizontally to view all dimensions.
EN 10248-1:2023 Chemical Composition (Product Analysis)
The figures below are the product-analysis maxima published with official mill reprints of EN 10248-1:2023. They are not heat-analysis limits. Silicon is not specified for S240GP and S270GP in that table. Copper is 0.60% maximum. The nitrogen maximum does not apply if a minimum total aluminium of 0.015%, or a minimum 0.013% acid-soluble aluminium, or sufficient other nitrogen-binding elements, is shown; those elements shall then be mentioned in the inspection document. The ordered edition governs if it differs.
Swipe horizontally to view all dimensions.
EN 10248-1:2023 Mechanical Properties
The tensile values and KV2 impact energies below are from the same EN 10248-1:2023 mill reprints. Elongation is on L0 = 5.65 √S0. Impact testing is at 20 °C for S240GP, S270GP and S320GP, and at 0 °C for S355GP and the higher GP grades, with a 27 J minimum in each case. Not every section is offered in every grade.
Swipe horizontally to view all dimensions.
Shape Tolerances and Identification
Shape and dimension tolerances are ordered to EN 10248-2:2024. That standard, including any agreed options on the order (for example a plus-side thickness option), governs. Do not assume a mill’s reduced or plus-side tolerance set unless it is written on the order.
A typical inspection mark identifies the steel standard and grade, the section geometry, the heat number, the producer and the length. An S355GP certificate is not an S430GP certificate, and an EN 10248-1 mark is not a JIS, CNS, GB or ASTM mark.
Delivery Conditions, Inspection and Identification
These piles are commonly supplied as-rolled. The inspection document should identify EN 10248-1:2023 or the edition on the order, the GP grade, the U-type or Z-type geometry, the length, the product analysis for the elements reported, CEV, the tensile results and the KV2 impact result at the specified temperature. A plate certificate or an H-beam certificate does not, by itself, identify an EN 10248-1 sheet pile.
Applications and Service Limits
EN 10248-1 S355GP and the other GP grades are used in cofferdams, retaining walls, quay walls and similar interlocking-wall structures where a European hot-rolled sheet-pile grade is named. They are not a silent substitute for JIS A 5528 SY295 U-type steel sheet pile, for ASTM A572 Grade 50 steel sheet pile, or for a GB/T 20933 U-type section. Interlocks of similar width are not interchangeable by depth or mass alone. Cold-formed piles to EN 10249 are a different product.
EN 10248-1 Compared with JIS A 5528 and ASTM A572
The comparisons below are an orientation only; they are not automatic substitutes.
Near-Equivalents: Not Automatic Substitutes
A near-equivalent is a starting point for a discussion, not a licence to swap certificates. If a project names EN 10248-1 S355GP, keep that standard, quality and geometry on the order. Related pages include JIS A 5528 SY295 U-type steel sheet pile and ASTM A572 Grade 50 steel sheet pile.
Sourcing EN 10248-1 S355GP U-Type and Z-Type Steel Sheet Piles from SHH STEEL
SHH STEEL supplies EN 10248-1 S355GP and the other GP grades as U-type and Z-type steel sheet piles against a named geometry, the material edition and the inspection document type. Enquiries should state the type and geometry, the grade, the length, and any coating, corner piles, galvanizing or interlock requirements.
The size tables are typical published mill series, not a claim that every section is rolled in every GP quality. Once the list is clear, a quotation can be prepared against the stated edition and certificate.
EN 10248-1 S355GP U-Type and Z-Type Steel Sheet Pile FAQs
-
Which EN 10248-1 grades are covered with S355GP?
- The 2023 GP family on this page is S240GP, S270GP, S320GP, S355GP, S390GP, S430GP, S460GP and S500GP. S355GP is the usual enquiry grade. A higher GP grade is not a silent substitute, and not every section is offered in every grade.
-
Does EN 10248-1:2023 require an impact test?
- Yes. The 2023 edition, as reprinted in official mill grade tables, specifies a minimum KV2 energy of 27 J, tested at 20 °C for S240GP, S270GP and S320GP, and at 0 °C for S355GP and the higher GP grades.
-
Are the size tables an official EN section list?
- No. They are typical hot-rolled U-type and Z-type mill series described by geometry (width, height and thickness). They are not an EN 10248-2 size table, and they are not JIS or Chinese U-type series of similar width.
-
Which edition of EN 10248-1 is used on this page?
- The numeric tables use EN 10248-1:2023 as reprinted in official mill programs (product analysis, mechanicals and the 2023 impact and CEV requirements). Shape tolerances are ordered to EN 10248-2:2024. The edition named on the order governs.
Request a Quotation for EN 10248-1 S355GP U-Type and Z-Type Steel Sheet Pile
EN 10248-1 S355GP U-type and Z-type steel sheet pile is a hot-rolled interlocking section with a 355 MPa minimum yield and a 480 MPa minimum tensile strength. Nominate the type and geometry, the GP grade, EN 10248-1:2023 or the edition on the order, EN 10248-2:2024 for tolerances, the length, and the inspection document type. Send the size list, grade, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.