BS 1501 243 Steel Plate
What is BS 1501 243 plate?
We produce and export BS 1501 243 as alloy steel plate (molybdenum family in peer catalogues; 1988 identity not photographed) for pressure purposes. Typical service is alloy pressure equipment that specifies this type.
BS 1501-2:1988 is the last final edition of the alloy-plate part of BS 1501. It was published on 29 July 1988 and superseded on 15 January 1995. It replaced Addendum No. 1 (1973) and Addendum No. 2 (1975) to BS 1501: Part 2: 1970. A photographed 1988 Table 1 was not opened for this page. Clause 3 of the 1988 book is titled Designation, but that clause text was not opened. Clause 19 makes elevated-temperature proof stress an optional requirement for section-two steels. The formal 1988 writing of type, tensile token and any A or B suffix therefore remains unverified. Peer catalogues sometimes write names such as 243 B, 620 B, 621 B or 622-515 B; those B forms are recorded as unverified formal-symbol candidates, not declared absent and not declared commercial-only.
Numeric cells below are taken only from the named public database or peer catalogue opened for this page. They are a reference basis, not a photographed BS 1501-2:1988 table and not an SHH proprietary guarantee. EN 10028-2 values for 16Mo3, 13CrMo4-5 or 10CrMo9-10 are not copied onto this legacy type. Missing chemistry or thickness-banded mechanical fields are project requirements to be agreed against the named edition.
SHH STEEL produces and exports BS 1501 243 plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.
Material specification for BS 1501 243
The items below follow BS 1501-2:1988 as the historical alloy-plate book. Numeric cells in the chemical and mechanical sections are from opened public-database listings and peer catalogues, each labelled by source. They are not photographed 1988 Table 1 values and not 1993 National Annex NC tables (that annex covers 271, 281, 621 and 660 only). Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | BS 1501-2:1988, Steels for pressure purposes — Specification for alloy steels: plates. Numeric cells below are public-database or peer-catalogue references, each labelled by source |
| Designation used here | Working name BS 1501 243 (formal 1988 full symbol unverified) |
| Steel type | Alloy steel plate (molybdenum family in peer catalogues; 1988 identity not photographed) |
| Product form | Alloy steel plate for pressure purposes (this part does not cover bars, sections, forgings, tubes or stainless sheet) |
| How designations are listed | This page uses the working name 243. Formal 1988 full symbols (type number plus any tensile token and any A or B suffix) were not photographed. Peer catalogues that print B forms are recorded as unverified formal-symbol candidates; they are not declared absent and not declared commercial-only |
| Applicable thickness in the opened tensile table | Not verified from an official thickness table |
| Usual heat treatment | Normalized at 900–940 °C, or normalized and tempered. |
| Chemical analysis | Opened public cells only, each labelled by source in the chemical table |
| Tensile properties | Single database tensile window only; thickness bands are a project requirement |
| Our supply | We produce and export 243 plate to the ordered edition, delivery condition, dimensions and extra tests |
Chemical composition of BS 1501 243
Numeric cells below are taken only from the named public database or peer catalogue opened for this page. They are a reference basis, not a photographed BS 1501-2:1988 table and not an SHH proprietary guarantee. EN 10028-2 values for 16Mo3, 13CrMo4-5 or 10CrMo9-10 are not copied onto this legacy type. Missing chemistry or thickness-banded mechanical fields are project requirements to be agreed against the named edition. The same peer mill brochure prints molybdenum as 0.025–0.35 for 243 and as 0.25–0.35 for 16Mo3 in the next block. That 243 molybdenum window is not used as a guaranteed cell. The brochure tensile bands for 243 (440–590 / 430–580 MPa with yields 275 / 270 / 260 / 240) duplicate that brochure’s own 16Mo3 rows and are not copied onto this page.
| Element | Value (wt. %) | Source opened for this cell |
|---|---|---|
| Carbon (C) | 0.12–0.20 | Public database listing opened 8 November 2026 (Asia/Shanghai) |
| Copper (Cu) | 0.25 max | Public database listing opened 8 November 2026 (Asia/Shanghai) |
| Aluminium (metal) (Al) | 0.012 max | Public database listing opened 8 November 2026 (Asia/Shanghai) |
| Silicon (Si) | 0.15–0.35 | Peer mill brochure, 243 chemistry row, opened 8 November 2026 (Asia/Shanghai) |
| Manganese (Mn) | 0.40–0.90 | Peer mill brochure, 243 chemistry row, opened 8 November 2026 (Asia/Shanghai) |
| Phosphorus (P) | 0.025 max | Peer mill brochure opened 8 November 2026 (Asia/Shanghai) |
| Sulfur (S) | 0.015 max | Peer mill brochure opened 8 November 2026 (Asia/Shanghai) |
| Chromium (Cr) | 0.25 max | Peer mill brochure opened 8 November 2026 (Asia/Shanghai) |
| Nickel (Ni) | 0.30 max | Peer mill brochure opened 8 November 2026 (Asia/Shanghai) |
Tensile, impact and elevated-temperature properties for BS 1501 243
Only the opened numeric cells are listed. Thickness-banded room-temperature yield and tensile values are a project requirement unless an edition table is named.
| Item | Value | Source opened for this cell |
|---|---|---|
| Tensile strength Rm | 430–630 MPa | Public database listing opened 8 November 2026 (Asia/Shanghai); single window; temperature bands shown on the page |
| Elongation A | ≥ 19 % | Public database listing opened 8 November 2026 (Asia/Shanghai) |
| Yield / Rp0.2 | ≥ 240 MPa, temperature association not confirmed as a room-temperature first band | Public database listing opened 8 November 2026 (Asia/Shanghai); omitted from any invented thickness table |
A database listing also showed normalizing at 900–940 °C or normalizing and tempering at 900–940 °C then 600–650 °C, and another normalizing mention at 900–960 °C. Hidden public-database fields including manganese, molybdenum, nickel, phosphorus, sulfur, silicon and tin were not filled. Numeric cells below are taken only from the named public database or peer catalogue opened for this page. They are a reference basis, not a photographed BS 1501-2:1988 table and not an SHH proprietary guarantee. EN 10028-2 values for 16Mo3, 13CrMo4-5 or 10CrMo9-10 are not copied onto this legacy type. Missing chemistry or thickness-banded mechanical fields are project requirements to be agreed against the named edition.
Delivery conditions for BS 1501 243
A public database listing shows normalizing at 900–940 °C, or normalizing and tempering at 900–940 °C then 600–650 °C. Name the required delivery condition on the purchase order.
If the project has moved to EN 10028-2, order the successor designation and edition expressly. A later European name is not by itself a substitute instruction for type 243.
The purchase order should name the official designation, the edition required, thickness, width and length, the delivery condition, any extra tests, and the inspection document required.
This page does not offer heat-treatment or fabrication services.
Welding and thermal cutting
Neither the opened historical book notes nor the later remaining-steel annex set a welding procedure for type 243 on this page. Welding and thermal cutting should be qualified for the alloy content, thickness and the specified delivery condition.
If the project treats type 243 as a molybdenum vessel steel, consumables should match the qualified procedure for that alloy. Do not assume 16Mo3 welding practice without a project review.
Heat input and any required post-weld heat treatment belong in the project specification.
Form, appearance, dimensions and thickness tolerances
Thickness, width, length, flatness and mass tolerances should be stated on the purchase order against the dimensional standard named by the project. The historical replacement set includes BS EN 10029 for plate tolerances when that standard is specified.
Appearance, repair welding and any ultrasonic class are taken from the enquiry. This page does not list stock sizes or mill capacity.
Applications and specification limits
We produce and export 243 plate as alloy steel plate for pressure purposes. Typical service is alloy pressure equipment that specifies type 243. A mill comparison table lists a British name 243 B beside 16Mo3; that is a peer near name, not a 1988 symbol verification.
BS 1501-2:1988 is a historical alloy-plate standard. It is not the current EN 10028-2 or EN 10028-4 order unless that successor standard is written on the enquiry, and it is not a BS 1501-1 carbon, BS 1501-3 stainless, BS 1502 bar or BS 1503 forging order.
Compare BS 1501 243 with other steel plates
BS 1501 243 is a historical BS 1501-2 alloy pressure-vessel plate. The comparison below is for selection only; these materials are not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| BS 1501 243 (this plate) | Alloy plate; peer catalogues place it near molybdenum vessel steels | Normalized at 900–940 °C, or normalized and tempered. | Database single tensile window 430–630 MPa and A ≥ 19 %; thickness bands not copied from 16Mo3 | Alloy pressure equipment that specifies this type | A later EN name or a different 1988 type is not an automatic substitute |
| EN 10028-2 16Mo3 | Molybdenum elevated-temperature vessel plate, steel number 1.5415 | As specified in EN 10028-2 | Live published yield 275 MPa at ≤ 16 mm and tensile 440–590 MPa | Modern European molybdenum vessel plate | Near name only; 16Mo3 numbers are not copied onto type 243 |
| EN 10028-2 13CrMo4-5 | Chromium-molybdenum elevated-temperature vessel plate, steel number 1.7335 | As specified in EN 10028-2 | Live published yield 300 MPa at ≤ 16 mm and tensile 450–600 MPa | Modern European 1Cr-0.5Mo vessel plate | Different chromium-molybdenum class |
| EN 10028-2 P355GH | Non-alloy elevated-temperature vessel plate, steel number 1.0473 | As specified in EN 10028-2 | Live published yield 355 MPa at ≤ 16 mm and tensile 510–650 MPa | Modern European carbon vessel plate | Different alloy class |
Equivalent and related grades by country
The designations below are near names, not automatic substitutes. Confirm chemistry, heat treatment, tensile properties, impact temperature and product form.
| Country / region | Standard | Grade or designation | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| United Kingdom | BS 1501-2:1988 working name | 243 (peer catalogues also 243 B) | This page uses the working name 243. A mill comparison table lists 243 B beside 16Mo3. Formal 1988 suffix status is unverified. | This product |
| Europe | EN 10028-2 | 16Mo3 (1.5415) | Later molybdenum vessel plate. Live published yield 275 MPa at ≤ 16 mm and tensile 440–590 MPa, against a database window of 430–630 MPa for type 243. | Near name only; EN numbers are not used as 243 values |
| United States | ASTM A204/A204M | Grade B (peer near name only) | Peer tables sometimes pair 243 with A204 Grade B. That pairing was not opened as a 1988 table. | Related product form only |
| China | — | — | No separately verified GB plate counterpart was established for type 243 on this page. | Do not assume a Chinese molybdenum vessel grade is a substitute |
Why choose SHH STEEL for BS 1501 243
- We produce and export BS 1501 243 alloy pressure-vessel steel plate
- We review the enquiry for edition, designation, delivery condition, dimensions and extra tests
- We keep the historical BS 1501-2 type number distinct from later EN 10028-2 names and from Part 1 A/B carbon grades, and we record peer B forms as unverified formal-symbol candidates until a 1988 table is opened
- We match documentation to what the purchase order requires
How to enquire for BS 1501 243 plate
| Item | What to specify |
|---|---|
| Standard and designation | BS 1501 243 and the edition required (BS 1501-2:1988 and/or the 1993 national-annex remaining-steel clauses) |
| Or successor standard | The EN 10028-2 designation and edition, if that is what the project now requires |
| Delivery condition | Normalized at 900–940 °C, or normalized and tempered. |
| Dimensions | Required thickness, width and length |
| Chemistry | Cast analysis to the named edition |
| Mechanical tests | Yield strength, tensile strength, elongation and, where specified, impact or elevated-temperature proof tests to the named edition |
| Other tests | Ultrasonic examination or other extra tests only when written on the order |
| Documentation | State the inspection document type required by the project |
Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.
FAQ
-
Is BS 1501-2 still a current product standard?
- No. BS 1501-2:1988 is the last final edition of the alloy-plate part. It was published on 29 July 1988 and superseded on 15 January 1995. EN 10028-2 superseded part of it. Projects still using a historical type number should name the edition required on the order.
-
Which numbers on this page are guaranteed 1988 table values?
- None are presented as a photographed 1988 table. Visible public-database cells and selected peer-brochure chemistry are shown with their sources. Brochure tensile bands that duplicate that catalogue’s 16Mo3 rows were not used.
-
Does this page treat 620B or similar B names as the official 1988 symbol?
- No. A photographed 1988 designation table was not opened. Peer catalogues do use B forms such as 620 B, 621 B, 622-515 B and 243 B. Those names are recorded as unverified formal-symbol candidates. They are not declared absent and not declared commercial-only.
-
Can 16Mo3 be used instead of type 243?
- Only after a project review. Live 16Mo3 is published as 275 MPa yield at ≤ 16 mm and 440–590 MPa tensile. A database listing for type 243 shows 430–630 MPa. The later name is not an automatic substitute, and those EN numbers are not copied onto this page.
-
What should a quotation enquiry include?
- BS 1501 243, the edition required or the successor designation, the delivery condition, plate thickness by width by length, quantity, any extra tests, and the inspection document required.
Request a quotation
Contact SHH STEEL for a quotation for BS 1501 243 steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the edition (BS 1501-2:1988 or the later United Kingdom national-annex remaining-steel clauses, or a named EN 10028-2 successor if that is what the project now requires), the delivery condition and any specimen heat treatment. If your project requires ultrasonic examination, a stated impact temperature or another extra test, include the acceptance criteria and the inspection document required.
If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com