ASTM A36 Round, Square and Flat Steel Bars

ASTM A36/A36M-19 carbon structural steel bars have 36 ksi [250 MPa] minimum yield and 58–80 ksi [400–550 MPa] tensile strength. Chemistry follows the bar columns of Table 3, which are not the same as the shape columns. The size tables are common round, square and flat sizes with theoretical masses at 490 lb/ft³, not a complete ASTM size list.
Keywords
ASTM A36 bars, A36 round bar, A36 square bar, A36 flat bar, carbon steel bars
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Size Chart
Applications
Equivalent Grades
Sourcing
FAQ
Conclusion

What are ASTM A36 Round, Square and Flat Steel Bars?

ASTM A36/A36M-19 is a carbon structural steel specification that covers bars as well as plates and shapes. This page is the bar product: rounds, squares and flats ordered as A36, not W-shapes, S-shapes or plates. The tensile requirements that apply to bars are the “Plates, Shapes, and Bars” strength pair in Table 2 and the “Plates and Bars” elongation lines, not the wide-flange footnotes.

Bars under this specification shall be killed steel and shall be delivered to the current edition of Specification A6/A6M for the product ordered, except where A36/A36M itself governs. The keyword list of A36/A36M explicitly includes bars.

Material, Manufacture and Scope for ASTM A36 Steel Bars

Use the bar columns of Table 3 for chemistry, not the “Shapes” column and not the wide-plate columns. Product analysis tolerances, when required, follow A6/A6M. Tension tests represent the material as required by Section 8; however, 8.2 states that bars other than flats less than 1/2 in. [12.5 mm] in thickness or diameter need not be tension-tested by the manufacturer if the chemical composition used is appropriate for obtaining the tensile properties in Table 2.

The 32 ksi [220 MPa] yield footnote in Table 2 applies to plates over 8 in. [200 mm] thick. It is not the default bar yield. Ordinary A36 bars are specified at 36 ksi [250 MPa] minimum yield and 58–80 ksi [400–550 MPa] tensile strength.

ASTM A36 Steel Bar Chemical Composition (Heat Analysis)

Table 3 of A36/A36M-19, “Bars; Plates ≤ 15 in. [380 mm] Width,” is the chemistry that applies to bars. Phosphorus is 0.04 % maximum and sulfur is 0.05 % maximum in every bar thickness band. Silicon is 0.40 % maximum. Copper, when copper steel is specified, is 0.20 % minimum. Manganese is not specified up to 3/4 in. [20 mm] inclusive; from over 3/4 in. through over 4 in. it is 0.60–0.90 %. Carbon rises with thickness as shown below. Footnote B permits a manganese increase of 0.06 % above the specified maximum for each 0.01 % carbon below the specified carbon maximum, up to 1.35 % manganese.

Swipe horizontally to view all dimensions.

Element To 3/4 in. [20 mm] incl. Over 3/4 to 1-1/2 in. [20 to 40 mm] Over 1-1/2 to 4 in. [40 to 100 mm] Over 4 in. [100 mm]
Carbon, max, % 0.26 0.27 0.28 0.29
Manganese, % — 0.60–0.90 0.60–0.90 0.60–0.90
Phosphorus, max, % 0.04 0.04 0.04 0.04
Sulfur, max, % 0.05 0.05 0.05 0.05
Silicon, max, % 0.40 0.40 0.40 0.40
Copper, min, % (when specified) 0.20 0.20 0.20 0.20

ASTM A36 Steel Bar Mechanical Properties

Table 2 requires a tensile strength of 58–80 ksi [400–550 MPa] and a minimum yield point of 36 ksi [250 MPa] for bars. For plates and bars, the minimum elongation is 20 % in 8 in. [200 mm] and 23 % in 2 in. [50 mm]. Those elongation lines are not the shape lines (the shape 2 in. elongation is 21 %, with a further wide-flange exception). Orientation and any elongation adjustments follow Specification A6/A6M as invoked by A36/A36M.

Swipe horizontally to view all dimensions.

Property Bars (Table 2)
Tensile strength 58–80 ksi [400–550 MPa]
Yield point, min 36 ksi [250 MPa]
Elongation in 8 in. [200 mm], min 20 %
Elongation in 2 in. [50 mm], min 23 %

ASTM A36 Round, Square and Flat Bar Sizes (Common Sizes, Theoretical Mass)

A36/A36M does not itself tabulate a closed list of bar diameters and flat widths. The tables below are common merchant-bar rounds, squares and flats, with theoretical mass calculated from the cross-section at 490 lb/ft³ (7.85 g/cm³): rounds 2.670 D² lb/ft and squares or flats 3.403 A lb/ft, with a kilogram-per-metre conversion of 1.48816. They are labeled as common sizes, not as every bar size permitted by A6/A6M, and they are not a mill stock list. Do not use a W-shape or S-shape mass table as a bar table.

Common round bars

Swipe horizontally to view all dimensions.

Diameter, in (mm) Area, in² (cm²) Theoretical mass, lb/ft (kg/m)
1/4 (6.35) 0.049 (0.32) 0.167 (0.248)
5/16 (7.94) 0.077 (0.49) 0.261 (0.388)
3/8 (9.52) 0.110 (0.71) 0.375 (0.559)
7/16 (11.11) 0.150 (0.97) 0.511 (0.761)
1/2 (12.70) 0.196 (1.27) 0.667 (0.993)
9/16 (14.29) 0.249 (1.60) 0.845 (1.257)
5/8 (15.88) 0.307 (1.98) 1.043 (1.552)
3/4 (19.05) 0.442 (2.85) 1.502 (2.235)
7/8 (22.22) 0.601 (3.88) 2.044 (3.042)
1 (25.40) 0.785 (5.07) 2.67 (3.973)
1-1/8 (28.57) 0.994 (6.41) 3.379 (5.029)
1-1/4 (31.75) 1.227 (7.92) 4.172 (6.208)
1-3/8 (34.92) 1.485 (9.58) 5.048 (7.512)
1-1/2 (38.10) 1.767 (11.40) 6.008 (8.94)
1-5/8 (41.27) 2.074 (13.38) 7.05 (10.49)
1-3/4 (44.45) 2.405 (15.52) 8.177 (12.17)
2 (50.80) 3.142 (20.27) 10.68 (15.89)
2-1/4 (57.15) 3.976 (25.65) 13.52 (20.12)
2-1/2 (63.50) 4.909 (31.67) 16.69 (24.83)
2-3/4 (69.85) 5.940 (38.32) 20.19 (30.05)
3 (76.20) 7.069 (45.60) 24.03 (35.76)
3-1/4 (82.55) 8.296 (53.52) 28.2 (41.97)
3-1/2 (88.90) 9.621 (62.07) 32.71 (48.67)
3-3/4 (95.25) 11.045 (71.26) 37.55 (55.88)
4 (101.60) 12.566 (81.07) 42.72 (63.57)
4-1/2 (114.30) 15.904 (102.61) 54.07 (80.46)
5 (127.00) 19.635 (126.68) 66.75 (99.33)
5-1/2 (139.70) 23.758 (153.28) 80.77 (120.2)
6 (152.40) 28.274 (182.41) 96.12 (143.04)

Common square bars

Swipe horizontally to view all dimensions.

Side, in (mm) Area, in² (cm²) Theoretical mass, lb/ft (kg/m)
1/4 (6.35) 0.062 (0.40) 0.213 (0.317)
3/8 (9.52) 0.141 (0.91) 0.479 (0.712)
1/2 (12.70) 0.250 (1.61) 0.851 (1.266)
5/8 (15.88) 0.391 (2.52) 1.329 (1.978)
3/4 (19.05) 0.562 (3.63) 1.914 (2.849)
1 (25.40) 1.000 (6.45) 3.403 (5.064)
1-1/4 (31.75) 1.562 (10.08) 5.317 (7.913)
1-1/2 (38.10) 2.250 (14.52) 7.657 (11.39)
2 (50.80) 4.000 (25.81) 13.61 (20.26)
2-1/2 (63.50) 6.250 (40.32) 21.27 (31.65)
3 (76.20) 9.000 (58.06) 30.63 (45.58)
4 (101.60) 16.000 (103.23) 54.45 (81.03)

Common flat bars

Swipe horizontally to view all dimensions.

Thickness × width, in Thickness × width, mm Area, in² (cm²) Theoretical mass, lb/ft (kg/m)
1/4 × 1 6.35 × 25.40 0.250 (1.61) 0.851 (1.266)
1/4 × 1-1/2 6.35 × 38.10 0.375 (2.42) 1.276 (1.899)
1/4 × 2 6.35 × 50.80 0.500 (3.23) 1.702 (2.532)
1/4 × 3 6.35 × 76.20 0.750 (4.84) 2.552 (3.798)
1/4 × 4 6.35 × 101.60 1.000 (6.45) 3.403 (5.064)
1/4 × 6 6.35 × 152.40 1.500 (9.68) 5.104 (7.596)
3/8 × 1 9.52 × 25.40 0.375 (2.42) 1.276 (1.899)
3/8 × 2 9.52 × 50.80 0.750 (4.84) 2.552 (3.798)
3/8 × 3 9.52 × 76.20 1.125 (7.26) 3.828 (5.697)
3/8 × 4 9.52 × 101.60 1.500 (9.68) 5.104 (7.596)
3/8 × 6 9.52 × 152.40 2.250 (14.52) 7.657 (11.39)
1/2 × 1 12.70 × 25.40 0.500 (3.23) 1.702 (2.532)
1/2 × 2 12.70 × 50.80 1.000 (6.45) 3.403 (5.064)
1/2 × 3 12.70 × 76.20 1.500 (9.68) 5.104 (7.596)
1/2 × 4 12.70 × 101.60 2.000 (12.90) 6.806 (10.13)
1/2 × 6 12.70 × 152.40 3.000 (19.35) 10.21 (15.19)
1/2 × 8 12.70 × 203.20 4.000 (25.81) 13.61 (20.26)
3/4 × 2 19.05 × 50.80 1.500 (9.68) 5.104 (7.596)
3/4 × 3 19.05 × 76.20 2.250 (14.52) 7.657 (11.39)
3/4 × 4 19.05 × 101.60 3.000 (19.35) 10.21 (15.19)
3/4 × 6 19.05 × 152.40 4.500 (29.03) 15.31 (22.79)
3/4 × 8 19.05 × 203.20 6.000 (38.71) 20.42 (30.39)
1 × 2 25.40 × 50.80 2.000 (12.90) 6.806 (10.13)
1 × 3 25.40 × 76.20 3.000 (19.35) 10.21 (15.19)
1 × 4 25.40 × 101.60 4.000 (25.81) 13.61 (20.26)
1 × 6 25.40 × 152.40 6.000 (38.71) 20.42 (30.39)
1 × 8 25.40 × 203.20 8.000 (51.61) 27.22 (40.51)

Applications and Service Limits for ASTM A36 Steel Bars

A36 bars are used for general structural and fabrication work: base plates of small section, fixtures, frames, pins, and miscellaneous welded or bolted details where the design names A36. They are not automatically a pin-quality, cold-finished, or machine-steel grade; those products are ordered to their own specifications (for example ASTM A108). Weldability is implied by the chemical limits and the killed-steel requirement, but procedure qualification still belongs to the fabricator and the code.

Near-Equivalents for ASTM A36 Steel Bars: Not Automatic Substitutes

JIS G 3101 SS400 and EN 10025-2 S235JR are often compared with A36 because their yield bands sit in a similar neighbourhood. The comparisons are a starting point for a substitution study, not a licence to restamp the bar. Chemistry columns, elongation gauge lengths, thickness bands and delivery standards all differ. SS400 bars, in particular, use Table 4 of G 3101, not the plate and section table, and carbon is not specified for SS400.

ASME SA-36 bars would follow the same Code-edition rule already used for SA-36 shapes: only with a cited BPVC Section II, Part A year and the identical-with statement from that book. An A36 bar certificate is not, by itself, an SA-36 certificate. A36 shapes and A36 plates are the same grade family but not this product form.

Sourcing ASTM A36 Steel Bars from SHH STEEL

SHH STEEL reviews enquiries for ASTM A36 bars against the A36/A36M edition, the product form (round, square or flat), the diameter or thickness and width, the length, and the certificate. The size tables are common-size theoretical masses, not a catalogue of guaranteed mill items. If a cold-finished finish, a special straightness, or an SA-36 designation is required, that requirement should be written on the enquiry.

ASTM A36 Steel Bar FAQs

Do A36 bars use the same chemistry as A36 W-shapes?
Not necessarily. Table 3 has a separate “Bars; Plates ≤ 15 in. Width” set of columns. Carbon, manganese and the phosphorus and sulfur maxima are not copied from the Shapes column. Use the bar columns for bars.
Are the size tables the official ASTM list?
No. They are common merchant-bar sizes with theoretical masses calculated at 490 lb/ft³. A36/A36M does not publish a closed bar-size table, and this page does not claim to list every A6 size.
Is the yield strength 32 ksi for thick bars?
Table 2’s 32 ksi footnote applies to plates over 8 in. thick. Bars are specified at 36 ksi [250 MPa] minimum yield and 58–80 ksi tensile strength.
Can SS400 be substituted for A36 bars?
Not automatically. SS400 bar mechanicals are in JIS G 3101 Table 4, and the chemistry rules differ. Any substitution has to be accepted by the purchaser.

Conclusion

ASTM A36/A36M-19 bars are killed carbon structural steel in round, square and flat form, specified at 36 ksi [250 MPa] minimum yield and 58–80 ksi [400–550 MPa] tensile strength, with chemistry taken from the bar columns of Table 3. The size tables are common sizes with theoretical masses, not a complete ASTM list and not a stock list. Name the form, the size and the edition on the order, and do not reuse a shape data sheet as a bar certificate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X