ASTM A572 Grade 50 Steel Sheet Pile

ASTM A572 Grade 50 steel sheet pile is high-strength low-alloy sheet piling with a 50 ksi [345 MPa] minimum yield and a 65 ksi [450 MPa] minimum tensile strength. The page also covers Grades 55, 60 and 65 as family variants and lists typical hot-rolled Z-type mill series by geometry.
Keywords
ASTM A572 Grade 50 Steel Sheet Pile, A572 Grade 50 sheet pile, ASTM A572, Grade 60 sheet pile, Z-type sheet pile
Equivalent Grades:
A572 Grades 55/60/65 (same specification); ASTM A328; ASTM A690; EN 10248-1 S355GP — comparisons only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of ASTM A572 Grade 50 Steel Sheet Pile
Chemical Composition of ASTM A572 Grade 50 and Related Grades
Mechanical Properties of ASTM A572 Grade 50 and Related Grades
Shape Tolerances and Identification
Delivery Conditions, Inspection and Identification
Applications and Service Limits
ASTM A572 Grade 50 Compared with A328, A690 and EN 10248-1
Near-Equivalents: Not Automatic Substitutes
Sourcing ASTM A572 Grade 50 Steel Sheet Piles from SHH STEEL
FAQ
Conclusion

What is ASTM A572 Grade 50 Steel Sheet Pile?

ASTM A572 Grade 50 steel sheet pile is high-strength low-alloy columbium-vanadium steel sheet piling to ASTM A572/A572M. Grade 50 has a minimum yield of 50 ksi [345 MPa], a minimum tensile strength of 65 ksi [450 MPa], a minimum elongation of 18% in 8 in. [200 mm], and a minimum elongation of 21% in 2 in. [50 mm]. This leaf is for sheet piles only; it is not the A572 beam, channel or angle category.

Grades 55, 60 and 65 in the same specification are listed on this page as family variants. Dimensions follow the ordered A6/A6M or project profile series. These piles are filed under the steel sheet piles category in the steel structural profiles catalog. A572 sheet piling is not A328 carbon sheet piling and is not A690 marine sheet piling, and it is not an A572 W-shape or an EN or JIS interlocking pile by size alone.

Material, Dimensions and the A572 Grade Family

The purchase order and the inspection document should name, separately:

  • ASTM A572/A572M and its edition (this page uses the A572/A572M-21ε1 text as published in SA-572/SA-572M; the edition named on the order governs), and the grade (Grade 50 unless another grade is named);
  • the section geometry and the required length, to A6/A6M or the project series;
  • the alloy type (Type 1, 2, 3 or 5) when it must be fixed, and any agreed copper addition, supplementary tensile or impact test, coating or interlock strength.

The steel shall be killed. A572 sheet piling is not A328 and is not A690.

ASTM A572 Grade 50 Sizes: Typical Hot-Rolled Mill Series

Dimensions follow the ordered ASTM A6/A6M or project profile series and are stated separately from the material grade. The tables below are typical published mill series, described by geometry only. They are not an ASTM A6 size table, and trade names are not used. A North American Z-type of a given width is not a European Z-type or a JIS U-type of similar width.

Some mill programs also offer this grade on the typical European hot-rolled U-type and Z-type series tabulated on the EN 10248-1 S355GP U-type and Z-type steel sheet pile page. Nominate the geometry on the enquiry; not every section is offered in every grade.

Typical North American hot-rolled Z-type mill series

Typical North American hot-rolled Z-type mill series, described by geometry only. These are published mill-series dimensions, not an ASTM A6 size table, and trade names are not used.

Swipe horizontally to view all dimensions.

Geometry (type × width × height × thickness) Effective width (mm) Height (mm) Flange thickness (mm) Web thickness (mm) Sectional area (cm²/m) Mass, single pile (kg/m) Wall mass (kg/m²) Moment of inertia (cm⁴/m) Elastic section modulus (cm³/m)
Z-type 559 × 229 × 9.50 559 229 9.50 9.50 136.9 60.0 107.4 11,500 973
Z-type 457 × 305 × 9.50 457 305 9.50 9.50 168.1 60.3 131.8 25,200 1,620
Z-type 575 × 378 × 15.21 / 12.67 575 378 15.21 12.67 217.8 98.2 170.9 49,300 2,608
Z-type 500 × 409 × 15.21 / 12.67 500 409 15.21 12.67 249.1 97.6 195.3 67,000 3,263

ASTM A572 Chemical Composition (Heat Analysis)

The figures below are the Table 2 heat-analysis limits for the A572 grades listed, from A572/A572M-21ε1. For Grade 50, manganese is 1.35% maximum, with the standard footnote that for each 0.01% carbon below the 0.23% maximum, manganese may rise 0.06% up to 1.60%. A manganese minimum of 0.50% by heat analysis (0.45% by product analysis) applies to products other than thicker plate, and the manganese-to-carbon ratio shall not be less than 2 to 1. Phosphorus and sulphur are tabulated at 0.030% maximum; for sheet piling the same table permits 0.04% phosphorus and 0.05% sulphur. Silicon is 0.40% maximum in the column that covers sheet piling with flange or leg thickness to 3 in. [75 mm]. Copper, when specified, is 0.20% minimum by heat analysis (0.18% by product analysis). Alloy content shall be Type 1, 2, 3 or 5 and shall be reported. Grade 65 has two thickness-dependent carbon and manganese rows in Table 2; the row used shall match the ordered thickness. The ordered edition governs if it differs.

Swipe horizontally to view all dimensions.

Grade C max Mn max P max S max Si max
Grade 50 [345] 0.23 1.35 0.030 0.030 0.40
Grade 55 [380] 0.25 1.35 0.030 0.030 0.40
Grade 60 [415] 0.26 1.35 0.030 0.030 0.40
Grade 65 [450], thicker product row 0.23 1.65 0.030 0.030 0.40
Grade 65 [450], thinner product row 0.26 1.35 0.030 0.030 0.40

ASTM A572 Mechanical Properties

The tensile values below are from Table 4 of the same edition. Elongation is given for both the 8 in. [200 mm] and the 2 in. [50 mm] gauge lengths. A supplementary 70 ksi tensile requirement that can be specified for Grade 50 at thicknesses of 3/4 in. [20 mm] and less is not a default value and is applied only when it is named on the order. There is no default Charpy requirement unless a supplementary impact test is agreed.

Grade Min. yield Min. tensile Min. elongation in 8 in. [200 mm] Min. elongation in 2 in. [50 mm]
Grade 50 [345] 50 ksi [345 MPa] 65 ksi [450 MPa] 18% 21%
Grade 55 [380] 55 ksi [380 MPa] 70 ksi [485 MPa] 17% 20%
Grade 60 [415] 60 ksi [415 MPa] 75 ksi [520 MPa] 16% 18%
Grade 65 [450] 65 ksi [450 MPa] 80 ksi [550 MPa] 15% 17%

Shape Tolerances and Identification

Shape, mass and length tolerances for these sections follow ASTM A6/A6M unless the order states otherwise. A typical mill mass tolerance under A6 is ± 2.5%, and length is commonly plus a stated allowance and minus zero; the ordered A6 edition governs.

A typical inspection mark identifies the specification and grade, the geometry, the heat number, the producer and the length. A Grade 50 certificate is not a Grade 60 certificate, and an A572 sheet-pile mark is not an A328, A690 or A572 W-shape mark.

Delivery Conditions, Inspection and Identification

These piles are commonly supplied as-rolled. The inspection document should identify ASTM A572/A572M and its edition, the grade, the alloy type, the section geometry, the length, the heat analysis, and the tensile results including the elongation gauge length. Coils are not qualified until they have been processed into finished sheet piling. An A572 plate or W-shape certificate does not, by itself, identify A572 sheet piling.

Applications and Service Limits

ASTM A572 Grade 50 steel sheet piles are used in retaining walls, cofferdams, dock work and similar interlocking-wall structures where a high-strength low-alloy sheet-piling grade is named. They are not a silent substitute for ASTM A328 carbon steel sheet pile, for ASTM A690 steel sheet pile, or for EN 10248-1 S355GP U-type and Z-type steel sheet pile. Interlocks of similar width are not interchangeable by depth or mass alone.

ASTM A572 Grade 50 Compared with A328, A690 and EN 10248-1

The comparisons below are an orientation only; they are not automatic substitutes.

Grade / designation Standard Relationship to ASTM A572 Grade 50 sheet pile Caution
A572 Grades 55, 60 and 65 ASTM A572/A572M Higher grades in the same specification, with different yield, tensile, elongation and carbon or manganese limits. A higher grade is not a silent upgrade of Grade 50, and not every section is offered in every grade.
ASTM A328 ASTM A328/A328M Carbon steel sheet piling, with a lower yield than Grade 50. A328 is not A572. See ASTM A328 carbon steel sheet pile.
ASTM A690 ASTM A690/A690M A marine sheet-pile grade with specified nickel, copper and phosphorus. A690 is not A572. See ASTM A690 steel sheet pile.
EN 10248-1 S355GP EN 10248-1:2023 A European hot-rolled grade with a similar yield level. Elongation gauge, impact and chemistry differ. See EN 10248-1 S355GP U-type and Z-type steel sheet pile.

Near-Equivalents: Not Automatic Substitutes

A near-equivalent is a starting point for a discussion, not a licence to swap certificates. If a project names ASTM A572 Grade 50 sheet piling, keep that specification, grade and geometry on the order. Related pages include ASTM A328 carbon steel sheet pile and ASTM A690 steel sheet pile.

Sourcing ASTM A572 Grade 50 Steel Sheet Piles from SHH STEEL

SHH STEEL supplies ASTM A572 Grade 50 steel sheet piles, and the other A572 grades named on the order, against a named geometry, the material edition and the inspection document type. Enquiries should state the type and geometry, the grade, the length, and any coating, corner piles or interlock-strength requirements.

The size tables are typical published mill series, not a claim that every section is rolled in every grade. Once the list is clear, a quotation can be prepared against the stated edition and certificate.

ASTM A572 Grade 50 Steel Sheet Pile FAQs

Is ASTM A572 Grade 50 sheet piling the same as an A572 W-shape?
No. This page is for interlocking sheet piles only. An A572 beam, channel or angle certificate does not identify A572 sheet piling, and this leaf is not the A572 beam, channel or angle category.
Can Grade 60 or Grade 65 be substituted for Grade 50?
Not automatically. Those grades have higher yield and tensile minima and different carbon or manganese limits. They are listed here as family variants and must be named on the order if they are required.
What phosphorus and sulphur limits apply to A572 sheet piling?
Table 2 tabulates 0.030% maximum for both. The same table permits 0.04% phosphorus and 0.05% sulphur for sheet piling. The ordered edition and the values reported on the certificate govern.
Which edition of A572 is used on this page?
The numeric tables use A572/A572M-21ε1 as published in SA-572/SA-572M. A later edition may be named on the order; the ordered edition governs.

Request a Quotation for ASTM A572 Grade 50 Steel Sheet Pile

ASTM A572 Grade 50 steel sheet pile is high-strength low-alloy sheet piling with a 50 ksi [345 MPa] minimum yield and a 65 ksi [450 MPa] minimum tensile strength. Nominate the geometry, the grade, ASTM A572/A572M or the edition on the order, the length, and the inspection document type. Send the size list, grade, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response