EN 10208-1 L290GA Steel Plate | EN 10208-1 Pipeline Steel - SHH STEEL

EN 10208-1 L290GA Steel Plate | Class A Pipeline Plate

EN 10208-1 L290GA is a requirement-class A pipeline steel grade under EN 10208-1:2009 for steel pipes for combustible fluids (primarily on-land gas supply). Minimum yield Rt0.5 ≥ 290 MPa with tensile Rm 415-555 MPa. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.
Equivalent Grades:
Approximate talk: API 5L X42 / L290; related ISO 3183 / API 5L PSL1 strength class; planned GB/T 21237 PSL1 counterparts where listed. Not automatic substitutes. Confirm against project specs.
Heat Treatment
GA = requirement class A in the steel name (not a delivery-condition letter). Route may be as-rolled, normalized / normalizing formed, quenched and tempered, or thermomechanical as applicable to the manufacturing table. Marking may add +Q or +M when those conditions are used.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Pipe feedstock and testing notes
Equivalent Material Grade
L290GA vs siblings
Why choose Us
Our Service
FAQ
Conclusion

What is EN 10208-1 L290GA steel plate?

EN 10208-1 L290GA (steel number 1.0483) belongs to EN 10208-1 requirement class A. EN 10208 is a pipe standard for on-land combustible-fluid pipelines, primarily gas supply systems, and excludes petroleum and natural gas industry pipeline transportation covered by ISO 3183 / API Spec 5L. Part 1 has less stringent quality and testing than Part 2 and specifies no Charpy impact energy requirements.

EN 10208-1:2009 and EN 10208-2:2009 specify technical delivery conditions for steel PIPES for pipelines for combustible fluids (primarily on-land gas supply systems). They are not plate product standards. SHH supplies pipeline steel plate as feedstock for forming welded line pipe to the ordered EN 10208 grade chemistry and mechanical package; plate is not automatically certified as finished EN 10208 pipe. Confirm plate-as-feedstock scope, testing and documentation at quotation. Both EN 10208 parts were withdrawn/replaced in CEN catalogs by EN ISO 3183:2012 (later editions of EN ISO 3183 / ISO 3183 and API Spec 5L cover petroleum and natural gas industry line pipe). Historical gas-distribution RFQs may still cite EN 10208; match the project specification.

This page covers pipeline steel plate intended as feedstock for forming welded line pipe to the L290GA chemistry and tensile package. Do not treat plate as certified finished EN 10208 pipe unless the order and MTC explicitly cover that scope.

Category hubs: Pipeline Steel Plates · EN 10208-1 · EN 10208-2 · API 5L.

Sibling EN 10208-1 grades: L210GA · L235GA · L245GA · L360GA.

Material Specification for EN 10208-1 L290GA

Parameter Specification
Reference standard EN 10208-1:2009 (withdrawn/replaced by EN ISO 3183 in CEN catalogs; confirm project edition)
Grade / number L290GA / 1.0483
Requirement class A (GA)
Product form on this page Pipeline steel plate for line-pipe forming (feedstock); confirm at quotation
Underlying EN product Seamless or welded steel pipe for combustible fluids
SHH supply focus About 6-50 mm plate (confirm thicker / thinner against mill practice and order)
Width / length About 1500-4000 mm width; length cut-to-size on request
Delivery condition GA = requirement class A in the steel name (not a delivery-condition letter). Route may be as-rolled, normalized / normalizing formed, quenched and tempered, or thermomechanical as applicable to the manufacturing table. Marking may add +Q or +M when those conditions are used.
Surface / edge As-rolled or shot blasted; mill edge or cut edge
Certification EN 10204 3.1 / 3.2 as ordered
Density 7.85 g/cm³

Chemical Composition of EN 10208-1 L290GA (heat and product analysis)

Heat (cast) and product analysis for L290GA under EN 10208-1. Steels are fully killed. V, Nb, Ti and combinations thereof may be added; sum shall not exceed 0.15%. Always verify the mill test certificate.

Analysis C Si Mn P S Al total V+Nb+Ti
Heat (cast) ≤0.20 ≤0.40 ≤1.40 ≤0.030 ≤0.030 0.015-0.060 ≤0.15 (sum; added at manufacturer discretion)

Product analysis may exceed cast maxima by: C +0.02, Si +0.05, Mn +0.10, P +0.005, S +0.005, Al ±0.005, V+Nb+Ti +0.02 (EN 10208-1 product-analysis tolerances).

No tabulated CEV / CE limit is specified for GA grades in the verified EN 10208-1 cast-analysis table. If a carbon-equivalent cap is required, state it on the purchase order.

Mechanical Properties of EN 10208-1 L290GA

Tensile requirements for the pipe body under EN 10208-1 (applicable to plate ordered against the L290GA mechanical package for line-pipe forming). Yield is Rt0.5 (0.5% total elongation); within normal scatter this is considered approximately equivalent to ReH or Rp0.2. Elongation A is transverse (L0 = 5.65√S0); longitudinal specimens are 2 percentage points higher when tested.

Grade Rt0.5 min (MPa) Rm (MPa) A transverse min (%) Bend mandrel (SAW/COW)
L290GA ≥290 415-555 ≥21 3T (SAW/COW weld bend)

Impact: EN 10208-1 does not specify Charpy impact energy. If toughness is required, order EN 10208-2 class B, ISO 3183 / API 5L PSL2, or an agreed CVN package on the plate PO.

Density approximately 7.85 g/cm³.

Delivery Conditions for EN 10208-1 L290GA plate

GA = requirement class A in the steel name (not a delivery-condition letter). Route may be as-rolled, normalized / normalizing formed, quenched and tempered, or thermomechanical as applicable to the manufacturing table. Marking may add +Q or +M when those conditions are used.

Unless otherwise agreed, choice of heat-treatment condition for EN 10208-1 pipe routes is left to the manufacturer within the allowed manufacturing table. For plate feedstock, state the required plate delivery condition on the order (for example as-rolled, normalized, or TMCP) so mill rolling practice matches the intended pipe route.

Hot forming or field heat treatment of material produced by Q or M routes can change mechanical properties; contact the mill when post-forming heat treatment is planned.

Weldability of EN 10208-1 L290GA

L290GA chemistry under EN 10208-1 is specified so the steel is considered weldable for pipe and pipeline fabrication. Actual welding behaviour also depends on consumables, joint design, heat input, preheat and procedure qualification. Use a qualified WPS. Low-hydrogen practices are preferred for many structural pipeline joints.

Related pages: EN 10208-2 class B when toughness-controlled welding packages are required · API 5L · API 5L X42.

Dimensional Tolerances for EN 10208-1 L290GA plate

EN 10208 dimensional tables address finished pipe (diameter, wall, out-of-roundness, weld bead, mass). For plate feedstock, dimensional tolerances follow the plate dimensional standard agreed on the order (for example EN 10029 or mill practice) unless the PO cites another agreement. State flatness class, edge condition and cut size when pipe-forming tolerances are tight.

Applications and service limits for EN 10208-1 L290GA

Typical purchasing contexts for L290GA plate feedstock:

  • On-land gas distribution / combustible-fluid pipeline projects citing EN 10208-1 class A
  • Welded line-pipe forming where class A tensile packages are specified without mandatory Charpy
  • RFQs comparing L290GA with API 5L X42 / L290

Not a substitute for ISO 3183 / API 5L petroleum and natural gas industry line pipe unless the project allows that substitution. Not an offshore or sour-service specification by itself.

Related: Pipeline Steel Plates · EN 10208-1 · API 5L X42 / L290 · GB/T 21237 related grade.

Pipe feedstock and testing notes for EN 10208-1 L290GA

EN 10208-1 pipe testing includes tensile, bend or flattening (by process), hydrostatic or agreed leak-tightness, visual and dimensional checks, and NDT per Annex. Plate ordered as feedstock should define which of those pipe tests will be performed after forming versus which plate tests (chemistry, tensile, UT) are required at plate stage.

Hard-spot rules in EN 10208 apply to cold-formed pipe surfaces (hardness < 35 HRC for hard spots > 50 mm; confirm HB conversion on the ordered Part 1 edition). Flattening is an EW/HFW pipe test, not a plate coupon test.

Equivalent and related grades for EN 10208-1 L290GA

These grades are commonly compared with L290GA. They are approximate, not automatic substitutes.

Standard / family Grade Relation Product page
EN 10208-1 L290GA This page –
API 5L / ISO 3183 API 5L X42 / L290 Approximate strength talk API 5L related
GB/T 21237 Related PSL1 grade Planned plate hub GB/T 21237
EN 10208-2 Class B NB/MB/QB Tougher / tighter class B track EN 10208-2
Category Pipeline hubs Navigation Pipeline Steel Plates · EN 10208-1 · API 5L

EN 10208-1 L290GA vs sibling GA grades (selection aid)

Class A GA grades share the EN 10208-1 framework; strength and chemistry caps differ.

Grade Rt0.5 min Rm A trans min Page
L210GA ≥210 335-475 ≥25 L210GA
L235GA ≥235 370-510 ≥23 L235GA
L245GA ≥245 415-555 ≥22 L245GA
L290GA ≥290 415-555 ≥21 This page
L360GA ≥360 460-620 ≥20 L360GA

Why choose SHH STEEL for EN 10208-1 L290GA

  • China mill-direct pipeline steel plate aligned to EN 10208-1 L290GA grade requirements for line-pipe forming
  • EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV) on request
  • Clear feedstock wording: plate for forming to EN 10208 grade requirements, confirm at quotation
  • Sibling coverage under EN 10208-1 and class B under EN 10208-2
  • API 5L / ISO 3183 and GB/T 21237 talk pages when the project cites those standards: API 5L related · GB/T 21237

Supply, cutting and inspection for EN 10208-1 L290GA

Item SHH STEEL supply note
Thickness About 6-50 mm focus; confirm against mill practice
Size Width about 1500-4000 mm; cut-to-size length on request
Delivery condition As ordered (AR / N / TMCP / Q&T as applicable)
Processing Cutting, beveling, shot blasting available
Mill certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV can be arranged
Quotation needs Grade L290GA, thickness × width × length, quantity, delivery condition, any CVN/UT extras, inspection level

FAQ

Is EN 10208-1 L290GA a plate standard?
No. EN 10208 is a steel pipe standard for combustible-fluid pipelines. This page covers pipeline steel plate for line-pipe forming to L290GA grade requirements; confirm at quotation.
Does Part 1 require Charpy impact?
No. EN 10208-1 specifies no Charpy energy. Use EN 10208-2 or ISO 3183 / API 5L PSL2 when toughness is mandatory.
What is the approximate API 5L talk grade?
API 5L X42 / L290. See API 5L related page. Substitution needs project approval.
Was EN 10208 superseded?
EN 10208-1:2009 was withdrawn/replaced by EN ISO 3183:2012 in CEN catalogs. Match the project specification before ordering.
What certificates are available?
EN 10204 3.1 standard; 3.2 on request. Do not assume additional mill system certificates beyond what the order states.

Request a quotation

Send EN 10208-1 L290GA, thickness × width × length, quantity, plate delivery condition, any extra toughness/UT requirements and inspection level. SHH STEEL will return mill availability, certification scope and a quotation for pipeline steel plate for line-pipe forming to EN 10208 grade requirements.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: EN 10208-1 · Pipeline Steel Plates · API 5L · EN 10208-2

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X