BS 1501 225 Grade 490A Steel Plate
What is BS 1501-225 Grade 490A plate?
We produce and export BS 1501-225 Grade 490A as fully killed, niobium- and aluminium-treated carbon-manganese steel plate for fired and unfired pressure equipment. Typical service includes welded boilers, vessels and similar parts that specify type 225 grade 490A.
BS 1501-1:1980 lists eight steel types, each with one or more tensile grades and, where Table 1 allows, suffix A or B and optional impact suffixes. This page specifies only 225 Grade 490A. It is not type 223 or 224, and it is not a BS 1501-2 alloy or BS 1501-3 stainless plate. Suffix A specifies room-temperature tensile properties only. LT20, LT30, LT50 and the L nickel limit are ordering options, not separate grades.
Composition and room-temperature tensile properties on this page follow BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates, the last final edition of Part 1. BS 1501-1:1980 was published on 28 November 1980 and withdrawn on 15 February 1993. It replaced BS 1501: Part 1: 1964 and that edition’s addenda. It was replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Those successor designations are not automatic aliases for the 1980 type-and-grade names. Name the edition or successor standard required on the purchase order.
The chemical and tensile figures below follow BS 1501-1:1980 as tabulated for this designation, including a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 values. BS 1501-2 (alloy plates) and BS 1501-3 (corrosion- and heat-resisting plates, sheet and strip) are different parts of the same historical series.
SHH STEEL produces and exports BS 1501-225 Grade 490A plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry.
Material specification for BS 1501-225 Grade 490A
The items below follow BS 1501-1:1980. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | BS 1501-1:1980, Steels for pressure purposes — Specification for carbon and carbon manganese steels: plates |
| Official designation | BS 1501-225 Grade 490A |
| Steel type | Fully killed niobium- and aluminium-treated carbon-manganese steel |
| Product form | Hot-rolled steel plate (this part does not cover bars, sections, forgings, tubes or stainless sheet) |
| How designations are listed | Type number, tensile grade and suffix A or B; optional LT or RT impact suffixes where Table 1 allows; optional L after types 223, 224 and 225 when nickel is limited to 0.30 % |
| Applicable thickness | Up to and including 150 mm |
| Usual heat treatment | Normalized, unless an alternative condition is agreed. |
| Chemical analysis | Ladle analysis as tabulated for this type and grade in BS 1501-1:1980 |
| Tensile properties | Yield strength, tensile strength and elongation, by thickness, from that edition |
| Our supply | We produce and export 225 Grade 490A plate to the ordered edition, delivery condition, dimensions and extra tests |
Chemical composition of BS 1501-225 Grade 490A
The figures below are ladle analysis for BS 1501-225 Grade 490A from BS 1501-1:1980. Values are in weight percent and follow BS 1501-1:1980, including a reprint incorporating Amendments No. 1 to No. 3. They are not current EN 10028 values.
| Element | 225 Grade 490A ladle analysis, BS 1501-1:1980 (wt. %) |
|---|---|
| Carbon (C) | 0.20 max |
| Silicon (Si) | 0.10–0.50 |
| Manganese (Mn) | 0.90–1.60 |
| Phosphorus (P) | 0.030 max |
| Sulfur (S) | 0.030 max |
| Aluminium (Al), metallic | 0.015 min |
| Niobium (Nb) | 0.010–0.060 |
| Chromium (Cr) | 0.25 max |
| Copper (Cu) | 0.30 max |
| Molybdenum (Mo) | 0.10 max |
| Nickel (Ni) | 0.75 max |
Figures are ladle analysis as tabulated for type 225 grade 490 in BS 1501-1:1980. Determination of total aluminium is deemed to meet the metallic aluminium requirement if the value obtained is not less than 0.018 %. The general residual nickel limit follows the same rule as types 223 and 224 (0.75 % maximum), with a combined total of chromium, copper and molybdenum of 0.50 % maximum. The optional L suffix after the type number limits nickel to 0.30 % and then limits chromium + copper + molybdenum + nickel to 0.70 %. L is an ordering option, not a separate product page. Project acceptance of the chemical analysis should be agreed against the named edition.
Tensile and related properties for BS 1501-225 Grade 490A
225 Grade 490A has thickness-dependent yield strength, tensile strength and elongation. Values below are from BS 1501-1:1980, including a reprint incorporating Amendments No. 1 to No. 3, and are not current EN 10028 values. Strength values are in N/mm², equivalent to MPa.
| Thickness | Tensile strength Rm, N/mm² | Yield strength Re, N/mm² min | Elongation A, % min |
|---|---|---|---|
| Over 3 mm up to and including 16 mm | 490–610 | 355 | 21 |
| Over 16 mm up to and including 40 mm | 490–610 | 345 | 21 |
| Over 40 mm up to and including 63 mm | 490–610 | 340 | 20 |
| Over 63 mm up to and including 100 mm | 490–610 | Reduced by the 1 % per 5 mm rule | 20 |
| Over 100 mm up to and including 150 mm | 490–610 | Reduced by the 1 % per 5 mm rule | 20 |
The tensile window is that stated for type 225 grade 490 in BS 1501-1:1980 (490–610 N/mm²). Type 225 covers plates up to and including 150 mm. For plates over 63 mm up to and including 150 mm, yield strength is the 40 mm to 63 mm value reduced by 1 % for each 5 mm or part thereof increase in thickness. Table 1 lists optional impact suffixes LT20, LT30 and LT50 for this grade; those are ordering options, not separate product pages. If impact tests are specified, the acceptance values shall be taken from the named edition. Project acceptance of the tensile figures should be agreed against the named edition.
Delivery conditions for BS 1501-225 Grade 490A
Type 225 is supplied as fully killed, niobium- and aluminium-treated carbon-manganese steel plate. The 1980 text specifies supply in the normalized condition, unless an alternative condition of supply is agreed. Controlled rolling may be agreed under the general supply clause that applies to types 223 and 225. Name the required delivery condition on the purchase order.
If the project has moved to EN 10028-2 or EN 10028-3, order the successor designation and edition expressly. A later name is not by itself a substitute instruction.
The purchase order should name the official designation including the A or B suffix, any required impact suffix, thickness, width and length, the delivery condition, any extra tests, and the inspection document required.
This page does not offer heat-treatment or fabrication services.
Welding and thermal cutting
BS 1501-1:1980 does not set a welding procedure. Type 225 is a fully killed, niobium- and aluminium-treated carbon-manganese vessel plate intended for welded pressure equipment. Welding and thermal cutting should be qualified for the carbon content, thickness and delivery condition.
Heat input and any required post-weld heat treatment belong in the project specification.
Form, appearance, dimensions and thickness tolerances
Thickness, width, length, flatness and mass tolerances should be stated on the purchase order against the dimensional standard named by the project. The historical replacement set includes BS EN 10029 for plate tolerances when that standard is specified.
Appearance, repair welding and any ultrasonic class are taken from the enquiry. This page does not list stock sizes or mill capacity.
Applications and specification limits
We produce and export 225 Grade 490A plate as fully killed, niobium- and aluminium-treated carbon-manganese steel plate for fired and unfired pressure equipment. Typical service includes welded boilers, vessels and similar parts that specify type 225 grade 490A. The 1980 type 225 clauses cover this niobium- and aluminium-treated carbon-manganese plate. This page specifies grade 490 only.
BS 1501-1:1980 is a historical carbon and carbon-manganese plate standard for pressure purposes. It is not the current EN 10028-2 or EN 10028-3 order unless that successor standard is written on the enquiry, and it is not a BS 1501-2 alloy, BS 1501-3 stainless, BS 1502 bar or BS 1503 forging order.
Compare BS 1501-225 Grade 490A with other steel plates
225 Grade 490A is a BS 1501-1:1980 pressure-vessel plate. The comparison below is for selection only; these materials are not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| BS 1501-225 Grade 490A (this plate) | BS 1501-1:1980 official designation | Normalized, unless an alternative condition is agreed. | Yield 355 N/mm² minimum up to 16 mm; tensile 490–610 N/mm² | Typical service includes welded boilers and vessels that specify type 225 grade 490A | A different standard, later EN name, or 1980 type is not an automatic substitute |
| EN 10028-3 P355NH | Weldable fine-grain elevated-temperature vessel plate, steel number 1.0565 | As specified in EN 10028-3 | Published yield 355 MPa and tensile 490–630 MPa | Modern European fine-grain boiler and vessel plate | Related strength class only; chemistry and impact rules follow EN 10028-3 |
| EN 10028-3 P355NL1 | Weldable fine-grain low-temperature vessel plate, steel number 1.0566 | As specified in EN 10028-3 | Published yield 355 MPa and tensile 490–630 MPa | Modern European fine-grain vessel plate with a specified −40 °C impact option | Related strength class only; LT suffixes of type 225 are not automatic P355NL1 aliases |
| GB/T 713 Q345R | Later Chinese carbon-manganese vessel plate | As specified in GB/T 713 | Published yield 345 MPa and tensile 510–640 MPa | Modern Chinese boiler and vessel plate | Related strength class only |
Equivalent and related grades by country
The designations below are near names, not automatic substitutes. A later EN 10028 designation does not by itself authorize substitution. Confirm chemistry, heat treatment, tensile properties, impact temperature and product form.
| Country / region | Standard | Grade or designation | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| United Kingdom (historical) | BS 1501-1:1980 | 225 Grade 490B | Same type and tensile grade with the opposite A/B suffix | Not an automatic substitute; suffix B adds characteristic elevated-temperature values |
| Europe | EN 10028-3 | P355NH (1.0565) | Later weldable fine-grain elevated-temperature vessel plate. Live published yield 355 MPa and tensile 490–630 MPa, against 355 N/mm² and 490–610 N/mm² for 225 Grade 490. | Near name only; LT suffixes of type 225 are not automatic P355NL1 or P355NH aliases |
| Europe | EN 10028-3 | P355NL1 (1.0566) | Later weldable fine-grain low-temperature vessel plate. Live published yield 355 MPa and tensile 490–630 MPa. | Related strength class only |
| Europe | EN 10028-2 | P355GH (1.0473) | Later non-alloy elevated-temperature vessel plate. Live published yield 355 MPa and tensile 510–650 MPa. | Related strength class only |
| China | GB/T 713 | Q345R | Later Chinese carbon-manganese vessel plate. Live published yield 345 MPa and tensile 510–640 MPa. | Related strength class only |
Why choose SHH STEEL for BS 1501-225 Grade 490A
- We produce and export BS 1501-225 Grade 490A pressure-vessel steel plate
- We review the enquiry for edition, designation, delivery condition, dimensions and extra tests
- We keep the 1980 type, tensile grade and A/B suffix distinct from later EN 10028 names and from BS 1501-2 / BS 1501-3
- We match documentation to what the purchase order requires
How to enquire for BS 1501-225 Grade 490A plate
| Item | What to specify |
|---|---|
| Standard and designation | BS 1501-225 Grade 490A and the edition required |
| Or successor standard | EN 10028-2 or EN 10028-3 designation and edition, if that is what the project now requires |
| Delivery condition | Normalized, unless an alternative condition is agreed. |
| Dimensions | Required thickness, width and length |
| Chemistry | Ladle analysis to BS 1501-1:1980, or to another named edition |
| Mechanical tests | Yield strength, tensile strength, elongation and, where specified, elevated-temperature or impact tests to the named edition |
| Other tests | Ultrasonic examination or other extra tests only when written on the order |
| Documentation | State the inspection document type required by the project |
Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.
FAQ
-
Is BS 1501 still a current product standard?
- No. BS 1501-1:1980 is the last final edition of Part 1. It was withdrawn on 15 February 1993 and replaced in the British collection by BS EN 10028-1, BS EN 10028-2, BS EN 10028-3 and BS EN 10029. Projects still using the 1980 designation should name that edition on the order.
-
Which edition do the tables on this page follow?
- They follow BS 1501-1:1980, including tabulated values from a reprint that incorporates Amendments No. 1 to No. 3. They are not current EN 10028 tables. Specify the edition or successor standard required on the purchase order.
-
Does BS 1501-1 cover alloy or stainless pressure-vessel plates?
- No. Part 1 covers carbon and carbon-manganese plates. Alloy plates belong to BS 1501-2:1988. Corrosion- and heat-resisting plates, sheet and strip belong to BS 1501-3:1990. Bars and sections belong to BS 1502, and forgings to BS 1503. This page is 225 Grade 490A only.
-
Can P355NH be used instead of 225 Grade 490A?
- Only after a project review. Live P355NH is stated as 355 MPa yield and 490–630 MPa tensile, against 355 N/mm² and 490–610 N/mm² for 225 Grade 490. Type 225 is niobium- and aluminium-treated and may be ordered with LT20, LT30 or LT50 impact options or with the L nickel limit. A later EN name is not an automatic substitute.
-
What should a quotation enquiry include?
- BS 1501-225 Grade 490A, the edition required or the successor designation, the delivery condition, plate thickness by width by length, quantity, any extra tests, and the inspection document required.
Request a quotation
Contact SHH STEEL for a quotation for BS 1501-225 Grade 490A steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the edition (BS 1501-1:1980 or a named successor such as EN 10028-2 or EN 10028-3), the A or B suffix, any required impact suffix, the delivery condition and any specimen heat treatment. If your project requires ultrasonic examination, a stated impact temperature or another extra test, include the acceptance criteria and the inspection document required.
If you are considering a related designation, send the applicable standard and project specification with your enquiry so we can review chemistry, heat treatment and toughness.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.