ASTM A240 UNS S17400 (Type 630) stainless steel sheet at SHH STEEL warehouse

ASTM A240 UNS S17400 Stainless Steel Sheet

ASTM A240 UNS S17400 stainless steel sheet: UNS S17400 (Type 630) is a precipitation-hardening grade ordered to ASTM A693 (not A240), supplied as sheet and strip. SHH STEEL advises on grade, finish and tolerance and supplies mill-direct sheet with third-party inspection, small-lot consolidation and in-house cutting.
Keywords
ASTM A240 UNS S17400 sheet, A240 S17400 stainless sheet, UNS S17400 cold rolled sheet, Type 630 stainless steel sheet, S17400 2B sheet, S17400 coil supplier
Equivalent Grades:
EN 1.4542 X5CrNiCuNb16-4; JIS SUS630; GB/T 05Cr17Ni4Cu4Nb (S51740) (nearest; check limits)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Surface Finishes
Tolerances
Coil and Cut Sheet
Heat Treatment
Properties in Service
Equivalent Grades
Related Sheet Grades
Applications and Fabrication
Testing and Inspection
Buyer Concerns
How to Order
FAQ
Conclusion

What is ASTM A240 UNS S17400 stainless steel sheet?

UNS S17400 (Type 630) is a precipitation-hardening Cr-Ni-Cu-Nb stainless steel. It is not listed in ASTM A240; sheet, strip and plate in this grade are covered by ASTM A693. This page keeps the A240-style title because buyers search for it, but all data below are quoted from A693 / SA-693. Sheet and strip in this grade are delivered solution treated (Condition A). They are cut, formed or machined and then aged at a single temperature to reach the required strength. Ageing at 482–621 °C causes little distortion, which suits precision flat parts. Under ASTM A480, “sheet” means flat material under 5.00 mm thick and at least 600 mm wide, and narrower cold-rolled material is strip. That makes UNS S17400 (Type 630) sheet a cold-rolled or thin hot-rolled product with its own finish, gauge-tolerance and flatness rules, quite different from plate. S17400 sheet is rolled in mill campaigns, so size, finish and lead time are confirmed against the campaign schedule.

This guide covers S17400 sheet from the buyer’s side of the order: the A693 and A480 requirements, heat and product analysis, properties, cold-rolled finishes, gauge and flatness tolerances, coil and cut-length supply, equivalent EN, JIS and GB/T grades, and the certificates to expect. SHH STEEL supplies S17400 sheet and coil mill-direct and can slit, cut and protect it to your drawings.

SHH STEEL quotes every value here from the standard named beside it; where a standard leaves a point to agreement, this page says so.

UNS S17400 (Type 630) sheet: specification summary

UNS S17400 is not in ASTM A240. Precipitation-hardening sheet, strip and plate are covered by ASTM A693, which uses ASTM A480 for general requirements. Buyers looking for “A240 S17400 sheet” should order A693 Type 630, and the certificate must name A693.

Property A240 sheet data for UNS S17400
Standard ASTM A693/A693M (precipitation-hardening plate, sheet and strip); not listed in ASTM A240
General requirements ASTM A480/A480M: ordering, finishes, tolerances, product analysis, testing, marking
ASME counterpart SA-693 for ASME Code use
UNS number UNS S17400
Type name Type 630
Structure precipitation-hardening martensitic
Sheet (A480 3.2.3) under 5.00 mm thick and 600 mm and over wide
Strip (A480 3.2.4) cold-rolled, under 5.00 mm thick and under 600 mm wide
Typical gauges Cold-rolled sheet and strip by enquiry, typically about 0.5–3.0 mm; supplied solution treated
Typical widths 1000, 1219, 1250 and 1500 mm; other widths by slitting
Supply forms coil, slit coil, cut-to-length sheet, blanks cut to size
Condition Solution treated at 1050 ± 25 °C, cooled as required (SA-693 Table 3); precipitation hardening at 482 to 621 °C as ordered
Cold-rolled finishes solution treated, descaled; finish as ordered
Dimensional tolerances A480 Annex A2 (inch-pound) or Annex A3 (A480M), e.g. Table A3.5 thickness and A3.8 flatness for cold-rolled wide sheet
Required tests heat analysis; solution-treated hardness (A693 Table 4); aged properties when an aged condition is ordered (Table 5)
Optional tests PMI, Charpy (S1 where applicable), as agreed
Marking specification, type or UNS, heat/identification number and producer; coils marked near the outside end plus inside tag; sheet under 6.4 mm is not die-stamped
Certificates mill test report per A480 Section 8; EN 10204 3.1 as standard; 3.2 with third-party witness on request

Related A693 products are listed in the ASTM A693/A693M range. Under A480 1.2, the product specification governs where the two conflict.

UNS S17400 sheet chemistry: heat analysis vs product analysis

Heat analysis limits for UNS S17400 (Type 630), in percent by mass (maximum unless a range or minimum is shown), from A693 / SA-693 Table 1:

Grade C Mn P S Si Cr Ni Cu Other
UNS S17400 0.07 1.00 0.040 0.030 1.00 15.00–17.50 3.00–5.00 3.00–5.00 Nb+Ta 0.15–0.45

Two different analyses can appear in a sheet purchase. The heat analysis is the steelmaker’s analysis of the melt, taken during pouring or from in-process product. It is the analysis printed on the mill certificate, and it must sit inside Table 1 (A480 6.2). The product analysis is a check the buyer may make on finished sheet or coil to confirm identity (A480 7.1). Because a thin cold-rolled product can show small local variation, A480 Table A1.1 allows product analysis to fall slightly outside Table 1. The comparison below applies those tolerances to S17400:

Element Heat analysis, % (A693 / SA-693 Table 1) A480 Table A1.1 tolerance Product analysis limit, %
Carbon (C) 0.07 max 0.01 over max ≤ 0.08
Manganese (Mn) 1.00 max 0.03 over max ≤ 1.03
Phosphorus (P) 0.040 max 0.005 over max ≤ 0.045
Sulfur (S) 0.030 max 0.005 over max ≤ 0.035
Silicon (Si) 1.00 max 0.05 over max ≤ 1.05
Chromium (Cr) 15.00–17.50 0.20 under min / 0.20 over max 14.80–17.70
Nickel (Ni) 3.00–5.00 0.07 under min / 0.07 over max 2.93–5.07
Copper (Cu) 3.00–5.00 0.15 under min / 0.15 over max 2.85–5.15
Nb+Ta 0.15–0.45 combined limit: Table A1.1 gives tolerances for individual elements only; agree treatment with the supplier (Nb alone: 0.05) by agreement

The tolerance band is picked by the specified limit, or by the top of a range, and applies below a minimum and above a maximum. Results for one element across several samples of a heat must not straddle the range, falling both above and below it (A480 7.2). For ratio requirements such as Ti ≥ 5×(C+N), product analysis must reach at least 0.90× the ratio (A480 A1.1). Limits on unspecified Cu, Mo, Ti and Nb (0.75, 0.75, 0.10 and 0.10 %) stop sheet of one grade being certified when it actually matches another (A480 6.3.1).

A practical note for receiving inspection: handheld XRF identifies the alloy family but cannot measure carbon or nitrogen. So it cannot tell 304 from 304L, or a standard grade from an H or N grade. Use spark-OES or a laboratory analysis when those elements decide acceptance.

Role of the main elements in S17400 sheet:

  • Carbon ≤ 0.07 %: a standard carbon level. Keep holding time in the sensitising range short when corrosion resistance after welding matters.
  • Chromium 15.00–17.50 %: forms the passive film that makes the steel stainless; higher chromium improves resistance to corrosion and oxidation.
  • Nickel 3.00–5.00 %: balances the microstructure and improves toughness.
  • Copper 3.00–5.00 %: provides the copper-rich precipitates that harden the steel during ageing.
  • Niobium: contributes to the precipitation-hardening response and ties up carbon.

Mechanical properties of S17400 sheet

Solution-treated UNS S17400 (Type 630) sheet is limited to 363 HBW / C38 maximum (A693 Table 4). After ageing, A693 / SA-693 Table 5 gives the following minimums for material under 4.76 mm thick, which covers most sheet and strip:

Condition Ageing Tensile, min Yield 0.2 %, min Elongation, min (under 4.76 mm) Rockwell min / max
H900 482 °C, 1 h 1310 MPa 1170 MPa 5 % C40 / C48
H925 496 °C, 4 h 1170 MPa 1070 MPa 5 % C38 / C48
H1025 552 °C, 4 h 1070 MPa 1000 MPa 5 % C35 / C43
H1075 579 °C, 4 h 1000 MPa 860 MPa 5 % C31 / C40
H1100 593 °C, 4 h 965 MPa 790 MPa 5 % C31 / C40
H1150 621 °C, 4 h 930 MPa 725 MPa 8 % C28 / C38

Thicker bands in Table 5 have higher elongation minimums and add reduction-of-area and Charpy requirements; check the band that matches the ordered gauge.

Cold-rolled finishes for S17400 sheet: 2B, BA, No.4, HL and more

For sheet, finish often matters as much as chemistry because it decides appearance, cleanability and how the part forms. A480 Section 11 lists the sheet finishes below, and all are available on S17400 subject to the mill route; precipitation-hardening sheet is normally supplied descaled in Condition A and finished as agreed:

Finish Description (A480 Section 11 and Note 3) Typical sheet use
No. 1 Hot-rolled, annealed and descaled; dull and non-reflective Hot-rolled sheet, heat-resisting and industrial parts
No. 2D Cold-rolled, dull; smooth, non-reflective and non-directional, holds lubricant in deep drawing Deep-drawn and severely formed parts
No. 2B Cold-rolled, bright; smooth, moderately reflective, from a final light pass on polished rolls; polishes more readily than No. 1 or 2D General-purpose sheet; the standard mill finish
BA (bright annealed) Smooth, bright, reflective; cold rolled then annealed in a protective atmosphere to prevent scaling Appliance panels, reflectors, hygienic and decorative parts
No. 3 Intermediate polish, linear texture; Ra generally up to 40 µin (about 1.0 µm) Pre-polished sheet for further finishing
No. 4 General-purpose polish, linear texture; Ra generally up to 25 µin (about 0.6 µm) Kitchen, architectural and elevator panels
No. 6 Dull satin, produced by Tampico brushing a No. 4 finish Architectural and decorative work
No. 7 High lustre, buffed from a finely ground surface with grit lines still present Ornamental and architectural parts
No. 8 Mirror; polished with successively finer abrasives and buffed Mirrors, reflectors, signage
TR Cold-worked to obtain specified properties Springs and high-strength formed parts
HL (hairline) Commercial long-line brushed finish; not defined in A480, so it is agreed by description or sample Elevators, doors, interior panels

Polished sheet can be ordered polished on one side or both; when only one side is polished, the other side may be rough ground to get flatness (A480 11.1.12). Architectural finishes, sometimes called No. 5, and special textures are negotiated between buyer and seller. A480 Note 3 is guidance, not a basis for rejection, so agree a reference sample for any decorative finish. Laser-grade PVC film, paper interleaving and grain direction should be stated on the order when the face side matters.

Gauge, width, length and flatness tolerances for S17400 sheet

Gauge and flatness tolerances come from A480 Annex A3 for A480M (metric) orders and Annex A2 for inch-pound orders. For cold-rolled wide coil and cut lengths, Table A3.5 gives these thickness tolerances, over and under:

Specified thickness, mm w ≤ 1000 mm 1000 < w ≤ 1300 mm 1300 < w ≤ 2100 mm
0.30 ± 0.03 — —
0.40 ± 0.04 ± 0.04 —
0.50 ± 0.045 ± 0.05 —
0.60 ± 0.05 ± 0.05 —
0.80 ± 0.05 ± 0.05 —
1.00 ± 0.055 ± 0.06 ± 0.07
1.20 ± 0.08 ± 0.08 ± 0.08
1.50 ± 0.08 ± 0.08 ± 0.10
2.00 ± 0.10 ± 0.10 ± 0.11
2.50 ± 0.10 ± 0.11 ± 0.13
3.00 ± 0.13 ± 0.13 ± 0.15
4.00 ± 0.17 ± 0.17 ± 0.17

Thickness is measured at least 15 mm from a slit edge or 25 mm from a mill edge. For a thickness between two rows, the next higher row applies. Some mills roll tighter than the table, and a tighter tolerance can be agreed on the order. Order thickness as a decimal or fraction, not a gauge number; under A480 4.1.7 the gauge number is not a basis for rejection.

Width tolerance for cut lengths and coil is plus-only (Table A3.6, selected rows):

Specified thickness, mm 600 < w ≤ 1000 mm 1000 < w ≤ 2100 mm
1.00 +1.5 / −0 +2.0 / −0
1.50 +1.5 / −0 +2.0 / −0
2.50 +2.0 / −0 +2.5 / −0
3.50 +3.0 / −0 +3.0 / −0

Length tolerance for cut lengths (not resquared) is +5 / −0 mm up to 2000 mm and +0.0025 × L / −0 above 2000 mm (Table A3.7). Flatness is the maximum deviation from a horizontal flat surface (Table A3.8):

Flatness standard Thickness / width / length Max. deviation from a flat surface
Not stretcher-levelled width under 1500 mm (any thickness) 10 mm
Not stretcher-levelled width 1500 mm and over 12 mm
Stretcher-levelled t ≤ 4.99 mm, w < 1200 mm, L < 2400 mm 4 mm
Stretcher-levelled t ≤ 4.99 mm, other width/length combinations 7 mm

The Table A3.8 values exclude hard tempers of 2xx and 3xx grades, dead-soft and deep-drawing sheet, which have their own rules. If panels will be laser cut, bonded or used as visible cladding, order stretcher-levelled flatness or a tighter flatness by agreement.

S17400 coil, slit coil and cut-to-length sheet supply

S17400 is supplied in four forms. Coil is the mill product, supplied at full width. Slit coil is cut to narrower widths; under 600 mm wide it becomes strip, ordered with edge No. 1 (rolled), No. 3 (slit) or No. 5 (square after slitting) per A480 Section 14. Cut-to-length sheet is levelled and sheared to length, and blanks are cut to drawing.

For coils, state the inside diameter your decoiler takes (often 508 or 610 mm) and the maximum coil weight. Coils are marked near the outside end, with an inside tag carrying the same data (A480 25.1.1.3), and packaging follows ASTM A700 unless the order says otherwise (A480 25.1.2).

SHH STEEL can slit, cut to length, level, apply protective film and pack S17400 sheet in its own workshop, so you receive sizes ready for your laser, press brake or production line.

Annealing and heat treatment of S17400 sheet

A480 condition for UNS S17400 (Type 630): solution treated at 1050 ± 25 °C, cooled as required (SA-693 Table 3); precipitation hardening at 482 to 621 °C as ordered.

Ageing after fabrication: 482 °C for 1 h (H900), or 4 h at 496, 552, 579, 593 or 621 °C (H925 to H1150), all air cooled (A693 / SA-693 Table 3).

How S17400 sheet performs in service

Corrosion resistance is broadly comparable with Type 304 in many atmospheric and mild environments. The ageing condition sets the balance: H900 gives the highest strength, while H1025 to H1150 trade strength for toughness and better resistance to stress-corrosion cracking.

S17400 sheet equivalents: ASTM, EN, JIS and GB/T compared

Buyers often send drawings that name an EN, JIS or GB grade rather than UNS S17400 (Type 630). The table shows the nearest cross-references for sheet. “Nearest” means the grades share the same metallurgical concept, not that they are interchangeable on a certificate. SHH STEEL checks each element and each property against every standard named on the enquiry before offering dual certification.

System Sheet standard Grade How close Notes for sheet buyers
ASTM A693 with A480 UNS S17400 (Type 630) reference State the edition and A240 or A240M
EN EN 10088-2 (also EN 10088-4, EN 10028-7) 1.4542 X5CrNiCuNb16-4 nearest; check each limit Proof strengths depend on product form (C = cold-rolled strip, H = hot-rolled strip, P = plate); elongation uses A80 or A gauge lengths
JIS JIS G4305 (cold-rolled) / G4304 (hot-rolled) SUS630 nearest; check each limit SUS grade with its own ranges; compare C, N and Ni with A240
GB/T GB/T 3280 (cold-rolled) / GB/T 4237 (hot-rolled) 05Cr17Ni4Cu4Nb (S51740) nearest; check each limit GB/T 20878 name and code; the S-code is not a UNS number

EN. EN 10088-2 is the main European standard for corrosion-resisting sheet, strip and plate for general purposes. Its property tables are split by product form: cold-rolled strip (C), hot-rolled strip (H) and hot-rolled plate (P). A thin cold-rolled sheet is therefore checked against the C-row values for its thickness. EN 10088-4 covers sheet and strip for construction, and EN 10028-7 covers flat stainless products for pressure equipment. EN tensile tests report 0.2 % and 1 % proof strength, and thin-sheet elongation is measured on an 80 mm gauge length, so the numbers do not convert one-for-one to the A240 50 mm elongation. See the EN 10088-2 stainless range for related steel numbers.

JIS. JIS G4305 covers cold-rolled stainless plate, sheet and strip, which includes most thin sheet, and JIS G4304 covers the hot-rolled product. SUS grades follow the AISI-type concept but their ranges are set independently. Japanese-specified sheet should be checked for carbon, nitrogen and nickel against the A240 row. The JIS G4305 range lists the SUS sheet grades.

GB/T. Chinese cold-rolled sheet is ordered to GB/T 3280 and hot-rolled sheet to GB/T 4237, with grade names and numeric codes from GB/T 20878. A code such as S30408 is a Chinese designation, not a UNS number, so certificates must state which standard the code belongs to. See the GB/T 4237 range for related Chinese grades.

Other ASTM and ASME specifications. A480 supplies the general rules for A240 sheet. Precipitation-hardening flat products are covered by A693. SA-240 is the ASME Code adoption of A240 and is needed only for ASME Code equipment. Other product forms in the same UNS grade, such as pipe, tube and bar, have their own ASTM specifications, so check each one when you need a matching set.

Other A240 sheet grades related to S17400

Sheet buyers comparing S17400 usually look at these grades in the same A240 sheet series:

For the same material in other product forms and designations, see ASME SA240 UNS S17400 stainless steel plate, ASTM A693 Type 630 stainless steel. Those pages cover plate or type-designation ordering, while this page covers thin sheet and coil.

More grades and standards are listed in the ASTM A240/A240M stainless steel range, stainless steel sheets and plates pages.

S17400 sheet applications, forming and welding

Typical uses of S17400 sheet and coil:

  • Precision springs and flat parts from strip
  • Aerospace fittings and brackets
  • Machined high-strength parts
  • Tooling and shims

Blank and form in Condition A, then age. Welded parts are normally re-solution-treated and aged to the specified condition.

Keep the protective film on during laser cutting and forming. Keep sheet away from carbon-steel dust and tools, because embedded iron rusts and spoils the finish, and pickle or passivate welds where appearance or corrosion resistance matters.

Certificates, testing and receiving inspection for S17400 sheet

Every S17400 sheet delivery from SHH STEEL comes with the original mill test report. Under A480 8.1, it names the specification and year, the grade or grades, the heat analysis and the required test results. A supplier that is not the mill must pass on a copy of the original manufacturer’s report (A480 8.4). EN 10204 3.1 is standard, and 3.2 with witness by TUV, ABS, CCS, BV, DNV, LR or your own inspector can be arranged.

On receipt, match the marking to the certificate, measure thickness at the A480 positions, check flatness and finish, and run PMI where required. Test-based rejections must be reported within 60 working days of receipt (A480 23.1).

Sourcing S17400 sheet: buyer concerns and SHH STEEL solutions

These are the questions sheet buyers ask SHH STEEL most often, and how we handle each one:

Buyer Concern SHH STEEL Solution
Fake material or certificates Coils and sheet lots can be witnessed by TUV, ABS, CCS or another class society, and partner laboratories run PMI, chemistry and tensile checks against the order. Third-party witness and EN 10204 3.2 certificates available.
Unsafe deposit TT and LC are accepted, including TT + LC splits. For large projects you can sign directly with the mill, with SHH STEEL coordinating documents and follow-up for a small service fee.
Small orders below mill MOQ Small sheet quantities are consolidated with other customers’ orders of the same grade, thickness and finish, so lots below the mill MOQ still come from genuine mill coils with full traceability.
Slow delivery Dedicated staff chase the mill schedule through cold rolling, annealing, finishing and slitting, and report progress at each stage.
Processing needs Our own workshop handles cutting to size, bevelling, machining to drawings and surface pretreatment such as film protection, so sheets arrive ready to fabricate.

How to order UNS S17400 sheet from SHH STEEL

A480 4.1 puts the responsibility for a complete order on the buyer. For S17400 sheet, include:

  • Quantity by weight and number of sheets or coils.
  • Specification and edition: ASTM A693, Type 630, plus any second standard for dual certification.
  • Grade: UNS S17400 (Type 630).
  • Condition and finish, for example annealed 2B, BA, or No.4 on one side with film.
  • Form and dimensions: thickness, width and length in the same units, or coil ID, OD and weight; strip edge type if slit.
  • Tolerances or flatness tighter than A480, if needed.
  • Tests and documents: PMI, corrosion or phase tests, EN 10204 3.1 or 3.2, inspector, marking and packing.

SHH STEEL combines mill-direct sourcing with its own processing workshop. We check your grade and finish choice, offer dual certification when a heat qualifies, consolidate small quantities, follow the mill schedule and cut or slit before shipment. TT and LC payment are accepted.

Send your S17400 sheet enquiry with sizes, finish and quantity. The SHH STEEL team will reply with a quotation, lead time and inspection plan.

FAQ

Can I buy S17400 sheet to ASTM A240?
No. S17400 is not in A240; order it to ASTM A693 Type 630, which covers plate, sheet and strip.
How is Type 630 sheet hardened?
It is supplied solution treated and then aged, for example 1 h at 482 °C for H900 or 4 h at 621 °C for H1150, per A693 / SA-693 Table 3. The ageing temperature is chosen to balance strength against toughness.
What hardness does solution-treated Type 630 sheet have?
A693 / SA-693 Table 4 sets a maximum of 363 HBW or C38 in the solution-treated condition. Sheet in that condition is soft enough to be cut and formed before ageing.
Can I buy S17400 stainless steel sheet cut to size in small quantities?
Yes. SHH STEEL consolidates small S17400 sheet orders with other customers’ orders of the same grade and finish, and cuts sheets or blanks to size in its own workshop. That way small lots still come from traceable mill coils.
What thickness tolerance applies to cold-rolled S17400 sheet?
For A480M orders, Table A3.5 applies. For example, 1.00 mm sheet up to 1000 mm wide is allowed ±0.055 mm, and 2.00 mm sheet ±0.10 mm. Tighter tolerances can be agreed on the order.
Which certificate comes with A693 S17400 sheet?
Each delivery carries the original mill test report to A693 and A480, normally as EN 10204 3.1. Third-party witness and EN 10204 3.2 certificates can be arranged with TUV, ABS, CCS or another inspector.

Conclusion

ASTM A240 UNS S17400 Stainless Steel Sheet is bought for its strength after ageing, so the order should define all three: the A693 edition and UNS number, the finish and protective film, and the A480 tolerance or flatness level. SHH STEEL supplies S17400 sheet and coil from mill partners, cut or slit to your needs, with certificates you can check line by line.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X