JIS G4312 SUH309 Heat Resistant Steel Plate at SHH STEEL warehouse

JIS G4312 SUH309 Heat Resistant Steel Plate

JIS G4312 SUH309 Heat Resistant Steel Plate: heat-resistant grade to JIS G 4312, hot-rolled plate from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
JIS G4312 SUH309 plate, SUH309 plate, SUH309 stainless plate supplier, JIS G 4312 SUH309, SUH309 plate stock China
Equivalent Grades:
UNS S30900; EN 1.4828 X15CrNiSi20-12 (nearest); GB/T 16Cr23Ni13 (S30920)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is JIS G4312 SUH309 Heat Resistant Steel Plate?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: SUH309 ≈ UNS S30900 ≈ EN 1.4828 X15CrNiSi20-12 (nearest) ≈ GB/T 16Cr23Ni13 (S30920).

SUH309 is a heat-resistant grade. SUH309 is the JIS heat-resisting 23Cr-13Ni grade with up to 0.20 % carbon. It is the high-carbon counterpart of SUS309S and is chosen for strength at temperature rather than for welded wet-corrosion service.

JIS G 4312 is the Japanese Industrial Standard for heat-resisting steel plate, sheet and strip. It includes the SUH heat-resisting grades and several SUS grades that are also used at temperature. Plate is hot rolled and supplied solution treated or annealed and pickled.

This page sets out the JIS G 4312 requirements for SUH309 plate: specification summary, chemistry, mechanical properties, high-temperature behaviour, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

SUH309 plate: specification summary

Item SUH309 data
Standard JIS G 4312, heat-resisting steel plate, sheet and strip
Product forms hot-rolled plate (No.1) and cold-rolled sheet and strip (2D, 2B)
Typical thickness 3–50 mm hot rolled; 0.5–6 mm cold rolled
Widths 1219, 1500, 2000 mm
Lengths 2438, 3048, 6000 mm or cut to size
Heat treatment solution treated (austenitic) or annealed (ferritic)
Tests chemical analysis, tensile, hardness
Certificates mill certificate; EN 10204 3.1 / 3.2 on request
Grade family heat-resistant

Size range. Plate is produced on Steckel or reversing mills from about 5 mm up to 80–100 mm depending on grade, with widths of 1500–2500 mm and lengths up to 12 m; thinner plate of 3–12 mm is often cut from hot-rolled coil. Very heavy or wide plates, and plates with tight flatness, should be confirmed before ordering. SUH309 is a specialty grade made by a limited number of mills in campaign rolling. Stock covers the common sizes listed below; for project quantities or unusual sizes, plan for a mill campaign and reserve the heat early.

Chemical composition of SUH309 (JIS G 4312)

Element wt %
C 0.20 max
Si 1.00 max
Mn 2.00 max
P 0.040 max
S 0.030 max
Cr 22.00–24.00
Ni 12.00–15.00

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

For heat-resistant grades the key elements are chromium (oxide scale), nickel (austenite stability, carburisation resistance) and silicon, aluminium or rare earths where present (scale adhesion). Sulfur and phosphorus are kept low to protect hot ductility and weldability.

Mechanical properties of SUH309 plate

0.2 % proof stress min, N/mm² Tensile strength min, N/mm² Elongation min, % Hardness max, HBW
205 560 40 201

The minimum proof strength is 205 MPa. For high-temperature design, room-temperature values are only an acceptance check; use creep and stress-rupture data from the standard’s informative annexes or the ASME allowable stresses where Code rules apply. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.

High-temperature behaviour of SUH309

This is a heat-resistant grade: it is selected for oxidation resistance, strength and structural stability at high temperature rather than for wet corrosion. Chromium forms the protective oxide, nickel stabilises the austenite against thermal cycling and carburisation, and silicon, rare earths or nitrogen, where present, improve scale adhesion or creep strength. The maximum useful temperature in air depends on atmosphere, thermal cycling and load, so published scaling temperatures are a guide, not a design value.

Sulfur-bearing gases attack high-nickel alloys, while carburising or nitriding atmospheres favour higher nickel; vanadium-bearing ash and molten salts need special evaluation. Long exposure in the 600–900 °C range can form sigma phase in high-chromium grades and reduce room-temperature toughness, which matters for parts that are cleaned or repaired cold. Creep-rupture values are given in the standard’s informative annexes or by the mill and should be used for design instead of room-temperature strength.

How SUH309 compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
SUH309 22.00–24.00 12.00–15.00 — — — 205
UNS S30815 20.0–22.0 10.0–12.0 — 0.14–0.20 — 310
UNS S30900 22.0–24.0 12.0–15.0 — — — 205
UNS S31000 24.0–26.0 19.0–22.0 — — — 205
UNS N08330 17.0–20.0 34.0–37.0 — — — 205

Choose SUH309 when oxidation resistance and strength at temperature drive the selection. For wet corrosion at room temperature, a low-carbon corrosion-resistant grade is usually a better choice, and in sulfur-rich gases a lower-nickel grade may outperform a high-nickel one.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of SUH309

Heat treatment: 1030–1150 °C, rapid cooling.

Heat-resistant plate is supplied solution annealed. For high-temperature service, a coarser grain size improves creep strength, while a finer grain improves fatigue and room-temperature ductility; where it matters, state the grain-size requirement on the order. Stress relief is not normally needed.

Surface finishes for SUH309 plate

Hot-rolled plate to JIS G4312 is supplied with a No.1 finish; cold-rolled sheet as 2D or 2B. Heat-resistant parts are rarely polished, but bright annealed thin sheet is possible for some ferritic grades.

Dimensions, tolerances and flatness

Dimensional tolerances follow JIS G 4312, which refers to the same tolerance tables used for JIS G4304/G4305 stainless plate and sheet. State the tolerance class and flatness requirement on the order.

JIS ordering practice. A JIS G4312 order gives the grade symbol, the product type (hot-rolled or cold-rolled), the dimensions, the finish and the tolerance requirements. Mill inspection certificates to JIS G 0415 are normal; EN 10204 3.1 or 3.2 certificates can be issued for export. Since many furnace projects in Asia are designed to JIS, while plate is bought from Chinese mills, buyers often ask for dual certification to JIS G4312 and GB/T 4238 or ASTM A240 where the limits overlap.

SUH309 plate stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
6 1500 / 2000 6000 No.1 100+ t China
8 1500 / 2000 6000 No.1 100+ t China
10 2000 6000 No.1 100+ t China
12 2000 6000 No.1 100+ t China
16 2000 / 2500 6000 No.1 100+ t China
20 2000 / 2500 6000 / 8000 No.1 100+ t China
30 2000 / 2500 6000 No.1 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Plate is bundled on steel or wooden skids with steel bands and edge protection, typically 3–8 t per bundle, and marked with heat and plate numbers. Cut pieces are crated. Heavy and wide plate ships in open-top or flat-rack containers or by break-bulk; we send loading photos with the shipping documents.

SUH309 equivalents in other standards

Standard Designation Comment
ASTM / UNS UNS S30900 same alloy family and limits closely matched; compare each limit on the certificate
EN 1.4828 X15CrNiSi20-12 nearest grade only; limits differ, check before substituting
GB/T 16Cr23Ni13 (S30920) same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Same standard

Other grades in this standard: SUS309S (G4304), SUS310S (G4304), SUS430 (G4304), SUS409L (G4305), SUH310, SUH330, SUH409L.

Heat-resistant

Heat-resistant grades ranked by chromium, nickel and silicon: A240 S30908, A240 S31008, A240 S30909, A240 S31009, 1.4948 (EN 10028-7).

Applications, forming and welding of SUH309

Typical uses: furnace parts, heat-treatment fixtures, burner parts and kiln components.

Heat-resistant plate is usually cut by plasma or waterjet, formed hot or cold, and welded with matching heat-resistant consumables. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a matching heat-resistant filler such as ER309, ER310 or ERNiCr-3 according to the service temperature. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Fabrication at temperature. Design furnace parts to allow for thermal expansion, which is about 1.5 times that of carbon steel, and avoid sharp corners where scale can spall. Welds should be full penetration where they carry load at temperature. For high-silicon grades, use low heat input to limit hot cracking. After long service, high-chromium plate may be embrittled by sigma phase, so repair welding of old parts needs care and sometimes a solution anneal first.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to JIS G4312 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: PMI, grain-size measurement (ASTM E112) where the grade requires it, elevated-temperature tensile tests by agreement, and ultrasonic testing of heavy plate. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying SUH309

  • Selecting by room-temperature strength instead of creep data.
  • Substituting a low-carbon corrosion grade (for example 310S for 310) without checking creep strength.
  • Ignoring the atmosphere: sulfur, carburising gas and vanadium ash change the ranking of grades.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing SUH309: buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Wrong grade substitution (for example 304 for 309/310) PMI of every plate before dispatch
Distortion of large furnace panels levelled plate and cut-to-size blanks with low-stress cutting
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order SUH309 plate

State the standard and edition (JIS G 4312), the grade (SUH309), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

Is SUH309 the same as SUS309S/SUS310S?
No. The SUH grades in JIS G4312 are heat-resisting grades, typically with higher carbon for strength at temperature; the SUS grades are corrosion-resistant grades with lower carbon. Choose by service temperature and welding needs.
Is SUH309 equivalent to UNS S30900?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
What is the maximum service temperature of SUH309?
It depends on the atmosphere, thermal cycling and load. Published scaling temperatures are a guide for oxidation in air only; for load-bearing parts use creep-rupture data.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

SUH309 plate should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X