BS 1501 503 Steel Plate | BS 1501 Steel - SHH STEEL

BS 1501 503 Steel Plate

BS 1501 503 is an alloy steel plate for pressure purposes under BS 1501-2. A public database listing shows carbon 0.15 % maximum, chromium 0.30 % maximum and aluminium 0.015–0.055 %. The same listing shows tensile strength of at least 450 MPa, yield of at least 265 MPa and elongation 22 % minimum. A peer catalogue adds nickel 3.25–3.75 % as a reference cell only. SHH STEEL produces and exports 503 plate to the ordered edition, delivery condition and dimensions.
Equivalent Grades:
Peer catalogues treat type 503 as a 3.5 % nickel vessel name (near name only).
Heat Treatment
Normalized at 870–900 °C and tempered at 580–630 °C.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is BS 1501 503 plate?

We produce and export BS 1501 503 as alloy steel plate (nickel family in peer catalogues; 1988 identity not photographed) for pressure purposes. Typical service is alloy pressure equipment that specifies this type.

BS 1501-2:1988 is the last final edition of the alloy-plate part of BS 1501. It was published on 29 July 1988 and superseded on 15 January 1995. It replaced Addendum No. 1 (1973) and Addendum No. 2 (1975) to BS 1501: Part 2: 1970. A photographed 1988 Table 1 was not opened for this page. Clause 3 of the 1988 book is titled Designation, but that clause text was not opened. Clause 19 makes elevated-temperature proof stress an optional requirement for section-two steels. The formal 1988 writing of type, tensile token and any A or B suffix therefore remains unverified. Peer catalogues sometimes write names such as 243 B, 620 B, 621 B or 622-515 B; those B forms are recorded as unverified formal-symbol candidates, not declared absent and not declared commercial-only.

Numeric cells below are taken only from the named public database or peer catalogue opened for this page. They are a reference basis, not a photographed BS 1501-2:1988 table and not an SHH proprietary guarantee. EN 10028-2 values for 16Mo3, 13CrMo4-5 or 10CrMo9-10 are not copied onto this legacy type. Missing chemistry or thickness-banded mechanical fields are project requirements to be agreed against the named edition.

SHH STEEL produces and exports BS 1501 503 plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.

Material specification for BS 1501 503

The items below follow BS 1501-2:1988 as the historical alloy-plate book. Numeric cells in the chemical and mechanical sections are from opened public-database listings and peer catalogues, each labelled by source. They are not photographed 1988 Table 1 values and not 1993 National Annex NC tables (that annex covers 271, 281, 621 and 660 only). Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.

Parameter Detail
Standard BS 1501-2:1988, Steels for pressure purposes — Specification for alloy steels: plates. Numeric cells below are public-database or peer-catalogue references, each labelled by source
Designation used here Working name BS 1501 503 (formal 1988 full symbol unverified)
Steel type Alloy steel plate (nickel family in peer catalogues; 1988 identity not photographed)
Product form Alloy steel plate for pressure purposes (this part does not cover bars, sections, forgings, tubes or stainless sheet)
How designations are listed This page uses the working name 503. Formal 1988 full symbols (type number plus any tensile token and any A or B suffix) were not photographed. Peer catalogues that print B forms are recorded as unverified formal-symbol candidates; they are not declared absent and not declared commercial-only
Applicable thickness in the opened tensile table Not verified from an official thickness table
Usual heat treatment Normalized at 870–900 °C and tempered at 580–630 °C.
Chemical analysis Opened public cells only, each labelled by source in the chemical table
Tensile properties Database minima only; thickness bands are a project requirement
Our supply We produce and export 503 plate to the ordered edition, delivery condition, dimensions and extra tests

Chemical composition of BS 1501 503

Numeric cells below are taken only from the named public database or peer catalogue opened for this page. They are a reference basis, not a photographed BS 1501-2:1988 table and not an SHH proprietary guarantee. EN 10028-2 values for 16Mo3, 13CrMo4-5 or 10CrMo9-10 are not copied onto this legacy type. Missing chemistry or thickness-banded mechanical fields are project requirements to be agreed against the named edition. A 1970 Part 2 catalogue abstract lists type 503 among the older imperial alloy plates. One peer catalogue’s mechanical figures for 503 (for example a tensile of 934 MPa with yield 738 MPa) are internally inconsistent and are not used.

Element Value (wt. %) Source opened for this cell
Carbon (C) 0.15 max Public database listing opened 8 November 2026 (Asia/Shanghai); the same carbon limit also appears on a peer catalogue
Chromium (Cr) 0.30 max Public database listing opened 8 November 2026 (Asia/Shanghai)
Aluminium (Al) 0.015–0.055 Public database listing opened 8 November 2026 (Asia/Shanghai)
Aluminium (metal) (Al) 0.020 min Peer catalogue opened 8 November 2026 (Asia/Shanghai); different aluminium definition from the public-database range
Silicon (Si) 0.15–0.35 Peer catalogue opened 8 November 2026 (Asia/Shanghai)
Manganese (Mn) 0.30–0.80 Peer catalogue opened 8 November 2026 (Asia/Shanghai)
Nickel (Ni) 3.25–3.75 Peer catalogue opened 8 November 2026 (Asia/Shanghai)
Phosphorus (P) 0.025 max Peer catalogue opened 8 November 2026 (Asia/Shanghai)
Sulfur (S) 0.020 max Peer catalogue opened 8 November 2026 (Asia/Shanghai)

Tensile, impact and elevated-temperature properties for BS 1501 503

Only the opened numeric cells are listed. Thickness-banded values and Charpy energies are a project requirement unless an edition table is named.

Item Value Source opened for this cell
Tensile strength Rm ≥ 450 MPa (minimum only, not a window) Public database listing opened 8 November 2026 (Asia/Shanghai)
Yield / Rp0.2 ≥ 265 MPa Public database listing opened 8 November 2026 (Asia/Shanghai)
Elongation A ≥ 22 % Public database listing opened 8 November 2026 (Asia/Shanghai)

A database listing showed normalizing at 870–900 °C and tempering at 580–630 °C. Hidden public-database fields were not filled. Numeric cells below are taken only from the named public database or peer catalogue opened for this page. They are a reference basis, not a photographed BS 1501-2:1988 table and not an SHH proprietary guarantee. EN 10028-2 values for 16Mo3, 13CrMo4-5 or 10CrMo9-10 are not copied onto this legacy type. Missing chemistry or thickness-banded mechanical fields are project requirements to be agreed against the named edition.

Delivery conditions for BS 1501 503

A public database listing shows normalizing at 870–900 °C and tempering at 580–630 °C. Name the required delivery condition on the purchase order.

If the project has moved to EN 10028-2, order the successor designation and edition expressly. A later European name is not by itself a substitute instruction for type 503.

The purchase order should name the official designation, the edition required, thickness, width and length, the delivery condition, any extra tests, and the inspection document required.

This page does not offer heat-treatment or fabrication services.

Welding and thermal cutting

Neither the opened historical book notes nor the later remaining-steel annex set a welding procedure for type 503 on this page. Welding and thermal cutting should be qualified for the alloy content, thickness and the specified delivery condition.

If the project treats type 503 as a 3.5 % nickel steel, consumables should match the qualified procedure for that nickel family.

Heat input and any required post-weld heat treatment belong in the project specification.

Form, appearance, dimensions and thickness tolerances

Thickness, width, length, flatness and mass tolerances should be stated on the purchase order against the dimensional standard named by the project. The historical replacement set includes BS EN 10029 for plate tolerances when that standard is specified.

Appearance, repair welding and any ultrasonic class are taken from the enquiry. This page does not list stock sizes or mill capacity.

Applications and specification limits

We produce and export 503 plate as alloy steel plate for pressure purposes. Typical service is alloy pressure equipment that specifies type 503, often low-temperature duty when a nickel grade is required.

BS 1501-2:1988 is a historical alloy-plate standard. It is not the current EN 10028-2 or EN 10028-4 order unless that successor standard is written on the enquiry, and it is not a BS 1501-1 carbon, BS 1501-3 stainless, BS 1502 bar or BS 1503 forging order.

Compare BS 1501 503 with other steel plates

BS 1501 503 is a historical BS 1501-2 alloy pressure-vessel plate. The comparison below is for selection only; these materials are not equivalents.

Material Alloy / type Delivery condition Mechanical requirements Typical service Substitution limit
BS 1501 503 (this plate) Alloy plate; peer catalogue nickel 3.25–3.75 % Normalized at 870–900 °C and tempered at 580–630 °C. Database minima: Rm ≥ 450 MPa, yield ≥ 265 MPa, A ≥ 22 % Alloy pressure equipment that specifies this type A later EN name or a different 1988 type is not an automatic substitute
EN 10028-4 12Ni14 3.5 % nickel low-temperature vessel plate, steel number 1.5637 As specified in EN 10028-4 Live published yield in the 355 MPa class and tensile 490–640 MPa; impact typically −100 °C Modern European 3.5Ni vessel plate Near name only; those EN numbers are not copied onto type 503
ASTM A203 Grade D 3.50 % nickel low-temperature vessel plate As specified in ASTM A203/A203M Live published yield 255 MPa and tensile 450–585 MPa ASTM 3.5Ni vessel plate Related nickel class only
EN 10028-4 13MnNi6-3 About 0.75 % nickel fine-grain low-temperature vessel plate, steel number 1.6217 As specified in EN 10028-4 Live published yield in the 355 MPa class and tensile 490–640 MPa; impact typically −80 °C Modern European lower-nickel vessel plate Different nickel level

Equivalent and related grades by country

The designations below are near names, not automatic substitutes. Confirm chemistry, heat treatment, tensile properties, impact temperature and product form.

Country / region Standard Grade or designation Similarity and key differences Substitution caveat
United Kingdom BS 1501-2:1988 working name 503 This page uses the working name 503. Formal 1988 suffix status is unverified. This product
Europe EN 10028-4 12Ni14 (1.5637) Later 3.5Ni vessel plate. Live published tensile 490–640 MPa and yield in the 355 MPa class, against database minima of 450 MPa and 265 MPa for type 503. Near name only
United States ASTM A203/A203M Grade D 3.50 % nickel vessel plate. Live published yield 255 MPa and tensile 450–585 MPa. Related nickel class only
China — — No separately verified GB plate counterpart was established for type 503 on this page. Do not assume a Chinese nickel vessel grade is a substitute

Why choose SHH STEEL for BS 1501 503

  • We produce and export BS 1501 503 alloy pressure-vessel steel plate
  • We review the enquiry for edition, designation, delivery condition, dimensions and extra tests
  • We keep the historical BS 1501-2 type number distinct from later EN 10028-2 names and from Part 1 A/B carbon grades, and we record peer B forms as unverified formal-symbol candidates until a 1988 table is opened
  • We match documentation to what the purchase order requires

How to enquire for BS 1501 503 plate

Item What to specify
Standard and designation BS 1501 503 and the edition required (BS 1501-2:1988 and/or the 1993 national-annex remaining-steel clauses)
Or successor standard The EN 10028-2 designation and edition, if that is what the project now requires
Delivery condition Normalized at 870–900 °C and tempered at 580–630 °C.
Dimensions Required thickness, width and length
Chemistry Cast analysis to the named edition
Mechanical tests Yield strength, tensile strength, elongation and, where specified, impact or elevated-temperature proof tests to the named edition
Other tests Ultrasonic examination or other extra tests only when written on the order
Documentation State the inspection document type required by the project

Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.

FAQ

Is BS 1501-2 still a current product standard?
No. BS 1501-2:1988 is the last final edition of the alloy-plate part. It was published on 29 July 1988 and superseded on 15 January 1995. EN 10028-2 superseded part of it. Projects still using a historical type number should name the edition required on the order.
Which numbers on this page are guaranteed 1988 table values?
None are presented as a photographed 1988 table. Visible public-database cells and a peer-catalogue chemistry set are shown with their sources. That catalogue’s mechanical figures were rejected as inconsistent.
Is type 503 officially a 3.5 % nickel steel?
A peer catalogue lists nickel 3.25–3.75 %. That cell is shown as a reference only. Nickel was hidden on the opened public-database page, so the official 1988 nickel window was not photographed.
Can 12Ni14 or A203 Grade D replace type 503?
Only after a project review. Those later names have their own published strengths and impact temperatures. They are not automatic substitutes.
What should a quotation enquiry include?
BS 1501 503, the edition required or the successor designation, the delivery condition, plate thickness by width by length, quantity, any extra tests, and the inspection document required.

Request a quotation

Contact SHH STEEL for a quotation for BS 1501 503 steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.

Specify the edition (BS 1501-2:1988 or the later United Kingdom national-annex remaining-steel clauses, or a named EN 10028-2 successor if that is what the project now requires), the delivery condition and any specimen heat treatment. If your project requires ultrasonic examination, a stated impact temperature or another extra test, include the acceptance criteria and the inspection document required.

If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response