ASTM A529 Grade 50 Round, Square and Flat Steel Bars
What are ASTM A529 Grade 50 Round, Square and Flat Steel Bars?
ASTM A529/A529M covers high-strength carbon-manganese steel shapes, plates and bars in Grades 50 and 55. This page is Grade 50 bars only — rounds, squares and flats. Grade 50 angles and channels remain on ASTM A529 Grade 50 Equal and Unequal Steel Angles and ASTM A529 Grade 50 C and MC Steel Channels. Those pages are not this product.
The chemistry and mechanical figures follow the same Table 1 and Table 2 recitation already used on the live Grade 50 angle and channel pages. Public listings describe A529/A529M-26 as the current ASTM edition; the official 2026 tables were not purchased for this page. The edition named on the purchase order governs delivery.
Material, Scope and Thickness Notes for ASTM A529 Grade 50 Bars
The specification covers shapes, plates and bars. Grade 50 shapes are limited to flange or leg thickness of 1-1/2 in. [40 mm] inclusive. That shape-thickness cap is stated clearly so it is not silently applied, or silently ignored, for bars. Any bar-thickness or bar-diameter limit in the named edition must be confirmed on the order; this page does not invent one.
Grade 55 is a different grade and is not this product. A36 bars (ASTM A36 Round, Square and Flat Steel Bars) have a different chemistry and a different tensile range; an A36 certificate is not an A529 Grade 50 certificate.
ASTM A529 Grade 50 Chemical Composition for Bars (Heat Analysis)
The table recites the Grade 50 and 55 heat-analysis limits used on the live Grade 50 angle page. Product-analysis variations, where permitted, follow ASTM A6/A6M and are not rewritten as tighter shop limits here.
Swipe horizontally to view all dimensions.
ASTM A529 Grade 50 Bar Mechanical Properties: Yield, Tensile and Elongation
Minimum yield strength for Grade 50 is 50 ksi [345 MPa]. Table 2 lists Grade 50 tensile strength as 70–100 ksi [485–690 MPa]. Footnote B reduces the minimum tensile strength to 65 ksi [450 MPa] for Grade 50 shapes with flange or leg thickness to 1-1/2 in. [40 mm] inclusive. This bar page uses the 70–100 ksi Grade 50 row and does not apply that shape footnote to bars. Minimum elongation is 18 % in 8 in. [200 mm] and 21 % in 2 in. [50 mm].
Swipe horizontally to view all dimensions.
ASTM A529 Grade 50 Round, Square and Flat Bar Sizes (Common Typographical Sizes, Theoretical Mass)
A529/A529M does not itself tabulate a closed list of bar diameters and flat widths. The tables below are the same common typographical merchant-bar rounds, squares and flats used on ASTM A36 Round, Square and Flat Steel Bars, with theoretical mass calculated from the cross-section at 490 lb/ft³ (7.85 g/cm³): rounds 2.670 D² lb/ft and squares or flats 3.403 A lb/ft, with a kilogram-per-metre conversion of 1.48816. They are labeled as common sizes, not as every bar size permitted by A6/A6M, and they are not a mill stock list. Do not use a W-shape or S-shape mass table as a bar table. Grade 50 shapes are limited to flange or leg thickness of 1-1/2 in. [40 mm] inclusive; confirm any bar-thickness cap in the named edition of A529/A529M on the order.
Common round bars
Swipe horizontally to view all dimensions.
Common square bars
Swipe horizontally to view all dimensions.
Common flat bars
Swipe horizontally to view all dimensions.
Applications and Service Limits for ASTM A529 Grade 50 Bars
Grade 50 bars are used in general structural and fabrication work where A529/A529M Grade 50 is specified. Weldability should be assessed against the named edition and the purchaser’s welding procedure; this page does not convert the specification into a welding-procedure qualification. Copper steel, when required, must be stated on the order because the copper minimum applies only when it is specified.
ASTM A529 Grade 50 Bars Compared with A529 Shapes and A36 Bars
The live Grade 50 angle and channel pages (ASTM A529 Grade 50 Equal and Unequal Steel Angles, ASTM A529 Grade 50 C and MC Steel Channels) use the 65–100 ksi tensile window that footnote B allows for Grade 50 shapes. This bar page uses the 70–100 ksi Table 2 row. Do not copy one tensile window onto the other product without reading that footnote.
ASTM A36 Round, Square and Flat Steel Bars remains a different specification. Yield and tensile ranges are not the same, and the certificates are not interchangeable.
Near-Equivalents for ASTM A529 Grade 50 Bars: Not Automatic Substitutes
Near-equivalents only, not automatic substitutes. ASTM A36 bars, ASTM A572 Grade 50 bars (when specified), and other carbon or high-strength low-alloy bar specifications have their own chemistry and mechanical tables. Do not treat an A529 Grade 50 shape certificate as automatic evidence for these bars, or the reverse, without checking the tensile footnote and the product form.
Sourcing ASTM A529 Grade 50 Steel Bars from SHH STEEL
SHH STEEL reviews the named A529/A529M edition, the Grade 50 certificate and the ordered bar size before quoting. The typographical merchant-bar tables on this page are not a warehouse list. State the form (round, square or flat), the diameter or thickness and width, and the length on the enquiry.
FAQ: ASTM A529 Grade 50 Steel Bars
-
Why is the tensile range 70–100 ksi here, but 65–100 ksi on the Grade 50 angle page?
- Table 2 lists 70–100 ksi for Grade 50. Footnote B lowers the minimum to 65 ksi for Grade 50 shapes with flange or leg thickness to 1-1/2 in. inclusive. This bar page does not apply that shape footnote.
-
Which edition is used?
- The chemistry and mechanical recitation is the same one used on the live Grade 50 angle and channel pages. Public listings describe A529/A529M-26 as current; official 2026 tables were not purchased for this page. The edition named on the order governs delivery.
-
Is there a 1-1/2 in. thickness cap for these bars?
- The 1-1/2 in. [40 mm] cap is stated in the specification for Grade 50 shapes. Any bar-thickness cap in the named edition must be confirmed on the order; this page does not invent one.
Conclusion
Specify ASTM A529/A529M Grade 50 bars with the Grade 50 chemistry, 50 ksi yield, and the 70–100 ksi tensile row, without importing the shape-only tensile footnote. Confirm the named edition and the ordered bar size before purchase.