BS 1501 151 Grade 360A Steel Plate
What is BS 1501-151 Grade 360A plate?
We produce and export BS 1501-151 Grade 360A as semi-killed or fully killed carbon steel plate for fired and unfired pressure equipment. Typical service includes welded boilers, vessels and similar parts that specify type 151 grade 360A.
BS 1501-1:1980 lists eight steel types, each with one or more tensile grades and, where Table 1 allows, suffix A or B and optional impact suffixes. This page specifies only 151 Grade 360A. It is not type 154, 161 or 164, a niobium-treated 223 plate, or a BS 1501-2 alloy or BS 1501-3 stainless plate. Suffix A specifies room-temperature tensile properties only.
Composition and room-temperature tensile properties on this page follow BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates, the last final edition of Part 1. BS 1501-1:1980 was published on 28 November 1980 and withdrawn on 15 February 1993. It replaced BS 1501: Part 1: 1964 and that edition’s addenda. It was replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Those successor designations are not automatic aliases for the 1980 type-and-grade names. Name the edition or successor standard required on the purchase order.
The chemical and tensile figures below follow BS 1501-1:1980 as tabulated for this designation, including a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 values. BS 1501-2 (alloy plates) and BS 1501-3 (corrosion- and heat-resisting plates, sheet and strip) are different parts of the same historical series.
SHH STEEL produces and exports BS 1501-151 Grade 360A plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.
Material specification for BS 1501-151 Grade 360A
The items below follow BS 1501-1:1980. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates |
| Official designation | BS 1501-151 Grade 360A |
| Steel type | Semi-killed or fully killed carbon steel |
| Product form | Hot-rolled steel plate (this part does not cover bars, sections, forgings, tubes or stainless sheet) |
| How designations are listed | Type number, tensile grade and suffix A or B; optional LT or RT impact suffixes where Table 1 allows; optional L after types 223, 224 and 225 when nickel is limited to 0.30 % |
| Applicable thickness | Up to and including 100 mm |
| Usual heat treatment | Normalized; hot-finished permitted through 40 mm. |
| Chemical analysis | Ladle analysis as tabulated for this type and grade in BS 1501-1:1980 |
| Tensile properties | Yield strength, tensile strength and elongation, by thickness, from that edition |
| Our supply | We produce and export 151 Grade 360A plate to the ordered edition, delivery condition, dimensions and extra tests |
Chemical composition of BS 1501-151 Grade 360A
The figures below are ladle analysis for BS 1501-151 Grade 360A from BS 1501-1:1980. Values are in weight percent.
| Element | 151 Grade 360A ladle analysis, BS 1501-1:1980 (wt. %) |
|---|---|
| Carbon (C) | 0.17 max |
| Silicon (Si) | 0.35 max |
| Manganese (Mn) | 0.40–1.20 |
| Phosphorus (P) | 0.030 max |
| Sulfur (S) | 0.045 max |
| Chromium (Cr) | 0.25 max |
| Copper (Cu) | 0.30 max |
| Molybdenum (Mo) | 0.10 max |
| Nickel (Ni) | 0.30 max |
Figures are ladle analysis as tabulated for this designation in BS 1501-1:1980. Type 151 may be supplied semi-killed or fully killed; when the steel is fully killed, silicon shall comply with table 16 (0.35 % maximum). Aluminium may be used in addition to silicon for deoxidation. The combined total of residual chromium, copper, molybdenum and nickel is 0.70 % maximum. Nitrogen shall not exceed 0.012 %. The 1980 edition allows the purchaser to specify tighter phosphorus and sulfur limits.
Tensile and related properties for BS 1501-151 Grade 360A
151 Grade 360A has thickness-dependent yield strength, tensile strength and elongation. Values below are from BS 1501-1:1980. Strength values are in N/mm², equivalent to MPa.
| Thickness | Tensile strength Rm, N/mm² | Yield strength Re, N/mm² min | Elongation A, % min |
|---|---|---|---|
| Over 3 mm up to and including 16 mm | 360–480 | 205 | 26 |
| Over 16 mm up to and including 40 mm | 360–480 | 195 | 26 |
| Over 40 mm up to and including 63 mm | 360–480 | 185 | 25 |
| Over 63 mm up to and including 100 mm | 360–480 | 175 | 24 |
The tensile window is that stated for this type 151 grade in BS 1501-1:1980. Type 151 clauses cover plates up to and including 100 mm; there is no 100 mm to 150 mm band in table 17. Impact properties are not listed as an available option for type 151 in the 1980 property-options table.
Delivery conditions for BS 1501-151 Grade 360A
Type 151 is supplied as semi-killed or fully killed carbon steel plate. The 1980 text specifies supply in the normalized condition, except that the manufacturer may omit normalizing for plates up to and including 40 mm thick provided all specified properties are met in the hot-finished condition. The purchaser may require normalized plate, or normalized test samples, through 40 mm if agreed at enquiry. Name the required delivery condition on the purchase order.
If the project has moved to EN 10028-2 or EN 10028-3, order the successor designation and edition expressly. A later name is not by itself a substitute instruction.
The purchase order should name the official designation including the A or B suffix, any required impact suffix, thickness, width and length, the delivery condition, any extra tests, and the inspection document required.
This page does not offer heat-treatment or fabrication services.
Welding and thermal cutting
BS 1501-1:1980 does not set a welding procedure. Type 151 is a carbon vessel plate intended for welded pressure equipment. Welding and thermal cutting should be qualified for the carbon content, thickness and delivery condition.
Heat input and any required post-weld heat treatment belong in the project specification.
Form, appearance, dimensions and thickness tolerances
Thickness, width, length, flatness and mass tolerances should be stated on the purchase order against the dimensional standard named by the project. The historical replacement set includes BS EN 10029 for plate tolerances when that standard is specified.
Appearance, repair welding and any ultrasonic class are taken from the enquiry. This page does not list stock sizes or mill capacity.
Applications and specification limits
We produce and export 151 Grade 360A plate as semi-killed or fully killed carbon steel plate for fired and unfired pressure equipment. Typical service includes welded boilers, vessels and similar parts that specify type 151 grade 360A. The 1980 type 151 clauses cover plates up to and including 100 mm thick in grades 360, 400 and 430. This page specifies grade 360 only.
BS 1501-1:1980 is a historical carbon and carbon-manganese plate standard for pressure purposes. It is not the current EN 10028-2 or EN 10028-3 order unless that successor standard is written on the enquiry, and it is not a BS 1501-2 alloy, BS 1501-3 stainless, BS 1502 bar or BS 1503 forging order.
Compare BS 1501-151 Grade 360A with other steel plates
151 Grade 360A is a BS 1501-1:1980 pressure-vessel plate. The comparison below is for selection only; these materials are not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| BS 1501-151 Grade 360A (this plate) | BS 1501-1:1980 official designation | Normalized; hot-finished permitted through 40 mm. | Yield 205 N/mm² minimum up to 16 mm; tensile 360–480 N/mm² | Typical service includes welded boilers and vessels that specify type 151 grade 360A | A different standard, later EN name, or 1980 type is not an automatic substitute |
| EN 10028-2 P265GH | Non-alloy elevated-temperature vessel plate, steel number 1.0425 | As specified in EN 10028-2 | Published yield 265 MPa and tensile 410–530 MPa | Modern European carbon boiler and vessel plate | Related carbon class only; a later EN name is not an automatic substitute |
| ASTM A516 Grade 60 | ASTM carbon vessel plate | As specified in ASTM A516/A516M | Published yield 220 MPa and tensile 415–550 MPa | Carbon pressure-vessel plate to the ASTM book | Related product form only |
| GB/T 713 Q245R | Later Chinese carbon vessel plate | As specified in GB/T 713 | Published yield 245 MPa and tensile 400–520 MPa | Modern Chinese carbon boiler and vessel plate | Related carbon class only |
Equivalent and related grades by country
The designations below are near names, not automatic substitutes. A later EN 10028 designation does not by itself authorize substitution. Confirm chemistry, heat treatment, tensile properties, impact temperature and product form.
| Country / region | Standard | Grade or designation | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| United Kingdom (historical) | BS 1501-1:1980 | 151 Grade 360B | Same type and tensile grade with the opposite A/B suffix | Not an automatic substitute; suffix B adds characteristic elevated-temperature values |
| United Kingdom (historical) | BS 1501-1:1980 | 161 Grade 360A | Same tensile grade as a fully killed type 161 plate. Type 161 has silicon 0.10–0.35 %, sulfur 0.030 % maximum and a 150 mm thickness limit, whereas type 151 allows semi-killed or fully killed steel, silicon 0.35 % maximum, sulfur 0.045 % maximum and a 100 mm thickness limit. | A different 1980 type, not an automatic substitute |
| Europe | EN 10028-2 | P265GH (1.0425) | Later non-alloy elevated-temperature vessel plate. Live published yield 265 MPa and tensile 410–530 MPa, against 205 N/mm² and 360–480 N/mm² for 151 Grade 360. | Near name only; a later EN designation is not an automatic substitute |
| United States | ASTM A516/A516M | Grade 60 | Carbon vessel plate. Live published yield 220 MPa and tensile 415–550 MPa. | Related product form only |
| China | GB/T 713 | Q245R | Later Chinese carbon vessel plate. Live published yield 245 MPa and tensile 400–520 MPa. | Related carbon class only |
Why choose SHH STEEL for BS 1501-151 Grade 360A
- We produce and export BS 1501-151 Grade 360A pressure-vessel steel plate
- We review the enquiry for edition, designation, delivery condition, dimensions and extra tests
- We keep the 1980 type, tensile grade and A/B suffix distinct from later EN 10028 names and from BS 1501-2 / BS 1501-3
- We match documentation to what the purchase order requires
How to enquire for BS 1501-151 Grade 360A plate
| Item | What to specify |
|---|---|
| Standard and designation | BS 1501-151 Grade 360A and the edition required |
| Or successor standard | EN 10028-2 or EN 10028-3 designation and edition, if that is what the project now requires |
| Delivery condition | Normalized; hot-finished permitted through 40 mm. |
| Dimensions | Required thickness, width and length |
| Chemistry | Ladle analysis to BS 1501-1:1980, or to another named edition |
| Mechanical tests | Yield strength, tensile strength, elongation and, where specified, elevated-temperature or impact tests to the named edition |
| Other tests | Ultrasonic examination or other extra tests only when written on the order |
| Documentation | State the inspection document type required by the project |
Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.
FAQ
-
Is BS 1501 still a current product standard?
- No. BS 1501-1:1980 is the last final edition of Part 1. It was withdrawn on 15 February 1993 and replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Projects still using the 1980 designation should name that edition on the order.
-
Which edition do the tables on this page follow?
- They follow BS 1501-1:1980, including tabulated values from a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 tables. Specify the edition or successor standard required on the purchase order.
-
Does BS 1501-1 cover alloy or stainless pressure-vessel plates?
- No. Part 1 covers carbon and carbon-manganese plates. Alloy plates belong to BS 1501-2:1988. Corrosion- and heat-resisting plates, sheet and strip belong to BS 1501-3:1990. Bars and sections belong to BS 1502, and forgings to BS 1503. This page is 151 Grade 360A only.
-
Can P265GH be used instead of 151 Grade 360A?
- Only after a project review. Live P265GH is stated as 265 MPa yield and 410–530 MPa tensile, against 205 N/mm² and 360–480 N/mm² for 151 Grade 360. Type 151 may be semi-killed or fully killed and is limited to 100 mm in the 1980 clauses. A later EN name is not an automatic substitute.
-
What should a quotation enquiry include?
- BS 1501-151 Grade 360A, the edition required or the successor designation, the delivery condition, plate thickness by width by length, quantity, any extra tests, and the inspection document required.
Request a quotation
Contact SHH STEEL for a quotation for BS 1501-151 Grade 360A steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the edition (BS 1501-1:1980 or a named successor such as EN 10028-2 or EN 10028-3), the A or B suffix, any required impact suffix, the delivery condition and any specimen heat treatment. If your project requires ultrasonic examination, a stated impact temperature or another extra test, include the acceptance criteria and the inspection document required.
If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com