ASTM A829 4142 Alloy Steel Plate
What is ASTM A829 Grade 4142 plate?
ASTM A829 4142 Alloy Steel Plate is structural-quality chromium-molybdenum alloy steel plate purchased to ASTM A829/A829M-25, Standard Specification for Alloy Structural Steel Plates. Grade 4142 is the chromium-molybdenum designation used for this A829 plate grade, and 4142 is the conventional AISI/SAE chemistry-family number. AISI/SAE 4142 is not itself a plate specification.
The plates are usually specified to chemical composition. Tensile properties may also be specified; when they are, the values must be compatible with the chemical composition, the delivery condition and the plate thickness.
This is an engineering alloy structural plate with a higher carbon window than Grade 4140. We supply it as-rolled for later heat treatment or in an agreed heat-treated condition. Typical quenched-and-tempered 4140 or 4142 bar strengths should not be read as automatic as-delivered plate minima.
SHH STEEL produces and exports ASTM A829/A829M-25 Grade 4142 plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry. This grade belongs to our Alloy Steel Plates range under ASTM A829/A829M.
Material specification for ASTM A829 Grade 4142
The items below follow ASTM A829/A829M-25. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | ASTM A829/A829M-25, Standard Specification for Alloy Structural Steel Plates |
| Grade designation | Grade 4142, chromium-molybdenum alloy plate under ASTM A829/A829M, higher carbon than Grade 4140 |
| Product form | Alloy structural steel plate |
| Usual ordering basis | Chemical composition; tensile properties may also be specified when compatible with composition, condition and thickness |
| Delivery conditions | Condition AR, as rolled (hot rolled); Condition A, annealed; Condition N, normalized; Condition NT, normalized and tempered; Condition QT, quenched and tempered |
| Forms | Form I rectangular; Form II circular and semi-circular; Form III sketch, including rings |
| Edge categories | Edge 1 mill edge; Edge 2 universal mill edge; Edge 3 sheared edge; Edge 4 gas-cut edge; Edge 5 special cut edge |
| Finishes | Finish 1 as-rolled (hot-rolled); Finish 2 blast cleaned; Finish 3 blast cleaned and oiled; Finish 4 pickled; Finish 5 pickled and oiled; Finish 6 painted, one prime coat; Finish 7 painted, one prime coat and one finish coat. Plates are usually specified to Finish 1 |
| Supplementary requirements | Additional requirements may be specified on the order |
| Heat-analysis elements named by ASTM | Carbon, manganese, phosphorus, sulfur, silicon, nickel, chromium, molybdenum, vanadium and copper |
| Units | SI units and inch-pound units are separate; do not combine the two systems |
| Our supply | We produce and export Grade 4142 to the ASTM form, edge, finish and delivery condition agreed on the order |
Chemical composition of ASTM A829 Grade 4142
ASTM A829/A829M-25 requires heat analysis to the composition specified for the ordered grade. The figures below are manufacturer ladle-analysis values published for ASTM A829 Grade 4142 plate. They are reference data, not a substitute for the official ASTM composition table. Contractual chemistry and delivery condition are those of the ordered ASTM A829/A829M edition and the mill test certificate.
| Element | Reference ladle analysis (wt. %) |
|---|---|
| Carbon (C) | 0.38-0.46 |
| Manganese (Mn) | 0.75-1.00 |
| Silicon (Si) | 0.15-0.35 |
| Chromium (Cr) | 0.80-1.10 |
| Molybdenum (Mo) | 0.15-0.25 |
Phosphorus and sulfur shall meet the ordered edition; some manufacturers apply tighter ladle maxima. Confirm both on the mill test certificate. If the project requires product analysis, agree it on the order and check the result on the certificate.
One manufacturer table notes that vanadium may be added depending on dimensions; no fixed vanadium range is listed here. Copper is named among the ASTM heat-analysis elements, but a numeric copper limit for Grade 4142 is not listed in that table.
Mechanical properties and optional tests
ASTM A829/A829M-25 plates are usually specified to chemical composition. Tensile properties may also be specified when they are compatible with the composition, delivery condition and plate thickness. Mechanical tests are not assumed for every as-rolled order; if you need tensile, hardness or toughness results, state the values, delivery condition and thickness so we can confirm they are compatible.
Typical quenched-and-tempered 4142 or 4140 bar yield or tensile figures should not be treated as automatic as-delivered plate minima. Manufacturer hardness figures published for one mill’s 4142 delivery conditions are not repeated here as ASTM or SHH minima.
Delivery conditions for ASTM A829 Grade 4142
ASTM A829/A829M-25 lists five delivery conditions:
- Condition AR — as rolled (hot rolled)
- Condition A — annealed
- Condition N — normalized
- Condition NT — normalized and tempered
- Condition QT — quenched and tempered
We produce and export Grade 4142 to the agreed condition. Not every production route offers every condition on every thickness, so the purchase order should name the required state. An enquiry that only says “4142 plate” is incomplete, because as-rolled, annealed, normalized and quenched-and-tempered plate are not interchangeable supply states.
As-rolled plate may be used for parts that will be heat treated later. Some production routes emphasize annealed, normalized-and-tempered or quenched-and-tempered supply; name the required condition on the order.
Welding and thermal cutting
When the steel is to be welded, ASTM A829/A829M-25 presupposes a welding procedure suitable for the grade and the intended use or service, and refers to Appendix X3 of ASTM A6/A6M for weldability information.
Chromium-molybdenum 4142 plate is commonly welded with low-hydrogen consumables and controlled hydrogen practice. Electrodes and fluxes should be dry and properly stored. Slow cooling after welding and a post-weld heat treatment may be required to limit cold cracking. Preheat and interpass temperature depend on thickness, joint restraint and the qualified procedure.
Thermal cutting can harden the adjacent material. That heat-affected zone should be considered, and removed where later forming or welding requires it. Qualify cutting and welding procedures to the project specification, the ordered delivery condition and the actual plate thickness.
Form, edge, finish and dimensions
ASTM A829/A829M-25 defines form, edge and finish options. Numeric thickness, width, length and flatness tolerances should be stated on the purchase order and confirmed on the mill documents for the ordered edition. If the project requires ASTM A6 or another dimensional standard, write that requirement on the enquiry.
Applications and specification limits
We produce and export this grade for heavy-machinery and general engineering work, including components cut from plate and then heat treated to a stated cycle. Buyers specify 4142 rather than 4140 when the project calls for the higher carbon window in the same chromium-molybdenum plate family.
As-rolled, annealed and quenched-and-tempered plate do not machine, form or finish at the same strength. Wear resistance, through-hardness and toughness should be treated as order-specific, not assumed from the grade name alone.
ASTM A829 is an alloy structural plate specification. It is not a tool-steel book such as ASTM A681, and it is not a boiler or pressure-vessel plate specification. Do not use this grade as an automatic substitute for those product standards or for Grade 4140 without checking carbon and tests.
Compare ASTM A829 4142 with other steel plates
ASTM A829 Grade 4142 is chemistry-ordered alloy structural plate. The comparison below uses other plates we already publish. These grades are related by engineering use, not equivalents.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| ASTM A829 Grade 4142 (this plate) | Chromium-molybdenum alloy structural plate, usually ordered by heat chemistry, with a higher carbon window than Grade 4140 | AR, annealed, normalized, NT or QT as ordered | No automatic as-delivered strength package; tensile or hardness only if specified and compatible with composition, condition and thickness | Heavy-machinery and general engineering parts, often heat treated after cutting | Not interchangeable with Grade 4140 without checking carbon and tests, and not a 2.25Cr-1Mo vessel plate |
| ASTM A829 4140 Alloy Steel Plate | Chromium-molybdenum alloy structural plate with a lower carbon window than 4142 | AR, annealed, normalized, NT or QT as ordered | No automatic as-delivered strength package; tensile or hardness only if specified and compatible | Machinery and general engineering parts, often heat treated after cutting | Closest A829 sibling, not an automatic substitute for Grade 4142 |
| ASTM A514 Grade B | Quenched-and-tempered alloy structural plate; chemistry includes chromium, molybdenum, vanadium, titanium and boron | Quenched and tempered | Strength-graded: to 32 mm, yield 100 ksi / 690 MPa min and tensile 110-130 ksi / 760-895 MPa (from our A514 Grade B page). Maximum thickness for Grade B is 1¼ in / 32 mm | Welded bridges and other structures that specify A514 QT plate | Not a substitute for chemistry-ordered A829 plate |
| ASTM A387 Grade 22 Class 2 | Chromium-molybdenum pressure-vessel plate, nominal 2.25Cr-1.00Mo — a different alloy level from 4142 | Usually normalized and tempered, or accelerated cooling plus temper | Strength-graded Class 2: tensile 75-100 ksi / 515-690 MPa and yield 45 ksi / 310 MPa min (from our A387 Grade 22 Class 2 page) | Welded boilers and elevated-temperature vessels | Similar only in being a Cr-Mo plate family; not an engineering-plate equivalent to A829 4142 |
Related published ranges: Structural Steel Plates, ASTM A514/A514M and ASTM A387.
Equivalent and related grades by country
The designations below are near equivalents or related chemistry-family grades, not certified or automatic equivalents. Chemistry windows, product form, delivery condition and any mechanical tests must match the project specification before a substitution is considered. Grades without a live page on this site are shown as plain text.
| Country / region | Standard | Grade | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| United States | ASTM A829/A829M-25 | Grade 4142 | This plate specification. Chromium-molybdenum alloy structural plate, usually ordered by heat chemistry, with a higher carbon window than Grade 4140 (manufacturer-published 4142 C 0.38-0.46 versus 4140 C 0.36-0.44). | This product |
| United States | AISI / SAE practice | 4142 | The conventional chemistry-family number used with this plate grade. AISI/SAE 4142 is not an independent plate specification. | Do not treat an AISI/SAE 4142 bar or forging enquiry as an ASTM A829 plate order without restating product form, condition and tests. |
| China | GB/T 11251 | 42CrMo (family comparison only) | 42CrMo is the published Chinese plate/strip near-equivalent documented for Grade 4140, not a dedicated 4142-only grade. Published 42CrMo heat analysis: C 0.38-0.45, Si 0.17-0.37, Mn 0.50-0.80, Cr 0.90-1.20, Mo 0.15-0.25. The carbon window overlaps 4142, but manganese and silicon ranges differ from manufacturer-published A829 4142 values (Mn 0.75-1.00, Si 0.15-0.35). | Not a certified 4142 equivalent. Confirm edition, product form and tests. No dedicated product page is published on this site yet. |
| Europe | EN ISO 683-2 (ISO 683-2) | 42CrMo4 (1.7225) (family comparison only) | 42CrMo4 is the European QT alloy grade documented as a 4140-family near equivalent, not a dedicated 4142-only plate grade. Manufacturer heat analysis published to DIN EN ISO 683-2: C 0.38-0.45, Si 0.10-0.40, Mn 0.60-0.90, Cr 0.90-1.20, Mo 0.15-0.30. Carbon overlaps 4142, but manganese, chromium and molybdenum windows are not identical to manufacturer-published A829 4142 values. | Not a certified 4142 equivalent. Different book and ordering model from ASTM A829 plate. |
| Japan | JIS G 4053 | SCM440 (family comparison only) | SCM440 is the machine-structural grade documented as a 4140-family comparison, not a dedicated 4142 plate grade. Published SCM440 heat analysis: C 0.38-0.43, Si 0.15-0.35, Mn 0.60-0.90, Cr 0.90-1.20, Mo 0.15-0.30. Carbon is narrower than manufacturer-published A829 4142 (0.38-0.46). JIS G 4053 is not a plate specification and does not itself specify tensile or hardness minima. | Not an automatic plate equivalent. |
| United Kingdom and other countries | — | — | No separately verified national plate counterpart dedicated to 4142 was established for this page. | Do not assume a local bar designation is an ASTM A829 4142 plate equivalent. |
A related live A829 plate grade is ASTM A829 4140. Other A829 family grades such as 4130 and 8620 are not substitutes and do not have product pages on this site yet.
Why choose SHH STEEL for ASTM A829 Grade 4142
- We produce and export ASTM A829/A829M-25 Grade 4142 alloy structural steel plate
- We review the enquiry for edition, grade, delivery condition, dimensions and any extra mechanical or NDE tests
- We keep chemistry-ordered plate distinct from optional tensile or hardness testing
- We match documentation to what the purchase order requires
How to enquire for ASTM A829 4142 plate
| Item | What to specify |
|---|---|
| Standard and grade | ASTM A829/A829M-25 Grade 4142 |
| Delivery condition | AR, annealed (A), normalized (N), normalized and tempered (NT), or quenched and tempered (QT) |
| Dimensions | Required thickness, width and length; we confirm production and export feasibility against the enquiry |
| Form, edge and finish | Use the ASTM options above if needed. Finish 1 is the usual finish |
| Chemistry | Heat analysis to the ordered edition; request product analysis only if the project needs it |
| Mechanical tests | State any tensile, hardness or toughness values and confirm they are compatible with composition, condition and thickness |
| Other tests | Ultrasonic examination or other NDE only when written on the order |
| Documentation | State the inspection document type required by the project |
| Processing | Cutting or other processing only when requested; thermal-cutting practice depends on condition and thickness |
FAQ
-
Is ASTM A829 4142 ordered by chemistry or by mechanical properties?
- Usually by chemical composition. Tensile properties may also be specified when they are compatible with the composition, delivery condition and plate thickness. If you need mechanical tests, write them on the enquiry.
-
How does Grade 4142 differ from Grade 4140?
- Manufacturer-published ladle analysis for A829 4142 uses a higher carbon window (0.38-0.46) than A829 4140 (0.36-0.44). Published manganese, silicon, chromium and molybdenum ranges match those 4140 values. The two grades are related, not automatic substitutes.
-
Does as-rolled ASTM A829 4142 plate meet typical quenched-and-tempered bar strengths?
- No. Those bar figures describe a heat-treated condition that as-rolled plate does not automatically carry. If a strength or hardness package is needed, state the values and the delivery condition on the purchase order.
-
Are 42CrMo, 42CrMo4 or SCM440 the same as ASTM A829 4142 plate?
- Those designations are 4140-family near equivalents that overlap the 4142 carbon range in part. They are not dedicated or automatic 4142 substitutes. JIS G 4053 SCM440 is not a plate specification.
-
What should a quotation enquiry include?
- The ordered ASTM edition, Grade 4142, delivery condition, thickness by width by length, quantity, any extra chemical or mechanical tests, any NDE, and the inspection document required by the project.
Request a quotation
Contact SHH STEEL for a quotation for ASTM A829/A829M-25 Grade 4142 alloy steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify the delivery condition: as-rolled, annealed, normalized, normalized and tempered, or quenched and tempered. If your project requires tensile, hardness, toughness or ultrasonic testing, include the acceptance criteria and the inspection document required. Any mechanical requirements must be compatible with the chemistry, delivery condition and plate thickness.
If you are considering Grade 4140, 42CrMo, 42CrMo4 or SCM440 as an alternative, send the applicable standard and project specification with your enquiry. We will review the differences in carbon window, product form and supply condition rather than assume that related grades are interchangeable.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com