ASME SA553 Type III 7% Nickel Steel Plate | ASME SA553 Nickel Steel - SHH STEEL

ASME SA553 Type III 7% Nickel Steel Plate

ASME SA553 Type III is quenched and tempered 7% nickel steel plate under ASME SA-553/SA-553M in Section II, Part A. The 2023 Code edition marks SA-553/SA-553M identical with ASTM A553/A553M-17, while the current ASTM publication is A553/A553M-22. That is not an automatic dual-compliance or identical-stamp claim. Type III is impact tested at −320 °F [−195 °C] unless another temperature is agreed. SHH STEEL produces and exports ASME SA553 Type III plate to the ordered Code edition and project requirements.
Equivalent Grades:
ASTM A553 Type III; 06Ni7DR (7% nickel). Edition, condition and tests differ; not automatic substitutes.
Heat Treatment
Water quenched and tempered (A553/A553M-17 reference; ASME 2023 adoption).
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
Conclusion

What is ASME SA553 Type III steel plate?

ASME SA553 Type III is water-quenched and tempered 7% nickel alloy steel plate to ASME SA-553/SA-553M. The official split is Type I (9% nickel), Type II (8% nickel) and Type III (7% nickel). This page is Type III only. Type I and Type II do not complete the specification.

ASME BPVC.II.A-2023 prints SA-553/SA-553M as identical with ASTM Specification A553/A553M-17. The current ASTM publication is A553/A553M-22. That identity statement is not a dual-stamp or automatic dual-compliance claim. Orders for Code use should name the Section II edition year, the SA designation and the Type.

SHH STEEL produces and exports ASME SA-553/SA-553M Type III 7% nickel steel plate to the ordered edition, heat treatment, dimensions and extra tests written on the enquiry. This plate belongs to our Boiler & Pressure Vessel Steel Plates range under ASME SA553.

Material specification for ASME SA553 Type III

The items below follow SA-553/SA-553M as printed in ASME BPVC.II.A-2023.

Parameter Detail
Standard ASME SA-553/SA-553M, Specification for Pressure Vessel Plates, Alloy Steel, Quenched and Tempered 7, 8, and 9% Nickel
Code location ASME BPVC Section II, Part A. The 2023 edition marks this specification identical with ASTM A553/A553M-17
Official split Type III (nominal 7% nickel)
Complete official types Type I, Type II and Type III
General requirements SA-20/SA-20M; SA-553 prevails in a conflict
Chemical analysis Table 1 heat and product analysis for Type III, including molybdenum and niobium
Delivery condition Water quenched and tempered; marked QT, or QTT when the optional intermediate treatment is used
Thickness Limited only by mechanical properties; see the mill-practice note below
Impact testing Mandatory at −320 °F [−195 °C] unless otherwise agreed; lateral expansion not less than 0.015 in. [0.381 mm]
Our supply We produce and export SA-553 Type III plate to the ordered Code edition, dimensions and extra tests

Clause 1.4 of the A553/A553M-17 text reproduced as SA-553 in 2023 says that maximum thickness is limited only by the capacity of the material to meet the specified mechanical properties, and it adds that current mill practice normally limits this material to 2 in. [50 mm] maximum. That mill-practice sentence is not a specification thickness ceiling. The public ASTM A553/A553M-22 scope statement does not include the mill-practice sentence.

Official types in SA-553/SA-553M:

Type Nominal nickel, % Default impact test temperature
I 9 −320 °F [−195 °C]
II 8 −275 °F [−170 °C]
III 7 −320 °F [−195 °C]

Chemical composition of ASME SA553 Type III

ASME BPVC.II.A-2023 SA-553/SA-553M is marked identical with ASTM A553/A553M-17 and already includes Type III. The chemical composition, tensile values and heat-treatment temperatures on this page are taken from that 2023 SA-553 text.

The current ASTM publication is A553/A553M-22. It is a separate ASTM document and is supplied when the purchase order names that ASTM edition. This page does not treat an ASTM A553/A553M-22 mark as automatic SA-553 documentation, and it does not treat the 2017 tables as the 2022 ASTM text.

Name the Section II, Part A edition year required by the project, together with SA-553/SA-553M and Type III.

Element Type III heat analysis (wt. %) Type III product analysis (wt. %)
Carbon (C), max 0.13 0.13
Manganese (Mn), max 0.90 0.98
Phosphorus (P), max 0.010 0.010
Sulfur (S), max 0.010 0.010
Silicon (Si) 0.05–0.30 0.05–0.30
Nickel (Ni) 6.50–7.50 6.50–7.50
Molybdenum (Mo) 0.10–0.30 0.10–0.30
Columbium / niobium (Nb), max 0.03 0.03

Carbon, phosphorus, sulfur, molybdenum and niobium limits carry footnote A in SA-553 Table 1 (identical with A553/A553M-17): they apply to both heat and product analyses. Type III silicon 0.05–0.30 and nickel 6.50–7.50 also carry footnote A on the heat-analysis cell; the product-analysis cells in those printed rows are blank because the same range applies to both analyses, not because a second range is missing. Columbium and niobium are interchangeable names for the same element. These figures are the A553/A553M-17 / SA-553 2023 table as published in ASME BPVC.II.A-2023 SA-553/SA-553M, not an SHH STEEL proprietary chemistry. They are not presented as the A553/A553M-22 text.

Tensile and impact requirements for ASME SA553 Type III

ASME BPVC.II.A-2023 SA-553/SA-553M is marked identical with ASTM A553/A553M-17 and already includes Type III. The chemical composition, tensile values and heat-treatment temperatures on this page are taken from that 2023 SA-553 text.

The current ASTM publication is A553/A553M-22. It is a separate ASTM document and is supplied when the purchase order names that ASTM edition. This page does not treat an ASTM A553/A553M-22 mark as automatic SA-553 documentation, and it does not treat the 2017 tables as the 2022 ASTM text.

Name the Section II, Part A edition year required by the project, together with SA-553/SA-553M and Type III.

Table 2 in the A553/A553M-17 / SA-553 2023 text lists one tensile package for the specification; it is not split by Type. Nickel content, some chemistry limits, tempering range and default impact temperature still differ by Type.

Property SA-553/SA-553M (identical with A553/A553M-17) requirement
Tensile strength 100–120 ksi [690–825 MPa]
Yield strength (0.2% offset), min 85 ksi [585 MPa]
Elongation in 2 in. [50 mm], min 20.0% (see SA-20/SA-20M for elongation adjustment)
Impact test method Charpy V-notch to SA-20/SA-20M
Specimen orientation Longitudinal axis of the specimen transverse to the final rolling direction
Default test temperature for Type III −320 °F [−195 °C], unless otherwise agreed
Mandatory acceptance Each specimen: lateral expansion opposite the notch not less than 0.015 in. [0.381 mm]

Optional S55 and S56 energy-absorption requirements apply only when ordered. They are not the default mandatory impact criterion.

Heat treatment for ASME SA553 Type III

Plates are supplied in the water-quenched and tempered condition. Shell plates and other parts heated for forming shall be heat treated after forming to the same procedure.

  • Hardening: heat to a suitable temperature in the range 1475–1700 °F [800–925 °C], hold long enough to obtain a uniform temperature through the thickness, and quench in water (the detailed hardening clause also says quench in a liquid medium).
  • Tempering 1000–1125 °F [540–615 °C] for Type III: hold at least 30 min/in. [1.2 min/mm] of thickness and not less than 15 min, then cool in air or quench at a rate not less than 300 °F/h [165 °C/h].

Before tempering, plates may receive an optional intermediate heat treatment (1205–1330 °F [650–720 °C] for Type III), held at least 15 min, then cooled as specified by thickness in the standard. When that optional treatment is used, plates are marked QTT instead of QT. The intermediate treatment may be performed at the manufacturer option or specified by the purchaser. This page does not offer heat-treatment or fabrication services.

These temperatures are those of SA-553/SA-553M as printed in ASME BPVC.II.A-2023 (identical with A553/A553M-17). Type III tempering is 1000–1125 °F [540–615 °C]. Name the Section II edition year required by the project.

Water quenched and tempered: heat 1475–1700 °F [800–925 °C] and water quench; temper 1000–1125 °F [540–615 °C] for Type III, hold at least 30 min/in. [1.2 min/mm] and not less than 15 min, then air cool or quench at not less than 300 °F/h [165 °C/h]. Optional intermediate treatment 1205–1330 °F [650–720 °C] is marked QTT. Temperatures are those of SA-553/SA-553M in ASME BPVC.II.A-2023 (identical with A553/A553M-17).

Welding and handling notes

SA-553 covers plates intended for the fabrication of welded pressure vessels. Welding procedures belong to the Code of construction, the project specification and the fabricator. This page does not offer fabrication or procedure qualification.

The specification warns that the material is susceptible to magnetization after heat treatment.

General requirements, marking and dimensions

Material supplied to SA-553/SA-553M shall conform to SA-20/SA-20M except where SA-553 prevails. Each plate is marked QT, or QTT when the optional intermediate heat treatment is used. Dimensional tolerances are those of the ordered SA-20 edition and the mill documents, not a stock list.

Applications and specification limits

We produce and export this plate for projects that specify ASME SA-553/SA-553M Type III. Name the Code of construction and the Section II edition on the order. This page does not claim automatic dual ASTM marking.

Compare ASME SA553 Type III with related nickel steel plates

SA-553 uses the same official Type split as ASTM A553. Type III is in the 2023 SA-553 text. An SA-553 order that omits the Type is incomplete.

Material Alloy / type Delivery condition Mechanical requirements Typical service Substitution limit
ASME SA553 Type III (this plate) SA-553 Type III, nominal 7% nickel Water quenched and tempered; Type III tempering range; QTT if used Tensile 100–120 ksi [690–825 MPa]; yield 85 ksi [585 MPa] min; impact −320 °F [−195 °C] Code work that names SA-553 Type III Not Type I, not Type II, not 06Ni7DR, and not an ASTM-only A553-22 mark
ASTM A553 Type III 7% nickel steel plate ASTM A553/A553M-22 Type III Water quenched and tempered Same official Type III identity; ASTM specification year is 22, while SA-553 in 2023 adopts 17 Orders written to the current ASTM publication Related, not an automatic SA stamp
ASME SA553 Type I 9% nickel steel plate SA-553 Type I Water quenched and tempered; different tempering range Same tensile table; default impact −320 °F [−195 °C] Code work that names Type I Different nickel, chemistry extras and tempering range
ASTM A553 Type II 8% nickel steel plate ASTM Type II Water quenched and tempered Default impact −275 °F [−170 °C] ASTM Type II orders Different Type and impact temperature
GB/T 713.4-2023 06Ni7DR Chinese 7% nickel vessel plate QT or double-QT on our 06Ni7DR page From our live 06Ni7DR page: about 7% nickel under GB/T 713.4-2023; yield 550 MPa in the mid-thickness band and 540 MPa above that; tensile 680–820 MPa; delivery quenched and tempered or double-quenched and tempered; lateral expansion not less than 0.64 mm. This is closer to A553 Type III (nominal 7% nickel) than to Type II (nominal 8% nickel). 7Ni vessel plate Near comparison only, not an SA-553 Type III designation
ASTM A353 9% nickel steel plate Double-normalized 9% nickel plate Double-normalized and tempered Yield 75 ksi [515 MPa] min ASTM A353 orders Different nickel, heat treatment and yield
ASME SA203 Grade E Nickel-alloy pressure-vessel plate in the normalized SA203 family. Normalized. Use its own ordered specification, thickness and delivery condition; no strength or toughness value is transferred to this grade. Low-temperature process vessels and refrigerated containment. Lower-nickel comparison, not a cryogenic-temperature substitute for ASME SA553 Type III 7% Nickel Steel Plate. Its Code edition, strength, impact temperature and certification must be selected separately.
EN 10028-4 X8Ni9 High-nickel cryogenic vessel plate; a different selection from lower-nickel normalized pressure plate. Usually quenched and tempered. Use its own ordered specification, thickness and delivery condition; no strength or toughness value is transferred to this grade. LNG and other cryogenic pressure containment. Different EN designation and treatment requirements. Similar nickel-family service does not transfer allowable temperature, strength or certification to ASME SA553 Type III 7% Nickel Steel Plate.

Related published ranges: EN 10028-4 and GB/T 713.4-2023.

Equivalent and related grades by country

Near comparisons only. The official SA-553 type list is Type I, Type II and Type III.

Country / region Standard Grade or designation Similarity and key differences Substitution caveat
United States ASME SA-553/SA-553M (BPVC.II.A-2023) Type III This Code specification, identical with ASTM A553/A553M-17, which includes Type III. This product
United States ASTM A553/A553M-22 Type III Current ASTM publication, different year from the 2023 SA adoption. Related ASTM page; not an automatic SA stamp.
United States ASME SA-553 Type I and Type II Type I and Type II Official sister types in the same Code specification. Different Types.
China GB/T 713.4-2023 06Ni7DR From our live 06Ni7DR page: about 7% nickel under GB/T 713.4-2023; yield 550 MPa in the mid-thickness band and 540 MPa above that; tensile 680–820 MPa; delivery quenched and tempered or double-quenched and tempered; lateral expansion not less than 0.64 mm. This is closer to A553 Type III (nominal 7% nickel) than to Type II (nominal 8% nickel). Near comparison only.
Europe EN 10028-4 No live 7% nickel grade Live EN 9Ni names are not Type III. Do not force X8Ni9 onto Type III.
Japan JIS G3127 No verified 7% nickel counterpart stated here Live-site JIS citations refer to 9% nickel plate. Do not invent a JIS Type III equivalent.

Why choose SHH STEEL for ASME SA553 Type III

  • We produce and export ASME SA-553/SA-553M Type III 7% nickel steel plate
  • We review the enquiry for the named standard edition, type or designation, heat treatment, dimensions and any extra tests
  • We keep ASTM and ASME orders distinct unless the purchase order requires dual documentation and both texts can be met
  • We keep A353 double-normalizing distinct from A553 quenching and tempering, and Type I distinct from Type II
  • We match the inspection document to what the purchase order requires

How to enquire for ASME SA553 Type III plate

Item What to specify
Standard and type ASME SA-553/SA-553M Type III, plus the Section II, Part A edition year
Heat treatment Water quenched and tempered to the Type III tempering range; say if QTT is required
Dimensions Required thickness, width and length
Chemistry Heat and product analysis for Type III, including molybdenum and niobium
Mechanical tests Tension to Table 2; Charpy V-notch at −320 °F [−195 °C] unless otherwise agreed
Other tests S55/S56 or NDE only when written on the order
Documentation State the inspection document and any Code marking language required
ASTM documents Request ASTM A553 Type III dual documentation only when the project actually needs it

Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.

Request a quotation

Contact SHH STEEL for a quotation for ASME SA-553/SA-553M Type III 7% nickel steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.

Specify ASME SA-553/SA-553M Type III and the Section II, Part A edition year. Type III is not Type I or Type II. Include ASTM dual documents, QTT, impact or NDE requirements if the project needs them.

If you are considering a related European, Chinese or Japanese nickel steel grade as an alternative, send the applicable standard and project specification with your enquiry. We will review the differences in chemistry, heat treatment, impact rules and documentation rather than assume that related grades are interchangeable.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X