EN 10208-1 L210GA Steel Plate | Class A Pipeline Plate
What is EN 10208-1 L210GA steel plate?
EN 10208-1 L210GA (steel number 1.0319) belongs to EN 10208-1 requirement class A. EN 10208 is a pipe standard for on-land combustible-fluid pipelines, primarily gas supply systems, and excludes petroleum and natural gas industry pipeline transportation covered by ISO 3183 / API Spec 5L. Part 1 has less stringent quality and testing than Part 2 and specifies no Charpy impact energy requirements.
EN 10208-1:2009 and EN 10208-2:2009 specify technical delivery conditions for steel PIPES for pipelines for combustible fluids (primarily on-land gas supply systems). They are not plate product standards. SHH supplies pipeline steel plate as feedstock for forming welded line pipe to the ordered EN 10208 grade chemistry and mechanical package; plate is not automatically certified as finished EN 10208 pipe. Confirm plate-as-feedstock scope, testing and documentation at quotation. Both EN 10208 parts were withdrawn/replaced in CEN catalogs by EN ISO 3183:2012 (later editions of EN ISO 3183 / ISO 3183 and API Spec 5L cover petroleum and natural gas industry line pipe). Historical gas-distribution RFQs may still cite EN 10208; match the project specification.
This page covers pipeline steel plate intended as feedstock for forming welded line pipe to the L210GA chemistry and tensile package. Do not treat plate as certified finished EN 10208 pipe unless the order and MTC explicitly cover that scope.
Category hubs: Pipeline Steel Plates · EN 10208-1 · EN 10208-2 · API 5L.
Sibling EN 10208-1 grades: L235GA · L245GA · L290GA · L360GA.
Material Specification for EN 10208-1 L210GA
| Parameter | Specification |
|---|---|
| Reference standard | EN 10208-1:2009 (withdrawn/replaced by EN ISO 3183 in CEN catalogs; confirm project edition) |
| Grade / number | L210GA / 1.0319 |
| Requirement class | A (GA) |
| Product form on this page | Pipeline steel plate for line-pipe forming (feedstock); confirm at quotation |
| Underlying EN product | Seamless or welded steel pipe for combustible fluids |
| SHH supply focus | About 6-50 mm plate (confirm thicker / thinner against mill practice and order) |
| Width / length | About 1500-4000 mm width; length cut-to-size on request |
| Delivery condition | GA = requirement class A in the steel name (not a delivery-condition letter). Route may be as-rolled, normalized / normalizing formed, quenched and tempered, or thermomechanical as applicable to the manufacturing table. Marking may add +Q or +M when those conditions are used. |
| Surface / edge | As-rolled or shot blasted; mill edge or cut edge |
| Certification | EN 10204 3.1 / 3.2 as ordered |
| Density | 7.85 g/cm³ |
Chemical Composition of EN 10208-1 L210GA (heat and product analysis)
Heat (cast) and product analysis for L210GA under EN 10208-1. Steels are fully killed. Other alloying elements shall not be added intentionally (beyond deoxidation/finishing). Always verify the mill test certificate.
| Analysis | C | Si | Mn | P | S | Al total |
|---|---|---|---|---|---|---|
| Heat (cast) | ≤0.21 | ≤0.40 | ≤0.90 | ≤0.030 | ≤0.030 | 0.015-0.060 |
Product analysis may exceed cast maxima by: C +0.02, Si +0.05, Mn +0.10, P +0.005, S +0.005, Al ±0.005 (EN 10208-1 product-analysis tolerances).
No tabulated CEV / CE limit is specified for GA grades in the verified EN 10208-1 cast-analysis table. If a carbon-equivalent cap is required, state it on the purchase order.
Mechanical Properties of EN 10208-1 L210GA
Tensile requirements for the pipe body under EN 10208-1 (applicable to plate ordered against the L210GA mechanical package for line-pipe forming). Yield is Rt0.5 (0.5% total elongation); within normal scatter this is considered approximately equivalent to ReH or Rp0.2. Elongation A is transverse (L0 = 5.65√S0); longitudinal specimens are 2 percentage points higher when tested.
| Grade | Rt0.5 min (MPa) | Rm (MPa) | A transverse min (%) | Bend mandrel (SAW/COW) |
|---|---|---|---|---|
| L210GA | ≥210 | 335-475 | ≥25 | 2T (SAW/COW weld bend) |
Impact: EN 10208-1 does not specify Charpy impact energy. If toughness is required, order EN 10208-2 class B, ISO 3183 / API 5L PSL2, or an agreed CVN package on the plate PO.
Density approximately 7.85 g/cm³.
Delivery Conditions for EN 10208-1 L210GA plate
GA = requirement class A in the steel name (not a delivery-condition letter). Route may be as-rolled, normalized / normalizing formed, quenched and tempered, or thermomechanical as applicable to the manufacturing table. Marking may add +Q or +M when those conditions are used.
Unless otherwise agreed, choice of heat-treatment condition for EN 10208-1 pipe routes is left to the manufacturer within the allowed manufacturing table. For plate feedstock, state the required plate delivery condition on the order (for example as-rolled, normalized, or TMCP) so mill rolling practice matches the intended pipe route.
Hot forming or field heat treatment of material produced by Q or M routes can change mechanical properties; contact the mill when post-forming heat treatment is planned.
Weldability of EN 10208-1 L210GA
L210GA chemistry under EN 10208-1 is specified so the steel is considered weldable for pipe and pipeline fabrication. Actual welding behaviour also depends on consumables, joint design, heat input, preheat and procedure qualification. Use a qualified WPS. Low-hydrogen practices are preferred for many structural pipeline joints.
Related pages: EN 10208-2 class B when toughness-controlled welding packages are required · API 5L · API 5L Grade A.
Dimensional Tolerances for EN 10208-1 L210GA plate
EN 10208 dimensional tables address finished pipe (diameter, wall, out-of-roundness, weld bead, mass). For plate feedstock, dimensional tolerances follow the plate dimensional standard agreed on the order (for example EN 10029 or mill practice) unless the PO cites another agreement. State flatness class, edge condition and cut size when pipe-forming tolerances are tight.
Applications and service limits for EN 10208-1 L210GA
Typical purchasing contexts for L210GA plate feedstock:
- On-land gas distribution / combustible-fluid pipeline projects citing EN 10208-1 class A
- Welded line-pipe forming where class A tensile packages are specified without mandatory Charpy
- RFQs comparing L210GA with API 5L Grade A / L210
Not a substitute for ISO 3183 / API 5L petroleum and natural gas industry line pipe unless the project allows that substitution. Not an offshore or sour-service specification by itself.
Related: Pipeline Steel Plates · EN 10208-1 · API 5L Grade A / L210 · GB/T 21237 related grade.
Pipe feedstock and testing notes for EN 10208-1 L210GA
EN 10208-1 pipe testing includes tensile, bend or flattening (by process), hydrostatic or agreed leak-tightness, visual and dimensional checks, and NDT per Annex. Plate ordered as feedstock should define which of those pipe tests will be performed after forming versus which plate tests (chemistry, tensile, UT) are required at plate stage.
Hard-spot rules in EN 10208 apply to cold-formed pipe surfaces (hardness < 35 HRC for hard spots > 50 mm; confirm HB conversion on the ordered Part 1 edition). Flattening is an EW/HFW pipe test, not a plate coupon test.
Equivalent and related grades for EN 10208-1 L210GA
These grades are commonly compared with L210GA. They are approximate, not automatic substitutes.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| EN 10208-1 | L210GA | This page | – |
| API 5L / ISO 3183 | API 5L Grade A / L210 | Approximate strength talk | API 5L related |
| GB/T 21237 | Related PSL1 grade | Planned plate hub | GB/T 21237 |
| EN 10208-2 | Class B NB/MB/QB | Tougher / tighter class B track | EN 10208-2 |
| Category | Pipeline hubs | Navigation | Pipeline Steel Plates · EN 10208-1 · API 5L |
EN 10208-1 L210GA vs sibling GA grades (selection aid)
Why choose SHH STEEL for EN 10208-1 L210GA
- China mill-direct pipeline steel plate aligned to EN 10208-1 L210GA grade requirements for line-pipe forming
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV) on request
- Clear feedstock wording: plate for forming to EN 10208 grade requirements, confirm at quotation
- Sibling coverage under EN 10208-1 and class B under EN 10208-2
- API 5L / ISO 3183 and GB/T 21237 talk pages when the project cites those standards: API 5L related · GB/T 21237
Supply, cutting and inspection for EN 10208-1 L210GA
| Item | SHH STEEL supply note |
|---|---|
| Thickness | About 6-50 mm focus; confirm against mill practice |
| Size | Width about 1500-4000 mm; cut-to-size length on request |
| Delivery condition | As ordered (AR / N / TMCP / Q&T as applicable) |
| Processing | Cutting, beveling, shot blasting available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV can be arranged |
| Quotation needs | Grade L210GA, thickness × width × length, quantity, delivery condition, any CVN/UT extras, inspection level |
FAQ
-
Is EN 10208-1 L210GA a plate standard?
- No. EN 10208 is a steel pipe standard for combustible-fluid pipelines. This page covers pipeline steel plate for line-pipe forming to L210GA grade requirements; confirm at quotation.
-
Does Part 1 require Charpy impact?
- No. EN 10208-1 specifies no Charpy energy. Use EN 10208-2 or ISO 3183 / API 5L PSL2 when toughness is mandatory.
-
What is the approximate API 5L talk grade?
- API 5L Grade A / L210. See API 5L related page. Substitution needs project approval.
-
Was EN 10208 superseded?
- EN 10208-1:2009 was withdrawn/replaced by EN ISO 3183:2012 in CEN catalogs. Match the project specification before ordering.
-
What certificates are available?
- EN 10204 3.1 standard; 3.2 on request. Do not assume additional mill system certificates beyond what the order states.
Request a quotation
Send EN 10208-1 L210GA, thickness × width × length, quantity, plate delivery condition, any extra toughness/UT requirements and inspection level. SHH STEEL will return mill availability, certification scope and a quotation for pipeline steel plate for line-pipe forming to EN 10208 grade requirements.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: EN 10208-1 · Pipeline Steel Plates · API 5L · EN 10208-2