JIS A 5528 SY295 U-Type Steel Sheet Pile
What is JIS A 5528 SY295 U-Type Steel Sheet Pile?
JIS A 5528 SY295 U-type steel sheet pile is a hot-rolled interlocking U-section whose material grade is SY295 under JIS A 5528, with SY390 listed on the same page as the higher-yield quality in the same standard. SY marks a steel sheet pile, and 295 is the minimum yield stress in N/mm². In JIS A 5528:2021 the minimum tensile strength of SY295 is 450 N/mm². Elongation is 18% minimum on test piece No. 1A and 24% minimum on test piece No. 14B. SY390 has a minimum yield of 390 N/mm², a minimum tensile strength of 490 N/mm², and elongation of 16% minimum (No. 1A) or 20% minimum (No. 14B).
This page covers the JIS A 5528 family in U-type form. The Taiwan sister standard of the same SY names is CNS 7851 SY295 U-type steel sheet pile; those tensile minima are not the JIS figures and must not be mixed on a certificate. These piles are filed under the steel sheet piles category in the steel structural profiles catalog. They are not H-beams, channels, or bearing piles, and a 400 mm U-type designation is not a Chinese or European U pile of similar width.
Material, Dimensions and the SY295 / SY390 Family
The purchase order and the inspection document should name, separately:
- JIS A 5528 and its edition (this page uses the 2021 edition as reprinted for these grades; the edition named on the order governs), and the grade SY295 or SY390;
- the U-type (for example Type IV, 400 × 170 × 15.5 mm) and the required length;
- the elongation test piece (No. 1A or No. 14B) when the order needs to fix it, and any agreed chemistry, impact test, coating or interlock check that is not in the tabulated mill reprint.
JIS A 5528 is not CNS 7851 and is not JIS A 5523.
JIS A 5528 SY295 U-Type Sizes: Type II to Type IVw
The table below is the common JIS U-type series published in official mill programs: Type II, Type III, Type IV, Type VL, Type VIL, and the 600 mm-wide Type IIw, Type IIIw and Type IVw. It is a standard U-type series, not a complete catalogue of every JIS sheet-pile shape (hat-type and straight-web piles are specified separately). A 400 mm U-type pile is not a Chinese PU400 or a European U pile of similar width.
Effective width and height are the interlocking-wall dimensions used for this series. Mass per metre of wall is the published figure for a continuous wall of this effective width, not a claim that every wall is built from this section alone.
Swipe horizontally to view all dimensions.
JIS A 5528 Chemical Composition
The figures below are the chemistry reprint for JIS A 5528:2021 SY295 and SY390. Carbon, silicon, manganese, nitrogen and carbon equivalent are not specified in that table. Phosphorus and sulphur are each 0.04% maximum. Do not invent a carbon or manganese limit, and do not read a Ceq from JIS A 5523 or another sheet-pile standard onto this certificate.
JIS A 5528 Mechanical Properties
The tensile values below are from the same JIS A 5528:2021 reprint. Elongation is given for both standard test pieces. There is no tabulated Charpy V-notch energy at 0 °C in that table. If an impact test is required, it must be agreed and written on the order.
U-Type Shape Tolerances and Identification
The tolerances below are the JIS A 5528 U-type shape and dimension tolerances as reprinted in official mill programs. If the ordered edition of the material standard gives different limits, the ordered edition governs.
A typical inspection mark identifies the steel standard and grade, the type or dimension number, the heat number, the producer, the length and the manufacturing number. An SY295 certificate is not an SY390 certificate, and a CNS 7851 mark is not a JIS A 5528 mark.
Delivery Conditions, Inspection and Identification
These piles are commonly supplied as-rolled. The inspection document should identify JIS A 5528 and its edition, the grade SY295 or SY390, the U-type, the length, the heat analysis for the elements reported, and the tensile results, including the elongation test piece when it is reported. A CNS 7851 certificate, a plate certificate, or an H-beam certificate does not, by itself, identify a JIS A 5528 U-type sheet pile.
Applications and Service Limits
JIS A 5528 SY295 and SY390 U-type piles are used in retaining walls, cofferdams, quay work and similar interlocking-wall structures where a Japanese sheet-pile grade is named. They are not a silent substitute for CNS 7851 SY295 U-type steel sheet pile, for a GB/T 20933 U-type section, or for a European U or Z pile such as EN 10248-1 S355GP U-type and Z-type steel sheet pile. Interlocks of similar width are not interchangeable by depth or mass alone.
JIS A 5528 Compared with CNS 7851 and JIS A 5523
The comparisons below are an orientation only; they are not automatic substitutes.
Near-Equivalents: Not Automatic Substitutes
A near-equivalent is a starting point for a discussion, not a licence to swap certificates. If a project names JIS A 5528 SY295 or SY390, keep that standard, quality and type on the order. The Taiwan sister page is CNS 7851 SY295 U-type steel sheet pile.
Sourcing JIS A 5528 SY295 U-Type Steel Sheet Piles from SHH STEEL
SHH STEEL supplies JIS A 5528 SY295 and SY390 U-type steel sheet piles against a named type, the material edition and the inspection document type. Enquiries should state the U-type and length, the grade, whether CNS 7851 SY295 U-type steel sheet pile is acceptable on part of the list, and any coating, corner piles or interlock requirements.
The size table is the common JIS U-type series, not a claim that every type is rolled in every quality on every enquiry. Once the list is clear, a quotation can be prepared against the stated edition and certificate.
JIS A 5528 SY295 U-Type Steel Sheet Pile FAQs
-
Is JIS A 5528 SY295 the same as CNS 7851 SY295?
- No. The yield minima are the same 295 N/mm², but JIS A 5528 SY295 has a 450 N/mm² tensile minimum and CNS 7851 SY295 has a 490 N/mm² tensile minimum. The same difference appears on SY390 (490 versus 540 N/mm²). Certify to the standard named on the order.
-
Which U-types are tabulated on this page?
- The common JIS U-type series: Type II, III, IV, VL, VIL, IIw, IIIw and IVw. Type IV is 400 × 170 × 15.5 mm. Hat-type and straight-web piles are a different shape family and are not in this table. A 400 mm U-type is not a Chinese or European U pile of similar width.
-
Does JIS A 5528 SY295 have a standard 0 °C impact test?
- The mill reprints used for this page do not tabulate a Charpy energy at 0 °C for SY295 or SY390. If an impact test is required, it should be agreed and written on the order.
-
Which edition of JIS A 5528 is used on this page?
- The numeric tables use the JIS A 5528:2021 reprint published in official mill programs. A later edition may be named on the order; the ordered edition governs.
Request a Quotation for JIS A 5528 SY295 U-Type Steel Sheet Pile
JIS A 5528 SY295 U-type steel sheet pile is a hot-rolled interlocking U-section with a 295 N/mm² minimum yield and a 450 N/mm² minimum tensile strength. Nominate the U-type (for example Type IV, 400 × 170 × 15.5 mm), the grade SY295 or SY390, JIS A 5528:2021 or the edition on the order, the length, and the inspection document type. Send the size list, grade, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.