EN 10248-1 S430GP U-Type and Z-Type Steel Sheet Pile

EN 10248-1 S430GP is a hot-rolled steel sheet pile grade with 430 MPa minimum yield, 510 MPa minimum tensile strength and 19 % elongation. The 2023 edition also requires 27 J at 0 C and a 0.52 % CEV maximum. Size tables are typical U-type and Z-type series, not a geometry-only page. SHH STEEL reviews grade, section and certificate before quoting.
Keywords
EN 10248-1 S430GP, S430GP sheet pile, S430GP U-type, S430GP Z-type, EN 10248 high-yield pile
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of EN 10248-1 S430GP Steel Sheet Pile
Chemical Composition
Mechanical Properties
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What is EN 10248-1 S430GP U-Type and Z-Type Steel Sheet Pile?

EN 10248-1 S430GP is a higher-yield hot-rolled steel sheet pile grade in the GP family. S marks a structural steel, 430 is the minimum yield in MPa, and GP is the sheet-pile quality of that standard. This page covers both U-type and Z-type sections in this grade. It is not a geometry-only companion to the live S355GP page, and it is not S270GP or a cold-formed EN 10249 pile.

The chemistry and mechanical figures follow EN 10248-1:2023. The edition named on the order governs acceptance. Not every published section is rolled in every grade; a 430 MPa quality in particular has to be confirmed on the enquiry.

Material, Dimensions and the EN 10248-1 S430GP Grade

EN 10248-1 is the material standard. Shape tolerances follow EN 10248-2 as named on the order. S430GP sits in the upper GP band: from S390GP through S500GP the 2023 product-analysis carbon, silicon, phosphorus, sulphur and CEV caps are the same group of limits, but the mechanical table is grade-specific. Do not treat S430GP as interchangeable with S390GP, S460GP or S500GP because those chemistry caps look similar.

EN 10248-1 S430GP Sizes: Typical Hot-Rolled U-Type and Z-Type Series

The tables below reuse the typical published hot-rolled U-type and Z-type series already tabulated on the S355GP page. They describe geometry only. Trade names are not used. These are typographical mill-series references, not an EN 10248-2 size table and not a mill stock list, and not every section is assumed to be available in S430GP.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
Z-type 800 × 449 × 8.5 800 449 8.5 8.5 129 80.7 101 41,320 1,840
Z-type 800 × 450 × 9.5 800 450 9.5 9.5 141 88.6 111 45,050 2,000
Z-type 800 × 451 × 10.5 800 451 10.5 10.5 153 96.4 120 48,790 2,165
Z-type 800 × 474 × 11.5 / 9.0 800 474 11.5 9.0 151 94.6 118 55,260 2,330
Z-type 800 × 475 × 12.5 / 10.0 800 475 12.5 10.0 163 102.6 128 59,410 2,500
Z-type 800 × 476 × 13.5 / 11.0 800 476 13.5 11.0 176 110.5 138 63,570 2,670

Typical hot-rolled Z-type series, 770 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
Z-type 770 × 344 × 8.5 770 344 8.5 8.5 120 72.6 94 21,430 1,245
Z-type 770 × 344 × 9.0 770 344 9.0 9.0 126 76.1 99 22,360 1,300
Z-type 770 × 345 × 9.5 770 345 9.5 9.5 132 79.5 103 23,300 1,355
Z-type 770 × 345 × 10.0 770 345 10.0 10.0 137 82.9 108 24,240 1,405

Typical hot-rolled Z-type series, 750 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
Z-type 750 × 509 × 12.0 / 10.0 750 509 12.0 10.0 171 100.8 134 71,540 2,810
Z-type 750 × 510 × 13.0 / 11.0 750 510 13.0 11.0 185 108.8 145 76,670 3,005
Z-type 750 × 511 × 14.0 / 12.0 750 511 14.0 12.0 198 116.7 156 81,800 3,200

Typical hot-rolled Z-type series, 700 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
Z-type 700 × 314 × 8.5 700 314 8.5 8.5 123 67.7 97 18,880 1,205
Z-type 700 × 315 × 9.5 700 315 9.5 9.5 135 74.0 106 20,540 1,305
Z-type 700 × 316 × 10.0 700 316 10.0 10.0 140 77.2 110 21,370 1,355
Z-type 700 × 316 × 10.5 700 316 10.5 10.5 146 80.3 115 22,190 1,405
Z-type 700 × 420 × 8.5 700 420 8.5 8.5 133 73.1 104 36,230 1,730
Z-type 700 × 420 × 9.0 700 420 9.0 9.0 139 76.5 109 37,800 1,800
Z-type 700 × 421 × 9.5 700 421 9.5 9.5 146 80.0 114 39,380 1,870
Z-type 700 × 421 × 10.0 700 421 10.0 10.0 152 83.5 119 40,960 1,945
Z-type 700 × 459 × 11.2 700 459 11.2 11.2 174 95.7 137 55,820 2,430
Z-type 700 × 460 × 12.2 700 460 12.2 12.2 187 102.9 147 59,720 2,600
Z-type 700 × 460 × 13.5 / 10.0 700 460 13.5 10.0 176 96.9 138 59,790 2,600
Z-type 700 × 461 × 13.2 700 461 13.2 13.2 200 110.0 157 63,620 2,760
Z-type 700 × 499 × 15.0 / 11.2 700 499 15.0 11.2 216 118.6 169 89,610 3,590
Z-type 700 × 499 × 18.0 / 14.0 700 499 18.0 14.0 259 142.1 203 104,930 4,205
Z-type 700 × 500 × 16.0 / 12.2 700 500 16.0 12.2 230 126.4 181 94,840 3,795
Z-type 700 × 500 × 19.0 / 15.0 700 500 19.0 15.0 273 149.9 214 110,150 4,405
Z-type 700 × 501 × 17.0 / 13.2 700 501 17.0 13.2 244 134.2 192 100,080 3,995
Z-type 700 × 501 × 20.0 / 16.0 700 501 20.0 16.0 287 157.7 225 115,370 4,605
Z-type 700 × 503 × 22.0 / 15.0 700 503 22.0 15.0 288 158.5 226 119,650 4,755
Z-type 700 × 504 × 23.0 / 16.0 700 504 23.0 16.0 303 166.3 238 124,890 4,955
Z-type 700 × 505 × 24.0 / 17.0 700 505 24.0 17.0 317 174.1 249 130,140 5,155

Typical hot-rolled Z-type series, 630 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
Z-type 630 × 380 × 9.5 630 380 9.5 9.5 150 74.4 118 34,200 1,800
Z-type 630 × 381 × 10.0 630 381 10.0 10.0 157 77.8 123 35,540 1,870
Z-type 630 × 427 × 13.0 / 12.2 630 427 13.0 12.2 198 97.8 155 55,510 2,600

Typical hot-rolled U-type mill series

Typical hot-rolled U-type series, 750 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. Duplicate geometries that appear in more than one mill series are listed once. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
U-type 750 × 408 × 10.0 / 8.3 750 408 10.0 8.3 132 77.9 104 28,680 1,405
U-type 750 × 411 × 11.5 / 9.3 750 411 11.5 9.3 147 86.3 115 32,850 1,600
U-type 750 × 441 × 10.5 / 9.1 750 441 10.5 9.1 150 88.5 118 39,300 1,780
U-type 750 × 444 × 12.0 / 10.0 750 444 12.0 10.0 165 96.9 129 44,440 2,000
U-type 750 × 447 × 13.0 / 9.5 750 447 13.0 9.5 173 102.1 136 50,700 2,270
U-type 750 × 450 × 14.5 / 10.2 750 450 14.5 10.2 188 110.4 147 56,240 2,500

Typical hot-rolled U-type series, 600 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. Duplicate geometries that appear in more than one mill series are listed once. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
U-type 600 × 309 × 6.0 600 309 6.0 6.0 89 41.9 70 9,670 625
U-type 600 × 310 × 6.5 / 6.4 600 310 6.5 6.4 94 44.1 74 10,450 675
U-type 600 × 311 × 7.2 / 6.9 600 311 7.2 6.9 98 46.3 77 11,540 740
U-type 600 × 312 × 7.3 / 6.9 600 312 7.3 6.9 101 47.4 79 11,620 745
U-type 600 × 312 × 7.5 / 7.1 600 312 7.5 7.1 103 48.5 81 12,010 770
U-type 600 × 313 × 8.0 / 7.5 600 313 8.0 7.5 108 50.8 85 12,800 820
U-type 600 × 316 × 9.0 / 6.8 600 316 9.0 6.8 118 55.8 93 15,700 995
U-type 600 × 318 × 10.0 / 7.4 600 318 10.0 7.4 128 60.2 100 17,450 1,095
U-type 600 × 320 × 11.0 / 8.0 600 320 11.0 8.0 137 64.6 108 19,220 1,200
U-type 600 × 360 × 9.8 / 9.0 600 360 9.8 9.0 140 66.1 110 21,600 1,200
U-type 600 × 360 × 10.0 600 360 10.0 10.0 151 71.0 118 22,660 1,260
U-type 600 × 418 × 9.0 / 7.4 600 418 9.0 7.4 127 59.9 100 26,590 1,270
U-type 600 × 420 × 10.0 / 8.0 600 420 10.0 8.0 136 64.3 107 29,410 1,400
U-type 600 × 422 × 11.0 / 8.6 600 422 11.0 8.6 146 68.7 115 32,260 1,530
U-type 600 × 430 × 10.2 / 8.4 600 430 10.2 8.4 154 72.6 121 35,950 1,670
U-type 600 × 430 × 11.2 / 9.0 600 430 11.2 9.0 163 76.9 128 38,650 1,800
U-type 600 × 430 × 12.2 / 9.5 600 430 12.2 9.5 172 81.1 135 41,320 1,920
U-type 600 × 450 × 11.1 / 9.0 600 450 11.1 9.0 174 81.9 137 46,380 2,060
U-type 600 × 450 × 12.1 / 9.5 600 450 12.1 9.5 183 86.1 144 49,460 2,200
U-type 600 × 450 × 13.1 / 10.0 600 450 13.1 10.0 192 90.4 151 52,510 2,335
U-type 600 × 452 × 14.2 / 9.7 600 452 14.2 9.7 207 97.4 162 60,580 2,680
U-type 600 × 452 × 18.5 / 10.6 600 452 18.5 10.6 233 109.9 183 69,210 3,065
U-type 600 × 452 × 19.5 / 11.0 600 452 19.5 11.0 242 114.1 190 72,320 3,200
U-type 600 × 452 × 20.5 / 11.4 600 452 20.5 11.4 251 118.4 197 75,410 3,340
U-type 600 × 454 × 15.2 / 10.1 600 454 15.2 10.1 216 101.8 170 64,460 2,840
U-type 600 × 456 × 16.2 / 10.5 600 456 16.2 10.5 226 106.2 177 68,380 3,000

Typical hot-rolled U-type series, 400 mm effective width. Geometry is given as type × effective width × height × flange thickness, with a second thickness where the web differs from the flange. Duplicate geometries that appear in more than one mill series are listed once. These are published mill-series dimensions, not an EN 10248-2 size table, and trade names are not used.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
U-type 400 × 290 × 12.7 / 9.4 400 290 12.7 9.4 197 62.0 155 22,580 1,560
U-type 400 × 292 × 15.0 / 9.7 400 292 15.0 9.7 221 69.3 173 26,090 1,785

EN 10248-1:2023 S430GP Chemical Composition (Product Analysis)

Product-analysis limits for S430GP are carbon 0.22 % maximum, manganese 1.80 % maximum, silicon 0.60 % maximum, phosphorus 0.045 % maximum, sulphur 0.045 % maximum, nitrogen 0.014 % maximum, copper 0.60 % maximum and CEV 0.52 % maximum. These figures are product analysis. Do not copy the looser S270GP phosphorus, sulphur or CEV caps onto an S430GP order.

Swipe horizontally to view all dimensions.

Element S430GP product analysis (EN 10248-1:2023)
Carbon, max 0.22 %
Manganese, max 1.80 %
Silicon, max 0.60 %
Phosphorus, max 0.045 %
Sulphur, max 0.045 %
Nitrogen, max 0.014 %
Copper, max 0.60 %
CEV, max 0.52 %

EN 10248-1:2023 S430GP Mechanical Properties

Minimum yield is 430 MPa, minimum tensile strength is 510 MPa, and minimum elongation is 19 % on L0 = 5.65 sqrt(S0). The 2023 edition requires a minimum KV2 impact energy of 27 J at 0 C. S355GP uses 355 / 480 / 22 % and the same 0 C impact temperature; S270GP uses 270 / 410 / 24 % and 27 J at +20 C. Those figures must not be pasted here.

Swipe horizontally to view all dimensions.

Property S430GP (EN 10248-1:2023)
Minimum yield ReH 430 MPa
Minimum tensile Rm 510 MPa
Minimum elongation, L0 = 5.65 sqrt(S0) 19 %
Minimum KV2 impact energy 27 J at 0 C

Applications and Service Limits for EN 10248-1 S430GP Sheet Piles

S430GP piles are used in retaining walls and heavier earth-retaining work where this yield class is named. The grade is not a cold-formed EN 10249 quality and not a weathering or marine alloy grade. If a lower-yield GP grade will do, or if a Japanese SY390 U-type is required, that product has to be ordered as such.

Near-Equivalents for EN 10248-1 S430GP: Not Automatic Substitutes

S390GP and S460GP are neighbouring GP grades with different yield and tensile minima, even where the 2023 chemistry caps look the same. JIS A 5528 SY390 is a Japanese sheet-pile grade with a different chemistry rule (only phosphorus and sulphur are specified) and a U-type series. ASTM A572 Grade 50 sheet piling follows a different standard.

Sourcing EN 10248-1 S430GP U-Type and Z-Type Steel Sheet Piles from SHH STEEL

Send the section type (U or Z), the width, height and thickness, the length, and the EN 10248-1 edition, and name S430GP explicitly. Do not use the S355GP term for this page, and do not create a Z-only duplicate page. SHH STEEL reviews the grade, the section and the certificate before quoting. The size tables are typographical references, not a warehouse list.

EN 10248-1 S430GP FAQs

Is this a Z-only duplicate of the S355GP page?
No. It is a different, higher-yield grade. U-type and Z-type geometry are both tabulated here rather than as a new geometry-only page.
Is S430GP interchangeable with S390GP?
No. The 2023 chemistry caps are in the same group, but the mechanical minima are different. Name the grade actually required.
What impact temperature applies?
27 J at 0 C in the 2023 edition, the same temperature as S355GP and above, not the +20 C test used for S240GP to S320GP.
Is every tabulated section available in S430GP?
Not necessarily. The tables are typographical mill-series references, not a stock list and not a claim that every section is rolled in this grade.

Conclusion

EN 10248-1:2023 S430GP is the 430 MPa hot-rolled sheet-pile grade, with 510 MPa tensile, 19 % elongation and 27 J at 0 C, tabulated here in both U-type and Z-type typical series. It is not a geometry-only duplicate of the S355GP page. Confirm the grade, the section and the edition on the order.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X