What is JIS G4312 SUH409L Heat Resistant Steel Plate?
Equivalent grades: SUH409L ≈ UNS S40920 (close) ≈ EN 1.4512 X2CrTi12 ≈ GB/T 022Cr11Ti (S11163).
SUH409L is a ferritic grade. SUH409L is the JIS low-carbon, titanium-stabilised 11Cr ferritic grade. It is the standard material for automotive exhaust systems in Japan and Asia because it combines heat and condensate corrosion resistance with low cost.
JIS G 4312 is the Japanese Industrial Standard for heat-resisting steel plate, sheet and strip. It includes the SUH heat-resisting grades and several SUS grades that are also used at temperature. Plate is hot rolled and supplied solution treated or annealed and pickled.
This page sets out the JIS G 4312 requirements for SUH409L plate: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.
SUH409L plate: specification summary
| Item | SUH409L data |
|---|---|
| Standard | JIS G 4312, heat-resisting steel plate, sheet and strip |
| Product forms | hot-rolled plate (No.1) and cold-rolled sheet and strip (2D, 2B) |
| Typical thickness | 3–50 mm hot rolled; 0.5–6 mm cold rolled |
| Widths | 1219, 1500, 2000 mm |
| Lengths | 2438, 3048, 6000 mm or cut to size |
| Heat treatment | solution treated (austenitic) or annealed (ferritic) |
| Tests | chemical analysis, tensile, hardness |
| Certificates | mill certificate; EN 10204 3.1 / 3.2 on request |
| Grade family | ferritic |
Size range. Plate is produced on Steckel or reversing mills from about 5 mm up to 80–100 mm depending on grade, with widths of 1500–2500 mm and lengths up to 12 m; thinner plate of 3–12 mm is often cut from hot-rolled coil. Very heavy or wide plates, and plates with tight flatness, should be confirmed before ordering. SUH409L is produced regularly by several mills; common sizes are held in stock, and other sizes are rolled in the mill’s scheduled campaigns for the grade.
Chemical composition of SUH409L (JIS G 4312)
| Element | wt % |
|---|---|
| C | 0.030 max |
| Si | 1.00 max |
| Mn | 1.00 max |
| P | 0.040 max |
| S | 0.030 max |
| Cr | 10.50–11.75 |
| Ti | Ti-stabilised, per JIS G 4312 |
Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.
Low carbon and nitrogen, together with titanium and/or niobium where specified, are what make modern ferritic grades weldable. Check that the stabiliser content on the certificate meets the formula in the standard for the actual C and N.
Mechanical properties of SUH409L plate
| 0.2 % proof stress min, N/mm² | Tensile strength min, N/mm² | Elongation min, % | Hardness max, HBW |
|---|---|---|---|
| 175 | 360 | 25 | 162 |
The minimum proof strength is 175 MPa. Ferritic grades have lower elongation than austenitic grades and work-harden less, which helps in stretch forming but limits deep drawing. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.
Corrosion resistance of SUH409L: PREN and limits
Ferritic stainless steels contain chromium but little or no nickel, so they are magnetic, cheaper and less sensitive to nickel price swings. They have good resistance to chloride stress-corrosion cracking, lower thermal expansion and higher thermal conductivity than austenitic grades, which helps in thermal cycling. Stabilisation with titanium and/or niobium ties up carbon and nitrogen and protects welds against intergranular corrosion.
The limits are toughness and formability in heavy sections: ferritic grades have a ductile-to-brittle transition, grain growth in the weld zone, and 475 °C embrittlement in the higher-chromium grades. They are therefore supplied mainly as sheet and light plate, and they are welded with low heat input.
How SUH409L compares with related grades
| Grade | Cr | Ni | Mo | N | PREN (min) | YS / Rp0.2 min, MPa |
|---|---|---|---|---|---|---|
| SUH409L | 10.50–11.75 | — | — | — | 10.5 | 175 |
| UNS S44100 | 17.5–19.5 | 1.00 max | — | 0.030 max | 17.5 | 241 |
| UNS S43940 | 17.5–18.5 | — | — | — | 17.5 | 250 |
| UNS S44600 | 23.0–27.0 | 0.75 max | — | 0.25 max | 23.0 | 275 |
| UNS S44100 | 17.5–19.5 | 1.00 max | — | 0.030 max | 17.5 | 241 |
Choose SUH409L when nickel-free cost, thermal-cycling behaviour or resistance to chloride stress-corrosion cracking matters more than toughness in heavy sections. It is not a good choice for heavy welded plate or for cryogenic service.
The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.
Heat treatment and delivery condition of SUH409L
Heat treatment: annealed 800–900 °C, air or slow cooling.
Ferritic grades are annealed and cooled rapidly or in air; they are not hardenable by quenching. Avoid long holding in the 400–550 °C range, which causes 475 °C embrittlement in higher-chromium grades.
Surface finishes for SUH409L plate
Hot-rolled plate to JIS G4312 is supplied with a No.1 finish; cold-rolled sheet as 2D or 2B. Heat-resistant parts are rarely polished, but bright annealed thin sheet is possible for some ferritic grades.
Dimensions, tolerances and flatness
Dimensional tolerances follow JIS G 4312, which refers to the same tolerance tables used for JIS G4304/G4305 stainless plate and sheet. State the tolerance class and flatness requirement on the order.
JIS ordering practice. A JIS G4312 order gives the grade symbol, the product type (hot-rolled or cold-rolled), the dimensions, the finish and the tolerance requirements. Mill inspection certificates to JIS G 0415 are normal; EN 10204 3.1 or 3.2 certificates can be issued for export. Since many furnace projects in Asia are designed to JIS, while plate is bought from Chinese mills, buyers often ask for dual certification to JIS G4312 and GB/T 4238 or ASTM A240 where the limits overlap.
SUH409L plate stock in China
| Thickness (mm) | Width (mm) | Length (mm) | Finish | Approx. quantity | Location |
|---|---|---|---|---|---|
| 6 | 1500 / 2000 | 6000 | No.1 | 200+ t | China |
| 8 | 1500 / 2000 | 6000 | No.1 | 200+ t | China |
| 10 | 2000 | 6000 | No.1 | 100+ t | China |
| 12 | 2000 | 6000 | No.1 | 100+ t | China |
| 16 | 2000 / 2500 | 6000 | No.1 | 100+ t | China |
| 20 | 2000 / 2500 | 6000 / 8000 | No.1 | 100+ t | China |
| 30 | 2000 / 2500 | 6000 | No.1 | 100+ t | China |
Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.
Packing and logistics. Plate is bundled on steel or wooden skids with steel bands and edge protection, typically 3–8 t per bundle, and marked with heat and plate numbers. Cut pieces are crated. Heavy and wide plate ships in open-top or flat-rack containers or by break-bulk; we send loading photos with the shipping documents.
SUH409L equivalents in other standards
| Standard | Designation | Comment |
|---|---|---|
| ASTM / UNS | UNS S40920 | close match; one or more limits (usually C, Si or N) differ |
| EN | 1.4512 X2CrTi12 | same alloy family and limits closely matched; compare each limit on the certificate |
| GB/T | 022Cr11Ti (S11163) | same alloy family and limits closely matched; compare each limit on the certificate |
Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.
Related grades by alloy family
Same standard
Other grades in this standard: SUS309S (G4304), SUS310S (G4304), SUS430 (G4304), SUS409L (G4305), SUH309, SUH310, SUH330.
Ferritic
Nickel-free, magnetic grades for heat and mild corrosion: A240 S43000, A240 S43932, A240 S44400, A240 S40920, A240 S40910.
Applications, forming and welding of SUH409L
Typical uses: automotive exhaust systems, mufflers and catalytic converter shells.
Ferritic sheet is formed cold; heavy gauges should be warmed to 100–200 °C before bending in cold weather. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a stabilised ferritic filler such as ER409Nb or ER430LNb, or an austenitic ER309L where weld ductility matters more than matching expansion. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.
Welding practice. Use low heat input and avoid preheat above about 200 °C to limit grain growth in the HAZ. Stabilised grades do not need post-weld heat treatment for corrosion resistance. Thin sheet is commonly joined by GTAW, plasma, laser or resistance welding. Cold forming should be done above room temperature for thicker gauges to avoid brittle fracture.
Certificates, testing and receiving inspection
Every delivery carries a mill certificate to JIS G4312 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: intergranular corrosion testing (ASTM A763 or equivalent), bend test, hardness, and PMI. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.
On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.
Common mistakes when specifying SUH409L
- Ordering heavy plate for welded pressure parts, where toughness is limited.
- Assuming all ferritic grades are stabilised; check Ti and Nb on the certificate.
- Using a ferritic grade in hot chloride solutions without checking pitting resistance.
Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.
Sourcing SUH409L: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Toughness of heavy gauges | thickness range agreed; bend tests on the heat |
| Weld-zone grain growth | low-heat-input welding advice and stabilised filler |
| Small quantities across many sizes | mixed thicknesses and grades combined in one shipment |
| Cutting and edge preparation | in-house shearing, plasma, laser and waterjet cutting, bevelling |
| Delivery delays | weekly production and shipping updates with photos |
How to order SUH409L plate
State the standard and edition (JIS G 4312), the grade (SUH409L), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.
FAQ
-
Is SUH409L the same as SUS309S/SUS310S?
- No. The SUH grades in JIS G4312 are heat-resisting grades, typically with higher carbon for strength at temperature; the SUS grades are corrosion-resistant grades with lower carbon. Choose by service temperature and welding needs.
-
Is SUH409L equivalent to UNS S40920?
- They are close; one or more limits differ, so check the certificate against both standards or order dual certification.
-
Is SUH409L magnetic?
- Yes. Ferritic grades are magnetic in all conditions.
-
Can I order small quantities or cut sizes?
- Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
-
Which certificates and tests can you provide?
- Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.
Conclusion
SUH409L plate should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.