ASTM A240 UNS S31050 Stainless Steel Sheet at SHH STEEL warehouse

ASTM A240 UNS S31050 Stainless Steel Sheet

ASTM A240 UNS S31050 Stainless Steel Sheet: urea-grade austenitic grade to ASTM A240/A240M, sheet in 2B and No.1 finishes from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
A240 UNS S31050 sheet, S31050 sheet, S31050 stainless sheet supplier, ASTM A240/A240M S31050, S31050 sheet stock China
Equivalent Grades:
EN 1.4466 X1CrNiMoN25-22-2; GB/T 022Cr25Ni22Mo2N (S31053)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is ASTM A240 UNS S31050 Stainless Steel Sheet?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: UNS S31050 ≈ EN 1.4466 X1CrNiMoN25-22-2 ≈ GB/T 022Cr25Ni22Mo2N (S31053).

UNS S31050 is a urea-grade austenitic grade. S31050 (310MoLN) is a fully austenitic 25Cr-22Ni-2Mo-N grade with extra-low carbon and silicon. It was developed for urea plants, where it resists ammonium carbamate better than 316L urea grade, and it also performs well in nitric acid and other strongly oxidising media. Its stable austenite gives low magnetic permeability and good toughness.

ASTM A240/A240M covers chromium, chromium-nickel and chromium-manganese-nickel stainless steel plate, sheet and strip for pressure vessels and general applications. Under ASTM A480, sheet is flat material under 5.00 mm thick and 600 mm or more wide, so UNS S31050 sheet is a cold-rolled 2B/2D product in thin gauges and a hot-rolled, annealed and pickled No.1 product toward the 4.75 mm end.

This page sets out the ASTM A240/A240M requirements for UNS S31050 sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

UNS S31050 sheet: specification summary

Item UNS S31050 data
Standard ASTM A240/A240M; general requirements ASTM A480/A480M
ASME counterpart SA-240 (ordered for ASME Code construction)
Product form (A480) sheet: under 5.00 mm thick, 600 mm and wider; plate 5.00 mm and over
Typical gauges 0.5–3.0 mm cold-rolled 2B/2D; 3.0–4.75 mm hot-rolled No.1
Widths 1000, 1219, 1250, 1500 mm; slit coil to order
Lengths 2000, 2438, 2500, 3000 mm or cut to size
Finishes No.1, 2D, 2B; BA and No.4 by agreement
Required tests heat analysis, tension test, hardness (and bend where the grade requires it)
Certificates EN 10204 3.1; 3.2 with third-party witness on request
Grade family austenitic

Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. UNS S31050 is a specialty grade made by a limited number of mills in campaign rolling. Stock covers the common sizes listed below; for project quantities or unusual sizes, plan for a mill campaign and reserve the heat early.

Chemical composition of UNS S31050 (ASTM A240/A240M)

Element wt %
C 0.020 max
Si 0.50 max
Mn 2.00 max
P 0.030 max
S 0.010 max
Cr 24.0–26.0
Ni 20.5–23.5
Mo 1.60–2.60
N 0.09–0.15

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

PREN check (Cr + 3.3 Mo + 16 N): about 30.7 at the specification minimums and about 33.9 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.

Mechanical properties of UNS S31050 sheet

Condition / thickness Tensile strength, min Yield strength 0.2 %, min Elongation in 50 mm, min Hardness, max
thickness ≤ 6.35 mm 580 MPa (84 ksi) 270 MPa (39 ksi) 25 % 217 HBW / 95 HRB
thickness > 6.35 mm 540 MPa (78 ksi) 255 MPa (37 ksi) 25 % 217 HBW / 95 HRB

The minimum yield strength of 270 MPa is about 1.6 times the 170 MPa minimum of ASTM 316L. Annealed austenitic and 200-series material work-hardens quickly, so cold-formed parts are stronger than these minimums. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.

Corrosion resistance of UNS S31050: PREN and limits

Austenitic stainless steels are non-hardenable by heat treatment, tough down to cryogenic temperatures and easy to form and weld. Corrosion resistance rises with chromium, molybdenum and nitrogen; the PREN of this grade at the specification minimum is about 30.7. Low-carbon (L) and stabilised versions protect welds against intergranular corrosion.

Austenitic grades are prone to chloride stress-corrosion cracking above about 60 °C in chloride environments. Where that risk exists, duplex or super-austenitic grades are the usual upgrade. Cold work raises strength but also makes some grades slightly magnetic.

How UNS S31050 compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
UNS S31050 24.0–26.0 20.5–23.5 1.60–2.60 0.09–0.15 30.7 270
1.4303 X4CrNi18-12 17.0–19.0 11.0–13.0 — 0.11 max 17.0 220
06Cr19Ni10 (S30408) 17.5–19.5 8–10.5 — 0.1 max 17.5 205
022Cr19Ni10 (S30403) 17.5–19.5 8–12 — 0.1 max 17.5 180
06Cr17Ni12Mo2 (S31608) 16–18 10–14 2–3 0.1 max 22.6 205

Choose UNS S31050 for general corrosion resistance with easy forming and welding. In warm chloride environments consider a molybdenum-bearing or duplex grade instead.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of UNS S31050

Heat treatment: 1050–1100 °C, rapid cooling.

Austenitic grades are solution annealed and cooled rapidly to keep carbides in solution. They cannot be hardened by heat treatment, only by cold work.

Surface finishes for UNS S31050 sheet

No.1 is hot-rolled, annealed and pickled, used for the 3–4.75 mm end of the sheet range. 2D is a dull cold-rolled, annealed and pickled finish that holds lubricant in deep drawing. 2B adds a light skin pass for a smoother, brighter surface and is the normal base for polishing. BA (bright annealed) and No.4 brushed finishes are available for many austenitic and ferritic grades by agreement. For highly alloyed grades, cold-rolled thin gauges are produced by fewer mills, so confirm the finish and gauge range before you fix a design.

Dimensions, tolerances and flatness

Thickness, width, length, flatness and camber tolerances follow ASTM A480/A480M. Cold-rolled sheet has tighter thickness tolerances than hot-rolled No.1 sheet. Higher-strength grades show more residual stress after slitting and laser cutting, so for laser blanks or long panels specify flatness and, where needed, tension-levelled material. Edge condition (mill or slit edge) and PVC film on one side should be stated on the order.

Ordering notes for A240 sheet. A240 refers to ASTM A480 for everything that is not grade-specific: definitions of sheet, strip and plate, dimensional tolerances, finishes, marking, retests and certification. A purchase order that says only “A240 S31050” therefore leaves several choices to the mill. State the finish (2B, 2D or No.1), the thickness tolerance basis, whether coil, slit coil or cut lengths are wanted, and whether the certificate must also show SA-240. If the sheet will be formed into vessel heads or pressure parts, say so, because some grades need specific heat-treatment records and supplementary tests that are only reported when requested. For export, also state the edition year if your specification fixes one; most mills certify to the current edition by default.

UNS S31050 sheet stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
0.5 1000 / 1219 2000 / 2438 2B 100+ t China
0.8 1219 2438 2B 100+ t China
1.0 1219 / 1250 2438 / 2500 2B 100+ t China
1.5 1219 / 1500 2438 / 3000 2B 100+ t China
2.0 1219 / 1500 2438 / 3000 2B 100+ t China
3.0 1500 3000 2B / No.1 100+ t China
4.0 1500 3000 / 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.

UNS S31050 equivalents in other standards

Standard Designation Comment
EN 1.4466 X1CrNiMoN25-22-2 same alloy family and limits closely matched; compare each limit on the certificate
GB/T 022Cr25Ni22Mo2N (S31053) same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Austenitic

General-purpose austenitic grades for comparison: A240 S30400, A240 S30403, A240 S31600, A240 S31603, A240 S30500, A240 S32100, A240 S30100, 1.4301 plate, 1.4307 plate, 1.4303 plate.

200 series (Cr-Mn-Ni-N)

Lower-nickel 200-series grades: GB/T 3280 S35350, GB/T 3280 S35450.

Same grade, other specification

SA-240 S31050.

Applications, forming and welding of UNS S31050

Typical uses: urea strippers, reactors, carbamate condensers and scrubbers, nitric-acid equipment, and oxidising chemical service.

Austenitic sheet and plate form and weld easily. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use an ER308L, ER316L or ER347 filler matching the grade (AWS A5.9). Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Welding practice. Austenitic sheet is welded with GTAW, GMAW, SMAW or laser without preheat. Keep the interpass temperature below about 150 °C, use back-purging on corrosion-critical joints and pickle afterwards. Low-carbon or stabilised grades avoid sensitisation; standard-carbon grades used at temperature may need a solution anneal after heavy welding.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to ASTM A480/A480M with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: intergranular corrosion testing (ASTM A262 Practice E or EN ISO 3651-2 / GB/T 4334), PMI and surface inspection. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying UNS S31050

  • Mixing L and standard-carbon grades in welded equipment.
  • Leaving out the finish and film side for visible parts.
  • Using the grade in warm chlorides where stress-corrosion cracking is likely.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing UNS S31050: buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Mixed-up 304/316 or L/non-L grades PMI and heat-number tracking for every sheet
Surface scratches on finished sheet PVC film, interleaving paper and wooden-case packing
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order UNS S31050 sheet

State the standard and edition (ASTM A240/A240M), the grade (UNS S31050), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

Can I use A240 S31050 sheet for ASME Code equipment?
Only if it is certified to SA-240 as well. Most mills dual-certify A240/SA-240; tell us when the sheet is for Code construction and we will supply dual-marked material with the certificate stating both.
Is UNS S31050 equivalent to EN 1.4466 X1CrNiMoN25-22-2?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
Is UNS S31050 magnetic?
It is essentially non-magnetic when annealed; cold work can make it slightly magnetic.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

UNS S31050 sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *