ASTM A302 Grade C Steel Plate | A302 Gr.C Mn-Mo-Ni Vessel Plate
What is ASTM A302 Grade C Steel?
As a professional China mill-Direct Supply and pressure-vessel plate exporter, SHH STEEL supplies ASTM A302 Grade C Steel Plate produced to ASTM A302/A302M.
On drawings, MTCs and RFQs this grade is written many ways: ASTM A302 Grade C, A302 Gr.C, A302 Gr C, A302GRC, A302 GR C, A-302 Grade C, A-302 Gr.C, ASME SA302 Grade C, SA302 Gr.C, SA302GRC, Mn-Mo-Ni vessel plate, manganese molybdenum nickel boiler plate and A/SA302 Grade C. All of these names refer to the same manganese-molybdenum-nickel alloy plate. ASTM A302/A302M is the ASTM product specification; ASME SA-302/SA-302M is the Boiler and Pressure Vessel Code companion.
A302 Gr.C sits in the nickel half of ASTM A302. Grades A and B are Mn-Mo with no specified nickel. Grades C and D add nickel at the Grade B strength table. Minimum yield of Grade C is 345 MPa (50 ksi). Tensile strength is 550–690 MPa (80–100 ksi). Nickel heat analysis is 0.40–0.70%. Molybdenum heat analysis is 0.45–0.60%.
The plate is intended for welded boilers and other pressure vessels when the designer wants Grade B strength plus nickel for toughness. For ASME Code work it is dual-certified to ASME SA-302 Grade C and used under ASME Section VIII. It is not a 3.5Ni low-temperature grade such as A203 Gr.D/E, and it is not a Cr-Mo elevated-temperature grade such as ASME SA387. Compared with carbon vessel steels such as ASTM A516 and ASME SA516, Grade C adds both molybdenum and nickel.
General requirements follow ASTM A20 / ASME SA-20. Steel is killed and produced to fine-grain practice. Plates 50 mm and under are normally supplied as-rolled unless normalizing or stress relieving is ordered. Plates over 50 mm shall be normalized.
SHH STEEL supplies A302 Gr.C as true China mill-Direct Supply. Dual marking ASTM A302 Grade C / ASME SA302 Grade C is available. Certificates can be EN 10204 3.1 or EN 10204 3.2.
If the project compares other coded vessel plates, SHH STEEL places A302 Gr.C next to ASTM A537, ASME SA537, ASME SA515 and ASTM A285.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | ASTM A302 Grade C / A302 Gr.C / A302GRC | Confirmed |
| Product Specification | ASTM A302/A302M | Applied |
| Companion Spec | ASME SA302 Grade C / SA302 Gr.C | Dual cert available |
| General Requirements | ASTM A20 / ASME SA-20 | Applied |
| Code Context | ASME Section VIII when dual certified | As specified |
| Product Form | Pressure vessel / boiler plate | Available |
| Alloy Type | Manganese-molybdenum-nickel | Confirmed |
| Delivery Condition | As-rolled ≤50 mm; normalized >50 mm | As specified |
| Typical Thickness | 6 mm – 150 mm | Heavier by enquiry |
| Width / Length | Up to about 4600 mm wide / 12000 mm long | Mill capability |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This product belongs to the Pressure Vessel Steel Plates family. It is a Mn-Mo-Ni coded vessel plate under ASTM A302, not a structural Carbon Steel Plates grade.
Chemical Composition
A302 Grade C chemistry under ASTM A302/A302M is reported as heat analysis (ladle analysis) and, when specified, product analysis.
Heat Analysis (Ladle Analysis) — Grade C
| Element | Thickness / Basis | Heat Analysis (%) |
|---|---|---|
| Carbon (C), max | ≤ 25 mm (1 in.) | 0.20 |
| Carbon (C), max | > 25 mm to 50 mm (1–2 in.) | 0.23 |
| Carbon (C), max | > 50 mm (2 in.) | 0.25 |
| Manganese (Mn) | All | 1.15 – 1.50 |
| Phosphorus (P), max | All | 0.025 |
| Sulfur (S), max | All | 0.025 |
| Silicon (Si) | All | 0.15 – 0.40 |
| Molybdenum (Mo) | All | 0.45 – 0.60 |
| Nickel (Ni) | All | 0.40 – 0.70 |
Product Analysis — Grade C
| Element | Thickness / Basis | Product Analysis (%) |
|---|---|---|
| Manganese (Mn) | All | 1.07 – 1.62 |
| Silicon (Si) | All | 0.13 – 0.45 |
| Molybdenum (Mo) | All | 0.41 – 0.64 |
| Nickel (Ni) | All | 0.37 – 0.73 |
| C, P, S | Product check per A20/A302 | Per order |
Grade C uses the same manganese and molybdenum bands as Grade B. The difference is nickel: heat 0.40–0.70%, product 0.37–0.73%. Grade D uses a higher nickel band (heat 0.70–1.00%). Tighter residuals or carbon equivalent limits are supplementary requirements.
SHH STEEL reports ladle analysis on every certificate. Product analysis is added when ASTM A20 product analysis or the vessel specification requires it.
Mechanical Properties
Tensile Requirements — ASTM A302 Grade C per ASTM A302/A302M
| Property | Requirement |
|---|---|
| Tensile strength | 550 – 690 MPa (80 – 100 ksi) |
| Yield strength, min (0.2%) | 345 MPa (50 ksi) |
| Elongation in 200 mm (8 in.), min | 17% |
| Elongation in 50 mm (2 in.), min | 20% |
Strength of Grade C matches Grade B and Grade D. Elongation minima are higher than Grade B (17%/20% versus 15%/18%) because of the nickel addition in ASTM A302. Density is 7.85 g/cm³. Hardness after the agreed heat treatment is typically in the 160–200 HB range unless a special window is ordered.
Specimens are prepared under ASTM A20. If simulated PWHT is specified, coupons are heat-treated to the vessel cycle before testing.
Material Comparison
| Grade | Alloy type | Ni (heat) | Yield min | Tensile | Typical use |
|---|---|---|---|---|---|
| A302 Gr.A | Mn-Mo | Not specified | 310 MPa | 515–655 MPa | Lower-strength Mn-Mo |
| A302 Gr.B | Mn-Mo | Not specified | 345 MPa | 550–690 MPa | Same strength as C, no Ni |
| A302 Gr.C | Mn-Mo-Ni | 0.40–0.70% | 345 MPa | 550–690 MPa | Grade B strength + nickel |
| A302 Gr.D | Mn-Mo-Ni | 0.70–1.00% | 345 MPa | 550–690 MPa | Same strength, higher Ni |
Order A302 Gr.C / A302GRC when the ASTM drawing needs 345 MPa yield and 0.40–0.70% nickel. If nickel is not required, Grade B is the lower-alloy option at the same strength. If higher nickel is written on the drawing, use Grade D. Carbon QT options include ASTM A537 and ASME SA537. HSLA Steel Plates are not a coded substitute for ASTM A302.
Elevated-Temperature and Vessel Service
A302 Grade C is specified for welded boilers and pressure vessels when Grade B strength plus nickel toughness is required. Molybdenum and nickel in ASTM A302/A302M support alloy vessel and boiler service. When dual certified to ASME SA-302 Grade C, allowable stress at temperature is taken from the applicable ASME Section II Part D table, not from a commercial datasheet.
Impact temperature, orientation and energy minimums are agreed on the order. They are not automatic on Grade C, but nickel is often the reason Charpy testing is added. When the vessel specification sets Charpy values, SHH STEEL produces A302 Gr.C Mn-Mo-Ni vessel plate with those sets and lists the results on the 3.1 or 3.2 certificate. Grade C is not a 3.5Ni cryogenic plate.
Weldability
A302 Grade C under ASTM A302 is a welded boiler and pressure-vessel plate. Mn-Mo-Ni steel is welded with low-hydrogen procedures. For Code work, procedures are qualified to ASME Section IX.
Consumables are selected to match molybdenum, nickel and the required joint toughness. Preheat depends on thickness, hydrogen control and restraint. When ASME Section VIII requires PWHT, the shop cycle is commonly in the 595–650°C range for this alloy family. If properties after that cycle are needed, simulated PWHT of mill coupons should be ordered before shipment.
SHH STEEL recommends a qualified WPS/PQR for each thickness break and can support procedure review through steel welding services. Do not assume an A302 Grade B procedure is automatically valid for Grade C if nickel matching or impact requirements change.
Heat Treatment
Heat treatment of A302 Grade C follows ASTM A302/A302M:
- Plates 50 mm (2 in.) and under are normally supplied in the as-rolled condition. They may be ordered normalized, stress relieved, or both.
- Plates over 50 mm (2 in.) shall be normalized.
Normalizing is heating into the austenite range followed by air cooling. Stress relieving, when ordered, is a separate lower-temperature hold to reduce residual stress. Quench-and-temper practice used for A533 / A537 Class 2 must not be applied to Grade C unless the order is changed to a QT specification.
If the specification fixes a normalizing temperature band or holding time per thickness under ASTM A20, SHH STEEL writes those parameters into the mill instruction and reports them on the certificate.
Delivery Condition
SHH STEEL delivers ASTM A302 Grade C / A302 Gr.C as follows:
- ≤ 50 mm: as-rolled as standard, or normalized / stress relieved when ordered
-
50 mm: normalized as required by ASTM A302
The certificate lists A302 Gr.C and, when dual certified, SA302 Gr.C; heat number; heat analysis; product analysis when ordered; tensile results; heat-treatment condition; agreed Charpy values; and supplementary tests. Plates are industrial vessel plate: heat-treated as required, then pickled or shot-blasted as agreed.
Decorative finishes such as 2B, BA or No.4 are not used. Surface condition is vessel-plate quality for welding, NDE and coating. Heat number and grade marking support mill and Code traceability.
Certificates may be EN 10204 3.1 or EN 10204 3.2. Third-party stamps (BV, LR, DNV, TUV, SGS or the purchaser’s agency) are arranged when written on the order.
Dimensions
Typical supply range from SHH STEEL for A302 Gr.C Mn-Mo-Ni vessel plate:
- Thickness: 6 mm – 150 mm (heavier by mill enquiry)
- Width: up to about 4600 mm
- Length: up to about 12000 mm
Because heat treatment changes at 50 mm in ASTM A302, the purchase order should state the ordered thickness and the required condition. Cut-to-length shells, heads and nest sizes are available.
Tolerances
Dimensional tolerances follow ASTM A20 / ASME SA-20 for pressure-vessel plates.
Thickness, width, length, flatness and camber are vessel-plate tolerances, not strip tolerances. Restricted thickness or extra-flatness can be accepted when the vessel drawing requires it. Ultrasonic testing to A435 or A578 is added when specified. Cutting to finished sizes is available through steel cutting services.
Supplementary Requirements
Vessel specifications for nickel-bearing plate often add tests beyond the base A302 Grade C table. SHH STEEL treats the following as supplementary requirements.
Simulated PWHT. Coupons from the same heat and thickness receive the vessel PWHT cycle. Tensile and Charpy tests are run on those coupons.
Nondestructive examination. UT to A435, A577 or A578 with purchaser acceptance levels. Edge MT/PT after cutting if required.
Impact testing. Test temperature, specimen size, orientation and minimum average/single values as written on the RFQ.
Special hardness. HBW or HV window after the agreed heat treatment or after simulated PWHT.
Restricted chemistry. Tighter C, P, S, residuals or carbon equivalent on heat and product analysis per ASTM A302 / A20.
HIC testing. NACE TM0284 with purchaser solution and CLR/CTR/CSR limits. Not automatic on A302 Gr.C.
NACE / sour-service notes. Review against NACE MR0175 / ISO 15156 or MR0103 only when the datasheet cites the clause.
Z-direction testing. ASTM A770 or purchaser Z15/Z25/Z35 for thick nozzles and restrained joints.
Third-party witnessing. Witness of heat treatment, mechanical tests, UT and documents. Output can be EN 10204 3.2.
Supplementary tests go through steel testing service and appear line by line on the certificate. Items not on the purchase order are not assumed.
Equivalent Material Grades
| Designation | Standard / Region | Notes |
|---|---|---|
| ASTM A302 Grade C / A302 Gr.C / A302GRC | ASTM A302/A302M | Product name on this page |
| ASME SA302 Grade C / SA302 Gr.C / SA302GRC | ASME SA-302/SA-302M | Code companion |
| Mn-Mo-Ni vessel plate | Commercial | Alloy-content search name |
| GB/T 713 related Ni-Mo vessel | GB | Project-specific comparison |
| EN 10028 related Mn-Mo-Ni vessel | EN | Project-specific comparison |
| JIS related Mo-Ni boiler plate | JIS | Project-specific dual cert |
For ASME stamping, the purchase order should say dual A302 / SA302 Grade C. Nearby carbon vessel grades include ASTM A516, ASME SA516, ASME SA515 and ASTM A285.
Applications
ASTM A302 Grade C / A302 Gr.C is selected for boilers and vessels that need Mn-Mo-Ni strength at 345 MPa yield. Typical applications of ASTM A302 Grade C Steel Plate include:
| Industry / Sector | Typical Components (with keywords) |
|---|---|
| Boilers & Steam Drums | A302 Gr.C boiler plate and A302GRC Mn-Mo-Ni vessel plate |
| Pressure Vessels | ASTM A302 Grade C shells, heads and welded pressure parts |
| Oil, Gas & Petrochemical | A-302 Grade C reactors, separators and process vessels |
| Energy & Power | A302 Grade C heat-exchange shells and power-plant vessels |
| Dual-Certified Export Jobs | A302 / SA302 Gr.C plate to ASTM A302 and ASME SA-302 |
| Heavy Vessel Fabrication | A302 Gr C plate cut to nest sizes |
SHH STEEL supplies A302 Gr.C with full heat traceability. Related industry pages include petrochemical industry and energy industry. Supporting services include steel cutting services, steel welding services, steel testing service and worldwide shipping service.
Why Choose SHH STEEL
SHH STEEL is a China mill-Direct Supply for plates to ASTM A302/A302M. For A302 Grade C we offer:
- China mill-Direct Supply pricing on A302 Gr.C / SA302 Gr.C
- Dual ASTM A302 / ASME SA302 marking
- Heat analysis and product analysis per ASTM A20 / A302, including nickel
- EN 10204 3.1 standard; EN 10204 3.2 or nominated third-party inspection on request
- As-rolled or normalized delivery per thickness rule
- Supplementary PWHT simulation, UT, HIC, NACE review and Z-direction testing
- Cutting to shell and head nest sizes
- Technical support to separate Grade C from A/B/D and from A516 / SA387 / A537
- Export packing through worldwide shipping service
For company scope and other vessel grades, visit China steel Mill Agent-SHH STEEL.
FAQ
-
What other names are used for ASTM A302 Grade C?
- Buyers also write A302 Gr.C, A302GRC, A-302 Grade C, ASME SA302 Grade C, SA302GRC and Mn-Mo-Ni vessel plate. They all mean the manganese-molybdenum-nickel Grade C plate in ASTM A302/A302M. SHH STEEL prints the exact name required on the purchase order.
-
Is A302 Grade C the same as SA302 Grade C?
- They are companion specifications. ASTM A302 is the product spec; ASME SA-302 is the Code version used with ASME Section VIII. Chemistry and tensile limits match. SHH STEEL dual-certifies when the vessel must be Code-stamped.
-
What is the nickel content of A302 Gr.C?
- Heat analysis is 0.40–0.70% Ni and product analysis is 0.37–0.73% Ni under ASTM A302. That is the lower nickel band. Grade D uses 0.70–1.00% Ni on heat analysis.
-
What is the difference between A302 Grade B and Grade C?
- Strength is the same (345 MPa yield, 550–690 MPa tensile). Grade B has no specified nickel. Grade C adds 0.40–0.70% Ni and has higher elongation minima. Choose Grade C when the drawing requires nickel.
-
What is the difference between A302 Grade C and Grade D?
- Same strength table in ASTM A302/A302M. Grade C nickel is 0.40–0.70%; Grade D nickel is 0.70–1.00%. Order the nickel band written on the drawing.
-
Must A302 Grade C be normalized?
- Plates over 50 mm shall be normalized per ASTM A302. Plates 50 mm and under are normally as-rolled unless the purchaser orders normalizing or stress relieving.
-
Can welding be qualified to ASME Section IX?
- Yes, when the plate is used on an ASME vessel. A302 Gr.C is a welded boiler and vessel plate. Procedures should be qualified to ASME Section IX with low-hydrogen consumables matched to the Mn-Mo-Ni chemistry. The fabricator owns the qualified WPS.
-
Can SHH STEEL issue EN 10204 3.2?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 or another third-party witness is arranged when it is written on the order.
-
What is the density of A302 Gr.C
- 7.85 g/cm³. SHH STEEL uses this value for shipping-weight estimates on ASTM A302 plate.
Conclusion
ASTM A302 Grade C Steel Plate is the manganese-molybdenum-nickel, 345 MPa yield vessel grade in ASTM A302/A302M. Whether the inquiry says A302 Gr.C, A302GRC, A-302 Grade C or Mn-Mo-Ni vessel plate, SHH STEEL supplies plate with heat and product analysis, thickness-correct heat treatment, optional supplementary tests, and EN 10204 3.1 or 3.2 certification.
As a professional China mill-Direct Supply, SHH STEEL provides ASTM A302 Grade C / A302 Gr.C Mn-Mo-Ni Vessel Plate with full traceability for boiler and ASME Section VIII fabrication.
Contact SHH STEEL today for stock, nickel analysis, dual A302/SA302 marking, 3.2 inspection or a quotation.
ASTM A302 Grade C Steel Plate, A302 Gr.C, A302GRC, A-302 Grade C, ASTM A302, ASME SA302 Grade C, Mn-Mo-Ni vessel plate, A302 Grade C supplier, China mill-Direct Supply