ASME SA240 UNS S44100 Stainless Steel Plate at SHH STEEL warehouse

ASME SA240 UNS S44100 Stainless Steel Plate

ASME SA240 UNS S44100 Stainless Steel Plate: dual-stabilised ferritic grade to ASME SA-240/SA-240M, hot-rolled plate from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
SA240 UNS S44100 plate, S44100 plate, S44100 stainless plate supplier, ASME SA-240/SA-240M S44100, S44100 plate stock China
Equivalent Grades:
EN 1.4509 X2CrTiNb18; GB/T 022Cr18NbTi (S11973)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is ASME SA240 UNS S44100 Stainless Steel Plate?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: UNS S44100 ≈ EN 1.4509 X2CrTiNb18 ≈ GB/T 022Cr18NbTi (S11973).

UNS S44100 is a dual-stabilised ferritic grade. S44100 (Type 441) is an 18Cr ferritic steel stabilised with both niobium and titanium. Niobium raises high-temperature strength and creep resistance, so 441 is used in exhaust systems up to about 900 °C, while titanium ties up carbon and nitrogen to protect the weld zone against intergranular corrosion. It is nickel-free, magnetic and has a lower thermal expansion than austenitic grades.

ASME SA-240 is the Boiler and Pressure Vessel Code version of ASTM A240, published in Section II Part A. It is ordered when plate will be used in Code construction such as Section VIII pressure vessels, Section I boilers or B31.3 piping components made from plate. Chemistry and tensile limits are the same as in A240, but the certificate and marking must state SA-240 so the Authorized Inspector can accept the material.

This page sets out the ASME SA-240/SA-240M requirements for UNS S44100 plate: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

UNS S44100 plate: specification summary

Item UNS S44100 data
Standard ASME BPVC Section II Part A, SA-240/SA-240M (identical with or adapted from ASTM A240/A240M)
General requirements SA-480/SA-480M
Product form plate 5.00 mm (3/16 in.) and over; sheet and strip also covered
Typical thickness 5–80 mm hot-rolled; heavier by mill enquiry
Widths 1500, 2000, 2500 mm; wider by enquiry
Lengths 6000 mm standard; up to 12000 mm or cut to size
Finish No.1 (hot-rolled, annealed and pickled)
Marking SA-240 with grade, heat and plate number; dual A240/SA-240 marking common
Certificates EN 10204 3.1 stating SA-240; 3.2 with third-party or AI witness on request
Grade family ferritic

Size range. Plate is produced on Steckel or reversing mills from about 5 mm up to 80–100 mm depending on grade, with widths of 1500–2500 mm and lengths up to 12 m; thinner plate of 3–12 mm is often cut from hot-rolled coil. Very heavy or wide plates, and plates with tight flatness, should be confirmed before ordering. UNS S44100 is produced regularly by several mills; common sizes are held in stock, and other sizes are rolled in the mill’s scheduled campaigns for the grade.

Chemical composition of UNS S44100 (ASME SA-240/SA-240M)

Element wt %
C 0.030 max
Si 1.00 max
Mn 1.00 max
P 0.040 max
S 0.030 max
Cr 17.5–19.5
Ni 1.00 max
N 0.030 max
Ti 0.10–0.50
Nb [0.30 + (9×C)] min, 0.90 max

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

Low carbon and nitrogen, together with titanium and/or niobium where specified, are what make modern ferritic grades weldable. Check that the stabiliser content on the certificate meets the formula in the standard for the actual C and N.

Mechanical properties of UNS S44100 plate

Condition / thickness Tensile strength, min Yield strength 0.2 %, min Elongation in 50 mm, min Hardness, max
all thicknesses 414 MPa (60 ksi) 241 MPa (35 ksi) 20 % 190 HBW / 90 HRBW

The minimum proof strength is 241 MPa. Ferritic grades have lower elongation than austenitic grades and work-harden less, which helps in stretch forming but limits deep drawing. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.

Corrosion resistance of UNS S44100: PREN and limits

Ferritic stainless steels contain chromium but little or no nickel, so they are magnetic, cheaper and less sensitive to nickel price swings. They have good resistance to chloride stress-corrosion cracking, lower thermal expansion and higher thermal conductivity than austenitic grades, which helps in thermal cycling. Stabilisation with titanium and/or niobium ties up carbon and nitrogen and protects welds against intergranular corrosion.

The limits are toughness and formability in heavy sections: ferritic grades have a ductile-to-brittle transition, grain growth in the weld zone, and 475 °C embrittlement in the higher-chromium grades. They are therefore supplied mainly as sheet and light plate, and they are welded with low heat input.

How UNS S44100 compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
UNS S44100 17.5–19.5 1.00 max — 0.030 max 17.5 241
UNS S43940 17.5–18.5 — — — 17.5 250
UNS S44600 23.0–27.0 0.75 max — 0.25 max 23.0 275
UNS S40910 10.5–11.7 0.50 max — 0.030 max 10.5 170
UNS S40930 10.5–11.7 0.50 max — 0.030 max 10.5 170

Choose UNS S44100 when nickel-free cost, thermal-cycling behaviour or resistance to chloride stress-corrosion cracking matters more than toughness in heavy sections. It is not a good choice for heavy welded plate or for cryogenic service.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of UNS S44100

Heat treatment: anneal 790–1050 °C, air cool.

Ferritic grades are annealed and cooled rapidly or in air; they are not hardenable by quenching. Avoid long holding in the 400–550 °C range, which causes 475 °C embrittlement in higher-chromium grades.

Surface finishes for UNS S44100 plate

Plate to SA-240 is normally supplied with a No.1 finish: hot rolled, solution annealed and pickled, with a matt grey surface. Shot-blasted and pickled surfaces are the norm on heavy plate. Ground or polished faces, and plates with protective film for the process side, can be produced after delivery in our workshop. Surface defects are judged against the A480/SA-480 workmanship clause; for vessel internals the purchaser may add surface-roughness or cleanliness requirements.

Dimensions, tolerances and flatness

Thickness, width, length, flatness and camber tolerances follow SA-480/A480 tables for hot-rolled plate; ordered thickness is a minimum unless the order states nominal. For pressure parts, the thickness at any point must not fall below the ordered minimum, so heavy plate is often ordered with a small plus allowance. Flatness of thin plate cut from coil should be checked after cutting. Mill edge, sheared, plasma or waterjet-cut edges and bevelling for welding are available.

Code use of SA-240 plate. Before welding, the manufacturer must identify the P-Number and group number of S44100 from ASME Section IX (QW/QG-422) for the welding procedure qualification, and the designer takes allowable stresses from Section II Part D. Impact-test exemptions for austenitic and duplex plate are given in Section VIII Division 1 (UHA-51) and depend on grade, thickness and minimum design metal temperature, so cryogenic or low-temperature duty should be stated when you order. For heavy plate, ultrasonic examination to SA-578 and PMI of each plate are common supplementary requirements. Ask for the plate number to be hard-stamped or stencilled so traceability survives cutting.

UNS S44100 plate stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
6 1500 / 2000 6000 No.1 200+ t China
8 1500 / 2000 6000 No.1 200+ t China
10 2000 6000 No.1 100+ t China
12 2000 6000 No.1 100+ t China
16 2000 / 2500 6000 No.1 100+ t China
20 2000 / 2500 6000 / 8000 No.1 100+ t China
30 2000 / 2500 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Plate is bundled on steel or wooden skids with steel bands and edge protection, typically 3–8 t per bundle, and marked with heat and plate numbers. Cut pieces are crated. Heavy and wide plate ships in open-top or flat-rack containers or by break-bulk; we send loading photos with the shipping documents.

UNS S44100 equivalents in other standards

Standard Designation Comment
EN 1.4509 X2CrTiNb18 same alloy family and limits closely matched; compare each limit on the certificate
GB/T 022Cr18NbTi (S11973) same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Ferritic

Nickel-free, magnetic grades for heat and mild corrosion: SA-240 S43000, SA-240 S43932, SA-240 S44400, SA-240 S40920, 1.4512 plate, 1.4016 plate, 1.4510 plate, SA-240 S40910, SA-240 S40930, SA-240 S43940.

Austenitic

General-purpose austenitic grades for comparison: SA-240 S30400, SA-240 S30403.

Same grade, other specification

A240 S44100.

Applications, forming and welding of UNS S44100

Typical uses: automotive exhaust manifolds and hot-end parts, catalytic converter shells, heat exchangers, solid-oxide fuel-cell interconnects, kitchen equipment and appliance parts.

Ferritic sheet is formed cold; heavy gauges should be warmed to 100–200 °C before bending in cold weather. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a stabilised ferritic filler such as ER409Nb or ER430LNb, or an austenitic ER309L where weld ductility matters more than matching expansion. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Welding practice. Use low heat input and avoid preheat above about 200 °C to limit grain growth in the HAZ. Stabilised grades do not need post-weld heat treatment for corrosion resistance. Thin sheet is commonly joined by GTAW, plasma, laser or resistance welding. Cold forming should be done above room temperature for thicker gauges to avoid brittle fracture.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to ASME SA-480/SA-480M with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: intergranular corrosion testing (ASTM A763 or equivalent), bend test, hardness, and PMI. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying UNS S44100

  • Ordering heavy plate for welded pressure parts, where toughness is limited.
  • Assuming all ferritic grades are stabilised; check Ti and Nb on the certificate.
  • Using a ferritic grade in hot chloride solutions without checking pitting resistance.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing UNS S44100: buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Toughness of heavy gauges thickness range agreed; bend tests on the heat
Weld-zone grain growth low-heat-input welding advice and stabilised filler
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order UNS S44100 plate

State the standard and edition (ASME SA-240/SA-240M), the grade (UNS S44100), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

What is the difference between SA-240 and A240 for S44100?
The chemistry and tensile requirements are the same. SA-240 is the ASME Code edition, so plate for pressure vessels must be certified and marked SA-240; dual-certified A240/SA-240 plate covers both.
Is UNS S44100 equivalent to EN 1.4509 X2CrTiNb18?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
Is UNS S44100 magnetic?
Yes. Ferritic grades are magnetic in all conditions.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

UNS S44100 plate should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response